887 resultados para Polymeric devices
Resumo:
This paper introduces an improved tabu-based vector optimal algorithm for multiobjective optimal designs of electromagnetic devices. The improvements include a division of the entire search process, a new method for fitness assignment, a novel scheme for the generation and selection of neighborhood solutions, and so forth. Numerical results on a mathematical function and an engineering multiobjective design problem demonstrate that the proposed method can produce virtually the exact Pareto front, in both parameter and objective spaces, even though the iteration number used by it is only about 70% of that required by its ancestor.
Resumo:
In this paper 4.5SiO(2)-3Al(2)O(3-x)Nb(2)O(5)-2CaO powders have been synthesized using a chemical process the Polymeric Precursor Method. The process of glass formation has been investigated by XRD and DTA, the results confirm that the prepared powders are glasses. Experimental data show that amount of Nb2O5 had a considerable effect on the T-g values. The structures of glasses prepared. have been determined by Si-29 and Al-27 MAS NMR and the results indicated that the network is formed by SiO4 and AlO4 tetrahedral linked and probably Si-O-Nb bonds are present in the vitreous network. (C) 2005 Elsevier B.V. All rights reserved.
Resumo:
The magneto-optical rotation at room temperature was measured for three Ga:S:La:O chalcogenide glasses at several laser lines in the visible. The first sample was a binary system constituted by 70 mol % Ga2S3 and 30 mol % La2O3, whereas in the second and third ones the lanthanum oxide was partially substituted by lanthanum sulfide, keeping the amount of gallium sulfide fixed. A pulsed magnetic field between 50 and 80 kG was used for the Faraday rotation measurements. The Verdet constant for one of the ternary samples was found to be as high as 0.205 min G(-1) cm(-1) at 543 nm, indicating that these chalcogenide glasses are very promising for magneto-optical applications. The data for each sample were fitted using the expected analytical expression for the magneto-optical dispersion. Measurements of the refractive index of the glasses at 632.8 nm are also reported. Data on the magneto-optical properties of two high Verdet constant, heavy-metal oxide diamagnetic glasses are also included for comparison. (C) 1999 Society of Photo-Optical Instrumentation Engineers. [S0091-3286(99)00102-6].
Resumo:
CaSnO3 was synthesized by the polymeric precursor method, using different precursor salts as (CH3COO)(2)Ca. H2O, Ca(NO3)(2). 4H(2)O, CaCl2. 2H(2)O and CaCO3, leading to different results. Powder precursor was characterized using thermal analysis. Depending on the precursor different thermal behaviors were obtained. Results also indicate the formation of carbonates, confirmed by IR spectra. After calcination and characterization by XRD, the formation of perovskite as single phase was only identified when calcium acetate was used as precursor. For other precursors, tin oxide was observed as secondary phase.
Resumo:
Thin films of perovskite-type materials such as PbTiO3, BaTiO3, (Pb,La)TiO3, (Pb, La)(ZrTi)O-3, KNbO3, and Pb(Mg,Nb)03 have been attracting great interest for applications like non-volatile memories, ultrasonic sensors and optical devices. Thin film should be epitaxially grown or at least highly textured since the properties of this anisotropic material depend on the crystallographic orientation. For optical devices, in particular, an epitaxial thin film without defects are essential to reduce optical propagation losses. Pb1-xLaxTiO3 (PLT) where x=0, 13 and 27% thin films were prepared by a chemical method (polymeric precursors method), and deposited by the spin coating technique onto substrates of SrTiO3 (STO) and LaAlO3 (LAO). The films were then beat treated at 500 degrees C in a controlled atmosphere of 0,. The orientation degree of the thin films was obtained from rocking curve technique, by means of X-ray difftaction analysis. A microstructural study revealed that the films were crack-free, homogeneous and have low roughness. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
PLZT ceramics belong to one of the very important groups of functional materials that make a basis for the production of a large range of electronic devices. The microstructure and properties of ceramics depend on the powder preparation and thermal processing conditions. Various techniques have been used to obtain chemically homogeneous and fine starting powders. PLZT powders have been prepared by two different production routes: by a modified Pechini method, using a polymeric precursor method (PMM) and by a partial oxalate method. A two-step sintering process, including a hot pressing, was carried out at 1100 and 1200degreesC Distinct phases obtained during the sintering process have been investigated by SEM and EDS techniques and dielectric properties such as permittivity and dielectric loss were measured in a frequency range from 1 to 20 kHz.. A significant difference in microstructure and dielectric properties, depending on powder origin and sintering procedure, has been noticed.
Resumo:
Reactive ZrxTi1-xO4 (x=0.65, 0.50 and 0.35) powder was prepared by the polymeric precursor method. Studies by X-ray diffraction (XRD), nitrogen adsorption/desorption, and thermogravimetric analysis (TG) showed that powders with high crystallinity (>90%) and high surface areas (>40 m(2)/g) are obtained after calcination at 700 degrees C for 3 h. Infrared spectroscopy and XRD results showed that these titanates nucleate from the amorphous phase with no intermediate phases, at low temperature (450 degrees C).
