840 resultados para Slow Strain Rate Testing
Analysis of deformation behavior and workability of advanced 9Cr-Nb-V ferritic heat resistant steels
Resumo:
Hot compression tests were carried out on 9Cr–Nb–V heat resistant steels in the temperature range of 600–1200 °C and the strain rate range of 10−2–100 s−1 to study their deformation characteristics. The full recrystallization temperature and the carbon-free bainite phase transformation temperature were determined by the slope-change points in the curve of mean flow stress versus the inverse of temperature. The parameters of the constitutive equation for the experimental steels were calculated, including the stress exponent and the activation energy. The lower carbon content in steel would increase the fraction of precipitates by increasing the volume of dynamic strain-induced (DSIT) ferrite during deformation. The ln(εc) versus ln(Z) and the ln(σc) versus ln(Z) plots for both steels have similar trends. The efficiency of power dissipation maps with instability maps merged together show excellent workability from the strain of 0.05 to 0.6. The microstructure of the experimental steels was fully recrystallized upon deformation at low Z value owing to the dynamic recrystallization (DRX), and exhibited a necklace structure under the condition of 1050 °C/0.1 s−1 due to the suppression of the secondary flow of DRX. However, there were barely any DRX grains but elongated pancake grains under the condition of 1000 °C/1 s−1 because of the suppression of the metadynamic recrystallization (MDRX).
Resumo:
China Low Activation Martensitic (CLAM) steel is considered to be the main candidate material for the first wall components of future fusion reactors in China. In this paper, the low cycle fatigue (LCF) behavior of CLAM steel is studied under fully reversed tension–compression loading at 823 K in air. Total strain amplitude was controlled from 0.14% to 1.8% with a constant strain rate of 2.4×10−3 s−1. The corresponding plastic strain amplitude ranged from 0.023% to 1.613%. The CLAM steel displayed continuous softening to failure at 823 K. The relationship between strain, stress and fatigue life was obtained using the parameters obtained from fatigue tests. The LCF properties of CLAM steel at 823 K followed Coffin–Manson relationship. Furthermore, irregular serration was observed on the stress–strain hysteresis loops of CLAM steel tested with the total strain amplitude of 0.45–1.8%, which was attributed to the dynamic strain aging (DSA) effect. During continuous cyclic deformation, the microstructure and precipitate distribution of CLAM steel changed gradually. Many tempered martensitic laths were decomposed into subgrains, and the size and number of M23C6 carbide and MX carbonitride precipitates decreased with the increase of total strain amplitude. The response cyclic stress promoted the recovery of martensitic lath, while the thermal activation mainly played an important role on the growth of precipitates in CLAM steel at 823 K. In order to have a better understanding of high-temperature LCF behavior, the potential mechanisms controlling stress–strain response, DSA phenomenon and microstructure changes have also been evaluated.
Resumo:
This paper presents a study on the bond behaviour of FRP-concrete bonded joints under static and dynamic loadings, by developing a meso-scale finite element model using the K&C concrete damage model in LS-DYNA. A significant number of single shear experiments under static pull-off loading were modelled with an extensive parametric study covering key factors in the K&C model, including the crack band width, the compressive fracture energy and the shear dilatation factor. It is demonstrated that the developed model can satisfactorily simulate the static debonding behaviour, in terms of mesh objectivity, the load-carrying capacity and the local bond-slip behaviour, provided that proper consideration is given to the selection of crack band width and shear dilatation factor. A preliminary study of the effect of the dynamic loading rate on the debonding behaviour was also conducted by considering a dynamic increase factor (DIF) for the concrete strength as a function of strain rate. It is shown that a higher loading rate leads to a higher load-carrying capacity, a longer effective bond length, and a larger damaged area of concrete in the single shear loading scenario.
Resumo:
Despite the abundance of studies investigating the performance of composite structures under crush loading, disagreement remains in the literature regarding the effect of increased strain rate on the crush response. This study reports an experimental investigation of the behaviour of a carbon-epoxy composite energy absorber under static and dynamic loading with a strain rate of up to 100s<sup>-1</sup>. Consistent damage modes and measured force responses were obtained in samples tested under the same strain rate. The energy absorption was found to be independent of strain rate as the total energy absorption appeared to be largely associated with fibre-dominated fracture, which is independent of strain rate within the studied range. The results from this study are beneficial for the design of energy absorbing structures.
