989 resultados para ER-YAG LASERS


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tm:YAG晶体是性能优异的LD泵浦激光晶体。本文总结了Tm:YAG晶体的生长、光谱性质以及激光性能的研究和发展,并指出了Tm:YAG晶体发展中需要解决的问题。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

本试验测试了Er^3+掺杂钨酸铅晶体(PbWO4:Er^3+)的吸收光谱,依据J-O理论,首次计算报道了光谱项特征:J-O强度参数、量子荧光效率、荧光分支比等,Ω2=3.75×10^-20cm^2,Ω4=0.67×10^-20cm^2,Ω6=0.41×10^-20cm^2。计算证实,PWO:Er^3+中几乎有80%的激发能量非辐射跃迁转移致^4I13/2能级,^4I13/2的计算寿命是5200μs,J-O计算显示,在PWO中产生^4I13/2→^4I15/2和发射1.53μm.有高的几率。讨论了不同浓度E

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A finite-element model is employed to analysis the thermal environments in Temperature Gradient Technique (TGT) furnace during the growth of large-sized Nd:YAG crystal. The obtained results show that when the crucible is located at the lower position inside of the heater, a flatter solid-liquid interface is established, which makes it easier to obtain the core-free Nd:YAG crystal. Meanwhile, the lower crucible position can induce higher axial temperature gradient, which is beneficial to the release of latent heat. (c) 2007 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent polycrystalline Nd:YAG ceramics were fabricated by solid-state reactive sintering a mixture of commercial Al2O3,Y2O3, and Nd2O3 powders. The powders were mixed in ethanol and doped with 0.5 wt% tetraethoxysilane, dried, and pressed. Pressed samples were sintered at 1750 degrees C in vacuum. Transparent fully dense samples with average grain sizes of 10 mu m were obtained. The 1 at.% Nd:YAG ceramic was used to research passively Q-switched laser output with a Cr4+:YAG crystal as a saturable absorber. An average output power of 94 mW with a pulse width of 50 ns was obtained when the incident pump power was 750 mW. The slope efficiency was 13%. The pulse energy is 5 mu J, and the peak power is about 100 W.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent polycrystalline Yb:YAG ceramics were fabricated by solid-state reactive sintering a mixture of commercial Al2O3, Y2O3, and Yb2O3 powders. The powders were mixed in ethanol and doped with 0.5 wt% tetraethoxysilane, dried, and pressed. Pressed samples were sintered at 1730 degrees C in vacuum. Transparent fully dense samples with grain sizes of several micrometers were obtained. The phase from 1500 degrees to 1700 degrees C was important for the grain growth, in which the grains grew quickly and a mass of pores were eliminated from the body of the sample. Annealing was an important step to remove the vacancies of oxygen and transform Yb2+ to Yb3+. The 1 at.% Yb:YAG ceramic sample was pumped by a diode laser to study the laser properties. The maximum output power of 1.02 W was obtained with a slope efficiency of 25% at 1030 nm. The size of the lasering sample was 4 mm x 4 mm x 3 mm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Gamma-rays radiation effects on Ce:YAG crystals grown by Czochralski (Cz) and temperature gradient techniques (TGT) have been studied by means of optical absorption and luminescence spectra. Valence of Ce3+ ion changes during the gamma-ray irradiation process and this result indicates Ce4+ ion may exist in both Cz-Ce:YAG and TGT-Ce:YAG crystals. Thermally stimulated luminescence measurements reveal intense thermoluminescence peaks in gamma-irradiated Ce:YAG crystals and trap parameters were calculated by general-order kinetics expression. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

制备了高质量的Yb:YAG透明陶瓷.Yb:YAG透明陶瓷的晶粒尺寸为10μm左右且分布均匀,晶界处和晶粒中没有杂质、气孔的存在.Yb:YAG样品中所有元素分布均匀,不同的晶粒间,晶粒和晶界间成分是一致的,没有出现成分的偏析.4mm厚样品的透过率为80%.LD泵浦获得了波长为1030nm,最大功率为268mW的连续激光输出.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

用温度梯度法生长了直径为75mm大尺寸的Nd:YAG激光晶体,通过退火排除了生长过程中进入晶体的碳原子.用正交偏光显微镜观察了晶体的核心分布以及生长条纹.测试了室温下的吸收谱并利用吸收谱研究了Nd离子在YAG晶体中的分布.比较了温度梯度法与提拉法生长晶体的区别.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

YAG单晶是高功率激光的重要材料,近年来高透明度多晶陶瓷作为激光介质引起人们广泛的注意。YAG陶瓷相对单晶具有易制造大尺寸、掺杂浓度高、易批量生产等优点。在Nd:YAG陶瓷获得长足发展的同时,Yb掺杂的陶瓷也得到了越来越多的关注。Yb:YAG陶瓷与Nd:YAG陶瓷相比具有许多优点:Yb掺杂的激光介质无交叉弛豫振荡和激发态吸收,有较宽的吸收带,较长的荧光寿命及较高的量子效率等。因此,高质量的Yb:YAG陶瓷将是非常理想的高功率激光材料。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Single-frequency output power of 7.3 W at 2.09 mu m from a monolithic Ho:YAG nonplanar ring oscillator (NPRO) is demonstrated. Resonantly pumped by a Tm-doped fiber laser at 1.91 mu m, the Ho:YAG NPRO produces 71% of slope efficiency with respect to absorbed pump power and nearly diffraction-limited output with a beam quality parameter of M-2 approximate to 1.1. (c) 2008 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The YAG crystal codoped with Yb3+ and Tm3+ has been grown by Czochralski (Cz) method. The crystal structure of the crystal has been determined by X-ray diffraction analysis. The absorption and emission spectra of Yb,Tm:YAG crystal at room temperature have also been studied. The emission cross-sections have been calculated by Fuechtbauer-Ladenburg formula and reciprocity method. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report both continuous-wave and passively mode-locked laser actions in a Yb3+-doped gadolinium yttrium oxyorthosilicate Yb:GdySiO(5) (Yb:GYSO) crystal. Continuous-wave (CW) laser operations were compared under different pump conditions with high-power diodes of different wavelengths and fiber cores. CW mode-locking was obtained with a semiconductor saturable absorber mirror.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An Ho3+-doped YAlO3 (Ho : YAP) single crystal has been grown by the Czochralski technique. The polarized absorption spectra, polarized fluorescence spectra and fluorescence decay curve of the crystal are measured at room temperature. The spectroscopic parameters are calculated based on Judd-Ofelt theory, and the effective phenomenological intensity parameters Omega(2,eff), Omega(4,eff) and Omega(6,eff) are obtained to be 2.89 x 10(-20), 2.92 x 10(-20) and 1.32 x 10(-20) cm(2), respectively. The room-temperature fluorescence lifetime of the Ho3+ 5I(7) -> I-5(8) transition is measured to be 8.1 ms. Values of the absorption and emission cross-sections with different polarizations are presented for the I-5(7) manifold, and the polarized gain cross-section curves are also provided and discussed.