922 resultados para InAlAs wetting layer


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Aim: The aim of the present study was to compare the removal of the smear layer and exposure of collagen fibers of the root surface following the application of five citric acid solution concentrations. Methods and Materials: Two hundred seventy (270) samples were equally divided into six groups (n=45) for treatment with saline solution (control) and five different concentrations of citric acid (0.5, 1, 2, 15, and 25 percent). Three acid application methods were used (passive, brushing, and burnishing) as well as three application periods (1, 2, and 3 minutes). A previously trained, calibrated (kappa score = 0.93), and blind examiner subsequently scored scanning electron micrographs (SEMs) of the samples. Statistical analyses were performed by using Kruskal-Wallis and Dunn's post-hoc tests. Results: According to the results obtained and within the limitations of the methodology used, the citric acid applications were more effective than the control treatment of applying saline solution (p<0.05). However, no statistically significant differences were observed among the three application methods and three application periods. Descriptive analyses showed that best results for exposure of collagen fibers were obtained with the application of citric acid at 25 percent by brushing for 1 or 3 minutes. Conclusions: The best results for exposure of collagen fibers in this study were obtained with application of citric acid at 25 percent by brushing for 1 or 3 minutes, even though there were no statistically significant differences among the groups. Clinical Significance: The best results for exposure of collagen fibers on root surfaces noted in this study were obtained with application of citric acid at 25 percent by brushing for 1 or 3 minutes. © 2010 Seer Publishing LLC.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of this study was to evaluate the use of a two-step total etch and rinse adhesive, the correlation between the hyybrid layer thickness (HL) and bond strength (BS), and between resin tag length (RT) and bond strength in the same teeth, and also to evaluate the fracture patterns of the tested specimens. Ten human molars were used for the restorative procedure and then sectioned in two halves (mesio-distally). The materials used were Adper Single Bond 2, 3M ESPE, Ultra etch gel, Ultradent and Filtek Z250, 3M ESPE. One half were utilized to measure the HL thickness and RT length through light microscopy analysis (400x), and the other half was subject to a microtensile test to measure the BS. The fractured surfaces were analyzed by scanning electron microscopy and fracture patterns classified. The Pearson correlation test was applied (p = 0.05). The results of the analyses of each specimen then were correlated: mean HL thickness = 4.39 (0.48) microm, mean length of RT = 9.94 (1.69) microm, mean BS = 23.98 (10.24) MPa. A statistically significant correlation between HL thickness and bond strength was found (r = 0.93). The two step etch and rinse adhesive system, showed a strong correlation between HL thickness and bond strength. The most common fractures were adhesive, followed by cohesive in resin.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the correlation between the hybrid layer thickness/resin tag length and the microtensile bond strength of conventional two-step adhesive system, when applied to healthy dentinal tissue. After performing the restorative adhesive procedures and tooth extractions, ten specimens were sectioned in the mesiodistal direction. One section was used for microscopic analysis of the resin tag lengths and the hybrid layer thickness, while the other was used for the microtensile bond strength test (0.5 mm/min). The fractured surface was classified according to the fracture pattern, under a stereoscopic microscope at 40x magnification. Data obtained were submitted to analysis using one-way ANOVA and Pearson's Correlation test (alpha=0.05). The means corresponding to the hybrid layer thickness, resin tag lengths and the microtensile test were 2.68 microm, 6.43 microm and 16.23 MPa, respectively. There was no correlation between the means of the values obtained for the microtensile test, and those presented by the hybrid layer (r2=0.40, p>0.05) and resin tags (r2=0.21, p>0.05). The microtensile bond strength of the conventional two-step adhesive system Adper Single Bond 2 did not depend on the thickness of the hybrid layer and length of resin tags.