The macroscopic properties of the superconducting phase in the multiphase compound YPd5B3 C.3 have been investigated. The onset of superconductivity was observed at 22.6 K, zero resistance at 21.2 K, the lower critical field Hel at 5 K was determined to be Hel (5) rv 310 Gauss and the compound was found to be an extreme type-II superconductor with the upper critical field in excess of 55000 Gauss at 15 K. From the upper and lower critical field values obtained, several important parameters of the superconducting state were determined at T = 15 K. The Ginzburg-Landau paramater was determined to be ~ > 9 corresponding to a coherence length ~ rv 80A and magnetic penetration depth of 800A. In addition measurements of the superconducting transition temperature Te(P) under purely hydrostatically applied pressure have been carried out. Te(P) of YPd5B3 C.3 decreases linearly with dTe/dP rv -8.814 X 10-5 J

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The Bi2Sr2CaCu20g single crystal with a superconducting transition temperature equal to 90 ± 2 K was prepared. The irreversibility line of the single crystal for a mgnetic field direction along the c-axis and T* in the ab-plane was determined. The reduced temperature (l - T ) is proportional to H 1.1 for fields below 004 T and proportional to HO.09 for fields above 0.4 T. The zero temperature upper critical field Hc2(0) and coherence length ~ (0) were determined from the magnetization meaurements to be H-lC2=35.9T , H//C2=31.2T, ~c(0)=35.0 A, and ~ab(0)=32.5A,and from the magnetoresistance measurements to be H-lc2 = 134.6T , H//C2=55.5T '~c(0)=38.1 A, and ~ab(0)=2404 A for both directions of the applied magnetic field. The results obtained for Hc2(0) and ~(O) are not reliable due to the rounding that the single crystal exhibits in the magnetization and magnetoresistance curves. The magnetization relaxation of the single crystal was investigated, and was found to be logarithmic in time, and the relaxation rate increases with temperature up to 50 -60 K, then decreases at higher temperatures.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The superconducting transition temperature Tc of metallic glasses ZrxFelOO-x (x=80, 75), Zr75(NixFelOO-x)25 (x=75, 50, 25), and CU2SZr75 were measured under quasi-hydrostatic pressure up to 8 OPa (80kbar). The volume (pressure) dependence of the electron-phonon coupling parameters Aep for CU25Zr75 was calculated using the McMillan equatio11. Using this volume dependence of Aep and the modified McMillan equation which incorporates spin-fluctuations, the volume dependence of the spin fluctuation parameter, Asf, was determined in Zr75Ni25, ZrxFelOO-x , a11d Zr75(NixFelOO-x)25. It was found that with increasing pressure, spinfluctuations are suppressed at a faster rate in ZrxFe lOO-x and Zr75(NixFelOO-x)25, as Fe concentration is increased. The rate of suppression of spin-fluctuations with pressure was also found to be higher in Fe-Zr glasses than in Ni-Zr glasses of similar composition.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

SrMg^Rui-iOa thin films were made by using pulsed laser deposition on SrTiOa (100) substrates in either O2 or Ar atmosphere. The thin films were characterized by x-ray diffraction, energy dispersive x-ray microanalysis, dc resistivity measurement, and dc magnetization measurement. The effect of Mg doping was observed. As soon as the amount of Mg increased in SrMg-cRui-iOa thin films, the magnetization decreased, and the resistivity increased. It had little effect on the Curie temperature (transition temperature). The magnetization states of SrMgiRui-iOa thin films, for x < 0.15, are similar to SrRuOs films. X-ray diffraction results for SrMga-Rui-iOa thin films made in oxygen showed that the films are epitaxial. The thin films could not be well made in Ar atmosphere during laser ablation as there was no clear peak of SrMg^Rui-iOa in x-ray diffraction results. Substrate temperatures had an effect on the resistivity of the films. The residual resistivity ratios were increased by increasing substrate temperature. It was observed that the thickness of thin films are another factor for film quality: Thin films were epitaxial, but thicker films were not epitaxial.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We prepared samples of MgB2 and ran sets of experiments aimed for investigation of superconducting properties under pressure. We found the value of pressure derivative of the transition temperature -1.2 ± 0.05 K/GPa. Then, using McMillan formula, we found that the main contribution to the change of the transition temperature under the pressure is due to the change in phonon frequencies. Griineisen parameter was calculated to be 7g = 2.4. Our results suggest that MgB2 is a conventional superconductor.