949 resultados para Cobalt phthalocyanine
Resumo:
Solid lipid nanoparticles (SLN) without drug and SLN loaded with chloroaluminum phthalocyanine (AlClPc) were prepared by solvent diffusion method in aqueous system and characterized by thermal analyses and X-ray diffraction (XRD) in this study. Determination of particle size, zeta potential (ZP), and encapsulation efficiency were also evaluated. SLN containing AlClPc of nanometer size with high encapsulation efficiency and ZP were obtained. The results indicated that the size of SLN loaded with AlClPc is larger than that of the inert particle, but ZP is not changed significantly with incorporation of the drug. In differential scanning calorimetry (DSC) curves, it was observed that the melting point of stearic acid (SA) isolated and in SLN occurred at 55 and 64 degrees C, respectively, suggesting the presence of different polymorphs. DSC also shows that the crystallinity state of SLN was much less than that of SA isolated. The incorporation of drug in SLN may have been favored by this lower crystallinity degree of the samples. XRD techniques corroborated with the thermal analytic techniques, suggesting the polymorphic modifications of stearic acid.
Resumo:
The aims of this study were two fold; to develop magnetoliposomes (MLs) loaded with zinc phthalocyanine (ZnPc) complexed with cucurbituril (CB) (CB:ZnPc-MLs) and to evaluate their in vitro photodynamic (PD) and/or hyperthermia (HT) effects while using melanoma cells (B16-F10) as model. The liposomal formulations were characterized by both average diameter and zeta potential. The vesicle average size ranged from 150 to 200 nm and the polydispersity index (PdI) from 0.093 to 0.230. The zeta potential was significantly positive with values between 48 and 57 mV. The cell viability (CV) after PD and HT treatments was assessed by colorimetric MTI method. Melanoma cells were initially treated with the liposome formulation without light and magnetic field application, revealing cell viability not different from the control cells (p > 0.05). Photodynamic and hyperthermia assays were also applied separately, demonstrating that PD is more effective than HT in reducing the CV of the neoplastic cells. Combined application of both PD and HT treatments was even more effective in reducing the CV of B16-F10 cells. At the highest light dose (2 J/cm(2)) and under magnetic field activation the CV was about half than PD applied alone. Therefore, the use of the photosensitizer-loaded magnetoliposome for combined photodynamic therapy (PDT) and magnetohyperthermia (MHT) application can be considered as a potential tool to treat malignant melanoma. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
The aim of this study was to evaluate the potential application of biodegradable nanoparticles containing a photosensitizer in photodynamic therapy. The poly (D,L lactic-co-glycolic acid) nanoparticles were studied by steady-state techniques, time-resolved fluorescence, and laser flash photolysis. The external morphology of the nanoparticles was established by scanning electron microscopy, and the biological activity was evaluated by in vitro cell culture by 3-(4,5 dimethylthiazol-2,5 biphenyl) tetrazolium bromide assay. The particles were spherical in shape exhibiting a 435 nm diameter with a low tendency to aggregate. The loading efficiency was 77%. The phthalocyanine-loaded-nanoparticles maintained their photophysical behavior after encapsulation. The cellular viability was determined, obtaining 70% of cellular death. All the performed physical-chemical, photophysical, and photobiological measurements indicated that the phthalocyanine-loaded-nanoparticles are a promising drug delivery system for photodynamic therapy and photoprocesses. (C) 2012 Laser Institute of America.
Resumo:
The biofilms formed by opportunistic yeasts serve as a persistent reservoir of infection and impair the treatment of fungal diseases. The aim of this study was to evaluate photodynamic inactivation (PDI) of biofilms formed by Candida spp. and the emerging pathogens Trichosporon mucoides and Kodamaea ohmeri by a cationic nanoemulsion of zinc 2,9,16,23-tetrakis(phenylthio)-29H,31H-phthalocyanine (ZnPc). Biofilms formed by yeasts after 48 h in the bottom of 96-well microtiter plates were treated with the photosensitizer (ZnPc) and a GaAlAs laser (26.3 J cm(-2)). The biofilm cells were scraped off the well wall, homogenized, and seeded onto Sabouraud dextrose agar plates that were then incubated at 37A degrees C for 48 h. Efficient PDI of biofilms was verified by counting colony-forming units (CFU/ml), and the data were submitted to analysis of variance and the Tukey test (p < 0.05). All biofilms studied were susceptible to PDI with statistically significant differences. The strains of Candida genus were more resistant to PDI than emerging pathogens T. mucoides and K. ohmeri. A mean reduction of 0.45 log was achieved for Candida spp. biofilms, and a reduction of 0.85 and 0.84, were achieved for biofilms formed by T. mucoides and K. ohmeri, respectively. Therefore, PDI by treatment with nanostructured formulations cationic zinc 2,9,16,23- tetrakis (phenylthio)- 29H, 31H- phthalocyanine (ZnPc) and a laser reduced the number of cells in the biofilms formed by strains of C. albicans and non-Candida albicans as well the emerging pathogens T. mucoides and K. ohmeri.
