932 resultados para poly(vinyl chloride)
Resumo:
A new class of polymeric amine, namely, sulfonated cardo poly(arylene ether sulfone) (SPES-NH2) was synthesized and used for the preparation of thin-film composite membrane. The TFC membranes were prepared on a polysulfone supporting film through interfacial polymerization with trimesoyl chloride (TMC) solutions and amine solutions containing SPES-NH2 and m-phenylenediamine (MPDA). The resultant membranes were characterized with water permeation performance, chemical structure, hydrophilicity of active layer and membrane morphology including top surface and cross-section.
Resumo:
A convenient and cost-effective strategy for synthesis of hyperbranched poly(ester-amide)s from commercially available dicarboxylic acids (A(2)) and multihydroxyl secondary amine (CB2) has been developed. By optimizing the conditions of model reactions, the AB(2)-type intermediates were formed dominantly during the initial reaction stage. Without any purification, the AB(2) intermediate was subjected to thermal polycondensation in the absence of any catalyst to prepare the aliphatic and semiaromatic hyperbranched poly(ester-amide)s bearing multi-hydroxyl end-groups.
Resumo:
Branched polystyrenes with abundant pendant vinyl functional groups were prepared via radical polymerization of an asymmetric divinyl monomer, which possesses a higher reactive styryl and a lower reactive butenyl. Employing a fast reversible addition fragmentation chain transfer (RAFT) equilibrium, the concentration of active propagation chains remained at a low value and thus crosslinking did not occur until a high level of monomer conversion. The combination of a higher reaction temperature (120 degrees C) and RAFT agent cumyl dithiobenzoate was demonstrated to be optimal for providing both a more highly branched architecture and a higher polymer yield.
Resumo:
Super-hydrophobic films with vinyl-modified silica nanoparticles (V-SiOx-NPs) were successfully prepared. The rough surface, which was composed of microstructures of disordered V-SiOx-NPs and nanostructures on the surface of V-SiOx-NPs, rather than the chemical composition devoted to the super-hydrophobicity of film. The relationship between contact angle and diameter of V-SiOx-NPs was then investigated. The sessile contact angles (CA) of films with 150-1600nm V-SiOx-NPs were around 166 regardless the diameter, while the film with 85 nm V-SiOx-NPs had the lowest CA of about 158. The packing manner of V-SiOx-NPs determined the air fraction on the surface and then the CA.
Resumo:
Hyperbranched vinyl polymers were prepared by reversible addition-fragmentation chain transfer ( RAFT) polymerization of a styrenic asymmetric divinyl monomer. This was achieved by using cumyl dithiobenzoate or S-dodecyl-S'-(alpha,alpha'-dimethyl-alpha ''-acetic acid) trithiocarbonate as the chain transfer agent, 1,1'-azobis(cyclohexanecarbonitrile) or thermal initiation as a source of radicals. Cross-linking was inhibited by a rapid RAFT-based equilibrium between active propagation chains and dormant species, and thus a hyperbranched polymer with a monomer conversion as high as 80% was obtained. The hyperbranched structure and properties of the resultant polymers were characterized by a combination of H-1-NMR spectroscopy and a triple detection size exclusion chromatography (TRI-SEC). The hyperbranched vinyl polymer has a broad molecular weight distributions and a low Mark-Houwink exponent alpha value compared with the linear counterpart.
Resumo:
A series of soluble poly(amide-imide)s (PAIs) bearing triethylammonium sulfonate groups were synthesized directly using trimellitic anhydride chloride (TMAC) polycondensation with sulfonated diamine such as 2,2'-benzidinedisulfonic acid (BDSA), 4,4'-diaminodiphenyl ether-2,2'-disulfonic acid (ODADS), and nonsulfonated diamine 4,4-diaminodiphenyl methane in the presence of triethylamine. The resulting copolymers exhibited high molecular weights (high inherent viscosity), and a combination of desirable properties such as good solubility in dipolar aprotic solvents, film-forming capability, and good mechanical properties. Wide-angle X-ray diffraction revealed that the polymers were amorphous. These copolymers showed high permeability coefficients of water vapor because of the presence of the hydrophilic triethylammonium sulfonate groups. The water vapor permeability coefficients (P-w) and permselectivity coefficients of water vapor to nitrogen and methane [alpha(H2O/N-2) and (alpha(H2O/CH4)] Of the films increased with increasing the amount of the triethylammonium sulfonated groups.
