982 resultados para CO2 laser annealing
Resumo:
We demonstrate the launching of laser-cooled Yb atoms in a continuous atomic beam. The continuous cold beam has significant advantages over the more-common pulsed fountain, which was also demonstrated by us recently. The cold beam is formed in the following steps: i) atoms from a thermal beam are first Zeeman-slowed to a small final velocity; ii) the slowed atoms are captured in a two-dimensional magneto-optic trap (2D-MOT); and iii) atoms are launched continuously in the vertical direction using two sets of moving-molasses beams, inclined at +/- 15 degrees to the vertical. The cooling transition used is the strongly allowed S-1(0) -> P-1(1) transition at 399 nm. We capture about 7x10(6) atoms in the 2D-MOT, and then launch them with a vertical velocity of 13m/s at a longitudinal temperature of 125(6) mK. Copyright (C) EPLA, 2013
Resumo:
Thin films of NiTi were deposited by DC magnetron sputtering from an equiatomic alloy target (Ni/Ti: 50/50 at.%). The films were deposited without intentional heating of the substrates. The thickness of the deposited films was approximately 2 mu m. The structure and morphology of NiTi films annealed at different temperatures were analyzed in order to understand the effect of annealing on physical properties of the films. The compositional investigations of fresh and annealed films were also evaluated by energy dispersive X-ray spectroscopy (EDS) and X-ray photo-electron spectroscopy (XPS) techniques. X-ray diffraction (XRD) studies showed that as-deposited films were amorphous in nature whereas annealed films were found to poly-crystalline with the presence of Austenite phase as the dominant phase. AFM investigations showed higher grain size and surface roughness values in the annealed films. In annealed films, the grain size and film roughness values were increased from 10 to 85 nm and 2-18 nm. Film composition measured by EDS were found to 52.5 atomic percent of Ni and 47.5 atomic percent of Ti. XPS investigations, demonstrated the presence of Ni content on the surface of the films, in fresh films, whereas annealed films did not show any nickel. From HR-XPS investigations, it can be concluded that annealed NiTi films have higher tendency to form metal oxide (titanium dioxide) layer on the surface of the films than fresh NiTi films. (C) 2013 Elsevier B. V. All rights reserved.
Resumo:
Charnockite is considered to be generated either through the dehydration of granitic magma by CO2 purging or by solid-state dehydration through CO2 metasomatism during granulite facies metamorphism. To understand the extent of dehydration, CO2 migration is quantitatively modeled in silicate melt and metasomatic fluid as a function of temperature, H2O wt%, pressure, basal CO2 flux and dynamic viscosity. Numerical simulations show that CO2 advection through porous and permeable high-grade metamorphic rocks can generate dehydrated patches close to the CO2 flow path, as illustrated by the occurrences of ``incipient charnockites.'' CO2 reaction-front velocity constrained by field observations is 0.69 km/m.y., a reasonable value, which matches well with other studies. On the other hand, temperature, rate of cooling, and basal CO2 flux are the critical parameters affecting CO2 diffusion through a silicate melt. CO2 diffusion through silicate melt can only occur at temperature greater than 840 degrees C and during slow cooling (<= 3.7 x 10(-5) degrees C/yr), features that are typical of magma emplacement in the lower crust. Stalling of CO2 fluxing at similar to 840 degrees C explains why some deep-level plutons contain both hydrous and anhydrous (charnockitic) mineral assemblages. CO2 diffusion through silicate melt is virtually insensitive to pressure. Addition of CO2 basal flux facilitates episodic dehydrated melt migration by generating fracture pathways.
Resumo:
In this work, we synthesized bulk amorphous GeGaS glass by conventional melt quenching technique. Amorphous nature of the glass is confirmed using X-ray diffraction. We fabricated the channel waveguides on this glass using the ultrafast laser inscription technique. The waveguides are written on this glass 100 mu m below the surface of the glass with a separation of 50 ae m by focusing the laser beam into the material using 0.67 NA lens. The laser parameters are set to 350 fs pulse duration at 100 KHz repetition rate. A range of writing energies with translation speeds 1 mm/s, 2 mm/s, 3 mm/s and 4 mm/s were investigated. After fabrication the waveguides facets were ground and polished to the optical quality to remove any tapering of the waveguide close to the edges. We characterized the loss measurement by butt coupling method and the mode field image of the waveguides has been captured to compare with the mode field image of fibers. Also we compared the asymmetry in the shape of the waveguide and its photo structural change using Raman spectra.
