The effects of constitution of precursor mixed powders and scan speed on microstructure and wear properties were designed and investigated during laser clad gamma/Cr7C3/TiC composite coatings on gamma-TiAl intermetallic alloy substrates with NiCr-Cr3C2 precursor mixed powders. The results indicate that both the constitution of the precursor mixed powders and the beam scan rate have remarkable influence on microstructure and attendant hardness as well as wear resistance of the formed composite coatings. The wear mechanisms of the original TiAl alloy and laser clad composite coatings were investigated. The composite coating with an optimum compromise between constitution of NiCr-Cr3C2 precursor mixed powders as well as being processed under moderate scan speed exhibits the best wear resistance under dry sliding wear test conditions. (C) 2008 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Metallic glass has since its debut been of great research interest due to its profound scientific significance. Magnetic metallic glasses are of special interest because of their promising technological applications. In this thesis, we introduced a novel series of Fe-based alloys and offer a holistic review of the physics and properties of these alloys. A systematic alloy development and optimization method was introduced, with experimental implementation on transition metal based alloying system. A deep understanding on the influencing factors of glass forming ability was brought up and discussed, based on classical nucleation theory. Experimental data of the new Fe-based amorphous alloys were interpreted to further analyze those influencing factors, including reduced glass transition temperature, fragility, and liquid-crystal interface free energy. Various treatments (fluxing, overheating, etc.) were discussed for their impacts on the alloying systems' thermodynamics and glass forming ability. Multiple experimental characterization methods were discussed to measure the alloys' soft magnetic properties. In addition to theoretical and experimental investigation, we also gave a detailed numerical analysis on the rapid-discharge-heating-and-forming platform. It is a novel experimental system which offers extremely fast heating rate for calorimetric characterization and alloy deformation.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The Hall coefficient and resistance in several specimens of an amorphous metallic alloy containing 80 at.% palladium and 20 at.% silicon have been investigated at temperatures between 4.2°K and room temperature. An ideal limiting behavior of these transport coefficients was analyzed on the basis of the nearly free electron model to yield a carrier density of 9 x 1022 cm.-3, or about 1.7 electrons per palladium atom, and a mean free path of about 9Å which is almost constant with temperature. The deviations of the individual specimens from this ideal behavior, which were small but noticeable in the relative resistivity and much greater in the Hall coefficient, can be explained by invoking disk-shaped crystalline regions with low resistivity and a positive Hall coefficient. A detailed calculation shows how a volume fraction of such crystalline material too small to be noticed in X-ray diffraction could have a significant effect on the resistivity and a much greater effect on the Hall coefficient.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The coarsening kinetics of Ni3 Si(γ') precipitate in a binary Ni-Si alloy containing 6.5 wt. % silicon was studied by magnetic techniques and transmission electronmicroscopy. A calibration curve was established to determine the concentration of silicon in the matrix. The variation of the Si content of the Ni-rich matrix as a function of time follows Lifshitz and Wagner theory for diffusion controlled coarsening phenomena. The estimated values of equilibrium solubility of silicon in the matrix represent the true coherent equilibrium solubilities.

The experimental particle-size distributions and average particle size were determined from dark field electron micrographs. The average particle size varies linearly with t-1/3 as suggested by Lifshitz and Wagner. The experimental distributions of particle sizes differ slightly from the theoretical curve at the early stages of aging, but the agreement is satisfactory at the later stages. The values of diffusion coefficient of silicon, interfacial free energy and activation energy were calculated from the results of coarsening kinetics. The experimental value of effective diffusion coefficient is in satisfactory agreement with the value predicted by the application of irreversible the rmodynamics to the process of volume constrained growth of coherent precipitate during coarsening. The coherent γ' particles in Ni-Sialloy unlike those in Ni-Al and Ni-Ti seem to lose coherency at high temperature. A mechanism for the formation of semi-coherent precipitate is suggested.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structure and the electrical and magnetic properties of an amorphous alloy containing approximately 80 at .% iron, 13 at.% phos phorus and 7 at.% carbon (Fe_(80)Fe_(13)C_7) obtained by rapid quenching from the liquid state have been studied. Transmission electron diffraction data confirm the amorphous nature of this alloy. An analysis of the radial distribution function obtained from X-ray diffraction data indicates that the number of nearest neighbors is approximately seven, at a distance of 2.6A. The structure of the alloy can be related to that of silicate glasses and is based on a random arrangement of trigonal prisms of Fe_2P and Fe_3C types in which the iron atoms have an average ligancy of seven. Electrical resistance measurements show that the alloys are metallic. A minimum in the electrical resistivity vs. temperature curve is observed between 10° K to 50° K depending on the specimen, and the temperature at which the minimum occurs is related to the degree of local ordering. The Fe-P-C amorphous alloys are ferromagnetic. The Curie temperature measured by the induction method and by Mossbauer spectroscopy is 315° C. The field dependence of the magneto-resistance at temperatures from liquid helium to room temperature is similar to that found in crystalline iron. The ordinary Hall coefficient is approximately 10^(-11) volt-cm/amp-G. The spontaneous Hall coefficient is about 0.6 x 10^(-9) volt-cm/amp-G and is practically independent of temperature from liquid helium temperature up to 300° c.