923 resultados para photocatalytic reactor


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Herein we demonstrate a facile, reproducible, and template-free strategy to prepare g-C3N4–Fe3O4 nanocomposites by an in situ growth mechanism. The results indicate that monodisperse Fe3O4 nanoparticles with diameters as small as 8 nm are uniformly deposited on g-C3N4 sheets, and as a result, aggregation of the Fe3O4 nanoparticles is effectively prevented. The as-prepared g-C3N4–Fe3O4 nanocomposites exhibit significantly enhanced photocatalytic activity for the degradation of rhodamine B under visible-light irradiation. Interestingly, the g-C3N4–Fe3O4 nanocomposites showed good recyclability without loss of apparent photocatalytic activity even after six cycles, and more importantly, g-C3N4–Fe3O4 could be recovered magnetically. The high performance of the g-C3N4–Fe3O4 photocatalysts is due to a synergistic effect including the large surface-exposure area, high visible-light-absorption efficiency, and enhanced charge-separation properties. In addition, the superparamagnetic behavior of the as-prepared g-C3N4–Fe3O4 nanocomposites also makes them promising candidates for applications in the fields of lithium storage capacity and bionanotechnology.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper analyzes the physical phenomena that take place inside an 1 kg/h bubbling fluidized bed reactor located at Aston University and presents a geometrically modified version of it, in order to improve certain hydrodynamic and gas flow characteristics. The bed uses, in its current operation, 40 L/min of N2 at 520 °C fed through a distributor plate and 15 L/min purge gas stream, i.e., N2 at 20 °C, via the feeding tube. The Eulerian model of FLUENT 6.3 is used for the simulation of the bed hydrodynamics, while the k - ε model accounts for the effect of the turbulence field of one phase on the other. The three-dimensional simulation of the current operation of the reactor showed that a stationary bubble was formed next to the feeding tube. The size of the permanent bubble reaches up to the splash zone of the reactor, without any fluidizaton taking place underneath the feeder. The gas flow dynamics in the freeboard of the reactor is also analyzed. A modified version of the reactor is presented, simulated, and analyzed, together with a discussion on the impact of the flow dynamics on the fast pyrolysis of biomass. © 2010 American Chemical Society.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study presents a report on pyrolysis of Napier grass stem in a fixed bed reactor. The effects of nitrogen flow (20 to 60 mL/min), and reaction temperature (450 to 650 degrees C) were investigated. Increasing the nitrogen flow from 20 to 30 mL/min increased the bio-oil yield and decreased both bio-char and non-condensable gas. 30 mL/min nitrogen flow resulted in optimum bio-oil yield and was used in the subsequent experiments. Reaction temperatures between 450 and 600 degrees C increased the bio-oil yield, with maximum yield of 32.26 wt% at 600 degrees C and a decrease in the corresponding bio-char and non-condensable gas. At 650 degrees C, reductions in the bio-oil and bio-char yields were recorded while the non-condensable gas increased. Water content of the bio-oil decreased with increasing reaction temperature, while density and viscosity increased. The observed pH and higher heating values were between 2.43 to 2.97, and 25.25 to 28.88 MJ/kg, respectively. GC-MS analysis revealed that the oil was made up of highly oxygenated compounds and requires upgrading. The bio-char and non-condensable gas were characterized, and the effect of reaction temperature on the properties was evaluated. Napier grass represents a good source of renewable energy when all pyrolysis products are efficiently utilized.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dimethyl methyl phosphonate (DMMP), diethyl methyl phosphonate (DEMP), and fluorophenols undergo rapid decomposition upon TiO$\sb2$ catalyzed photooxidation in air saturated aqueous solution. The degradation rates of DMMP were determined over a range of temperatures, under solar and artificial irradiation with and without simultaneous sonication. Solar illumination is effective for the degradation and the use of low energy of sonication increases the rate of mineralization. The surface area and the type of TiO$\sb2$ dramatically affect the photoactivity of the catalyst. A number of intermediate products are formed and ultimately oxidized to phosphate and carbon dioxide. Possible reaction mechanisms and pathways for DMMP and DEMP are proposed. The Langmuir-Hinshelwood kinetic parameters for the photocatalysis of fluorophenols suggest modestly different reactivity for each isomer. The adsorption constant is largest for the ortho isomer consistent with the adsorption onto TiO$\sb2$ through both hydroxyl and fluoride groups to form a chelated type structure. ^

