814 resultados para GAASN ALLOYS
Resumo:
Soldering alloys based oft the Sn-Cu alloy system are amongst the most favourable lead-free alternatives due to a range of attractive properties. Trace additions of Ni have been found to significantly improve the soldering characteristics of these alloys (reduced bridging etc.). This paper examines the mechanisms underlying the improvement in soldering properties of Sn-0.7 mass%Cu eutectic alloys modified with concentrations of Ni ranging front 0 to 1000 ppm. The alloys were investigated by thermal analysis during solidification, as well as optical/SEM microanalyses of fully solidified samples anti samples quenched during solidification. It is concluded that Ni additions dramatically alter the nucleation patterns and solidification behaviour of the Sn-Cu6Sn5 eutectic anti that these changes are related to the superior soldering characteristics of the Ni-modified Sn-0.7 mass%Cu alloys.
Resumo:
A new modification phenomenon is reported for Al-Si alloys, where the Al-Si eutectic is refined by segregated TiB2 particles. The TiB2 particles are pushed to the Al-Si phase boundary during solidification of the eutectic and it is believed that at high concentrations the TiB2 particles restrict solute redistribution causing refinement of the Si. (c) 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
This work studied the effect of the impurity iron and the alloying elements aluminium and zinc in single-phase substrate magnesium alloys on the corrosion resistance of the alloys after anodisation. It was found that increasing zinc content (0-2%) led to increased corrosion resistance of an anodised single-phase Mg-Zn alloy. The addition of Al lowered the corrosion resistance of an anodised commercial purity Mg-Al single-phase alloy, whereas the same addition was found to be beneficial to the corrosion resistance of an anodised high purity Mg-Al single-phase alloy. Heat-treatment made the substrate Mg-Al and Mg-Zn alloys more uniform and hence improved the corrosion resistance of the alloys after anodisation. The detrimental effect of iron impurity on corrosion performance of the unanodised substrate single-phase magnesium alloys was inherited by the anodised alloys. The corrosion resistance of the anodised Mg alloys was found to be closely correlated with the corrosion performance of the unanodised as-cast Mg alloys. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Grain size is one of the most important microstructural characteristics determining the mechanical properties and therefore the service performance of polycrystalline materials. Heterogeneous nucleation involves the addition or in situ formation of potent nuclei in the system to promote nucleation events, leading to a fine grain structure. This paper reports experimental results using graphite and SiC as potential grain refining agents to form in situ nuclei for Mg in Mg-Al alloys, and demonstrates the key role of Al4C3 in grain refilling this important alloy system. This insight will contribute to the design and development of the most cost effective, eco-friendly grain refining agents for Mg-Al alloys. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The addition of SiC particles effectively grain refined a range of Mg-Al alloys. The greatest reductions in grain size were found for the alloys with lower Al contents. The presence of Mg2Si in the microstructure after that SiC addition, and consideration of phase equilibria suggested that the SiC transforms to Al4C3, and this is the actual nucleant. The addition of Mn poisoned the grain refining effect of the SiC addition, probably due to the formation of less potent Al-Mn-carbides. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
An experimental program has been undertaken to explore the effect of iron concentration on porosity levels in Al-Si alloy sand castings. The effect of iron concentrations above, below and equal to the critical iron content for alloys with either 5 or 9% Si and either 0, 1 or 3% Cu has been determined. Increasing iron concentrations were found to increase porosity in all alloys except the copper-containing Al-5% Si alloys which displayed a porosity minimum at the critical iron content. Porosity was observed to be higher in the Al-9% Si castings than the Al-5% Si castings. Differences in the primary phase volume fraction and morphology may explain this observation. The results of this experimental work do not support the existing published theories that have been proposed to explain the effect the iron on porosity. An alternative theory is therefore developed. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
This paper investigates the relationship between mechanical properties and microstructure in high pressure die cast binary Mg-Al alloys. As-cast test bars produced using high pressure die casting have been tested in tension in order to determine the properties for castings produced using this technique. It has been shown that increasing aluminium levels results in increases in yield strength and a decrease in ductility for these alloys. Higher aluminium levels also result in a decrease in creep rate at 150 degrees C. It has also been shown that an increase in aluminium levels results in an increase in the volume fraction of eutectic Mg17Al12 in the microstructure.
Resumo:
This paper reviews various aspects of anodizing of magnesium alloys, such as the basics, processes, properties and applications. It systematically summarises the existing fundamental studies and technical developments of anodizing of magnesium alloys, and concludes that new anodizing processes based on electrolytic plasma anodizing that convert the surface of a magnesium alloy into a hard ceramic coating in an electrolytic bath using high energy electric discharges can offer improved wear and corrosion resistance. These new anodized coatings are often claimed to perform better than the traditional ones obtained through older anodizing processes, such as DOW17 or HAE. The new anodizing techniques are chromate free and hence environment friendly. It is expected that more cost-effective, environment-friendly and non-toxic anodizing techniques will be developed and applied to magnesium alloy components in the future.
Resumo:
Manganese is a grain refiner for high purity Mg-3%Al, Mg-6%Al, Mg-9%Al, and commercial AZ31 (Mg-3%Al-1%Zn) alloys when introduced in the form of an Al-60%Mn master alloy splatter but the use of pure Mn flakes and ALTAB (TM) Mn75 tablets shows no grain refinement. Long time holding of the melt at 730 degrees C leads to an increase in grain size. The mechanism is attributed to the presence of all epsilon-AlMn phase (hexagonal close-packed) in the master alloy splatter. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Recently it has been shown that modification with strontium causes an increase in the size of eutectic grains. The eutectic grain size increases because there are fewer nucleation events, possibly due to the poisoning of phosphorus-based nuclei that are active in the unmodified alloy. The current paper investigates the effect of strontium concentration on the eutectic grain size. In the aluminium-10 wt.% silicon alloy used in this research, for fixed casting conditions, the eutectic grain size increases as the strontium concentration increases up to approximately 150ppm, beyond which the grain size is relatively stable. This critical strontium concentration is likely to differ depending on the composition of the base alloy, including the concentration of minor elements and impurities. It is concluded that processing and in-service properties of strontium modified aluminium-silicon castings are likely to be more stable if a minimum critical strontium concentration is exceeded. If operating below this critical strontium concentration exceptional control over composition and casting conditions is required. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Using modifications to the Rappaz-Drezet-Gremaud hot tearing model, and using empirical equations developed for grain size and dendrite arm spacing (DAS) on the addition of grain refiner for a range of cooling rates, the effect of grain refinement and cooling rate on hot tearing susceptibility has been analysed. It was found that grain refinement decreased the grain size and made the grain morphology more globular. Therefore refining the grain size of an equiaxed dendritic grain decreased the hot tearing susceptibility. However, when the alloy was grain refined such that globular grain morphologies where obtained, further grain refinement increased the hot tearing susceptibility. Increasing the cooling decreased the grain size and made the grain morphology more dendritic and therefore increased the likelihood of hot tearing. The effect was particularly strong for equiaxed dendritic grain morphologies; hence grain refinement is increasingly important at high cooling rates to obtain more globular grain morphologies to reduce the hot tearing susceptibility.