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Although in vitro studies have shown encouraging results for root surface conditioning with demineralizing agents, in vivo studies have failed to show its benefits in periodontal healing. This can be attributed to several factors, among which, the hypermineralization of dental surface. Therefore, this in vitro study compared, using scanning electron microscopy (SEM), the effect of root surface conditioning with different conditioners (1% and 25% citric acid, 24% EDTA and 50 mg/mL tetracycline hydrochloride) in impacted teeth and in teeth that had their roots exposed to the oral environment. One trained examiner assessed the SEM micrographs using a root surface modification index. There was a tendency of more root surface modification in the group of impacted teeth, suggesting that the degree of root mineralization influences its chemical demineralization.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Influence of cutting instruments and The aim of this study was to analyze the hybrid layer in noncarious dentin prepared by different cutting instruments and restored with composite resin. The cavities were randomly prepared in 40 specimens using a high-speed diamond bur (KG Sorensen 1013) and an ultrasonic tip (CVDentus C22). The cavities were restored with composite resin by varying the adhesive system between the Adper™ Single Bond (2 x 1 system, primer+adhesive) and the Prompt L-Pop™ (3 x 1 system, self-etching). The restorations were hemisected longitudinally and analyzed in the SEM (Scanning electron microscopy) in order to evaluate the hybrid layer and resinous tags characteristics, using scores ranging from 1 to 6. The Pearson test revealed a high correlation coefficient and good significance levels for both intra- and inter-raters values (r=0.90). The data were statistically analyzed using the Mann-Whitney test (P≤0.05). A larger proportion of regular hybrid layers with numerous tags were observed in the dentin prepared using the high-speed diamond burs and restored with a 2 × 1 adhesive system. Alternatively, the 3 × 1 adhesive system promoted the generation of a thin hybrid layer with few tags. After preparation using an ultrasonic tip revealed few or no tags after the preparation and 2 × 1 or 3 × 1 adhesive system application. The high-speed diamond burs produced a dentin surface that was more favorable to restorative material adhesion than the ultrasonic tips, regardless of the adhesive system used.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the correlation between the hybrid layer thickness, resin tag length and resin bond strength of a self-etching adhesive system to sound dentin tissue in vivo. After performing restorative procedures and tooth extractions, ten specimens were sectioned in a mesiodistal direction. One dental section was used for light microscope analysis, in which both the resin tag length and hybrid layer thickness were measured, while the other section was analyzed using a microtensile test (0.5 mm/min). The fractured surface of the latter section was characterized using a stereoscopic magnifying glass (40x magnifcation). The results were subject to statistical analysis using the Pearson Correlation Test (a = 0.05). The hybrid layer thickness, resin tag length and resin bond strength mean values were 2.19 microm (0.34), 4.34 microm (0.28) and 9.73 MPa (5,55), respectively. In addition, correlation tests between the resin tag length and the resin bond strength (r=0.014) and also between the hybrid layer thickness and bond strength (r=0.43), showed no statistically significant correlation. The microtensile bond strength of Adper Prompt L Pop self-etching adhesive system does not depend on hybrid layer thickness or resin tag length.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Cimetidine, histamine H2 receptors antagonist, has caused adverse effects on the male hormones and reproductive tract due to its antiandrogenic effect. In the testes, peritubular myoid cells and muscle vascular cells death has been associated to seminiferous tubules and testicular microvascularization damages, respectively. Either androgen or histamine H2 receptors have been detected in the mucosa and smooth muscular layer of vas deferens. Thus, the effect of cimetidine on this androgen and histamine-dependent muscular duct was morphologically evaluated.Methods: The animals from cimetidine group (CMTG; n=5) received intraperitoneal injections of 100 mg/kg b.w. of cimetidine for 50 days; the control group (CG) received saline solution. The distal portions of vas deferens were fixed in formaldehyde and embedded in paraffin. Massońs trichrome-stained sections were subjected to morphological and the following morphometrical analyzes: epithelial perimeter and area of the smooth muscular layer. TUNEL (Terminal deoxynucleotidyl-transferase mediated dUTP Nick End Labeling) method, NF-kB (nuclear factor kappa B) and AR (androgen receptors) immunohistochemical detection were also carried out. The birefringent collagen of the muscular layer was quantified in picrosirius red-stained sections under polarized light. The muscular layer was also evaluated under Transmission Electron Microscopy (TEM).Results: In CMTG, the mucosa of vas deferens was intensely folded; the epithelial cells showed numerous pyknotic nuclei