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The optical response to far infrared radiation has been measured on a mosaic of heavy fermion CeCoIns single crystals. The superconducting transition temperature of the crystals has been determined by van der Pauw resistivity and ac-susceptibility measurements as Tc = 2.3 K. The optical measurements were taken above and below the transition temperature using a ^He cryostat and step and integrate Martin-Puplett type polarizing interferometer. The absolute reflectance of the heavy fermion CeCoIns in the superconducting state in range (0, 100)cm~^ was calculated from the measured thermal reflectance, using the normal state data of Singley et al and a low frequency extrapolation for a metallic material in the Hagen-Rubens regime. By means of Kramers-Kronig analysis the absolute reflectance was used to calculate the optical conductivity of the sample. The real part of the calculated complex conductivity a{u)) of CeCoIns indicates a possible opening of an energy gap close to 50 cm~^.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pressure variations of the superconducting transition temperature Ic of a series of amorphous NixZr 1 OO-x alloys have been studied under quasmydrostatic pressures upto 8 G Pa. For amorphous samples having Ni-concentration less than 40%, i)Tc/dP is positive in sign and it decreases non linearly with increase in I. whereasdTcldP is negative in sign for Ni concentration of 45%. Comparison with the Hall coefficient (I) and the thermoelectric power (2) results for the same amorphous alloys leads to the conclusion that s-d hybridization nature of the d-band (Nil plays a central role in the sign reversal behaviour. Application of pressures greater than 2 G Pa to Ni20ZrgO led to the formation of a new phase, w-Zr. which retains its form after the pressure is released.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Reflectance measurements along the c-axis of La1.875 Bao.125CU04 at temperatures above(6K) and below(O.5K) the bulk superconducting transition temperature(3K) were performed using a Bruker rapid scan spectrometer and a Martin-Puplett polarizing spectrometer. It was found that when polarized light reflected from a sample the Bruker rapid scan spectrometer has a low frequency cutoff of lOcm-1 while the Martin-Puplett polarizing spectrometer has a low frequency cutoff of 6cm-1 A superconducting pla ma edge was absent in all measurements taken. It was concluded that if a superconducting plasma edge exists in La1.875Bao.125CU04 it is below 6cm-1.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Lead chromium oxide is a photoconductive dielectric material tha t has great potential of being used as a room temperature photodetector. In this research, we made ceramic pellets of this compound as well as potassium doped compound Pb2-xKxCr05, where x=O, 0.05, 0.125. We also investigate the properties of the lanthanum doped sample whose chemical formula is Pb1.85Lao.15Cr05' The electronic, magnetic and thermal properties of these materials have been studied. Magnetization measurements of the Pb2Cr05 sample indicate a transition at about 310 K, while for the lanthanum doped sample the transition temperature is at about 295 K indicating a paramagnetic behavior. However, the potassium doped samples are showing the transition from paramagnetic state to diamagnetic state at different temperatures for different amounts of potassium atoms present in the sample. We have studied resistivity as a function of temperature in different gas environments from 300 K to 900 K. The resistivity measurement of the parent sample indicates a conducting to insulating transition at about 300 K and upon increasing the temperature further, above 450 K the sample becomes an ionic conductor. As temperature increases a decrease in resistance is observed in the lanthanum/potassium doped samples. Using Differential Scanning Calorimetry experiment an endothermic peak is observed for the Pb2Cr05 and lanthanum/potassium doped samples at about 285 K.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Chlorhexidine is an effective antiseptic used widely in disinfecting products (hand soap), oral products (mouthwash), and is known to have potential applications in the textile industry. Chlorhexidine has been studied extensively through a biological and biochemical lens, showing evidence that it attacks the semipermeable membrane in bacterial cells. Although extremely lethal to bacterial cells, the present understanding of the exact mode of action of chlorhexidine is incomplete. A biophysical approach has been taken to investigate the potential location of chlorhexidine in the lipid bilayer. Deuterium nuclear magnetic resonance was used to characterize the molecular arrangement of mixed phospholipid/drug formulations. Powder spectra were analyzed using the de-Pake-ing technique, a method capable of extracting both the orientation distribution and the anisotropy distribution functions simultaneously. The results from samples of protonated phospholipids mixed with deuterium-labelled chlorhexidine are compared to those from samples of deuterated phospholipids and protonated chlorhexidine to determine its location in the lipid bilayer. A series of neutron scattering experiments were also conducted to study the biophysical interaction of chlorhexidine with a model phospholipid