917 resultados para Zumba Gold


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The first thiazolium gold(III) compound that qualifies as an ionic liquid has been prepared and crystallographically characterized. Hydration of phenylacetylene with this compound as catalyst precursor in ionic liquids indicates that gold(Ill)based ionic liquids could serve both as solvents and catalysts for organic transformations. The potential re-use of catalysts is an advantage achieved by recycling the ionic liquid phase. Various imidazolium-derived ionic liquids as well as the new thiazolium compound can be converted into gold carbene complexes by sequential deprotonation and coordination, opening the way for in situ catalyst tailoring. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The active site in supported gold catalysts for the carbonylation of methanol has been identified as dimers/trimers of gold which are formed from large gold particles >10 nm in diameter. Methyl iodide was found to be critical for this dispersion process and to maintain the catalyst in the active form. This study also shows that it may be possible to redisperse gold catalysts, in general, after reaction.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The reduction of oxygen was studied over a range of temperatures (298-318 K) in n-hexyltriethylammonium bis(trifluoromethanesulfonyl)imide, [N-6,N-2,N-2,N-2][NTf2], and 1-butyl-2,3-methylimidazolium bis(trifluoromethanesulfonyl)imide, [C(4)dmim][NTf2] on both gold and platinum microdisk electrodes, and the mechanism and electrode kinetics of the reaction investigated. Three different models were used to simulate the CVs, based on a simple electron transfer ('E'), an electron transfer coupled with a reversible homogeneous chemical step ('ECrev') and an electron transfer followed by adsorption of the reduction product ('EC(ads)'), and where appropriate, best fit parameters deduced, including the heterogeneous rate constant, formal electrode potential, transfer coefficient, and homogeneous rate constants for the ECrev mechanism, and adsorption/desorption rate constants for the EC(ads) mechanism. It was concluded from the good simulation fits on gold that a simple E process operates for the reduction of oxygen in [N-6,N-2,N-2,N-2][NTf2], and an ECrev process for [C(4)dmim][NTf2], with the chemical step involving the reversible formation of the O-2(center dot-)center dot center dot center dot [C(4)dmim](+) ion-pair. The E mechanism was found to loosely describe the reduction of oxygen in [N-6,N-2,N-2,N-2][NTf2] on platinum as the simulation fits were reasonable although not perfect, especially for the reverse wave. The electrochemical kinetics are slower on Pt, and observed broadening of the oxidation peak is likely due to the adsorption of superoxide on the electrode surface in a process more complex than simple Langmuirian. In [C(4)dmim][NTf2] the O-2(center dot-) predominantly ion-pairs with the solvent rather than adsorbs on the surface, and an ECrev quantitatively describes the reduction of oxygen on Pt also.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Isolated cationic gold deposited on sulfated lanthanum oxide has been shown to exhibit remarkable stability opening a promising way of stabilising ionic gold for catalytic reactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ionic liquid stabilized gold(III) chloride is shown to be a very active catalyst in the cyclization of sterically hindered and unhindered acetylenic carboxylic acid substrates even in the absence of a base.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

[AuAg3(C6F5)(CF3CO2)(3)(CH2PPh3)](n) (2) was prepared by reaction of [Au(C6F5)(CH2PPh3)] (1) and [Ag(CF3CO2)] (1:3). The crystal structures of complexes I and 2 were determined by X-ray diffraction, and the latter shows a polymeric 2D arrangement built by Au - Ag, Ag - Ag, and Ag - O contacts. The metallophilic interactions observed in 2 in the solid state seem to be preserved in concentrated THF solutions, as suggested by EXAFS, pulsed-gradient spin-echo NMR, and photophysical studies, which showed that the structural motif [AuAg3(C6F5)(CF3CO2)(3)(CH2PPh3)] is maintained under such conditions. Time-dependent DFT calculations agree with the experimental photophysical energies and suggest a metal-to-ligand charge-transfer phosphorescence process. Ab initio calculations give an estimated interaction energy of around 60 kJ mol(-1) for each Au - Ag interaction.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Successive treatment of 9-(phenylethynyl)fluoren-9-ol (1a), with HBr, butyllithium and chlorodiphenylphosphine furnishes 3,3-(biphenyl-2,2'-diyl)-1-diphenylphosphino-1-phenylallene (5). Moreover, reaction of 1a directly with chlorodiphenylphosphine yields the corresponding allenylphosphine oxide (6). The allenylphosphine (5), and Fe-2(CO)(9) initially form the phosphine-Fe(CO)(4) complex, 11, which is very thermally sensitive and readily loses a carbonyl ligand. In the resulting phosphine-Fe(CO)(3) system, 12, the additional site at iron is coordinated by the allene double bond adjacent to phosphorus; the Fe(CO) 3 tripod in 12 exhibits restricted rotation on the NMR time-scale even at room temperature. The corresponding chromium complex, (5)-Cr(CO)5 (9), has also been prepared. The gold complexes (5)AuCl (13), and [(5)-Au(THT)](+) X-, where (THT) is tetrahydrothiophene, and X = PF6 (14a), or ClO4 (14b), are analogous to the known triphenylphosphine-gold complexes. In contrast, in the (arene)(allenylphosphine) RuCl2 system the allene double bond adjacent to phosphorus displaces a chloride, and the resulting cationic species undergoes nucleophilic attack by water yielding ultimately a five-membered Ru-P-C=C-O ruthenacycle (17). Thus, the allenylphosphine (5), reacts initially as a conventional mono-phosphine but, when the metal centre has a readily displaceable ligand such as a carbonyl or halide, the allene double bond adjacent to the phosphorus can also function as a donor. X- ray crystal structures are reported for 5, 6, 11, 12, 13, 14a, 14b and 17.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The results of an investigation into the damage caused to dry plasmid DNA after irradiation by fast (keV) hydrogen atoms are presented. Agarose gel electrophoresis was used to assess single and double strand break yields as a function of dose in dry DNA samples deposited on a mica substrate. Damage levels were observed to increase with beam energy. Strand break yields demonstrated a considerable dependence on sample structure and the method of sample preparation. Additionally, the effect of high-Z nanoparticles on damage levels was investigated by irradiating DNA samples containing controlled amounts of gold nanoparticles. In contrast to previous (photonic) studies, no enhancement of strand break yields was observed with the particles showing a slight radioprotective effect. A model of DNA damage as a function of dose has been constructed in terms of the probability for the creation of single and double strand breaks, per unit ion flux. This model provides quantitative conclusions about the effects of both gold nanoparticles and the different buffers used in performing the assays and, in addition, infers the proportion of multiply damaged fragments.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The title compound, [Au-III(C9H10NO2)(2)][(AuCl4)-Cl-III], contains [Au-III(C9H10NO2)(2)](+) cations and [(AuCl4)-Cl-III](-) anions with each of the gold(III) ions in a typical four-coordinate square-planar geometry. Both gold(III) metal centers are located on inversion centers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Scanning tunnelling microscope (STM) tip-induced light emission from Au and Ag has been studied. Thin film samples similar to100nm thick were prepared by thermal evaporation at 0.5nm/s onto a room-temperature glass substrate to produce grains of 20-50nm in lateral dimension at the surface. Light emission from the samples in the STM was quasi-simultaneously recorded with the topography, at 1.8V tip bias and 3-40nA current, alternating pixel by pixel at the same bias. Typically, a surface scan range of 150 nm x 150 nm was surveyed. Au, W and PtIr tips were used.