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two studies were performed to obtain fundamental mechanistic information on the TiO2 catalyzed degradation of organic substrates irradiated at 350 nm in dilute aqueous solutions under oxygenated conditions: (a) The photodecomposition of methyl tert-butyl ether (MTBE) and its intermediate products from β-oxidation, 2-methoxy-2-methylpropanol and 2-methoxy-2-methylpropanol. (b) The photodecomposition of two haloethers, bis-(2-chloroethyl) ether, and bis-(2-chloroisopropyl) ether. Controls were carried out throughout the two studies in the absence of light, and without the semiconductor in order to evaluate the role of photolysis. ^ The syntheses of proposed intermediate products, 2-methoxy-2-methylpropanol, 2-methoxy-2-methylpropanal, 2-methoxy-2-methylpropanoic acid, 2-chloroethyl formate, and 1-chloro-2-propyl acetate, were performed. The formation of these products in the titanium dioxide photocatalytic oxidation of the substrates of interest was also confirmed. TiO2 photocatalysis is a very effective method for the mineralization of aliphatic ethers and their primary oxidation products. ^

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dimethyl methyl phosphonate (DMMP), diethyl methyl phosphonate (DEMP), and fluorophenols undergo rapid decomposition upon TiO2 catalyzed photooxidation in air saturated aqueous solution. The degradation rates of DMMP were determined over a range of temperatures, under solar and artificial irradiation with and without simultaneous sonication. Solar illumination is effective for the degradation and the use of low energy of sonication increases the rate of mineralization. The surface area and the type of TiO2 dramatically affect the photoactivity of the catalyst. A number of intermediate products are formed and ultimately oxidized to phosphate and carbon dioxide. Possible reaction mechanisms and pathways for DMMP and DEMP are proposed. The Langmuir- Hinshelwood kinetic parameters for the photocatalysis of fluorophenols suggest modestly different reactivity for each isomer. The adsorption constant is largest for the ortho isomer consistent with the adsorption onto TiO2 through both hydroxyl and fluoride groups to form a chelated type structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The modern industrial progress has been contaminating water with phenolic compounds. These are toxic and carcinogenic substances and it is essential to reduce its concentration in water to a tolerable one, determined by CONAMA, in order to protect the living organisms. In this context, this work focuses on the treatment and characterization of catalysts derived from the bio-coal, by-product of biomass pyrolysis (avelós and wood dust) as well as its evaluation in the phenol photocatalytic degradation reaction. Assays were carried out in a slurry bed reactor, which enables instantaneous measurements of temperature, pH and dissolved oxygen. The experiments were performed in the following operating conditions: temperature of 50 °C, oxygen flow equals to 410 mL min-1 , volume of reagent solution equals to 3.2 L, 400 W UV lamp, at 1 atm pressure, with a 2 hours run. The parameters evaluated were the pH (3.0, 6.9 and 10.7), initial concentration of commercial phenol (250, 500 and 1000 ppm), catalyst concentration (0, 1, 2, and 3 g L-1 ), nature of the catalyst (activated avelós carbon washed with dichloromethane, CAADCM, and CMADCM, activated dust wood carbon washed with dichloromethane). The results of XRF, XRD and BET confirmed the presence of iron and potassium in satisfactory amounts to the CAADCM catalyst and on a reduced amount to CMADCM catalyst, and also the surface area increase of the materials after a chemical and physical activation. The phenol degradation curves indicate that pH has a significant effect on the phenol conversion, showing better results for lowers pH. The optimum concentration of catalyst is observed equals to 1 g L-1 , and the increase of the initial phenol concentration exerts a negative influence in the reaction execution. It was also observed positive effect of the presence of iron and potassium in the catalyst structure: betters conversions were observed for tests conducted with the catalyst CAADCM compared to CMADCM catalyst under the same conditions. The higher conversion was achieved for the test carried out at acid pH (3.0) with an initial concentration of phenol at 250 ppm catalyst in the presence of CAADCM at 1 g L-1 . The liquid samples taken every 15 minutes were analyzed by liquid chromatography identifying and quantifying hydroquinone, p-benzoquinone, catechol and maleic acid. Finally, a reaction mechanism is proposed, cogitating the phenol is transformed into the homogeneous phase and the others react on the catalyst surface. Applying the model of Langmuir-Hinshelwood along with a mass balance it was obtained a system of differential equations that were solved using the Runge-Kutta 4th order method associated with a optimization routine called SWARM (particle swarm) aiming to minimize the least square objective function for obtaining the kinetic and adsorption parameters. Related to the kinetic rate constant, it was obtained a magnitude of 10-3 for the phenol degradation, 10-4 to 10-2 for forming the acids, 10-6 to 10-9 for the mineralization of quinones (hydroquinone, p-benzoquinone and catechol), 10-3 to 10-2 for the mineralization of acids.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We thank the INSA-RSE bilateral exchange programme for financial assistance (PD) and the Petroleum Technology Development Fund (PTDF, Nigeria) for the award of PhD scholarship, as well as Abubakar Tafawa Balewa University, Bauchi-Nigeria for the granted fellowship (H.A).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We thank the INSA-RSE bilateral exchange programme for financial assistance (PD) and the Petroleum Technology Development Fund (PTDF, Nigeria) for the award of PhD scholarship, as well as Abubakar Tafawa Balewa University, Bauchi-Nigeria for the granted fellowship (H.A).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We thank the European Commission for financial support through the European Project Light2CAT, funded by the European Union’s Seventh Framework Programme (FP7) under the grant agreement no. 283062 Eco-Innovation, Theme Environment