Resumo:
Reversible addition-fragmentation chain transfer (RAFT) mediated radical polymerizations of allyl methacrylate and undecenyl methacrylate, compounds containing two types of vinyl groups with different reactivities, were investigated to provide hyperbranched polymers. The RAFT agent benzyl dithiobenzoate was demonstrated to be an appropriate chain-transfer agent to inhibit crosslinking and obtain polymers with moderate-to-high conversions. The polymerization of allyl methacrylate led to a polymer without branches but with five- or six-membered rings. However, poly(undecenyl methacrylate) showed an indication of branching rather than intramolecular cycles. The hyperbranched structure of poly(undecenyl methacrylate) was confirmed by a combination of H-1, C-13, H-1-H-1 correlation spectroscopy, and distortionless enhancement by polarization transfer 135 NMR spectra. The branching topology of the polymers was controlled by the variation of the reaction temperature, chain-transfer-agent concentration, and monomer conversion. The significantly lower inherent viscosities of the resulting polymers, compared with those of linear analogues, demonstrated their compact structure,
Resumo:
A new straightforward strategy for synthesis of novel hyperbranched poly (ether amide)s from readily available monomers has been developed. By optimizing the reaction conditions, the AB(2)-type monomers were formed dominantly during the initial reaction stage. Without any purification, the AB(2) intermediate was subjected to further polymerization in the presence (or absence) of an initiator, to prepare the hyperbranched polymer-bearing multihydroxyl end-groups. The influence of monomer, initiator, and solvent on polymerization and the molecular weight (MW) of the resultant polymers was studied thoroughly. The MALDI-TOF MS of the polymers indicated that the polymerization proceeded in the proposed way. Analyses of H-1 NMR and C-13 NMR spectra revealed the branched structures of the polymers obtained. These polymers exhibit high-moderate MWs and broad MW distributions determined by gel permeation chromatography (GPC) in combination with triple detectors, including refractive index, light scattering, and viscosity detectors. In addition, the examination of the solution behavior of these polymers showed that the values of intrinsic viscosity [eta] and the Mark-Houwink exponent a were remarkably lower compared with their linear analogs, because of their branched nature.
Microwave-assisted synthesis of high-molecular-weight poly(ether imide)s by phase-transfer catalysis
Resumo:
A facile and rapid polycondensation reaction of disodium bisphenol A with bis(chlorophthalimide)s was preformed with a domestic microwave oven in o-dichlorobenzene by phase-transfer catalysis. The polymerization reactions, in comparison with conventional heating polycondensation, proceeded rapidly and were completed within 25 min. The polymerizations gave the corresponding poly(ether imide)s with inherent viscosities of 0.55-0.92 dL g(-1). The effects of various factors on the polymerization, such as the amount of the catalyst, the reaction time, and the microwave power were studied. The properties of the polymers were briefly characterized.
Resumo:
Poly(L-lactide) (PLLA) and poly(epsilon-caprolactone) (PCL) ultrafine fibers were prepared by electrospinning. The influence of cationic and anionic surfactants on their enzymatic degradation behavior was investigated by measuring weight loss, molecular weight, crystallinity, and melting temperature of the fibers as a function of degradation time. Under the catalysis of proteinase K, the PLLA fibers containing the anionic surfactant sodium docecyl sulfate (SDS) exhibited a faster degradation rate than those containing cationic surfactant triethylbenzylammonium chloride (TEBAC), indicating that surface electric charge on the fibers is a critical factor for an enzymatic degradation. Similarly, TEBAC-containing PCL fibers exhibited a 47% weight loss within 8.5 h whereas SDS-containing PCL fibers showed little degradation in the presence of lipase PS. By analyzing the charge status of proteinase K and lipase PS under the experimental conditions, the importance of the surface charges of the fibers and their interactions with the charges on the enzymes were revealed. Consequently, a "two-step" degradation mechanism was proposed: (1) the enzyme approaches the fiber surface; (2) the enzyme initiates hydrolysis of the polymer.