and the epithelial perimeter and the area of the muscular layer decreased significantly. Numerous TUNEL-labeled nuclei were found either in the epithelial cells, mainly basal cells, or in the smooth muscle cells which also showed typical features of apoptosis under TEM. While an enhanced NF-kB immunoexpression was found in the cytoplasm of muscle cells, a weak AR immunolabeling was detected in these cells. In CMTG, no significant difference was observed in the birefringent collagen content of the muscular layer in comparison to CG.Conclusions: Cimetidine induces significant damages in the epithelium; a possible antiandrogenic effect on the basal cells turnover should be considered. The cimetidine-induced muscle cells apoptosis confirms the susceptibility of these cells to this drug. The parallelism between enhanced cytoplasmic NF-kB immunolabeling in the damaged muscular tissue and muscle cell apoptosis suggests that this drug may avoid the translocation of NF-kB to the nucleus and interfere in the control of NF-kB-mediated smooth muscle cell apoptosis. The decreased immunoexpression of ARs verified in the damaged muscular tissue reinforces this possibility. © 2013 Koshimizu et al.; licensee BioMed Central Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we demonstrate that the intrinsic electric field created by a poly(o-methoxyaniline) (POMA) cushion layer hinders the changes in molecular conformation of poly(p-phenylenevinylene) (PPV) in layer-by-layer with dodecylbenzene sulfonic acid (DBS). This was modeled with density functional theory (DFT) calculations where an energy barrier hampered molecular movements of PPV segments when they were subjected to an electric field comparable to that caused by a charged POMA layer. With restricted changes in molecular conformation, the PPV film exhibited Franck-Condon transitions and the photoexcitation spectra resembled the absorption spectra, in contrast to PPV/DBS films deposited directly on glass, with no POMA cushion. Other effects from the POMA cushion were the reduced number of structural defects, confirmed with Raman spectroscopy, and an enhanced PPV emission at high temperatures (300 K) in comparison with the films on bare glass. The positive effects from the POMA cushion may be exploited for enhanced opto-electronic devices, especially as the intrinsic electric field may assist in separating photoexcited electron-hole pairs in photovoltaic devices. © 2013 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of the present study was to evaluate the efficacy of QMiX, SmearClear, and 17% EDTA for the debris and smear layer removal from the root canal and its effects on the push-out bond strength of an epoxy-based sealer by scanning electron microscopy (SEM). Forty extracted human canines (n=10) were assigned to the following final rinse protocols: G1-distilled water (control), G2-17% EDTA, G3-SmearClear, and G4-QMiX. The specimens were submitted to a SEM analysis to evaluate the presence of debris and smear layer, respectively, in the apical or cervical segments. In sequence, forty extracted human maxillary canines with the root canals instrumented were divided into four groups (n=10) similar to the SEM analysis study. After the filling with AH Plus, the roots were transversally sectioned to obtain dentinal slices. The specimens were submitted to a push-out bond strength test using an electromechanical testing machine. The statistical analysis for the SEM and push-out bond strength studies were performed using the Kruskal-Wallis and Dunn tests (α=5%). There was no difference among the G2, G3, and G4 efficacy in removing the debris and smear layer (P>0.05). The efficacy of these groups was superior to the control group. The push-out bond strength values of G2, G3, and G4 were superior to the control group. The ability to remove the debris and smear layer by SmearClear and QMiX was as effective as the 17% EDTA. The final rinse with these solutions promoted similar push-out bond strength values. © 2013 Wiley Periodicals, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By combining galvanic displacement and electrodeposition techniques, an ordered Fe20Rh80 structure deposited onto brass was investigated by X-ray diffractometry, Mössbauer spectroscopy and magnetization measurements. Mössbauer and X-ray diffraction analyses suggest that the Fe-Rh alloy directly electrodeposited onto brass displays a nanocrystalline state while a similar alloy deposited onto Ag/brass shows a faced centered cubic-like structure, with dendrites-like features. These results directly indicate that the presence of Ag seed layer is responsible for the Fe-Rh alloy crystallization process. In addition, room temperature Mössbauer data indicate firstly paramagnetic states for two Fe-species. In the dominant Fe-species (major fraction of the Mössbauer spectra), Fe atoms are situated at a cubic environment and it can be attributed to the γ-Fe20Rh80 