The aim of this study was to verify the average fiber length and the juvenile and mature wood zones from Hevea brasiliensis proveniences from a reforestation area in São Paulo, Brazil. For this purpose, five Hevea brasiliensis trees were randomly collected from a 50-year-old plantation, located in Balsamo, São Paulo, Brazil. The trees were cut and five flat sawn boards were obtained. The juvenile and mature wood zones were determined by fiber length measurement from the pith to the bark. The results showed that: (a) the juvenile wood of this species occurred approx. between 40 and 55 mm, from the pith, and from this point forward, the mature wood zone was found; (b) there was a significant difference between the average fiber length of juvenile wood (1.26 mm) and mature wood (1.51 mm).
Resumo:
Metal/ceramic interfaces using zirconia have dominated the industrial applications in the last decade, due to the high mechanical strength and fracture toughness of zirconia, especially at temperatures below 300 ºC. Also noteworthy is the good ionic conductivity in high temperatures of this component. In this work joining between ZrO2 Y-TZP and ZrO2 Mg-PSZ with austenitic stainless steel was studied. These joints were brazed at high-vacuum after mechanical metallization with Ti using filler alloys composed by Ag-Cu and Ag-Cu-Ni. The influence of the metallization, and the affinity between the different groups (ceramic / filler alloys) was evaluated, in order to achieve strong metal/ceramic joints. Evaluation of joints and interfaces, also the characterization of base materials was implemented using various techniques, such as: x-ray diffraction, leak test, three-point flexural test and scanning electron microscopy with chemical analysis. The microstructural analysis revealed physical and chemical bonds in the metal/ceramic interfaces, providing superior leak proof joints and stress cracking, in order to a good joint in all brazed samples. Precipitation zones and reaction layers with eutetic characteristics were observed between the steel and the filler metal
Resumo:
A method has been developed to obtain quantitative information about grain size and shape from fractured surfaces of ceramic materials. One elaborated a routine to split intergranular and transgranular grains facets of ceramic fracture surfaces by digital image processing. A commercial ceramic (ALCOA A-16, Al2O3-1.5% of CrO) was used to test the proposed method. Microstructural measurements of grain shape and size taken from fracture surfaces have been compared through descriptive statistics of distributions, with the corresponding measurements from polished and etched surfaces. The agreement between results, with the expected bias on grain size values from fractures, obtained for both types of surfaces allowed to infer that this new technique can be used to extract the relevant microstructural information from fractured surfaces, thus minimising the time consuming steps of sample preparation. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The stretch zone width (SZW) data for 15-5PH steel CTOD specimens fractured at -150 degrees C to + 23 degrees C temperature were measured based on focused images and 3D maps obtained by extended depth-of-field reconstruction from light microscopy (LM) image stacks. This LM-based method, with a larger lateral resolution, seems to be as effective for quantitative analysis of SZW as scanning electron microscopy (SEM) or confocal scanning laser microscopy (CSLM), permitting to clearly identify stretch zone boundaries. Despite the worst sharpness of focused images, a robust linear correlation was established to fracture toughness (KC) and SZW data for the 15-5PH steel tested specimens, measured at their center region. The method is an alternative to evaluate the boundaries of stretched zones, at a lower cost of implementation and training, since topographic data from elevation maps can be associated with reconstructed image, which summarizes the original contrast and brightness information. Finally, the extended depth-of-field method is presented here as a valuable tool for failure analysis, as a cheaper alternative to investigate rough surfaces or fracture, compared to scanning electron or confocal light microscopes. Microsc. Res. Tech. 75:11551158, 2012. (C) 2012 Wiley Periodicals, Inc.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fatigue, corrosion and wear resistance are important parameters in aircraft components development as landing gear. High strength/weight ratio and effective corrosion resistance make of titanium alloys an alternative choice to replace steel and aluminum alloys. However, titanium alloys have poor tribological properties, which reduce devices performance under friction. PVD coatings tribological systems has been increased due to their attractive mechanical properties as low environmental impact, low friction coefficient, low wear rate and hardness up to 2000 HV.In this study the influence of TiN deposited by PVD on the fatigue strength of Ti-6Al-4V alloy was evaluated. Comparison of fatigue strength of coated specimens and base material shows also a decrease when parts are coated. It was observed that the influence is more significant in high cycle fatigue tests. Scanning electron microscopy technique (SEM) was used to observe crack origin sites and fracture features. (C) 2010 Published by Elsevier Ltd.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Introduction. The postoperative acute renal failure (ARF) incidence in different kinds of surgery has rarely been studied. Age, cardiac dysfunction, previous renal dysfunction, intraoperative hypoperfusion, and use of nephrotoxic medications are mentioned as risk factors for ARF at the postoperative period. The postoperative ARF definition was based on the creatinine increase by the RIFLE classification (R = risk, I = injury, F = failure, L = loss, E = end stage), which corresponds to a 1.5 creatinine increase, two to three times, respectively, above the basal value. This study aimed to evaluate the postoperative ARF incidence in elderly patients who underwent femur fracture surgery under subarachnoid anesthesia and stratify it by the RIFLE criteria. Methods. Ninety patients older than 65 years under spinal anesthesia with fixed dosage of 15 mg of 0.5% isobaric bupivacaine associated with morphine 50 g were studied. Immediate postoperative creatinine was considered basal and compared with maximal creatinine evaluated at 24, 48, and 72 postoperative hours. Results. The mean age of the patients was 80.27 years. ARF incidence was 24.44% and stratified this way: R = 21.11% and I = 3.33%. Conclusions. In conclusion, the postoperative ARF incidence after femur fracture surgery in patients over 65 years was 24.44%. By analyzing the stratification based on the RIFLE classification, the incidence was categorized as Risk (R) = 21.11% and Injury (I) = 3.33%.