membrane of DMPC, a common saturated lipid found in bacterial cell membranes. The results found the hexamethylene linker to be located at the depth of the glycerol/phosphate region of the lipid bilayer. As drug concentration was increased in samples, a dramatic decrease in bilayer thickness was observed. Differential scanning calorimetry experiments have revealed a depression of the DMPC bilayer gel-to-lamellar phase transition temperature with an increasing drug concentration. The enthalpy of the transition remained the same for all drug concentrations, indicating a strictly drug/headgroup interaction, thus supporting the proposed location of chlorhexidine. In combination, these results lead to the hypothesis that the drug is folded approximately in half on its hexamethylene linker, with the hydrophobic linker at the depth of the glycerol/phosphate region of the lipid bilayer and the hydrophilic chlorophenyl groups located at the lipid headgroup. This arrangement seems to suggest that the drug molecule acts as a wedge to disrupt the bilayer. In vivo, this should make the cell membrane leaky, which is in agreement with a wide range of bacteriological observations.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fermi patches in quasi-two dimensional charge density waves (CDW) have not described the connection to superconductivity (SC) according to theory adequately at this point in time. The connection between CDW and SC in the quasi-two dimensional material CuxTiSe2 is an interesting one which might reveal mechanisms in unconventional superconductors. A previous Brock graduate student grew crystals of CuxTiSe2. The precise doping of the samples was not known. In order to determine the doping parameter x in CuxTiSe2, a sensitive resistivity measurement system was necessary. A new resistivity measurement system was designed and implemented utilizing an Infrared Labs HDL-10 He3 cryostat. By comparing with data from the literature, doping of two samples was investigated using the new measurement system and a Quantum Design Magnetic Property Measurement System (MPMS). Methods for determining the doping revealed that the old resistivity system would not be able to determine the CDW transition temperature of highly doped samples or doping for elongated samples due to electronic noise. Doping in one sample was found to be between x=0.06 and x=0.065. Values of doping in the second sample had a discrepancy but could be explained by incorrect sample orientation.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Durant les dernières décennies, la technique Langmuir-Blodgett (LB) s’est beaucoup développée dans l’approche « bottom-up » pour la création de couches ultra minces nanostructurées. Des patrons constitués de stries parallèles d’environ 100 à 200 nm de largeur ont été générés avec la technique de déposition LB de monocouches mixtes de 1,2-dilauroyl-sn-glycéro-3-phosphatidylcholine (DLPC) et de 1,2-dipalmitoyl-sn-glycéro-3-phosphatidylcholine (DPPC) sur des substrats de silicium et de mica. Afin d’amplifier la fonctionnalité de ces patrons, la 1-palmitoyl-2-(16-(S-methyldithio)hexadécanoyl)-sn-glycéro-3-phosphatidylcholine (DSDPPC) et la 1-lauroyl-2-(12-(S-methyldithio)dodédecanoyl)-sn-glycéro-3-phosphatidylcholine (DSDLPC) ont été employées pour la préparation de monocouches chimiquement hétérogènes. Ces analogues de phospholipide possèdent un groupement fonctionnel méthyldisulfide qui est attaché à la fin de l’une des chaînes alkyles. Une étude exhaustive sur la structure de la phase des monocouches Langmuir, Langmuir-Schaefer (LS) et LB de la DSDPPC et de la DSDLPC et leurs différents mélanges avec la DPPC ou la DLPC est présentée dans cette thèse. Tout d’abord, un contrôle limité de la périodicité et de la taille des motifs des stries parallèles de DPPC/DLPC a été obtenu en variant la composition lipidique, la pression de surface et la vitesse de déposition. Dans un mélange binaire de fraction molaire plus grande de lipide condensé que de lipide étendu, une vitesse de déposition plus lente et une plus basse pression de surface ont généré des stries plus continues et larges. L’addition d’un tensioactif, le cholestérol, au mélange binaire équimolaire de la DPPC/DLPC a permis la formation de stries parallèles à de plus hautes pressions de surface. La caractérisation des propriétés physiques des analogues de phospholipides a été nécessaire. La température de transition de phase de la DSDPPC de 44.5 ± 1.5 °C comparativement à 41.5 ± 0.3 °C pour la DPPC. L’isotherme de la DSDPPC est semblable à celui de la DPPC. La monocouche subit une transition de phase liquide-étendue-à-condensée (LE-C) à une pression de surface légèrement supérieure à celle de la DPPC (6 mN m-1 vs. 4 mN m-1) Tout comme la DLPC, la DSDLPC demeure dans la phase LE jusqu’à la rupture de la monocouche. Ces analogues de phospholipide existent dans un état plus étendu tout au long de la compression de la monocouche et montrent des pressions de surface de rupture plus basses que les phospholipides non-modifiés. La morphologie des domaines de monocouches