940 resultados para Flexural bond strengths
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Despite a plethora of in situ studies and clinical trials evaluating the efficacy of fluoridated dentifrices on caries control, in vitro pH cycling models are still broadly used because they mimic the dynamics of mineral loss and gain involved in caries formation. This paper critically reviews the current literature on existing pH-cycling models for the in vitro evaluation of the efficacy of fluoridated dentifrices for caries control, focusing on their strengths and limitations. A search was undertaken in the MEDLINE electronic journal database using the keywords "pH-cycling", "demineralization", "remineralization", "in vitro", "fluoride", "dentifrice". The primary outcome was the decrease of demineralization or the increase of remineralization as measured by different methods (e. g.: transverse microradiography) or tooth fluoride uptake. Inclusion of studies, data extraction and quality assessment were undertaken independently and in duplicate by two members of the review team. Disagreements were solved by discussion and consensus or by a third party. One hundred and sixteen studies were included, of which 42 addressed specifically the comparison of dentifrices using different pH-cycling models. The other studies included meta-analysis or reviews, data about the effect of different fluoride sources on de-remineralization, different methods for analysis de-remineralization and chemical variables and characteristics of dental hard tissues that might have influence on de-remineralization processes. Generally, the studies presented ability to detect known results established by clinical trials, to demonstrate dose-related responses in the fluoride content of the dentifrices, and to provide repeatability and reproducibility between tests. In order to accomplish these features satisfactorily, it is mandatory to take into account the type of substrate and baseline artificial lesion, as well as the adequate response variables and statistical approaches to be used. This critical review of literature showed that the currently available pH-cycling models are appropriate to detect dose-response and pH-response of fluoride dentifrices, and to evaluate the impact of new active principles on the effect of fluoridated dentifrices, as well as their association with other anti-caries treatments.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Objective. The aim of this study was to evaluate the pulp response following cementation of inlays using two different resin cements.Methods. Deep Class V cavities were prepared on the buccal surface of 34 sound human premolars. impressions were taken and inlays were prepared which were cemented with the following luting materials-Group 1: Rely X(TM) Unicem. (3M ESPE); Group 2: Variolink(R) II (Ivoclar Vivadent). in Group 3 (control), after lining the cavity floor with Dycal(R) (Dentsply Caulk) the inlays were cemented with Rely X(TM) Unicem. Four additional teeth were used as an intact control group. For Variolink(R) II, the adhesive system Excite was used as part of the cementation procedure. After 7 or 60 days, the teeth were extracted and processed for histological assessment.Results. At 7 days, Rely X(TM) Unicern and Variolink(R) II system triggered in two samples a mild and moderate inflammatory response, respectively. At 60 days, the pulpal response decreased for both groups. A discrete persistent inflammatory response occurred in Group 2 in which displacement of resin components across the dentin tubules was observed. In the control group, normal histological characteristics were observed. The inflammatory response and tissue disorganization were related to the remaining dentin thickness between the cavity floor and the pulp tissue.Significance. Techniques for inlay cementation using distinct luting cements may cause specific pulpal damage. Variolink(R) II associated with the adhesive system Excite cause more aggressive effects to the pulp-dentin complex than Rely X(TM) Unicern cement when both are used to cement inlay restorations. (C) 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Objectives. This study was undertaken to evaluate the shear bond strength of four materials used as aesthetic material bonded to Ni-Cr alloy.Methods. Sixty-eight alloy discs were prepared and divided equally into four groups, and received four treatments for veneering: conventional feldspathic porcelain (Noritake EX-3) and three light-cured prosthodontic composite resins (Artglass, Solidex and Targis). The aesthetic materials were applied after metal structure conditioning in accordance with the manufacturers' recommendations. The specimens were stored in distilled water at 37 degreesC for 7 days. A universal testing machine was used to measure the shear bond strength of the specimens at a cross head speed of 0.5 mm/min. Fractured specimens were examined by using both optical and scanning electron microscope.Results. The analysis of variance and Tukey's test showed that the strongest mean shear bond was obtained with Noritake EX-3 (mean shear bond strength 42.90 +/- 7.82 MPa). For composites, the highest mean shear bond strength was observed for Targis (12.30 +/- 1.57 MPa); followed by Solidex (11.94 +/- 1.04 MPa) and Artglass (10.04 +/- 0.75 MPa). Optical analysis of the fractured surf aces indicated that for Targis and Noritake EX-3 all failures were a mixture of both cohesive and adhesive patterns. As for Artglass and Solidex, the fractures were mainly adhesive in nature.Conclusions. The Solidex system was equivalent to the Targis system in bond strength and exhibited greater strength than the Artglass system. The porcelain fused-to-metal showed considerably higher shear bond strength than the three metal-resin bonding techniques. (C) 2003 Elsevier B.V. Ltd. Ali rights reserved.