Resumo:
Pure and niobium doped bismuth titanate ceramics (Bi4Ti3-xNbxO12 (BTN)), with x ranging from 0 to 0.4 were prepared by the polymeric precursor method. X-ray diffraction showed no secondary phases. Increasing niobium content leads to more resistive ceramics. The shape and size of the grains are strongly influenced by the niobiurn added to the system. The dielectric constant is not influenced by the niobium addition while hysteresis loops are significantly narrowed. (c) 2006 Elsevier B.V All rights reserved.
Resumo:
BaxSr1-xTiO3 (x = 0.6) (BST) thin films were successfully prepared on a Pt(111)/TiO2/SiO2/Si(100) substrate by spin coating, using the polymeric precursor method. BST films with a perovskite single phase were obtained after heat treatment at 700 degrees C. The multilayer BST thin films had a granular structure will a grain size of approximately 60 nm. A 480-nm-thick film was obtained by carrying out five cycles of the spin-coating/heating process. Scanning electron microscopy and atomic force microscopy analyses showed that the thin films had a smooth, dense, crack-free surface with low surface roughness (3.6 nm). At room temperature and at a frequency of 100 kHz, the dielectric constant and the dissipation factor were, respectively, 748 and 0.042. The high dielectric constant value was due to the high microstructural quality and chemical homogeneity of the thin films obtained by the polymeric precursor method.
Resumo:
Pb1- xCaxTiO3 thin films with x = 0.24 composition were prepared by the polymeric precursor method on Pt/Ti/SiO2/Si substrates. The surface morphology and crystal structure, and the ferroelectric and dielectric properties of the films were investigated. X-ray diffraction patterns of the films revealed their polycrystalline nature. Scanning electron microscopy (SEM) and atomic force microscopy (AFM) analyses showed the surface of these thin films to be smooth, dense and crack-free with low surface roughness. The multilayer Pb1-xCaxTO3 thin films were granular in structure with a grain size of approximately 60-70 nm. The dielectric constant and dissipation factor were, respectively, 174 and 0.04 at a 1 kHz frequency. The 600-nm thick film showed a current density leakage in the order of 10(-7) A/cm(2) in an electric field of about 51 kV/cm. The C-V characteristics of perovskite thin films showed normal ferroelectric behavior. The remanent polarization and coercive field for the deposited films were 15 muC/cm(2) and 150 kV/cm, respectively. (C) 2001 Kluwer Academic Publishers.
Resumo:
In this work we report the synthesis procedure, crystallographic, structural and magnetic properties of the Li2ZnTi3O8 spinel obtained using a modified polymeric precursor method. This synthesis method generates very reactive and property-controlled nanoparticles. The samples were characterized using X-ray powder diffraction (XRD) associated to the Rietveld refinement method, thermogravimetric analysis (TG), specific surface area, scanning electron microscopy (SEM) and magnetic susceptibility measurements.The phase formation temperature of the lithium zinc titanate spinel was observed to decrease due to the homogeneity and highly controlled nanometric particle size. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Pure and lanthanum-doped Bi4Ti3O12 thin films were deposited on Pt/Ti/SiO2/Si substrate using a polymeric precursor solution. The spin-coated films were specular and crack-free and crystalline after annealing at 700 degreesC for 2 h. Crystallinity and morphological evaluation were examined by X-ray diffraction (XRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). Multilayered films obtained using the intermediate-crystalline layer route present a dense microstructure with spherical grains. Films obtained using the intermediate-amorphous layer, present elongated grains around 250 nm in size. The dielectric and ferroelectric properties of the lanthanum-doped Bi4Ti3O12 films are strongly affected by the crystallization route. The hysteresis loops are fully saturated with a remnant polarization and drive voltage of the films, heat-treated by the intermediate-crystalline (P-r = 20.2 muC/cm(2) and V = 1.35 V) and for the film heat-treated by amorphous route (P-r = 22.4 muC/cm(2) and V = 2.99 V). (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Thin films of potassium niobate were deposited on MgO (100) substrates by the polymeric precursor method and annealing in static air at 600 degreesC for 20 h. The obtained films were characterized by X-ray diffraction, atomic force microscopy (AFM) and the prism coupling method. The phi-scan diffraction evidenced the growth of the films with fourfold symmetry. AFM study shows that the films are homogeneous, dense and present a smooth surface. The refractive index and optical losses were strongly influenced by the degree of crystallinity. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Lanthanum-doped Bi4Ti3O12 thin films (BLT) were deposited on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution. The spin-coated films were specular, crack-free and crystalline after annealing at 700 degrees C for 2 h. Crystallinity and morphological evaluation were examined by X ray diffraction (YRD) and atomic force microscopy (AFM). The stability of the formed complex is of extreme importance for the formation of the perovskite phase. Films obtained from acid pH solution present elongated grains around 200 ran in size, whereas films obtained from basic solution present a dense microstructure with spherical grains (100 nm). The dielectric and ferroelectric properties of the BLT films are strongly affected by the solution pH. The hysteresis loops are fully saturated with a remnant polarization and coercive voltage of P-r=20.2 mu C/cm(2) and V-c = 1.35 V and P-r= 15 mu C/cm(2) and V-c = 1.69 V for the films obtained from basic and acid solutions, respectively. (C) 2005 Elsevier B.V. All rights reserved.