Resumo:
A new method for syntheses of hyperbranched poly(ester-amide)s from commercially available A(2) and CBx type monomers has been developed on the basis of a series of model reactions. The aliphatic and semiaromatic hyperbranched poly(ester-amide)s with multihydroxyl end groups are prepared by in situ thermal polycondensation of intermediates obtained from dicarboxylic acids (A(2)) and multihydroxyl primary amines (CBx) in N,N-dimethylformamide. Analyses of FTIR, H-1 NMR, and C-13 NMR spectra revealed the structures of the polymers obtained. The MALDI-TOF MS of the polymers indicated that cyclization side reactions occurred during polymerization. The hyperbranched poly(ester-amide) s contain configurational isomers observed by C-13 and DEPT C-13 NMR spectroscopy. The DBs of the polymers were determined to be 0.38-0.62 by H-1 NMR or quantitive C-13 NMR and DEPT 135 spectra. These polymers exhibit moderate molecular weights, with broad distributions determined by size exclusion chromatography ( SEC), and possess excellent solubility in a variety of solvents such as N, N- dimethylacetamide, dimethyl sulfoxide, tetrahydrofuran, and ethanol, and display glass-transition temperatures (T(g)s) between -2.3 and 53.2 degrees C, determined by DSC measurements.
Resumo:
Poly(ether ketone ether ketone ketone) containing meta-phenylene linkage (PEKEKK(T/I)) was synthesized by electrophilic Friedel-Crafts acylation condensation of 1, 4-diphenoxybenzophenone with terephthaloyl chloride (T) and isophthaloyl chloride (I) with a T/I ratio of 1 and characterized by LR,DSC,TGA and WAXD. PEKEKK(T/I) has two different crystal structures: a conventional Farm I structure, the same as that observed in PEEK and PEK, wich is usually developed from melt crystallization, and a new Form II structure which can be developed from cold crystallization or solvent induced crystallization (by exposing the glassy sample to methylene chloride).
Resumo:
In this paper, the synthesis and crystallization behavior of poly(ether ether ketone ether ketone) (PEEKEK) are reported. PEEKEK was prepared from 4,4'-bis(p-fluorobenzoyl) diphenyl ether (4,4'-FBDE) and hydroquinone along the nucleophilic substitution route. The thermal properties were investigated by using DSC and TGA. The crystallization behavior of PEEKEK under several conditions, i.e., crystallization from the molten state (melt crystallization), crystallization from a quenched sample (cold crystallization) and crystallization induced by exposing glassy sample to methylene chloride (solvent-induced crystallization) has also been investigated. The results show that crystallization of PEEKEK could be induced by the above methods, and no polymorphism was found. The differences in the crystallization of PEEKEK induced by the above methods are seen in their degree of crystallinity.
Resumo:
Novel poly(amide imide)s (PAI) containing alkyl-substituted cyclohexylidene moieties were synthesized by conventional polycondensation of trimellitic anhydride chloride with novel aromatic diamines followed by chemical imidization using acetic anhydride and pyridine. The inherent viscosities of the resulting PAIs are relatively high and range from 71 to 112 mt g(-1). The prepared PAIs show excellent thermal stability and good solubility. The glass transition temperatures (T-g) measured by DSC are observed in the range of 312-342 degrees C. Furthermore, all the polymers are readily soluble in less hygroscopic organic solvents like cyclohexanone, gamma-butyrolactone as well as aprotic polar solvents.
Resumo:
Block copolymers of poly(ethersulphone) (PES) oligomers with liquid crystalline polyester units were synthesized by the reaction of dihydroxy-terminated poly(ether sulphone) oligomers (number-average molecular weights: 704, 1,158 and 2570) and terephthaloyl bis(4-oxybenzoyl chloride), and their properties were investigated. The results indicated that the copolymer with PES segments of molecular weight of 704 possessed birefringent features when annealed at 360 degrees C, while the copolymer with PES segments of molecular weight of 2,570 became isotropic. Also, the block copolymers had a better chemical resistance and high-temperature stability than PES.