Resumo:
Objective. To evaluate the content of inorganic particles and the flexural strength of new condensable composites for posterior teeth in comparison to hybrid conventional composites.Method. The determination of the content of inorganic particles was performed by mass weighing of a polymerized composite before and after the elimination of the organic phase. The volumetric particle content was determined by a practical method based on Archimedes' principle, which calculates the volume of the composite and their particles by differential mass measured in the air and in water. The flexural. strength of three points was evaluated according to the norm ISO 4049:1988.Results. The results showed the following filter content: Alert, 67.26%; Z-100, 65.27%; Filtek P 60, 62.34%; Ariston pHc, 64.07%; Tetric Ceram, 57.22%; Definite, 54.42%; Solitaire, 47.76%. In the flexural strength test, the materials presented the following decreasing order of resistance: Filtek P 60 (170.02 MPa) > Z-100 (151.34 MPa) > Tetric Ceram (126.14 MPa) = Alert (124.89 MPa) > Ariston pHc (102.00 MPa) = Definite (93.63 MPa) > Solitaire (56.71 MPa).Conclusion. New condensable composites for posterior teeth present a concentration of inorganic particles similar to those of hybrid composites but do not necessarily present higher flexural strength. (C) 2003 Elsevier B.V. Ltd. Alt rights reserved.
Resumo:
Objectives: This study investigated the effect of relining, water storage and cyclic loading on the ultimate flexural strength (FSU) and on the flexural strength at the proportional limit (FSPl) of a denture base acrylic resin (Lucitone 550-L).Methods: Rectangular bars of L were made (64 mm x 10 mm x 2 mm) and relined (1.3 mm) with four relining resins (Kooliner-K, Ufi Gel Hard-UGH, Tokuso Rebase Fast-TR and New Truliner-NT). In addition, specimens relined with L and intact L specimens were made (64 mm x 10 mm x 3.3 mm). A three-point flexural test was applied on the specimens (n = 10) after (1) polymerization; (2) water storage (30 days); (3) cyclic loading (10,000 cycles at 5 Hz) and (4) water storage (30 days) + cyclic loading. Data (MPa) were analyzed with three-way ANOVA and Tukey's HSD tests (alpha = 0.05). To test for a possible correlation between FSU and FSPl, a linear regression coefficient 'r' was calculated.Results: After water storage, L-UGH and L-TR demonstrated an increased FSU (41.4950.64 MPa and 49.95-57.36 MPa, respectively) (P < 0.05). Only L-TR demonstrated an increased FSPl (20.58-24.21 MPa) after water storage (P < 0.05). L-L had the highest FSU (between 78.57 and 85.09 MPa) and FSPl (between 31.30 and 34.17 MPa) (P < 0.05). The cyclic loading decreased the FSU and FSPl of all materials (P < 0.05). Regression analysis showed a strong linear correlation between the two variables (r = 0.941).Conclusions: Water storage improved the FSU of L-UGH and L-TR and the FSPl of L-TR. L-L produced the highest FSU and FSPl. The FSU and FSPl of all materials were detrimentally influenced by cyclic loading.