Resumo:
We report here, a finite difference thermal diffusion (FDTD) model for controlling the cross-section and the guiding nature of the buried channel waveguides fabricated on GeGaS bulk glasses using the direct laser writing technique. Optimization of the laser parameters for guiding at wavelength 1550 nm is done experimentally and compared with the theoretical values estimated by FDTD model. The mode field diameter (MFD) between 5.294 mu m and 24.706 mu m were attained by suitable selection of writing speed (1mm/s to 4 mm/s) and pulse energy (623 nJ to 806 nJ) of the laser at a fixed repletion rate of 100 kHz. Transition from single-mode to multi-mode waveguide is observed at pulse energy 806nJ as a consequence of heat accumulation. The thermal diffusion model fits well for single-mode waveguides with the exception of multi-mode waveguides.
Resumo:
Many of the conducting polymers though having good material property are not solution processable. Hence an alternate method of fabrication of film by pulsed laser deposition, was explored in this work. PDTCPA, a donor-acceptor-donor type of polymer having absorption from 900 nm to 300 nm was deposited by both UV and IR laser to understand the effect of deposition parameters on the film quality. It was observed that the laser ablation of PDTCPA doesn't alter its chemical structure hence retaining the chemical integrity of the polymer. Microscopic studies of the ablated film shows that the IR laser ablated films were particulate in nature while UV laser ablated films are deposited as smooth continuous layer. The morphology of the film influences its electrical characteristics as current-voltage characteristic of these films shows that films deposited by UV laser are p rectifying while those by IR laser are more of resistor in nature.
Resumo:
Titanium dioxide (TiO2) thin films are deposited on unheated p-Si (100) and quartz substrates by employing DC reactive magnetron sputtering technique. The effect of post-deposition annealing in air at temperatures in the range 673-973 K on the structural, electrical, and dielectric properties of the films was investigated. The chemical composition of the TiO2 films was analyzed with X-ray photoelectron spectroscopy. The surface morphology of the films was studied by atomic force microscope. The optical band gap of the as-deposited film was 3.50 eV, and it increased to 3.55 eV with the increase in annealing temperature to 773 K. The films annealed at higher temperature of 973 K showed the optical band gap of 3.43 eV. Thin film capacitors were fabricated with the MOS configuration of Al/TiO2/p-Si. The leakage current density of the as-deposited films was 1.2 x 10(-6) A/cm(2), and it decreased to 5.9 x 10(-9) A/cm(2) with the increase in annealing temperature to 973 K. These films showed high dielectric constant value of 36. (C) 2013 Elsevier Ltd. All rights reserved.
Resumo:
In this paper we report the quantitative oxygen quenching effect on laser-induced fluorescence of acetone, methyl ethyl ketone, and 3-pentanone at low pressures (approximate to 700torr) with oxygen partial pressures up to 450torr. Nitrogen was used as a bath gas in which these molecular tracers were added in different quantities according to their vapor pressure at room temperature. These tracers were excited by using a frequency-quadrupled, Q-switched, Nd:YAG laser (266nm). Stern-Volmer plots were found to be linear for all the tracers, suggesting that quenching is collisional in nature. Stern-Volmer coefficients (k(sv)) and quenching rate constants (k(q)) were calculated from Stern-Volmer plots. The effects of oxygen on the laser-induced fluorescence of acetone, methyl ethyl ketone, and 3-pentanone were compared with each other. Further, the Smoluchowski theory was used to calculate the quenching parameters and compared with the experimental results.
Resumo:
Waveguides were fabricated on GeGaSEr chalcogenide glass using ultrafast laser inscription method. The thermal diffusion model is discussed for understanding the light matter interaction and shown the effect of net-fluence in waveguide formation on chalcogenide glass. (C) 2012 Optical Society of America
Resumo:
We report a simple method to fabricate multifunctional polyelectrolyte thin films to load and deliver the therapeutic drugs. The multilayer thin films were assembled by the electrostatic adsorption of poly (allylamine hydrochloride) (PAH) and dextran sulfate (DS). The silver nanoparticles (Ag NPs) biosynthesized from novel Hybanthus enneaspermus leaf extract as the reducing agent were successfully incorporated into the film. The biosynthesized Ag NPs showed excellent antimicrobial activity against the range of enteropathogens, which could be significantly enhanced when used with commercial antibiotics. The assembled silver nano composite multilayer films showed rupture and deformation when they are exposed to laser. The Ag NPs act as an energy absorption center, locally heat up the film and rupture it under laser treatment. The antibacterial drug, moxifloxacin hydrochloride (MH) was successfully loaded into the multilayer films. The total amount of MH release observed was about 63% which increased to 85% when subjected to laser light exposure. Thus, the polyelectrolyte thin film reported in our study has significant potential in the field of remote activated drug delivery, antibacterial coatings and wound dressings. (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
In the present work, we report spectroscopic studies of laser-induced plasmas produced by focusing the second harmonic (532nm) of a Nd:YAG laser onto the laminar flow of a liquid containing chromium. The plasma temperature is determined from the coupled Saha-Boltzmann plot and the electron density is evaluated from the Stark broadening of an ionic line of chromium Cr(II)] at 267.7nm. Our results reveal a decrease in plasma temperature with an increase in Cr concentration up to a certain concentration level; after that, it becomes approximately constant, while the electron density increases with an increase in analyte (Cr) concentration in liquid matrix.
