610 resultados para Corrosão eletroquímica
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
The activation of aluminum surface has the most various purposes as for example the search for the surface activation mechanism and the corrosion products by mercury ions. The objective of this work is to study the reactivity of the surface of aluminum metal when activated by mercury ions (Hg2+), with the consequent formation of an Al-Hg amalgam. Results demonstrate that the kinetics of the reaction, by measuring the mass change with time of the corrosion product formed between Al and Hg, and analysis by infrared spectroscopy (IR) that the product of the reaction between the amalgam, located on the surface, and the atmospheric oxygen is Al2O3 (aluminum hydroxide). The results also indicate that the kinetics of the reaction between the amalgam (Hg-Al) and atmospheric oxygen is of first order and reach a region where there is no more formation of product
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
With advances in health care, has been na increase of demand for material that could replace the functions of the human body parts, thus evolved biomedic prosthesis which today are responsible for the constant improvement of the quality of life. The Titanium alloys are widely used as implants due to its properties, like high mechanical resistance, biocompatibility and corrosion resistance, and the addition alloying elements like Zirconium, may improve some of those properties. Such properties are related to the microstructure and consequently to the type of processing performed. The purpose of this dissertation was to characterize the experimental alloy Ti15Zr after route of processsing and heat treatment in order to extend the knowledge about this alloy. The latter has been abtained by fusion of pure metals in a arc melting furnace with an inert argon atmosphere. The material has been homogenized in a tube furnace at 950ºC for 24h and cold worked by swaging, after that, bars with 10 mm of diameter were obtained by the process of rotary forging. The samples were solubilized at 900º C for 2 hours and quenched in water. After that, 4 samples were submitted to the aging, at 400º C, 450º C, 500º C and 550º C. The microstructure and phase analysis was done by optical microscopy and X-rays diffraction (XRD), the mechanical characterization was carried out by microhardness test and finally, evaluation of corrosion resistance of the alloy by electrochemical tests. The XRD and the optical microscopy made it possible to analyze that the heat treatment influenced the phase shifting from α to α', and probably affected the alloy hardness, at the first aged sample at 500º Chas been a sudden increase in the value of hardness, probably by appearance of omega phase, unwanted phase to the medical application duo to great fragility, and finally ... (Complete abstract click electronic access below)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Direct methanol fuel cells (DMFCs) without external pumps or other ancillary devices for fuel and oxidant supply are known as passive DMFCs and are potential candidates to replace lithium-ion batteries in powering portable electronic devices. This paper presents the results obtained from a membrane electrode assembly (MEA) specifically designed for passive DMFCs. Appropriated electrocatalysts were prepared and the effect of their loadings was investigated. Two types of gas diffusion layers (GDL) were also tested. The influence of the methanol concentration was analyzed in each case. The best MEA performance presented a maximum power density of 11.94 mW cm-2.
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
With advances in health care, has been na increase of demand for material that could replace the functions of the human body parts, thus evolved biomedic prosthesis which today are responsible for the constant improvement of the quality of life. The Titanium alloys are widely used as implants due to its properties, like high mechanical resistance, biocompatibility and corrosion resistance, and the addition alloying elements like Zirconium, may improve some of those properties. Such properties are related to the microstructure and consequently to the type of processing performed. The purpose of this dissertation was to characterize the experimental alloy Ti15Zr after route of processsing and heat treatment in order to extend the knowledge about this alloy. The latter has been abtained by fusion of pure metals in a arc melting furnace with an inert argon atmosphere. The material has been homogenized in a tube furnace at 950ºC for 24h and cold worked by swaging, after that, bars with 10 mm of diameter were obtained by the process of rotary forging. The samples were solubilized at 900º C for 2 hours and quenched in water. After that, 4 samples were submitted to the aging, at 400º C, 450º C, 500º C and 550º C. The microstructure and phase analysis was done by optical microscopy and X-rays diffraction (XRD), the mechanical characterization was carried out by microhardness test and finally, evaluation of corrosion resistance of the alloy by electrochemical tests. The XRD and the optical microscopy made it possible to analyze that the heat treatment influenced the phase shifting from α to α', and probably affected the alloy hardness, at the first aged sample at 500º Chas been a sudden increase in the value of hardness, probably by appearance of omega phase, unwanted phase to the medical application duo to great fragility, and finally ... (Complete abstract click electronic access below)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Three nanostructured platinum-niobium supported on Vulcan XC-72R carbon black materials were prepared as catalysts for the ethanol electroxidation: (i) deposition of platinum and niobium on Vulcan XC-72R carbon black, (ii) platinum decorated on a mixture of commercial amorphous Nb2O5/carbon black, and (iii) the same than ii but using crystalline Nb2O5, by reduction of the precursors with sodium borohydride in ethanol. All the catalysts showed platinum crystal sizes in the range of 3-4 nm, with no or little modification of the lattice parameter. The analyses of the electronic structure from the XANES region of the XAS spectra displayed some interactions between platinum and niobium, despite the niobium was primarily in the form of pentoxide in all the catalysts. CO stripping exhibited a promising low onset potential and a large current density, especially in the case of the deposited catalyst. Ethanol electroxidation experiments revealed that the Pt-Nb(2)O(5)crystalline/C generated the largest current. However it was not effective to completely oxidize ethanol, leading to acetic acid as the main product. In this sense, the highest efficiency for the complete oxidation of ethanol was obtained for the deposited catalyst. These results were interpreted in terms of the physico-chemical characteristic displayed by the different catalysts. (C) 2012 The Electrochemical Society. [DOI: 10.1149/2.040210jes] All rights reserved.
