972 resultados para AG NANOPARTICLES


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Reports on the alloys formed from immiscible atoms when they are contained in a nano-sized system have initiated several research activities in the recent years. Bridging of the miscibility gap at nanoscale is significant as it has the potential to produce novel alloy materials with useful technological applications. Although the literature contains noticeable number of reports on the formation of solid solution between bulk immiscible atoms, several issues related to phase stability and microstructure remain unaddressed. This article discusses some of these issues using examples from the work done by the author's research group on isolated nanoparticles of bulk immiscible binary systems such as Ag-Ni, Ag-Fe and Ag-Co.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A zinc-nicotinate complex has been prepared by direct reaction of zinc acetate and nicotinic acid in the presence of template tetramethylethylenediamine and is characterized by elemental analysis, FTIR, and TGA/DTA. The Zn complex was a precursor for the synthesis of ZnO nanoparticles. A correlation of the thermal and spectral properties of the precursor complex with its structure has been discussed. Thermolysis under air was studied by thermogravimetry, and the resulting ZnO product was characterized by XRD and TEM, showing compact particles with a diameter of about 1750nm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have studied the preparation of zinc oxide nanoparticles loaded in various weight percentages in ortho-chloropolyaniline by in situ polymerization method. The length of the O-chloropolyaniline tube is found to be 200 nm and diameter is about 150 nm wherein the embedded ZnO nanoparticles is of 13 nm as confirmed from scanning electron microscopy as well as transmission electron microscopy characterizations. The presence of the vibration band of the metal oxide and other characteristic bands confirms that the polymer nanocomposites are characterized by their Fourier transmission infrared spectroscopy. The X-ray diffraction pattern of nanocomposites reveals their polycrystalline nature. Electrical property of nanocomposites is a function of the filler as well as the matrix. Cole-Cole plots reveal the presence of well-defined semicircular arcs at high frequencies which are attributed to the bulk resistance of the material. Among all nanocomposites, 30 wt% shows the low relaxation time of 151 s, and hence it has high conductivity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The growing commercial applications had brought aluminium oxide nanoparticles under,toxicologists' purview. In the present study, the cytotoxicity of two different sized aluminium oxide nanoparticles (ANP(1), mean hydrodynamic diameter 82.6 +/- 22 nm and ANP(2), mean hydrodynamic diameter 246.9 +/- 39 nm) towards freshwater algal isolate Chlorella ellipsoids at low exposure levels (<= 1 mu g/mL) using sterile lake water as the test medium was assessed. The dissolution of alumina nanoparticles and consequent contribution towards toxicity remained largely unexplored owing to its presumed insoluble nature. Herein, the leached Al3+ ion mediated toxicity has been studied along with direct particulate toxicity to bring out the dynamics of toxicity through colloidal stability, biochemical, spectroscopic and microscopic analyses. The mean hydrodynamic diameter increased with time both for ANP(1) 82.6 +/- 22 nm (0 h) to 246.3 +/- 59 nm (24h), to 1204 +/- 140 nm (72 h)] and ANP(2) 246.9 +/- 39 nm (Oh) to 368.28 +/- 48 nm (24 h), to 1225.96 +/- 186 nm (72 h)] signifying decreased relative abundance of submicron sized particles (<1000 nm). The detailed cytotoxicity assays showed a significant reduction in the viability dependent on dose and exposure. A significant increase in ROS and LDH levels were noted for both ANPs at 1 mu g/mL concentration. The zeta potential and FT-IR analyses suggested surface chemical interaction between nanoparticles and algal cells. The substantial morphological changes and cell wall damage were confirmed through microscopic analyses (SEM, TEM, and CLSM). At 72 h, significant Al3+ ion release in the test medium 0.092 mu g/mL for ANP(1), and 0.19 mu g/mL for ANP(2)] was noted, and the resulting suspension containing leached ions caused significant cytotoxicity, revealing a substantial ionic contribution. This study indicates that both the nano-size and ionic dissolution play a significant role in the cytotoxicity of ANPs towards freshwater algae, and the exposure period largely determines the prevalent mode of nano-toxicity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The impact of high enthalpy shock wave on graphitic carbon nanoparticle (GCNP) films has been investigated and discussed in view of space and chemical engineering applications. The GCNP films were developed by using spray method and exposed to high enthalpy shock wave under an inert atmosphere. Upon shock wave treatment, two typical amendments such as weight loss in the deposited material and growth of second order nanostructures (SONS) have been observed. While increasing test gas pressure, the loss of material and density of SONs are gradually increased. Most of the shock wave induced SONS are highly crystalline and belong to the cubic diamond structure. Upon shock treatment as well as with increase of test gas pressure, a considerable improvement in the quality of GCNP films has been observed. Further, ablation of GCNPs exclusively on the top surface of the coatings and formation of hierarchical NPs (diamond NPs on GCNPs) has been observed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