Effect of low oxygen pressure on structural and magnetic properties of quenched SrFe12O19 thin films
Resumo:
Strontium hexaferrite thin films have been grown on glass substrates at room temperature in oxygen environment by pulsed laser deposition method. The effect of oxygen pressure (p(o2)) on the structural and magnetic properties has been investigated. The as-deposited films were found to be amorphous in nature. The crystallization of these films was achieved by annealing at a temperature of 850 A degrees C in air. The thickness of the film increased with p(o2). The film grown at p(o2) = 0.455 Pa had a clear hexagonal structure. The values of coercivity for the films were found to increase with p(o2).
Resumo:
The electrocaloric effect (ECE) of 0.85PbMg(1/3)Nb(2/3)O(3-)0.15PbTiO(3) (0.85PMN-0.15PT) thin films deposited on (111) Pt/TiO2/SiO2/Si substrate by pulsed laser deposition (PLD) has been calculated. The reversible adiabatic temperature was calculated indirectly using the Maxwell's relation Delta T = -T/C rho integral(E2)(E1) (partial derivative P/partial derivative T)(sigma,E)dE. Permittivity and P-E measurements show an anomaly at 11 degrees C on heating only. This anomaly previously reported are claimed to arise due to the PNR depolarization upon heating. The absence of this anomaly during cooling suggests that no structural phase transition takes place. A negative electrocaloric effect is observed which is explained by the increase in the entropy term.
Guided-wave-based damage detection in a composite T-joint using 3D scanning laser Doppler vibrometer
Resumo:
Composite T-joints are commonly used in modern composite airframe, pressure vessels and piping structures, mainly to increase the bending strength of the joint and prevents buckling of plates and shells, and in multi-cell thin-walled structures. Here we report a detailed study on the propagation of guided ultrasonic wave modes in a composite T-joint and their interactions with delamination in the co-cured co-bonded flange. A well designed guiding path is employed wherein the waves undergo a two step mode conversion process, one is due to the web and joint filler on the back face of the flange and the other is due to the delamination edges close to underneath the accessible surface of the flange. A 3D Laser Doppler Vibrometer is used to obtain the three components of surface displacements/velocities of the accessible face of the flange of the T-joint. The waves are launched by a piezo ceramic wafer bonded on to the back surface of the flange. What is novel in the proposed method is that the location of any change in material/geometric properties can be traced by computing a frequency domain power flow along a scan line. The scan line can be chosen over a grid either during scan or during post-processing of the scan data off-line. The proposed technique eliminates the necessity of baseline data and disassembly of structure for structural interrogation.
Resumo:
We report high aspect-ratio micromechanical structures made of SU-8 polymer, which is a negative photoresist. Mask-less direct writing with 405 nm laser is used to pattern spin-cast SU-8 films of thickness of more than 600 um. As compared with X-ray lithography, which helps pattern material to give aspect ratios of 1:50 or higher, laser writing is a less expensive and more accessible alternative. In this work, aspect ratios up to 1:30 were obtained on narrow pillars and cantilever structures. Deep vertical patterning was achieved in multiple exposures of the surface with varying dosages given at periodic intervals of sufficient duration. It was found that a time lag between successive exposures at the same location helps the material recover from the transient changes that occur during exposure to the laser. This gives vertical sidewalls to the resulting structures. The time-lags and dosages were determined by conducting several trials. The micromechanical structures obtained with laser writing are compared with those obtained with traditional UV lithography as well as e-beam lithography. Laser writing gives not only high aspect ratios but also narrow gaps whereas e-beam can only give narrow gaps over very small depths. Unlike traditional UV lithography, laser writing does not need a mask. Furthermore, there is no adjustment for varying the dosage in traditional UV lithography. A drawback of this method compared to UV lithography is that the writing time increases. Some test structures as well as a compliant microgripper are fabricated.