Resumo:
Shape memory alloys (SMAs) have the ability to undergo large deformations with minimum residual strain and also the extraordinary ability to undergo reversible hysteretic shape change known as the shape memory effect. The shape memory effect of these alloys can be utilised to develop a convenient way of actively confine concrete sections to improve their shear strength, flexural ductility and ultimate strain. Most of the previous work on active confinement of concrete using SMA has been carried out on circular sections. In this study retrofitting strategies for active confinement of non-circular sections have been proposed. The proposed schemes presented in this paper are conceived with an aim to seismically retrofit beam-column joints in non-seismically designed reinforced concrete buildings. SMAs are complex materials and their material behaviour depends on number of parameters. Depending upon the alloying elements, SMAs exhibit different behaviour in different conditions and are highly sensitive to variation in temperature, phase in which it is used, loading pattern, strain rate and pre-strain conditions. Therefore, a detailed discussion on the behaviour of SMAs under different thermo-mechanical conditions is presented first.
Resumo:
Melt-mixed high density polyethylene (HDPE)/multi-walled carbon nanotube (MWCNT) nanocomposites with 1–10 wt% MWCNTs were prepared by twin screw extrusion and compression moulded into sheet form. The compression moulded nanocomposites exhibit a 112% increase in modulus at a MWCNT loading of 4 wt%, and a low electrical percolation threshold of 1.9 wt%. Subsequently, uniaxial, sequential (seq-) biaxial and simultaneous (sim-) biaxial stretching of the virgin HDPE and nanocomposite sheets was conducted at different strain rates and stretching temperatures to investigate the processability of HDPE with the addition of nanotubes and the influence of deformation on the structure and final properties of nanocomposites. The results show that the processability of HDPE is improved under all the uniaxial and biaxial deformation conditions due to a strengthened strain hardening behaviour with the addition of MWCNTs. Extensional deformation is observed to disentangle nanotube agglomerates and the disentanglement degree is shown to depend on the stretching mode, strain rate and stretching temperatures applied. The disentanglement effectiveness is: uniaxial stretching < sim-biaxial stretching < seq-biaxial stretching, under the same deformation parameters. In sim-biaxial stretching, reducing the strain rate and stretching temperature can lead to more nanotube agglomerate breakup. Enhanced nanotube agglomerate disentanglement exhibits a positive effect on the mechanical properties and a negative effect on the electrical properties of the deformed nanocomposites. The ultimate stress of the composite containing 4 wt% MWCNTs increased by ∼492% after seq-biaxial stretching, while the resistivity increased by ∼1012 Ω cm.
Resumo:
A meso-scale finite element model is presented for investigating the FRP-concrete bond behaviour under static and dynamic loadings. It adopts a local concrete damage model. A large number of single shear tests under static pull-off loading were modeled. It is demonstrated that the developed model can satisfactorily simulate the static debonding behaviour, in terms of the load-carrying capacity and the local bond-slip behaviour. A preliminary study of the effect of the dynamic loading rate on the debonding behaviour was also conducted by considering a dynamic increase factor for the concrete strength as a function of strain rate. It is shown that a higher loading rate leads to a higher load-carrying capacity, a longer effective bond length, and a larger damaged area of concrete in the single shear loading scenario.
Resumo:
Strengthening reinforced concrete (RC) structures by externally bonded FRP composites has been widely used for static loading and seismic retrofitting since 1990s. More recently many studies on strengthening concrete and masonry structures with externally bonded FRP for improved blast and impact resistance in protective engineering have also been conducted. The bond behaviour between the FRP and concrete plays a critical role in a strengthening system with externally bonded FRP. However, the understanding of how the bond between FRP and concrete performs under high strain rate is severely limited. Due to the dynamic characteristics of blast and impact loading, the bond behaviour between FRP and concrete under such loading is very different from that under static loading. This paper presents a study on the dynamic bond-slip behaviour based on both the numerical analysis and test results. A dynamic bond-slip model is proposed in this paper.