CoFe2O4 nanoparticles were prepared by solution combustion method. The nanoparticle are characterized by powder X-ray diffraction (PXRD), Fourier transform infrared spectroscopy and scanning electron microscopy (SEM). PXRD reveals single phase, cubic spinel structure with Fd (3) over barm (227) space group. SEM micrograph shows the particles are agglomerated and porous in nature. Electron paramagnetic resonance spectrum exhibits a broad resonance signal g=2.150 and is attributed to super exchange between Fe3+ and Co2+. Magnetization values of CoFe2O4 nanoparticle are lower when compared to the literature values of bulk samples. This can be attributed to the surface spin canting due to large surface-to-volume ratio for a nanoscale system. The variation of dielectric constant, dielectric loss, loss tangent and AC conductivity of as-synthesized nano CoFe2O4 particles at room temperature as a function of frequency has been studied. The magnetic and dielectric properties of the samples show that they are suitable for electronic and biomedical applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present study, ZnFe2O4 nanoparticles were synthesized by the chemical co-precipitation followed by calcinations at 473 and 673K for 4h. Particle sizes obtained were 4 and 6nm for the calcination temperatures of 473 and 673K, respectively. To study the origin of system's low temperature spin dynamic behaviour, temperature dependence of susceptibility was investigated as a function of particle size and frequency. Slight increase in the grain size from 4nm at 473K to 6nm at 673K has led to a peak shift of temperature dependence of susceptibility measured at a constant frequency of 400Hz. Temperature dependence of at different frequencies also resulted in peak shift. Relaxation time dependence of peak temperature obeys a power law, which provides the fitting parameters within the range of superparamagnetic nature of the particles. Further, dependence of relaxation time and peak temperature obeys VogelFulcher law rather than NeelBrown equation demonstrating that the particles follow the behaviour of superparamagnetism of slightly interacting system. Spinlattice, T-1 and spinspin, T-2 relaxivity of proton of the water molecule in the presence of chitosan-coated superparamagnetic ZnFe2O4 nanoparticle yields the values of 0.002 and 0.360s(1)perppm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A porous carbon foam (CF) electrode modified with a reduced graphene oxide-Ag (rGO-Ag) nanocomposite has been fabricated to purify water. It can perform as an antibacterial device by killing pathogenic microbes with the aid of a 1.5 V battery, with very little power consumption. The device is recycled ten times with good performance for long term usage. It is shown that the device may be implemented as a fast water purifier to deactivate the pathogens in drinking water.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Water-dispersible, photocatalytic Fe3O4@TiO2 core shell magnetic nanoparticles have been prepared by anchoring cyclodextrin cavities to the TiO2 shell, and their ability to capture and photocatalytically destroy endocrine-disrupting chemicals, bisphenol A and dibutyl phthalate, present in water, has been demonstrated. The functionalized nanoparticles can be magnetically separated from the dispersion after photocatalysis and hence reused. Each component of the cyclodextrin-functionalized Fe3O4@TiO2 core shell nanoparticle has a crucial role in its functioning. The tethered cyclodextrins are responsible for the aqueous dispersibility of the nanoparticles and their hydrophobic cavities for the capture of the organic pollutants that may be present in water samples. The amorphous TiO2 shell is the photocatalyst for the degradation and mineralization of the organics, bisphenol A and dibutyl phthalate, under UV illumination, and the magnetism associated with the 9 nm crystalline Fe3O4 core allows for the magnetic separation from the dispersion once photocatalytic degradation is complete. An attractive feature of these ``capture and destroy'' nanomaterials is that they may be completely removed from the dispersion and reused with little or no loss of catalytic activity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three samples of multiwall carbon nanotubes (MWCNT) TF200, TF150 and TF100, where T and F stand for toluene and ferrocene respectively, and numeral denotes the amount (mg) of ferrocene] filled with iron-nanoparticles (Fe-NPs) of different aspect ratios are grown by chemical vapor deposition of toluene-ferrocene mixture. Energy dispersive X-ray analysis shows a systematic variation in the intensities of peak corresponding to Fe, indicating that Fe is present in different amounts in the three MWCNT samples. The lengths of Fe-NPs lie in the range of 200-250; 80-120; and 30-40 nm for TF200, TF150 and TF100, respectively, as estimated statistically from transmission electron microscopy micrographs. However, the diameter of the encapsulated Fe-NPs does not vary significantly for different samples and is 20-30 