We report an easy synthesis of highly branched gold particles through a seed-mediated growth approach in the presence of citrate. The addition of citrate in the growth solution is found to be crucial for the formation of these branched gold particles. Their size can be varied from 47 to 185 nm. The length of the thumb-like branch is estimated to be between about 5 and 20 nm, and changes slightly as the particle size increases. Owing to these obtuse and short branches, their surface plasmon resonance displays a marked red-shift with respect to the normal spherical particles. These branched gold particles exhibit stronger SERS activity than the non-branched ones, which is most likely related to these unique branching features.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Flow-mode static and dynamic laser light scattering (SLS/DLS) studies of polymers, including polystyrene, polyethylene, polypropylene and poly(dimethylsiloxane) (PDMS), in 1,2,4-trichlorobenzene (TCB) at 150 degreesC were performed on a high temperature gel permeation chromatography (GPC) coupled with a SLS/DLS detector. Both absolute molecular weight (M) and molecular sizes (radius of gyration, R-g and hydrodynamic radius, R-h) of polymers eluting from the GPC columns were obtained simultaneously. The conformation of different polymers in TCB at 150 degreesC were discussed according to the scaling relationships between R-g, R-h and M and the rho-ratio (p = R-g/R-h). Flow-mode DLS results of PDMS were verified by batch-mode DLS study of the same sample. The presented technique was proved to be a convenient and quick method to study the shape and conformation of polymers in solution at high temperature. However, the flow-mode DLS was only applicable for high molecular weight polymers with a higher refractive index increment such as PDMS.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thickness of the gold film and its morphology, including the surface roughness, are very important for getting a good, reproducible response in the SPR technique. Here, we report a novel alternative approach for preparing SPR-active substrates that is completely solution-based. Our strategy is based on self-assembly of the gold colloid monolayer on a (3-aminopropyl)trimethoxysilane-modified glass slide, followed by electroless gold plating. Using this method, the thickness of films can be easily controlled at the nanometer scale by setting the plating time in the same conditions. Surface roughness and morphology of gold films can be modified by both tuning the size of gold nanoparticles and agitation during the plating. Surface evolution of the Au film was followed in real time by UV-vis spectroscopy and in situ SPRS. To assess the surface roughness and electrochemical stability of the Au films, atomic force microscopy and cyclic voltammetry were used. In addition, the stability of the gold adhesion is demonstrated by three methods. The as-prepared Au films on substrates are reproducible and stable, which allows them to be used as electrodes for electrochemical experiments and as platforms for studying SAMs.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By fitting the spinodals of poly(vinyl methyl ether)/deuterated polystyrene (PVME/PSD) systems, the adjustable parameters epsilon (12)* and delta epsilon* in the Sanchez-Balasz lattice fluid (SBLF) theory could be determined for different molecular weights. According to these parameters, Flory-Huggins and scattering interaction parameters were calculated for PVME/PSD with different molecular weights by means of the SELF theory. From our calculation, Flory-Huggins and scattering interaction parameters are both Linearly dependent on the reciprocal of the temperature, and almost linearly on the concentration of PSD. Compared with the scattering interaction parameters, the Flory-Huggins interaction parameters decreased more slowly with an increase in the concentration for all three series of blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A successful micronization of water-insoluble poly(epsilon-caprolactone) (PCL) into narrowly distributed nanoparticles stable in water has not only enabled us to study the enzymatic biodegradation of PCL in water at 25 degrees C by a combination of static and dynamic laser light scattering (LLS), but also to shorten the biodegradation time by a factor of more than 10(3) compared with using a thin PCL film, i.e. a 1 week conventional experiment becomes a 4 min one. The time-average scattering intensity decreased linearly. It was interesting to find that the decrease of the scattering intensity was not accompanied by a decrease of the average size of the PCL nanoparticles, indicating that the enzyme, Lipase Pseudomonas (PS), ''eats'' the PCL nanoparticles one-by-one, so that the biodegradation rate is determined mainly by the: enzyme concentration. Moreover, we found that using anionic sodium lauryl sulphate instead of cationic hexadecyltrimethylammonium bromide as surfactant in the micronization can prevent the biodegradation, suggesting that the biodegradation involves two essential steps: the adsorption of slightly negatively charged Lipase PS onto the PCL nanoparticles and the interaction between Lipase PS and PCL. