913 resultados para FUNCTIONALIZED OLIGOANILINES
Resumo:
Ternary europium complex Eu(tta)(3)phen was covalently bonded with the general mesoporous. material SBA-15 and SBA-15-type of periodic mesoporous organosilica (PMO) material via impregnation of Eu(tta)(3)center dot 2H(2)O into phen-S15 and phen-PMO, respectively, through a ligand exchange reaction. The parent materials of phen-S15 and phen-PMO were synthesized by co-condensation of tetraethylorthosilicate (TEOS) or 1,2-bis(triethoxysilyl)ethane (BTESE) and the functionalized chelate ligand 5-(N,N-bis(3-triethoxysilyl)propyl)ureyl-1,10-phenanthroline (phen-Si) in the presence of Pluronic P123 surfactant as template, which were confirmed by SEM, XRD, FTIR, Si-29 CP-MAS NMR, and N-2 adsorption measurements.
Resumo:
Two beta-diketones 4,4,4-trifluoro-1-2-thenoyl-1,3-butanedione (Htta) and 4,4,4-trifluoro-1-(2-naphthyl)-1,3-butanedione (Htfnb), which contain trifluoroalkyl chain, were selected as the main sensitizer for synthesizing Tm(L)(3)phen (L = tta, tfnb) complexes. The two near-infrared (NIR) luminescent thulium complexes have been covalently bonded to the ordered mesoporous material MCM-41 via a functionalized 1,10-phenanthroline (phen) group 5-(N,N-bis-3-(triethoxysilyl)propyl)ureyl-1,10-phenanthroline (phen-Si) [The resultant mesoporous materials are denoted as Tm(L)(3)phen-MCM-41 (L = tta, tfnb)]. The Tm(L)(3)phen-MCM-41 (L = tta, tfnb) mesoporous materials were characterized by small-angle Xray diffraction (XRD) and N-2 adsorption/desorption, and they show characteristic mesoporous structure of MCM-41.
Resumo:
A novel periodic mesoporous organosilica (PMO) material was synthesized through one-step co-condensation of 1,2-bis(triethoxysilyl)ethane (BTESE) and benzoic acid-functionalized organosilane (BA-Si) using cetyltrimethylammonium bromide (CTAB) as a structure-directing agent under basic conditions. The materials were fully characterized by FTIR, XRD, N-2 adsorption-desorption isotherms and FESEM. FTIR spectra proved that BA-Si was successfully incorporated into the PMO materials (PMOs) via benzyl group as a linker. XRD and N-2 adsorption-desorption isotherms revealed the characteristic mesoporous structure with highly uniform pore size distributions. FESEM confirmed that the morphology of the PMOs was significantly dependent cri the molar ratio of two organosilica precursors.
Resumo:
We report a facile method to create the chemically converted graphene oxide/epoxy resin nanocomposites from graphene oxide sheets through two-phase extraction. Great improvements in mechanical properties such as compressive failure strength and toughness have been achieved for the chemically converted graphene oxide/epoxy resin for a 0.0375 wt% loading of chemically converted graphene oxide sheets in epoxy resin by 48.3% and 1185.2%, respectively. In addition, the loading of graphene is also conveniently tunable even to 0.15 wt% just by increasing the volume of the graphene oxide dispersion.
Resumo:
A facile method to obtain polydisperse chemically-converted graphene sheets that are covalently functionalized with ionic liquid was reported-the resulting graphene sheets, without any assistance from polymeric or surfactant stabilizers, can be stably dispersed in water, DMF, and DMSO.
Resumo:
Chemically converted graphene (CCG)/3,4,9,10-perylene tetracarboxylic acid (PTCA)/Au-ionic liquid (Au-IL) composites (CCG/PTCA/Au-IL) have been prepared by a chemical route that involves functionalization of CCG with PTCA followed by deposition of Au-IL. Transmission electron microscopy revealed well-distributed Au with a high surface coverage. The identity of the hybrid material was confirmed through X-ray diffraction and X-ray photoelectron spectroscopy. The CCG/PTCA/Au-IL composites exhibited good electrocatalytic behavior toward oxygen reduction. The results indicate that modification of CCG with Au-IL could play an important role in increasing the electrocatalytic activity of CCG.
Resumo:
Polydisperse, functionalized, chemically converted graphene (f-CCG) nanosheets, which can be homogeneously distributed into water, ethanol, DMF, DMSO and 3-aminopropyltriethoxysilane (APTS), were obtained via facile covalent functionalization with APTS. The resulting f-CCG nanosheets were characterized by FTIR, XPS, TGA, EDX, AFM, SEM, and TEM. Furthermore, the f-CCG nanosheets as reinforcing components were extended into silica monoliths. Compressive tests revealed that the compressive failure strength and the toughness of f-CCG-reinforced APTS monoliths at 0.1 wt% functionalized, chemically converted graphene sheets compared with the neat APTS monolith were greatly improved by 19.9% and 92%, respectively.
Resumo:
We first reported that polyvinylpyrrolidone-protected graphene was dispersed well in water and had good electrochemical reduction toward O-2 and H2O2. With glucose oxidase (GOD) as an enzyme model, we constructed a novel polyvinylpyrrolidone-proteeted graphene/polyethylenimine-ftmctionalized ionic liquid/GOD electrochemical biosensor, which achieved the direct electron transfer of GOD, maintained its bioactivity and showed potential application for the fabrication of novel glucose biosensors with linear glucose response up to 14 mM.
