915 resultados para Metallic-Glass
Resumo:
The electrical properties of poly p-phenylene sulfide (PPS) samples sandwiched between metallic electrodes are studied as a function of the applied voltage, temperature, time, electrode materials, and sample thickness. Superlinear current-voltage characteristics are observed, which are explained in terms of Schottky effect and space-charge limited currents (SCLC). The conductivity data for variable-range hopping have also been studied, but the calculated values of density of states are approximately one order of magnitude higher than those obtained by SCLC measurements. From thermally stimulated polarization currents we observed a current peak around 80°C that was related with the glass transition temperature of PPS. © 1993.
Resumo:
PURPOSE: To evaluate the penetration of a light-cured glass ionomer and a resin sealant into occlusal fissures and etched enamel. MATERIALS AND METHODS: Forty-eight maxillary and mandibular caries-free premolars scheduled for extraction for orthodontic reasons were isolated, the occlusal surfaces subjected to prophylaxis and acid-etched with orthophosphoric acid prior to the application of the VariGlass VLC glass ionomer and Concise resin sealants. The teeth were extracted, two longitudinal median sectiors from each tooth were ground to a thickness of 80-100 microns, and the sealant penetration into the fissures evaluated. The sections were placed in nitric acid to dissolve the enamel so the lengths of the tags which had penetrated into the etched enamel could be measured at different sites on the walls of the fissures. RESULTS: Both sealants adapted well to the fissures but penetrated deeper into shallow, open fissures than into deep, constricted fissures. The VariGlass VLC tags into etched enamel were generally longer than the Concise projections.
Resumo:
Two wafers of the NIST (formerly NBS) glass standard SRM 612 recently irradiated have been compared to the pre-irradiated wafers RT3 and RT4 of glass SRM 962-7, stored for 9 years at 5°C, and SRM 962, stored for 20 years at room temperature. Track area densities on internal surfaces of the glass as well as track size measurements suggest that (1) the old SRM 962 and the more recent SRM 962a calibrations are consistent and (2) annealing of the fission tracks in the pre-irradiated wafers is negligible. This last experimental result enables a direct comparison of contemporary and previous fission track age calibrations. © 1995.
Resumo:
The purpose of this study was to observe the quality of seal of the glass ionomer cement, Ketac-Endo, after treatment of the root canal wall. The root canals of 140 extracted human teeth were prepared biomechanically. The root canals were treated with either EDTA or received an intracanal dressing of calcium hydroxide or camphorated paramonochlorphenol. The root canals were filled by the lateral condensation technique with gutta-percha points and the sealer Ketac-Endo, or zinc oxide-eugenol cement or Sealapex. The teeth were placed into a 2% methylene blue dye solution inside a flask, which was attached to a vacuum pump. Leakage was measured linearly. Sealapex exhibited significantly less leakage than Ketac-Endo or zinc oxide-eugenol cement (P<0.01). The use of EDTA and intermediary dressings reduced significantly (P<0.01) the leakage observed with the zinc oxide-eugenol sealer and Ketac-Endo.
Resumo:
Pre-resonant Raman effect of chromate ion, CrO2- 4, was observed in a metasilicate glass with molar composition 2Na2O · 1CaO · 3SiO2 containing 1.0 wt% of Cr2O3. Raman spectra were measured by the conventional 90° scattering geometry and by the microprobe Raman spectroscopic techniques. The presence of chromate ions in the glass is favoured by the glass composition and oxidizing conditions during the glass melting, and they are responsible for optical absorption bands at 370 and 250 nm. Raman spectrum of the undoped glass presents bands at 625, 860 and 980 cm-1, and the presence of chromate ions gives rise to additional bands at 365, 850 and a shoulder at 890 cm-1. An enhancement of the 850 cm-1 Raman band is observed with decreasing laser exciting wavelength. The exciting frequency dependence of the intensity of this band is discussed in terms of theoretical models given in the literature.
Resumo:
With suitable thermal treatments, a nearly stoichiometric cordierite glass (2 MgO.2 Al2O3. 5 SiO2) shows a variety of crystal morphologies on the external surfaces: lozenges, regular and elongated hexagons, spherical and square shaped particles. We initially identified these morphologies through optical and scanning electron microscopy techniques. Their structural features were distinguished by x-ray diffraction patterns, infrared and Roman microprobe spectra. We concluded that there are close structural similarities for: lozenges and glass matrix; regular and elongated hexagons; spherical and square particles. The ordering degree increases in the following sequence: glass matrix, lozenges, hexagons, squares and spheres. The lozenge crystals are known as X-phase. The hexagons belong to the μ-cordierite (high quartz solid solution) metastable phase and the squares and spheres to the α-cordierite stable phase.