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The interface thickness in two-component interpenetrating polymer networks (IPN) system based on polyacrylate and epoxy were determined using small-angle X-ray scattering (SAXS) in terms of the theory proposed by Ruland. The thickness was found to be nonexistent for the samples at various compositions and synthesized at variable conditions-temperature and initiator concentration. By viewing the system as a two-phase system with a sharp boundary, the roughness of the interface was described by fractal dimension, D, which slightly varies with composition and synthesis condition. Length scales in which surface fractals are proved to be correct exist for each sample and range from 0.02 to 0.4 Angstrom(-1). The interface in the present IPN system was treated as fractal, which reasonably explained the differences between Pored's law and experimental data, and gained an insight into the interaction between different segments on the interface. (C) 1997 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two unfractionated samples of phenolphthalein poly( aryl ether sulfone) (PES-C) were characterized in CHCl3 at 25 degrees C by applying a recently developed laser light-scattering (LLS) procedure. The Laplace inversion of precisely measured intensity-intensity time correlation function lead us first to an estimate of the characteristic line-width distribution G(Gamma) and then to the translational diffusion coefficient distribution G(D). A combination of static and dynamic LLS results enabled us to determine D = (2.69 x 10(-4))M(-0.553), which agrees with the calibration of D = (2.45 x 10(-4))M(-0.55) previously established by a set of narrowly distributed PES-C samples. Using this newly obtained scaling between D and M, we were able to convert G(D) into a differential weight distribution f(w)(M) for the two PES-C samples. The weight-average molecular weights calculated from f(w)(M) are comparable to that obtained directly from static LLS. Our results showed that using two broadly distributed samples instead of a set of narrowly distributed samples have provided not only similar final results, but also a more practical method for the PES-C characterization. (C) 1997 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two soluble high-performance polyimides, poly(BCPOBDA/DMMDA) and poly(ODPA/DMMDA), in CHCl3 at 25 degrees C have been studied using laser light scattering. We found that the z-average radius of gyration ([R(g)]) can be scaled to the weight-average molecular weight (M(w)) as [R(g)] (nm) = 4.95 x 10(-2)M(w)(0.52) and [R(g)] (nm) = 1.25 x 10(-2)M(w)(0.66) respectively for poly(BCPOBDA/DMMDA) and poly(ODPA/DMMDA), indicating that poly(ODPA/DMMDA) in CHCl3 at 25 degrees C has a more extended chain conformation than poly(BCPOBDA/DMMDA). Using the wormlike chain model approach, we found that the Flory characteristic ratios (C*) of poly(BCPOBDA/DMMDA) and poly(ODPA/DMMDA) are similar to 20 and similar to 31, respectively, indicating that both of them have a slightly extended chain conformation in comparison with typical flexible polymer chains, such as polystyrene, whose C-infinity is similar to 10. A combination of the weight-average molar mass (M(w)) with the translational diffusion coefficient distributions (G(D)) has led to D (cm(2)/s) = 3.53 x 10(-4)M(-0.579) and D (cm(2)/s) = 4.30 x 10(-4)M(-0.613) respectively for two soluble high-performance polyimides, poly(BCPOBDA/DMMDA) and poly(ODPA/DMMTA), in CHCl3 at 25 degrees C. Using these two calibrations, we have successfully characterized the molar mass distributions of the two polyimides from their corresponding G(D)s. The exponents of these two calibrations further confirm that both of the polyimides have a slightly extended coil chain conformation in CHCl3. The chain flexibility difference between these two polyimides has also been discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The surface of superground Mn-Zn ferrite single crystal may be identified as a self-affine fractal in the stochastic sense. The rms roughness increased as a power of the scale from 10(2) nm to 10(6) nm with the roughness exponent alpha = 0.17 +/- 0.04, and 0.11 +/- 0.06, for grinding feed rate of 15 and 10 mu m/rev, respectively. The scaling behavior coincided with the theory prediction well used for growing self-affine surfaces in the interested region for magnetic heads performance. The rms roughnesses increased with increase in the feed rate, implying that the feed rate is a crucial grinding parameter affecting the supersmooth surface roughness in the machining process.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using a recently developed laser light-scattering (LLS) procedure, we accomplished the characterization of a broadly distributed unfractionated phenolphthalein poly(aryl ether ketone) (PEK-C) in CHCl3 at 25 degrees C. The laplace inversion of precisely measured intensity-intensity time correlation function from dynamic LLS leads us first to an estimate of the characteristic line-width distribution G(Gamma) and then to the translational diffusion coefficient distribution G(D). By using a previously established calibration of D (cm(2)/s) = 2.37 X 10(-4)M(-0.57), were able to convert G(D) into a differential weight distribution f(w)(M). The weight-average molecular weight M(w) calculated from f(w)(M) agrees well with that directly measured in static LLS. Our results indicate that both the calibration and LLS procedure used in this study are ready to be applied as a routine method for the characterization of the molecular weight distribution