alloy based on their hyperfine parameters. In the second species, Fe atoms are placed in a non-local symmetry, which can be related to Fe atoms at the grain boundaries or/and Fe small clusters. These Fe-clusters are in superparamagnetic state at room temperature, but they may be ordered below 45 K, as suggested by magnetization data. © 2013 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The control of molecular architectures has been exploited in layer-by-layer (LbL) films deposited on Au interdigitated electrodes, thus forming an electronic tongue (e-tongue) system that reached an unprecedented high sensitivity (down to 10-12 M) in detecting catechol. Such high sensitivity was made possible upon using units containing the enzyme tyrosinase, which interacted specifically with catechol, and by processing impedance spectroscopy data with information visualization methods. These latter methods, including the parallel coordinates technique, were also useful for identifying the major contributors to the high distinguishing ability toward catechol. Among several film architectures tested, the most efficient had a tyrosinase layer deposited atop LbL films of alternating layers of dioctadecyldimethylammonium bromide (DODAB) and 1,2-dipalmitoyl-sn-3-glycero-fosfo-rac-(1-glycerol) (DPPG), viz., (DODAB/DPPG)5/DODAB/Tyr. The latter represents a more suitable medium for immobilizing tyrosinase when compared to conventional polyelectrolytes. Furthermore, the distinction was more effective at low frequencies where double-layer effects on the film/liquid sample dominate the electrical response. Because the optimization of film architectures based on information visualization is completely generic, the approach presented here may be extended to designing architectures for other types of applications in addition to sensing and biosensing. © 2013 American Chemical Society.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Structural, microstructural and ferroelectric properties of Pb0.90Ca0.10TiO3 (PCT10) thin films deposited using La0.50Sr0.50CoO3 (LSCO) thin films which serve only as a buffer layer were compared with properties of the thin films grown using a platinum-coated silicon substrate. LSCO and PCT10 thin films were grown using the chemical solution deposition method and heat-treated in an oxygen atmosphere at 700 °C and 650 °C in a tube oven, respectively. X-ray diffraction (XRD) and Raman spectroscopy results showed that PCT10 thin films deposited directly on a platinum-coated silicon substrate exhibit a strong tetragonal character while thin films with the LSCO buffer layer displayed a smaller tetragonal character. Surface morphology observations by atomic force microscopy (AFM) revealed that PCT10 thin films with a LSCO buffer layer had a smoother surface and smaller grain size compared with thin films grown on a platinum-coated silicon substrate. Additionally, the capacitance versus voltage curves and hysteresis loop measurement indicated that the degree of polarization decreased for PCT10 thin films on a LSCO buffer layer compared with PCT10 thin films deposited directly on a platinum-coated silicon substrate. This phenomenon can be described as the smaller shift off-center of Ti atoms along the c-direction 〈001〉 inside the TiO6 octahedron unit due to the reduction of lattice parameters. Remnant polarization (P r ) values are about 30 μC/cm2 and 12 μC/cm2 for PCT10/Pt and PCT10/LSCO thin films, respectively. Results showed that the LSCO buffer layer strongly influenced the structural, microstructural and ferroelectric properties of PCT10 thin films. © 2013 Elsevier Ltd and Techna Group S.r.l.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this report, hierarchical ZnO nano- and microstructures were directly grown for the first time on a bacterial cellulose substrate and on two additional different papers by hydrothermal synthesis without any surface modification layer. Compactness and smoothness of the substrates are two important parameters that allow the growth of oriented structures. © 2013 The Royal Society of Chemistry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Alumina thin films have been obtained by resistive evaporation of Al layer, followed by thermal oxidation by means of annealing in appropriate atmosphere (air or O2-rich), with variation of annealing time and temperature. Optical and structural properties of the investigated films reveal that the temperature of 550 °C is responsible for reasonable oxidation, which is accelerated up to 8 times for O2-rich atmosphere. Results of surface electrical resistivity and Raman spectroscopy are in good agreement with these findings. Surprisingly, X-ray and Raman data suggest also the crystallization of Si nuclei at glass substrate-alumina interface, which would come from the soda-lime glass used as substrate. © 2013 Elsevier Ltd and Techna Group S.r.l.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)