Resumo:
Shape memory alloys (SMAs) have the ability to undergo large deformations with minimum residual strain and also the extraordinary ability to undergo reversible hysteretic shape change known as the shape memory effect. The shape memory effect of these alloys can be utilised to develop a convenient way of actively confining concrete sections to improve their shear strength, flexural ductility and ultimate strain capacity. Most of the previous work on active confinement of concrete using SMA has been carried out on circular sections. In this study retrofitting strategies for active confinement of non-circular sections have been proposed. The proposed schemes presented in this paper are conceived with an aim to seismically retrofit a beam-column joint in non-seismically designed reinforced concrete buildings.
The complex material behaviour of SMAs depends on number of parameters. Depending upon the alloying elements, SMAs exhibit different behaviour in different conditions and are highly sensitive to variation in temperature, phase in which it is used, loading pattern, strain rate and pre-strain conditions. Therefore, a detailed discussion on the behaviour of SMAs under different thermo-mechanical conditions is presented first in this paper.
Resumo:
Recombinant Adenoviruses (Ads) have been shown to have potential applications in three areas: gene therapy, high level protein expression and recombinant vaccines.' At least three different locations within the Ad genome can be deleted and subsequently used for the insertion of foreign sequences. These include the Early 3 (E3), Early 1 (E1) and Early 4 (E4) regions. Viral vectors of this type have been well studied in Human Ads 2 and 5, however one has not yet been constructed for Bovine Adenovirus Type 2 (BAV2). The E3 region is located between 76.6 and 86 m.u. on the r-strand and is transcribed in a rightward direction. The gene products of the Early 3 region (E3) have been shown to be non-essential for viral replication, in vitro, but are required for host immunosurveillance. This study represents the cloning and reconstitution of a BAV2 E3 deletion mutant. A deletion of 1800bp was made within the E3 region of BAV2 and the thymidine kinase gene was subsequently inserted in the deleted area . . The plasmid pdlE3-4tk1 (23.4Kbp) was constructed and used to to facilitate homologous recombination with the wild type BAV2 to produce a mutant. Southern Blotting and Hybridization results suggest the presence of a BAV2 E3 deletion mutant with thymidine kinase sequences present. The E4 region of Human Adenovirus types 2 and 5 is located at the extreme right end of the genome (91.3 map units - 99.1 map units) and is transcribed in a leftward direction giving rise to a complicated set of differentially spliced mRNAs. Essentially there are 7 open reading frames (ORFs) encoding for at least 7 polypeptides. The gene products encoded by the E4 region have been shown to be essential for the expression of late viral genes, host cell shutoff and normal viral growth. We have cloned and sequenced the right end segment between 90.5 map units and 100 map units of the BAV2 genome. The results show several open reading frames which encode polypeptides exhibiting homology to three polypeptides encoded by the E4 region of human adenovirus type 2. These include the 14kDa protein encoded by ORF1, the 34kDa protein encoded by ORF6 and the 13kDa protein encoded by ORF3. The nucleotide sequence, restriction enzyme map, and ORF map of the E4 region could be very useful in future molecular manipulation of this region and could possibly explain the slow growth rate of BAV2 in MDBK cells.
Resumo:
The stress relaxation behavior of polyurethane elastomer and short polyester fiber filled elastomer composites with and without bonding agents at different strain levels and strain rates was studied. It was found that these compounds exhibit a multistage relaxation mechanism and that the rate of relaxation and cross-over time depend on the strain level and strain rate. The incorporation of fibers reduced the stage-I relaxation rate and increased the cross-over time of the gum vulcanisate. A higher rate of relaxation (first stage) was shown by the composites with longitudinal fiber orientation and composites with bonding agents.