of PEK-C. (C) 1996 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Five narrowly distributed fractions of phenolphthalein poly(ether sulfone) (PES-C) were studied in CHCl3 by both static and dynamic laser light scattering (LLS) at 25 degrees C. The dynamic LLS showed that the PES-C samples contain some large polymer clusters as in previously studied phenolphthalein poly(ether ketone)(PEK-C). These large clusters can be removed by a 0.1-mu m filter. Our results showed that [R(g)(2)](1/2)(z) = (3.35 +/- 0.13) x 10(-2) M(w)((0.52 +/- 0.03)) and [D] = (2.26 +/- 0.02) x 10(-4)M(w)-((0.54) +/- 0.03)) with [R(g)(2)](1/2)(z), M(w) and [D] being the z-average radius of gyration, the weight-average molecular weight, and the z-average translational diffusion coefficient, respectively. A combination of static and dynamic LLS results enabled us to determine D = (2.45 +/- 0.04) x 10(-4)M-((0.55 +/- 0.05)), where D and M correspond to monodisperse species. Using this scaling relationship, we have successfully converted the translational diffusion coefficient distribution into the molecular weight distribution for each of the five PES-C fractional The weight-average molecular weights obtained from dynamic light scattering have a good agreement with that obtained from static laser light-scattering measurements.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Five different molecular weight phenolphthalein poly(aryl ether ketone) (PEK-C) fractions in CHCl3 were studied by static and dynamic laser light scattering(LLS). The dynamic LLS revealed that the PEK-C samples contain some large polymer clusters. These large clusters can be removed by filtering the solution with a 0.1-mu m filter. We found that the persistence length of PEK-C in CHCl3 at 25 degrees C is similar to 2 nm and the Flory characteristic ratio, C-infinity is similar to 25. Our results showed that [R(g)(2)](1/2)(z) = (3.50+/-0.20) x 10(-2)M(w)(0.54+/-0.01) and [D] = (2.37+/-0.05) x 10(-4)M(w)(-0.55+/-0.01), with [R(g)(2)](1/2)(z), M(w), and [D] being the z-average radius of gyration, the weight-average molecular weight, and the z-average translational diffusion coefficient, respectively. A combination of static and dynamic LLS results enabled us to determine D = (2.20+/-0.10) x 10(-4)M(-0.555+/-0.015), where D and M correspond to monodisperse species. Using this calibration between D and M,we have determined molecular weight distributions of five PEK-C fractions from their corresponding translational diffusion coefficient distribution.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structural parameters of the aggregated state in the polyamide PA1010 and N,N'-bismaleimide-4,4'-diphenyl methane (BMI) system were computed by means of the desmearing intensity from SAXS and using the concept of the distance distribution function. The results revealed that the parameters Q, I(0), l(c) and L decreased with the increase BMI component, whereas O-s increased. The particle dimension Z for different BMI contents was less than 13.2 nm, and the maximum value of the distance distribution function P(Z) was found to be in the range Z = 6.5-7.0 nm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A set of AM-AA copolymer samples with the same comonomer content and different average molecular weight have been characterized by C-13 NMB and light scattering methods in this paper. The chemical composition (comonomer AA, mole content 16.9 +/- 1.1%) of these samples is uniform. the sequence of AA in the macromolecular chain is of alone and random distribution and the light scattering theory from polyelectrolyte in added-salt solutions is suitable for the AM-AA copolymers-0.12 mol/L NaCl water systems. The actual values of M(w), the second Virial coefficient A(2) and the mean square radius of gyration (R(2)), for the studied samples have been obtained. The relationships between the molecular parameters are as follows: A(2)=0.0619 ($) over bar M(w)(-0.24), < R(2) >(1/2)(t)= 0.0210 ($) over bar M(w)(0.54).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The solution behavior of four chitosans (91% deacetylated chitin) with different molecular weights in 0.2M CH3COOH/0.1M CH3COONa aqueous solution was investigated at 25 degrees C by dynamic laser light scattering (LLS). The Laplace inversion of the precisely measured intensity-intensity time correlation function leads us to an estimate of the line-width distribution G(Gamma), which could be further reduced to a translational diffusion coefficient distribution G(D). By using a combination of static and dynamic LLS results, i.e. Mw and G(D), we were able to establish a calibration of D = k(D)M(-alpha D) with k(D) = (3.14 +/- 0.20) X 10(-4) and alpha(D) = 0.655 +/- 0.015. By using this calibration, we successfully converted G(D) into a molecular weight distribution f(w)(M). The larger alpha(D) value confirms that the chitosan chain is slightly extended in aqueous solution even in the presence of salts. This is mainly due to its backbone and polyelectrolytes nature. As a very sensitive technique, our dynamic LLS results also revealed that even in dilute solution chitosan still forms a small amount of larger sized aggregates that have ben overlooked in previous studies. The calibration obtained in this study will provide another way to characterize the molecular weight distribution of chitosan in aqueous solution at room temperature. (C) 1995 John Wiley & Sons, Inc.