1000 resultados para luminescence mechanism
Resumo:
We investigate the mechanism of formation of periodic void arrays inside fused silica and BK7 glass irradiated by a tightly focused femtosecond (fs) laser beam. Our results show that the period of each void array is not uniform along the laser propagation direction, and the average period of the void array decreases with increasing pulse number and pulse energy. We propose a mechanism in which a standing electron plasma wave created by the interference of a fs-laser-driven electron wave and its reflected wave is responsible for the formation of the periodic void arrays.
Resumo:
Infrared (IR) luminescence covering 1.1 to similar to 1.6 mu m wavelength region was observed from bismuth-doped barium silicate glasses, excited by a laser diode at 808 nm wavelength region, at room temperature. The peak of the IR luminescence appears at 1325 nm. A full width half-maximum (FWHM) and the lifetime of the fluorescence is more than 200 nm and 400 mu s, respectively. The fluorescence intensity increases with Al2O3 content, but decreases with BaO content. We suggest that the IR luminescence should be ascribed to the low valence state of bismuth Bi2+ or Bi+, and Al3+ ions play an indirect dispersing role for the infrared luminescent centers.
Resumo:
Transparent Ni2+-doped beta-Ga2O3 glass-ceramics were synthesized. The nanocrystal phase in the glass-ceramics was identified to be beta-Ga2O3 and its size was about 3.6 nm. It was confirmed from the absorption spectra that the ligand environment of Ni2+ ions changed from the trigonal bi-pyramid fivefold sites in the as-cast glass to the octahedral sites in the glass-ceramics. The broadband infrared emission centering at 1270 nm with full width at half maximum (FWHM) of more than 250 nm was observed. The fluorescence lifetime was about 1.1 mu s at room temperature. The observed infrared emission could be attributed to the T-3 (2g) (F-3) -> (3)A (2g) (F-3) transition of octahedral Ni2+ ions. It is suggested that the Ni2+-doped transparent beta-Ga2O3 glass-ceramics with broad bandwidth and long lifetime have a potential as a broadband amplification medium.
Resumo:
We report transparent Ni2+-doped ZnO-Al2O3-SiO2 system glass-ceramics with broadband infrared luminescence. After heat-treatment, ZnAl2O4 crystallite was precipitated in the glasses, and its average size increased with increasing heat-treatment temperature. No infrared emission was detected in the as-prepared glass samples, while broadband infrared luminescence centered at 1310 nm with full width at half maximum (FWHM) of about 300 nm was observed from the glass-ceramics. The peak position of the infrared luminescence showed a blue-shift with increasing heat-treatment temperature, but a red-shift with an increase in NiO concentration. The mechanisms of the observed phenomena were discussed. These glass-ceramics are promising as materials for super broadband optical amplifier and tunable laser. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Near-infrared to UV and visible upconversion luminescence was observed in single-crystalline ZnO under an 800 nm infrared femtosecond laser irradiation. The optical properties of the crystal reveal that the UV and VIS emission band are due to the exciton transition (D0X) bound to neutral donors and the deep luminescent centers in ZnO, respectively. The relationship between the upconversion luminescence intensity and the pump power of the femtosecond laser reveals that the UV emission belongs to three-photon sequential band-to-band excitation and the VIS emission belongs to two-photon simultaneous defect-absorption induced luminescence. A saturation phenomenon and polarization-dependent effect are also observed in the upconversion process of ZnO. A very good optical power limiting performance at 800 nm has been demonstrated. The two- and three-photon absorption coefficients of ZnO crystal were measured to be 0.2018 cm GW(-1) and 7.102 x 10(-3) cm(3) GW(-2), respectively. The two- and three-photon cross sections were calculated to be 1.189 x 10(-51) cm(4) s and 1.040 x 10(-80) cm(6) s(2), respectively. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Fluorescence spectra of Nd: YVO4 under excitation of a continuous wave (CW) diode laser and a femtosecond laser at 800nm were investigated. It was found that Nd: YVO4 shows different upconversion and downconversion luminescencent behaviors when excited by the diode laser and the femtosecond laser. The dependence of the upconversion luminescence intensity on the pump power of the femtosecond laser was discussed. The populations of the upper energy levels for upconversion and downconversion luminescence were calculated based on the Bloch equations. The calculations agree well with the experimental results. (c) 2007 Optical Society of America.
Resumo:
This work contains 4 topics dealing with the properties of the luminescence from Ge.