Langmuir de la DPPC et de la DSDPPC à l’interface eau/air a été comparée par la microscopie à angle de Brewster (BAM). La DPPC forme une monocouche homogène à une pression de surface (π) > 10 mN/m, alors que des domaines en forme de fleurs sont formés dans la monocouche de DSDPPC jusqu’à une π ~ 30 mN m-1. La caractérisation de monocouches sur substrat solide a permis de démontrer que le patron de stries parallèles préalablement obtenu avec la DPPC/DLPC était reproduit en utilisant des mélanges de la DSDPPC/DLPC ou de la DPPC/DSDLPC donnant ainsi lieu à des patrons chimiquement hétérogènes. En général, pour obtenir le même état de phase que la DPPC, la monocouche de DSDPPC doit être comprimée à de plus hautes pressions de surface. Le groupement disulfide de ces analogues de phospholipide a été exploité, afin de (i) former des monocouches auto-assemblées sur l’or et de (ii) démontrer la métallisation sélective des terminaisons fonctionnalisées des stries. La spectrométrie de photoélectrons induits par rayons X (XPS) a confirmé que la monocouche modifiée réagit avec la vapeur d’or pour former des thiolates d’or. L’adsorption de l’Au, de l’Ag et du Cu thermiquement évaporé démontre une adsorption préférentielle de la vapeur de métal sur la phase fonctionnalisée de disulfide seulement à des recouvrements sub-monocouche.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

L'aimant organique NIT-2Py a été caractérisé expérimentalement et ses propriétés ont été simulées numériquement à partir de la théorie de la fonctionnelle de la densité. Le magnétisme dans ce matériau provient de la présence d'un électron non apparié sur chaque molécule qui a ainsi un moment magnétique non nul. Ceci a été confirmé par des simulations sur une molécule isolée. Les molécules de NIT-2Py cristallisent dans le groupe d'espace P21/c avec huit molécules par maille élémentaire pour former la structure cristalline Alpha étudiée dans ce document. Le moment effectif de la susceptibilité et l'entropie magnétique totale montre que ce matériau est un système de spins 1/2 avec un spin par molécule. Les mesures de chaleur spécifique ont mis en évidence la présence de deux phases magnétiques ordonnées à basse température qui sont séparées par un plateau en aimantation. Une première phase est observée à des champs magnétiques inférieurs à 2.2 T et a une température de transition de 1.32 K en champ nul. Les mesures de susceptibilité magnétique et d'aimantation ont permis d'établir que cette phase ordonnée est antiferromagnétique. Ceci est confirmé par les simulations numériques. La deuxième phase est induite par le champ magnétique avec une température de transition de 0.53 K à 6 T. L'information disponible sur cette phase est limitée et l'étude du système à l'extérieur des phases ordonnées en donne une meilleure compréhension. Un modèle de spins S=1/2 isolés et de dimères S=0 isolés reproduit bien les mesures d'aimantation et de chaleur spécifique au-dessus de 3 K. L'application d'un champ magnétique réduit l'écart d'énergie entre le singulet et le triplet du dimère jusqu'au croisement qui se produit à 6 T. La phase induite émerge précisément à ce croisement et on spécule l'existence d'un condensat de Bose-Einstein des états triplets.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The Schiff base, 3-hydroxyquinoxaline-2-carboxalidine-4-aminoantipyrine, was synthesized by the condensation of 3-hydroxyquinoxaline-2-carboxaldehyde with 4-aminoantipyrine. HPLC, FT-IR and NMR spectral data revealed that the compound exists predominantly in the amide tautomeric form and exhibits both absorption and fluorescence solvatochromism, large stokes shift, two electron quasireversible redox behaviour and good thermal stability, with a glass transition temperature of 104oC. The third-order non-linear optical character was studied using open aperture Z-scan methodology employing 7 ns pulses at 532 nm. The third-order non-linear absorption coefficient, b, was 1.48 x 10-6 cm W-1 and the imaginary part of the third-order non-linear optical susceptibility, Im c(3), was 3.36 x10-10 esu. The optical limiting threshold for the compound was found to be 340 MW cm-2.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The Schiff base, 3-hydroxyquinoxaline-2-carboxalidine-4-aminoantipyrine, was synthesized by the condensation of 3-hydroxyquinoxaline-2-carboxaldehyde with 4-aminoantipyrine. HPLC, FT-IR and NMR spectral data revealed that the compound exists predominantly in the amide tautomeric form and exhibits both absorption and fluorescence solvatochromism, large stokes shift, two electron quasireversible redox behaviour and good thermal stability, with a glass transition temperature of 104 oC. The third-order non-linear optical character was studied using open aperture Z-scan methodology employing 7 ns pulses at 532 nm. The third-order non-linear absorption coefficient, b, was 1.48 x 10-6 cm W-1 and the imaginary part of the third-order non-linear optical susceptibility, Im c(3), was 3.36x10-10 esu. The optical limiting threshold for the compound was found to be 340 MW cm-2.