nm for all samples. Hysteresis loop measurements on these MWCNT samples were done at 10, 150 and 300 K up to an applied field of 1.5 T. At 10 K, values of coercivity are 2584, 2315, and 2251 Oe for TF200, TF150 and TF100 respectively. This is attributed to the strong shape anisotropy of the Fe-NPs and significant dipolar interactions between them. Further, M-H loops reveal that saturation magnetization of TF200 is almost four times that of TF100 at all temperatures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Results of a high resolution photoemission and electrochemistry study of Se adsorption Au(111) and Ag(111) surfaces performed by immersion of pristine samples into an aqeuous solution of Na2Se are presented. Cyclic voltammetry on Au shows formation of selenium adsorbed species and the structures observed in reductive desorption are to the atomic and polymeric species observed in XPS. In the case of Au(111) XPS spectra in the Se(3d) region indeed show two main features attributed to Se chemisorbed atomically and polymeric Se-8 features.' Smaller structures due to other types of Se conformations were also observed. The Au(4f) peak line, shape does not show core level, shifts: indicative of Au selenide formation the case of silver, XPS spectra for the Ag(3d) show a broadening of the peak and a deconvolution into Ag-B bulk like Ag-Se components shows that the Ag-Se is located at a lower binding energy, an effect similar to oxidation and sulfidation of Ag. The Se(3d) XPS spectrum is found to be substantially different from the Au case and dominated by atomic type Se due to the selenide, though a smaller intensity Se structure at an energy similar to the Se-8 structure for Au is also observed. Changes in the valence band region. related to Se adsorption are reported.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Metal-doped anatase nanosized titania photocatalysts were successfully synthesized using a sal gel process. Different amounts of the dopants (0.2, 0.4, 0.6, 0.8 and 1.0%) of the metals (Ag, Ni, Co and Pd) were utilized. The UV-Vis spectra (solid state diffuse reflectance spectra) of the doped nanoparticles exhibited a red shift in the absorption edge as a result of metal doping. The metal-doped nanoparticles were investigated for their photocatalytic activity under visible-light irradiation using Rhodamine B (Rh B) as a control pollutant. The results obtained indicate that the metal-doped titania had the highest activity at 0.4% metal loading. The kinetic models revealed that the photodegradation of Rh B followed a pseudo first order reaction. From ion chromatography (IC) analysis the degradation by-products Rhodamine B fragments were found to be acetate, chloride, nitrite, carbonate and nitrate ions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ag-Ni films were electrodeposited over a Cu substrate. Structural characterization revealed a fibrous microstructure with an amorphous structure for the as-deposited film. Isothermal annealing at 400 degrees C of the film inside transmission electron microscope led to amorphous-to-crystalline transition along with the evolution of nano-sized particles in the microstructure. The crystalline phase was Ni-Ag solid solution. The relative volume fraction of the nano-sized particles increased gradually with time. There was however no detectable decomposition of solid solution phase till about 4 h of annealing. Beyond 4 h phase separation initiated and pure Ag and Ni phases formed in the film. This study provides a methodology by which microstructural engineering of as-electrodeposited amorphous Ag-Ni films can be conducted to isolate a particular microstructure in order to tap specific potentially usable functionalities. (C) 2013 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new class of steroid dimers (bile acid derivatives) linked through ester functionalities were synthesized, which gelled various aromatic solvents. The organogels formed by the three dimeric ester molecules showed birefringent textures and fibrous nature by polarizing optical microscopy and scanning electron microscopy, respectively. A detailed rheological study was performed to estimate the mechanical strengths of two sets of organogels. In these systems, the storage modulus varied in the range of 0.8-3.5 X 10(4) at 1% w/v of the organogelators. The exponents of scaling of the storage modulus and yield stress of the two systems agreed well with those expected for viscoelastic soft colloidal gels with fibrillar flocs. The nanofibers in the organogel were utilized to engineer gold nanoparticles of different sizes and shapes and generate new gel-nanoparticle hybrid materials.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Present work provides an electrodeposition based methodology for synthesizing Ni-rich, Ag-Ni nanowires using an alumina template. Ag-Ni system shows negligible solid solubility in the bulk. Detailed structural and compositional characterization of as-synthesized nanowires using transmission electron microscopy technique revealed a two phase microstructure. Regions along and near the nanowire axis contained crystalline Ag-Ni solid solution phase with Ag-rich composition. Whereas, regions away from the axis and near the nanowire boundary predominantly contained nanocrystalline Ni-rich, Ni-Ag solid solution phase. (C) 2013 Elsevier B. V. All rights reserved.