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Surface modification of rutile TiO2 with extremely small SnO2 clusters gives rise to a great increase in its UV light activity for degradation of model organic water pollutants, while the effect is much smaller for anatase TiO2. This crystal form sensitivity is rationalized in terms of the difference in the electronic modification of TiO2 through the interfacial Sn−O−Ti bonds. The increase in the density of states near the conduction band minimum of rutile by hybridization with the SnO2 cluster levels intensifies the light absorption, but this is not seen with modified anatase. The electronic transition from the valence band to the conduction band causes the bulk-to-surface interfacial electron transfer to enhance charge separation. Further, electrons relaxed to the conduction minimum are smoothly transferred to O2 due to the action of the SnO2 species as an electron transfer promoter.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Smart inks as a redox indicators of photocatalytic activity were applied on several paints with acrylic and silicate binder exposed to accelerated weathering test. The results show, that self-cleaning paints need some weathering to develop full photocatalytic activity. On the other side weathering may negatively influence the durability of the paint as shown for a silicate based exterior paint, which was significantly degraded after 350 h of weathering test. Smart inks proved to be suitable and rapid indicators of paint photoactivity. Resazurin ink is convenient only for unexposed paint with low photocatalytic activity while an Acid Violet 7 ink was appropriate for most of the paints, especially those that were weathered

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The photocatalytic activity of self-cleaning glass is assessed using a resazurin (Rz) photocatalyst activity indicator ink, i.e. Rz paii, via both the rate of change in the colour of the ink (blue to pink), R(Abs), and the rate of change in the fluorescence intensity, R(Fl), (λ(excitation) = 593 nm; λ(emission) = 639 nm) of the ink. In both cases the kinetics are zero order. Additional work with a range of glass samples of different photocatalytic activity reveal R(Abs) is directly related to R(Fl), thereby showing that the latter, like the former, can be used to provide a measure of the photocatalytic activity of the sample under test. The measured value of R(Fl) is found to be the same for 5 pieces of, otherwise identical, selfcleaning glass with: black, red, blue, yellow and no coloured tape stuck to their backs, which demonstrates that R(Fl) measurements can be used to measure photocatalytic activity under conditions of high colour and opacity under which R(Abs) cannot be measured. The relevance of this novel, fluorescence-based paii to the assessment of the activity of highly coloured, opaque photocatalytic samples, such as paints and tiles, is discussed briefly.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The adsorption and photocatalytic degradation of acetate on TiO2 surfaces was investigated in H2O and D2O by ATR-FTIR and EPR Spectroscopy respectively. These studies were carried out in the dark and under UV(A) illumination to gain additional insights into the adsorption behaviour with the identification of paramagnetic species formed during the oxidation of acetate. Isotopic exchange during the adsorption of D2O on TiO2 surface led to different interactions between the adsorbate and OD groups. At different pH levels, several surface complexes of acetate can be formed such as monodentate, or bidentates. Under UV(A) irradiation of TiO2 aqueous suspensions, the formation of hydroxyl and methoxy radicals evidenced as the corresponding spin-adducts, were found to dominate in alkaline and acidic suspensions respectively. Two possible pathways for the oxidation of acetate have been suggested at different pH levels in solution in terms of the source of the spin adduct formed. These proposed pathways were found to be in good agreement with ATR-FTIR and EPR results.