The temperature, pump-power and time dependences of the photoluminescence spectra of Li-, As-, Ga-, and Sb-doped Ge crystals were studied. For impurity concentrations less than about 1015cm-3, emissions due to electron-hole droplets can clearly be identified. For impurity concentrations on the order of 1016cm-3, the broad lines in the spectra, which have previously been attributed to the emission from the electron-hole-droplet, were found to possess pump-power and time dependent line shape. These properties show that these broad lines cannot be due to emission of electron-hole-droplets alone. We interpret these lines to be due to a combination of emissions from (1) electron-hole- droplets, (2) broadened multiexciton complexes, (3) broadened bound-exciton, and (4) plasma of electrons and holes. The properties of the electron-hole-droplet in As-doped Ge were shown to agree with theoretical predictions.
The time dependences of the luminescence intensities of the electron-hole-droplet in pure and doped Ge were investigated at 2 and 4.2°K. The decay of the electron-hole-droplet in pure Ge at 4.2°K was found to be pump-power dependent and too slow to be explained by the widely accepted model due to Pokrovskii and Hensel et al. Detailed study of the decay of the electron-hole-droplets in doped Ge were carried out for the first time, and we find no evidence of evaporation of excitons by electron-hole-droplets at 4.2°K. This doped Ge result is unexplained by the model of Pokrovskii and Hensel et al. It is shown that a model based on a cloud of electron-hole-droplets generated in the crystal and incorporating (1) exciton flow among electron-hole-droplets in the cloud and (2) exciton diffusion away from the cloud is capable of explaining the observed results.
It is shown that impurities, introduced during device fabrication, can lead to the previously reported differences of the spectra of laser-excited high-purity Ge and electrically excited Ge double injection devices. By properly choosing the device geometry so as to minimize this Li contamination, it is shown that the Li concentration in double injection devices may be reduced to less than about 1015cm-3 and electrically excited luminescence spectra similar to the photoluminescence spectra of pure Ge may be produced. This proves conclusively that electron-hole-droplets may be created in double injection devices by electrical excitation.
The ratio of the LA- to TO-phonon-assisted luminescence intensities of the electron-hole-droplet is demonstrated to be equal to the high temperature limit of the same ratio of the exciton for Ge. This result gives one confidence to determine similar ratios for the electron-hole-droplet from the corresponding exciton ratio in semiconductors in which the ratio for the electron-hole-droplet cannot be determined (e.g., Si and GaP). Knowing the value of this ratio for the electron-hole-droplet, one can obtain accurate values of many parameters of the electron-hole-droplet in these semiconductors spectroscopically.
Energy transfer and enhanced broadband near-infrared luminescence in Yb-Bi codoped phosphate glasses
Resumo:
The photochemically induced reductive elimination of cyclopropanes from bis(η5-cyclopentadienyl)titanacyclobutanes has been examined. Stereochemical labelling studies indicate that the cyclopropane is initially formed in a 6±1:1, ratio favoring retention of stereochemistry. The starting titanacyclobutane is isomerized during the course of the reaction. The isomerization of the starting material results from metal-carbon bond homolysis to yield a 1,4-biradical, which can either close to give the starting material or generate cyclopropane. The 1,4-biradical can be observed through a cyclopropyl carbinyl rearrangement employing 2-bis(η5- cyclopentadienyl)titana-5,5-dimethylbicyclo[2.1.0]pentane, to give the titanium alkylidene, 1-bis(η5-cyclopentadienyl)titana-3,3-dimethyl-1,4- pentadiene, which can be observed directly by NMR at low temperature.
The oxidation of titanacyclobutanes by chemical and electrochemical methods also yields cyclopropanes. Reduction of the metal center does not yield cyclopropanes. Depending on the oxidant, stereochemically labelled titanacyclobutanes yield cyclopropanes that are between 7:1 and 100:1 retention:isomerization. The fragmentation reaction resembles the photochemically induced reductive elimination. Both result from formal oxidation of a metal-carbon bond, which then results in very rapid formation of cyclopropane.
The titanocene generated photochemically reacts with a variety of substrates even at low temperature. Titanocene can be generated in a glass at 77 K. The titanocene can be trapped in noncoordinating solvents in high yield with bulky internal acetylenes to give monoacetylene adducts of titanocene. Less bulky acetylenes give the titanacyclopentadienes. The titanocene can be trapped with olefins to give less stable adducts, which appear by NMR analysis to be intermediate in structure between a titanacyclopropane and an η2 olefin adduct of titanocene. Reaction of titanocene with butadiene gives a stable product, which appears to be the s-trans butadiene adduct of titanocene. It does not isomerize on heating. Titanocene reacts with epoxides to give titanocene-µ-oxo polymer and olefin. Stereochemically labelled epoxides and episulfides yield isomerized olefin upon deoxygenation by titanocene. The observations are rationalized as a result of a 1,4-biradical formed by stepwise insertion of titanocene into a carbon-oxygen bond.