Resumo:
In this paper, hydrothermal synthesized Fe3O4 microspheres have been encapsulated with nonporous silica and a further layer of ordered mesoporous silica through a simple sol-gel process. The surface of the outer silica shell was further functionalized by the deposition of YVO4:Eu3+ phosphors, realizing a sandwich structured material with mesoporous, magnetic and luminescent properties. The multifunctional system was used as drug carrier to investigate the storage and release properties using ibuprofen (IBU) as model drug by the surface modification. X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray photoelectron spectra (XPS), Fourier transform infrared spectroscopy (FT-IR), N-2 adsorption/desorption, photoluminescence (PL) spectra, and superconducting quantum interference device (SQUID) were used to characterized the samples.
Resumo:
Magnetically functionalized mesoporous silica spheres with different size (average diameter, A.D.) from 150 nm to 2 mu m and pore size distribution were synthesized by generating magnetic FexOy nanoparticles onto the mesoporous silica hosts using the sol-gel method. The X-ray diffraction (XRD), field emission scanning electron microscope (FESEM), N-2 adsorption/desorption results show that these composites conserved regular sphere morphology and ordered mesoporous structure after the formation of FexOy nanoparticles. XRD and X-ray photoelectron spectroscopy (XPS) analysis confirmed that the FexOy generated in these mesoporous silica hosts is mainly composed of gamma-Fe2O3. Magnetic measurements reveal that these composites with different gamma-Fe2O3 loading amounts possess super-paramagnetic properties at 300 K, and the saturation magnetization increases with increasing Fe ratio loaded.
Resumo:
NaYF4:Yb3+, Er3+ nanoparticles were successfully prepared by a polyol process using diethyleneglycol (DEG) as solvent. After being functionalized with SiO2-NH2 layer, these NaYF4:Yb3+, Er3+ nanoparticles can conjugate with activated avidin molecules (activated by the oxidation of the oligosaccharide chain). The as-formed NaYF4:Yb3+, Er3+ nanoparticles, NaYF4:Yb3+, Er3+ nanoparticles functionalized with amino groups, avidin conjugated amino-functionalized NaYF4:Yb3+, Er3+ nanoparticles were characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), atomic force microscopy (AFM), Fourier transform infrared (FT-IR), UV/Vis absorption spectra, and up-conversion luminescence spectra, respectively. The biofunctionalization of the NaYF4:Yb3+, Er3+ nanoparticles has less effect on their luminescence properties, i.e., they still show the up-conversion emission (from Er3+, with S-4(3/2) -> I-4(15/2) at similar to 540 nm and F-4(9/2) -> I-4(15/2) at similar to 653 nm), indicative of the great potential for these NaYF4:Yb3+, Er3+ nanoparticles to be used as fluorescence probes for biological system.
Resumo:
Styrene-b-(ethylene-co-1-butene)-b-styrene (SEBS) triblock copolymer functionalized with epsilon-caprolactam blocked allyl (3-isocyanate-4-tolyl) carbamate (SEBS-g-BTAI) was used to toughen polyamide 6 (PA6) via reactive blending. Compared to the PA6/SEBS blends, mechanical properties such as tensile strength, Young's modulus, especially Izod notched strength of PA6/SEBS-g-BTAI blends were improved distinctly. Both theological and FTIR results indicated a new copolymer formed by the reaction of end groups of PA6 and isocyanate group regenerated in the backbone of SEBS-g-BTAI. Smaller dispersed particle sizes with narrower distribution were found in PA6/SEBS-g-BTAI blends, via field emitted scanning electron microscopy (FESEM). The core-shell structures with PS core and PEB shell were also observed in the PA6/SEBS-g-BTAI blends via transmission electron microscopy (TEM), which might improve the toughening ability of the rubber particles.
Resumo:
The epsilon-caprolactam was used to block the isocyanate group to enhance the storage stability of allyl (3-isocyanate-4-tolyl) carbamate. The spectra of FTIR and NMR showed that blocked allyl (3-isocyanate-4-tolyl) carbamate (BTAI) possesses two chemical functions, an 1-olefin double bond and a blocked isocyanate group. The FTIR spectrum showed BTAI could regenerate isocyanate group at elevated temperature. DSC and TG/DTA indicated the minimal dissociation temperature was about 135 degrees C and the maximal dissociation rate appeared at 226 degrees C. Then the styrene-b-(ethylene-co-1-butene)-b-styrene triblock copolymer (SEBS) was functionalized by BTAI via melt free radical grafting. The effect of temperature, monomer and initiator concentrations on the grafting degree and grafting efficiency was evaluated. The highest grafting degree was obtained at 200 degrees C. The grafting degree and grafting efficiency increased with the enhanced concentration of BTAI or initiator.
Resumo:
Linear low density polyethylene (LLDPE) was functionalized with 2-acrylamido-2-methyl-1-propanesulfonic acid (AMPS) by using -ray pre-irradiation in air in a twin-screw extruder. Fourier-transformed infrared spectroscopy (FT-IR) and electron spectroscopy for chemical analysis (ESCA) were used to characterize the formation of LLDPE-g-AMPS copolymers. The content of AMPS in LLDPE-g-AMPS was determined by using element analysis instrument. The effects of concentrations of monomer, reaction temperature and pre-irradiation dose on degree of grafting were investigated. The critical surface tension of LLDPE-g-AMPS was measured by using contact angle method. The influences of the degree of grafting on crystallization properties were studied by using DSC. Compared with neat LLDPE, the crystallization temperature increased about 4C, and crystallinity decreased with increasing degree of grafting. Crystallization rates of grafted LLDPE were faster than that of plain LLDPE at the same crystallization temperature.