Resumo:

Grain boundaries (GBs), particularly ferrite: ferrite GBs, of X70 pipeline steel were characterized using analytical electron microscopy (AEM) in order to understand its intergranular stress corrosion cracking (IGSCC) mechanism(s). The microstructure consisted of ferrite (alpha), carbides at ferrite GBs, some pearlite and some small precipitates inside the ferrite grains. The precipitates containing Ti, Nb, V and N were identified as complex carbo-nitrides and designated as (Ti, Nb, WC, N). The GB carbides occurred (1) as carbides along ferrite GBs, (2) at triple points, and (3) at triple points and extending along the three ferrite GBs. The GB carbides were Mn rich, were sometimes also Si rich, contained no micro-alloying elements (Ti, Nb, V) and also contained no N. It was not possible to measure the GB carbon concentration due to surface hydrocarbon contamination despite plasma cleaning and glove bag transfer from the plasma cleaner to the electron microscope. Furthermore, there may not be enough X-ray signal from the small amount of carbon at the GBs to enable measurement using AEM. However, the microstructure does indicate that carbon does segregate to alpha : alpha GBs during microstructure development. This is particularly significant in relation to the strong evidence in the literature linking the segregation of carbon at GBs to IGSCC. It was possible to measure all other elements of interest. There was no segregation at alpha : alpha GBs, in particular no S, P and N, and also no segregation of the micro-alloying elements, Ti, Nb and V. (C) 2003 Kluwer Academic Publishers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this article is to demonstrate that the apparent controversy between the infinitesimal deformation (ID) approach and the phenomenological theory of martensitic transformations (PTMTs) in predicting the crystallographic characteristics of a martensitic transformation is entirely based on unjustified approximations associated with the way in which the ID calculations are performed. When applied correctly, the ID approach is shown to be absolutely identical to the PTMT. Nevertheless, there may be some advantages in using the ID approach. In particular, it is somewhat simpler than the PTMT; it is based on a physical concept that is easier to understand and, most important, it may provide a tool for investigating some of the features of martensitic transformations that have eluded explanation via the PTMT.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A comparative study of the mechanical properties of 20 experimental alloys has been carried out. The effect of different contents of Si, Cu, Mg, Fe and Mn, as well as solidification rate, has been assessed using a strength-ductility chart and a quality index-strength chart developed for the alloys. The charts show that the strength generally increases and the ductility decreases with an increasing content of Cu and Mg. Increased Fe (at Fe/Mn ratio 0.5) dramatically lowers the ductility and strength of low Si alloys. Increased Si content generally increases the strength and the ductility. The increase in ductility with increased Si is particularly significant when the Fe content is high. The charts are used to show that the cracking of second phase particles imposes a limit to the maximum achievable strength by limiting the ductility of strong alloys. The (Cu + Mg) content (at.%), which determines the precipitation strengthening and the volume fraction of Cu-rich and Mg-rich intermetallics, can be used to select the alloys for given strength and ductility, provided the Fe content stays below the Si-dependent critical level for the formation of pre-eutectic alpha-phase particles or beta-phase plates.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Different amorphous structures have been induced in monocrystalline silicon by high pressure in indentation and polishing. Through the use of high-resolution transmission electron microscopy and nanodiffraction, it was found that the structures of amorphous silicon formed at slow and fast loading/unloading rates are dissimilar and inherit the nearest-neighbor distance of the crystal in which they are formed. The results are in good agreement with recent theoretical predictions. (C) 2004 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The morphology and distribution of high-pressure metastable phases BC8 and R8, formed in monocrystalline silicon under microindentation, were identified and assessed using transmission electron microscopy nanodiffraction analysis. It was discovered that the crystal growth inside the transformation zone was stress-dependent with large crystals in its central region. The crystal size could also be increased using higher maximum indentation loads. The BC8 and R8 phases distributed unevenly across the transformation zone, with BC8 crystals mainly in the center of the zone and smaller R8 fragments in the peripheral regions. Such phase distribution was in agreement with the theoretical residual stress analysis.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The addition of 1 wt-%Sr to AE42 results in an improvement in the tensile strength of the alloy at elevated temperatures of 150 and 175degreesC and an improvement in the constant load creep properties at 175degreesC. The improved elevated temperature tensile and creep strength of the alloy can be attributed to the presence of a strontium-containing phase in the microstructure of the alloy along with an increase in the stability of the microstructure of the alloy at high temperatures. (C) 2004 W. S. Maney Son Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Multi-layer hydrogen storage thin films with Mg and MmNi(3.5)(CoAlMn)(1.5) (here Mm denotes La-rich mischmetal) as alternative layers were prepared by direct current magnetron sputtering. Transmission electron microscopy investigation shows that the microstructure of the MmNi(3.5)(CoAlMn)(1.5) and Mg layers are significantly different although their deposition conditions are the same. The MmNi(3.5)(CoAlMn)(1.5) layer is composed of two regions: one is an amorphous region approximately 4 nm thick at the bottom of the layer and the other is a nanocrystalline region on top of the amorphous region. The Mg layer is also composed of two regions: one is a randomly orientated nanocrystalline region 50 nm thick at the bottom of the layer and the other is a columnar crystallite region on top of the nanocrystalline region. These Mg columnar crystallites have their [001] directions parallel to the growth direction and the average lateral size of these columnar crystallites is about 100 nm. A growth mechanism of the multi-layer thin films is discussed based on the experiment results. Wiley-Liss, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of increasing levels of silicon on the microstructure and creep properties of high-pressure die-cast Mg-Al-Si (AS) alloys has been investigated. The morphology of the Mg2Si phase in die-cast AS alloys was found to be a function of the silicon content. The Mg2Si particles in castings with up to 1.14 wt pct Si have a Chinese script morphology. For AS21 alloys with silicon contents greater than 1.4 wt pet Si (greater than the alpha-Mg2Si binary eutectic point), some Mg2Si particles have a coarse blocky shape. Increasing the silicon content above the eutectic level results in an increase in the number of coarse faceted Mg2Si particles in the microstructure. Creep rates at 100 hours were found to decrease with increasing silicon content in AS-type alloys. The decrease in creep rate was most dramatic for silicon contents up to 1.1 wt pct. Further additions of silicon of up to 2.64 wt pct also resulted in significant decreases in creep rate.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The mesoporous nanoscale zircoina zeolite was firstly synthesized via solid state - Structure directing method without addition of any stabilizer. The sample bears lamellar or worm pore structures, relatively high surface area compared with that reported. The mesoporous nanosize structure can also resist higher calcination temperature. The introduction of above zirconia to the catalyst of methanol synthesis dedicates the nanosize particle size to the catalyst, which significantly changes the physical structure and electronic effect of the catalyst. The catalyst shows higher catalytic activity and selectivity to methanol. The active sites for methanol synthesis are demonstrated over various catalysts in this paper.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reviews the recent developments in the mechanics of superplasticity and its applications in industrial practice. After introducing the phenomena of superplasticity, the basic experiments for determining material deformation behavior and related parameters, and constructing superplastic constitutive equations, are reviewed. Finite element related formulations and techniques for simulating superplastic forming are discussed, together with some practical applications. (C) 2004 Elsevier B.V. All rights reserved.