Resumo:
We have observed ultraviolet upconversion fluorescence from the 4D3/2 and 2P3/2 levels of Nd3+ in fluoroindate glass under infrared pumping. It was found that the excitation of a large population in the 4F3/2 metastable level allows to achieve strong upconversion emissions at 354 and 382 nm. A simple rate equation model reproduces the temporal behavior of the upconverted emission and allows us to estimate the energy transfer rate among three Nd3+ ions participating in the process. © 1997 American Institute of Physics.
Resumo:
We report the observation of frequency upconversion in fluoroindate glasses with the following compositions: (mol%) (39 - x)InF3-20ZnF2-20SrF2-16BaF 2-2GdF3-2NaF-1GaF3-xNdF3 (x = 0.05, 0.1, 0.5, 1, 2, 3). The excitation source was a dye laser in resonance with the 4I9/2→(2G5/2, 2G7/2) transition of the Nd3+ ions. The upconverted fluorescence spectra show emissions from ∼ 350 to ∼ 450 nm, corresponding to transitions 4D3/2→4I9/2 ;4D3/2→4I11/2; 2P3/2→ 4I9/2; 4D3/2→4I13/2; 2P3/2→4I11/2; 4D3/2→4I15/2; and 2P3/2 → 4I13/2. The dependence of the fluorescence signals on the laser intensity indicates that two laser photons participate in the process. The temporal behavior of the signal indicates that energy transfer among the Nd3+ ions is the main mechanism which contributes to upconversion at 354 and 382 nm.
Resumo:
Carboxymethylcellulose packed in to a glass column was used to pre-concentrate metallic cations from aqueous solutions. The pre-concentrated metal cations are directly eluted from the column using 5.0 mL of 1.0 mol L -1 hydrochloric acid. The optimum pre-concentration conditions are given (glass column, 16 cm length, 0.80 cm i.d., stationary phase height of 12 cm, flow-rate, 1.5 mL min -1). The recuperation efficiency achieved is greater than 95%, while the enrichment factor is 10 for 50 mL of solution (0.50 mg L -1 each).
Resumo:
Purpose: To evaluate the surface roughness and staining of a glass ionomer cement when subjected to different finishing procedures. Materials and Methods: Sixty-four discs of Chem-Fil II glass ionomer cement were submitted to staining test with methylene blue by spectrophotometry and roughness test by profilometry. Four groups were evaluated: Mylar matrix (control), Sof-Lex discs, Enhance points, and diamond bur. Results: Staining and roughness test, analyzed by ANOVA and Tukey's test, showed that the best surface was obtained when the material cured in contact with the Mylar matrix strip or when treated with Sof-Lex discs. The poorest results were obtained after using the diamond bur.
Resumo:
The efficiency of energy transfer (ET) between Pr3+ ions in a fluoroindate glass is determined. ET rates, WET, were determined for dilute samples and the results show a dependence of WET on the Pr3+ concentration. ET processes which contribute to resonance fluorescence and frequency upconversion emission were studied. The origin of the interaction energy among the Pr3+ ions was determined to be dipole - dipole. © 1998 Elsevier Science B.V. All rights reserved.
Resumo:
Bright fluorescence in the visible range has been observed in Pr3+-Yb3+ doped fluoroindate glass under infrared diode laser irradiation. The mechanism which contributes for the upconversion emission is identified and the energy transfer rate between Pr3+-Yb3+ is obtained for different concentrations. © 1998 Elsevier Science B.V. All rights reserved.
Resumo:
We report the observation of cooperative frequency upconversion in a fluoroindate glass. The experiments were performed by exciting Yb3+-Tb3+ codoped samples with an infrared diode laser. The process is monitored through the green fluorescence emitted by Tb3+ ions due to a cooperative energy transfer from a pair of excited Yb3+ ions. © 1998 Elsevier Science B.V. All rights reserved.
Resumo:
Non-linear absorption is observed in Er3+-doped fluoroindate glass (in mol% 37InF2:20ZnF2:20SrF2:16BaF2:2GdF2: 2NaF:1GaF3:2ErF3) when the sample is irradiated with a CW laser emitting at 650 nm. An intensity dependence of the optical transmittance is detected. Saturation and sequential absorption of two photons are responsible for the decrease of 50% in the transmittance. The results are explained by simple models which are solved based on rate-equations for the populations of energy levels.
Resumo:
The preparation and characterization of transparent glass-ceramics in the composition of 30Li2O:5ZrO2:xBaO:(100-x) SiO2 with x = 0, 5, 10, 15, and 20 mol% are described. Glasses were melted in a platinum crucible at 1100°C for 2 h and then heat-treated at 900°C for 3 h. The characterizations were performed by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), Raman and infrared spectroscopy, and scanning electron microscopy (SEM). The experimental results indicate that there was a structural change in the glass-ceramics as the BaO concentration in the mixture increased. In the XRD patterns of samples without heat treatment, only the halo was observed. After heat treatment, the appearance of the materials was verified by X-ray diffraction peaks. The reorganization of the amorphous solid was confirmed by Raman and IR spectroscopy along with XPS and SEM, with a more homogeneous phase formation being observed.