Resumo:
Purpose: Implant-abutment connections still present failures in the oral cavity due to the loosening of mechanical integrity by detorque and corrosion of the abutment screws. The objective of this study was to evaluate the detorque of dental abutment screws before and after immersion in fluoridated solutions. Materials and Methods: Five commercial implant-abutment assemblies were assessed in this investigation: (C) Conex˜aoR , (E) EmfilsR , (I) INPR , (S) SINR , and (T) Titanium FixR . The implants were embedded in an acrylic resin and then placed in a holding device. The abutments were first connected to the implants and torqued to 20Ncmusing a handheld torque meter. The detorque values of the abutments were evaluated after 10 minutes. After applying a second torque of 20 Ncm, implant-abutment assemblies were withdrawn every 3 hours for 12 hours in a fluoridated solution over a period of 90 days. After that period, detorque of the abutments was examined. Scanning electronicmicroscopy (SEM) associated to energy dispersive spectroscopy (EDS) was applied to inspect the surfaces of abutments. Results: Detorque values of systems C, E, and I immersed in the fluoridated solution were significantly higher than those of the initial detorque. ANOVA demonstrated no significant differences in detorque values between designs S and T. Signs of localized corrosion could not be detected by SEM although chemical analysis by EDS showed the presence of elements involved in corrosive processes. Conclusion: An increase of detorque values recorded on abutments after immersion in fluoridated artificial saliva solutions was noticed in this study. Regarding chemical analysis, such an increase of detorque can result from a corrosion layer formed between metallic surfaces at static contact in the implant-abutment joint during immersion in the fluoridated solutions.
Resumo:
As fibras cerâmicas se caracterizam por ser um material leve, com alto grau de pureza, baixo armazenamento de calor, baixa condutividade térmica, resistência a choque térmico e alta resistência à corrosão em altas temperaturas. Essas características levam a uma grande procura das indústrias mínero-metalúrgicas e de outros setores para revestimentos de distribuidores, muflas, fornos de aquecimentos, entre outros. Após utilização no processo, por perderem sua capacidade de isolamento, os resíduos gerados precisam de destinação. Esse trabalho enfoca, especificamente, resíduos de lã cerâmica e lã de vidro. Pelo fato de a composição das fibras cerâmicas ser rica em sílica e alumina, efetuou-se uma investigação acerca da atividade pozolânica das mesmas com a cal e o cimento, especificamente CPV ARI, CPII E32 e CPIII 32RS, para avaliação da perspectiva de reciclagem em possível incorporação no concreto.
Resumo:
O objetivo da pesquisa é recuperar os principais metais presentes em um lote com uma mistura de diversos tipos de pilhas e de baterias descartadas após o uso, lote obtido em um posto de coleta. Para esse estudo, o resíduo das pilhas e das baterias foi moído, reduzido em forno elétrico, submetido à separação magnética e lixiviado. A composição química, após a lixiviação, foi reproduzida em uma solução sintética, que foi submetida à extração por solventes e reextração sendo que as soluções obtidas, após as reextrações, foram utilizadas como eletrólitos. Manganês, cobre, cobalto e níquel são recuperados na forma metálica após um tratamento que inclui as etapas pirometalúrgica, hidrometalúrgica e eletroquímica. Estudos anteriores definiram os parâmetros das etapas pirometalúrgica, lixiviação e extração por solventes que proporcionaram separação mais seletiva dos íons metálicos que se pretende recuperar. A contribuição do presente estudo é encontrar um processo que trate de todos os tipos de pilhas e de baterias juntos e recuperar seus metais mais importantes, evitando, assim, a etapa de separação prévia das baterias. Os filmes foram analisados quanto à sua espessura e composição.
Resumo:
Tantalum coatings are of particular interest today as promising candidates to replace potentially hazardous electrodeposited chromium coatings for tribological and corrosion resistant applications, such as the internal lining on large-caliber gun barrels. Tantalum coatings have two crystalline phases, α-Ta (body-centered-cubic) and β-Ta (metastable tetragonal) that exhibit relatively different properties. Alpha-Ta is typically preferred for wear and corrosion resistant applications and unfortunately, is very difficult to deposit without the assistance of substrate heating or post-annealing treatments. Furthermore, there is no general consensus on the mechanism which causes α or β to form or if there is a phase transition or transformation from β → α during coating deposition. In this study, modulated pulsed power (MPP) magnetron sputtering was used to deposit tantalum coatings with thicknesses between 2 and 20 μm without external substrate heating. The MPP Ta coatings showed good adhesion and low residual stress. This study shows there is an abrupt β → α phase transition when the coating is 5–7 μm thick and not a total phase transformation. Thermocouple measurements reveal substrate temperature increases as a function of deposition time until reaching a saturation temperature of ~ 388 °C. The importance of substrate temperature evolution on the β → α phase transition is also explained.