Resumo:
Introducción: La ecocardiografía es actualmente la técnica de imagen diagnóstica más utilizada para la evaluación de la anatomía y la función cardiovascular. En la actualidad se está utilizando la ecocardiografía por speckle tracking la cual permite una evaluación mas objetiva y confiable de la función ventricular, sin embargo se requieren valores de referencia que hagan que los valores obtenidos sean válidos y útiles para determinar en forma mas oportuna conductas previas al deterioro de su función. Objetivo general: Determinar los valores de referencia para mecánica ventricular izquierda mediante ecocardiografía bidimensional por speckle tracking con equipo Toshiba Artida con transductor multifrecuencia de 3 megahertzios en pacientes sin patología cardiaca conocida en la Fundación Clínica Shaio en el año 2014. Metodología: Análisis de una cohorte prospectiva de todos los pacientes que ingresaron a la Fundación Clínica Shaio para evaluación ecocardiográfica sin patología cardiaca conocida entre los meses Agosto y Diciembre del 2014. Resultados: Se presenta este estudio de la evaluación de la mecánica ventricular izquierda en adultos sanos, los resultados son similares a los obtenidos en estudios de referencia, sin embargo se consideran de gran importancia ya que de acuerdo a la guía actual de evaluación de la mecánica ventricular por strain rate es importante que cada equipo se encuentre estandarizado con el fin de tener resultados válidos de acuerdo a las diferentes patologías en las que se puede aplicar y a nuestra población.
Resumo:
RESUMEN Introducción El papel de las nuevas técnicas ecocardiográficas para el diagnóstico de infarto agudo del miocardio se encuentra en desarrollo y la realización de mecánica ventricular izquierda podría sugerir la presencia de enfermedad coronaria hemodinámicamente significativa. Objetivos Determinar si en pacientes con infarto agudo del miocardio la medición de strain longitudinal global y regional sirve para predecir la presencia de enfermedad coronaria significativa. Métodos Es un estudio de pruebas diagnósticas en el que se evaluaron las características operativas de la mecánica ventricular izquierda para la detección de enfermedad coronaria significativa comparado contra el cateterismo cardiaco, considerado el patrón de oro. Se analizaron 54 pacientes con infarto agudo del miocardio llevados a cateterismo cardiaco, a quienes se les realizó un ecocardiograma transtorácico con medición de strain longitudinal global y regional. Resultados De los 54 pacientes analizados, el 83% tenía enfermedad coronaria significativa. El hallazgo de un strain longitudinal global < -17.5 tuvo una sensibilidad del 85% y una especificidad del 78% para predecir la presencia de enfermedad coronaria; para la arteria descendente anterior un strain longitudinal regional < – 17.4 tuvo una sensibilidad de 82% y una especificidad de 44%, para la arteria circunfleja una sensibilidad del 87% y una especificidad del 37% y para la arteria coronaria derecha una sensibilidad de 73% y una especificidad de 32%. Conclusiones La realización de ecocardiografía con mecánica ventricular en pacientes con infarto agudo del miocardio es útil para predecir la presencia de enfermedad coronaria hemodinámicamente significativa.
Resumo:
Measurement or prediction of the mechanical and fracture properties of foods is very important in the design, operation and optimization of processes, as well as for the control of quality of food products. This paper describes the measurement of yield stress of frozen sucrose solutions under indentation tests using a spherical indenter. Effects of composition, temperature and strain rate on yield stress of frozen sucrose solutions have also been investigated.
Resumo:
The rheological properties of gas cell walls in bread doughs are considered to be important in relation to their stability and gas retention during proof and baking. Large deformation rheological properties of gas cell walls were measured using biaxial extension for a number of doughs of varying breadmaking quality at constant strain rate and elevated temperatures of 25-60degreesC. Strain hardening and failure strain of cell walls both decreased with temperature, with cell walls in good breadmaking doughs remaining stable and retaining their strain hardening properties at higher temperatures (60degreesC), while the cell walls of poor breadmaking doughs became unstable at lower temperatures (45-50degreesC) and had lower strain hardening. Strain hardening measured at 50degreesC gave good correlations with baking volume, with the best correlations achieved between rheological measurements and baking tests that used similar mixing conditions. As predicted by the considered failure criterion, a strain hardening value of I defines a region below which gas cell walls become unstable, and discriminates well between the baking quality of a range of commercial flour blends of varying quality. This indicates that the stability of gas cell walls during baking is strongly related to strain hardening properties, and that extensional rheological measurements can be used as indicators of baking quality.