Resumo:
Considerable effort has been made in recent years to optimize materials properties for magnetic hyperthermia applications. However, due to the complexity of the problem, several aspects pertaining to the combined influence of the different parameters involved still remain unclear. In this paper, we discuss in detail the role of the magnetic anisotropy on the specific absorption rate of cobalt-ferrite nanoparticles with diameters ranging from 3 to 14 nm. The structural characterization was carried out using x-ray diffraction and Rietveld analysis and all relevant magnetic parameters were extracted from vibrating sample magnetometry. Hyperthermia investigations were performed at 500 kHz with a sinusoidal magnetic field amplitude of up to 68 Oe. The specific absorption rate was investigated as a function of the coercive field, saturation magnetization, particle size, and magnetic anisotropy. The experimental results were also compared with theoretical predictions from the linear response theory and dynamic hysteresis simulations, where exceptional agreement was found in both cases. Our results show that the specific absorption rate has a narrow and pronounced maxima for intermediate anisotropy values. This not only highlights the importance of this parameter but also shows that in order to obtain optimum efficiency in hyperthermia applications, it is necessary to carefully tailor the materials properties during the synthesis process. (C) 2012 American Institute of Physics. [http://dx.doi.org/10.1063/1.4729271]
Resumo:
Ultra-thin (thicknesses of 50-90 nm) nanocomposite films of cobalt ferrite nanoparticles (np-CoFe2O4, 18 nm in diameter) and polyelectrolytes (doped polyaniline-PANI, poly-3,4-ethylenedioxy thiophene: polystyrene sulfonic acid-PEDOT:PSS, and sulfonated lignin-SL) are assembled layer-by-layer onto interdigitated microelectrodes aiming at to create novel nanostructured sensoactive materials for liquid media chemical sensors. The nanocomposites display a distinctive globular morphology with nanoparticles densely-packed while surrounded by polyelectrolytes. Due to the presence of np-CoFe2O4 the nanocomposites display low electrical conductivity according to impedance data. On the other hand, this apparent shortcoming turns such nanocomposites much more sensitive to the presence of ions in solution than films made exclusively of conducting polyelectrolytes. For example, the electrical resistance of np-CoFe2O4/PEDOT:PSS and PANI/SL/np-CoFe2O4/SL architectures has a 10-fold decrease when they are immersed in 20 mmol. L-1 NaCl solution. Impedance spectra fitted with the response of an equivalent circuit model suggest that the interface created between nanoparticles and polyelectrolytes plays a major role on the nanocomposites electrical/dielectrical behavior. Since charge transport is sensitive to nanoparticle-polyelectrolyte interfaces as well as to the physicochemical conditions of the environment, the np-CoFe2O4-based nanocomposites can be used as sensing elements in chemical sensors operated under ac regime and room temperature.
Resumo:
Multilayered nanocomposite films (thickness 50-90 nm) of cobalt ferrite nanoparticles (np-CoFe2O4, 18 nm) were deposited on top of interdigitated microelectrodes by the layer-by-layer technique in order to study their dielectric properties. For that purpose, two different types of nanocomposite films were prepared by assembling np-CoFe2O4 either with poly(3,4-ethylenedioxy thiophene):poly(styrene sulfonic acid) or with polyaniline and sulfonated lignin. Despite the different film architectures, the morphology of both was dominated by densely-packed layers of nanoparticles surrounded by polyelectrolytes. The dominant effect of np-CoFe2O4 was also observed after impedance spectroscopy measurements, which revealed that dielectric behavior of the nanocomposites was largely influenced by the charge transport across nanoparticle-polyelectrolyte interfaces. For example, nanocomposites containing np-CoFe2O4 exhibited a single low-frequency relaxation process, with time constants exceeding 15 ms. At 1 kHz, the dielectric constant and the dissipation factor (tan ᵟ) of these nanocomposites were 15 and 0.15, respectively. These values are substantially inferior to those reported for pressed pellets made exclusively of similar nanoparticles. Impedance data were further fitted with equivalent circuit models from which individual contributions of particle's bulk and interfaces to the charge transport within the nanocomposites could be evaluated. The present study evidences that such nanocomposites display a dielectric behavior dissimilar from that exhibited by their individual counterparts much likely due to enlarged nanoparticle- polyelectrolyte interfaces.
Resumo:
Verdünnte magnetische Halbleiter (DMS) sind technologisch vielversprechende Materialien mit sowohl ferromagnetischen als auch halbleitenden Eigenschaften. Sie gehören zu den entscheidenden Verbindungen bei der Entwicklung neuartiger Spintronikanwendungen. Bisher scheiterte der technologische Einsatz jedoch daran, dass die Curie Temperatur der meisten magnetischen Halbleiter viel zu niedrig ist. Neue Verbindungen auf Basis von ZnO wie Zn1-xCoxO sollen jedoch Ferromagnetismus oberhalb von Raumtemperatur zeigen. Die theoretischen Grundlagen der magnetischen Wechselwirkungen sind jedoch nicht verstanden und erfordern daher umfangreiche experimentelle Untersuchungen. Im Rahmen dieser Arbeit wurden dünne Filme aus Zn0.95Co0.05O mittels Laserablation hergestellt und bezüglich ihrer magnetischen, elektrischen und strukturellen Eigenschaften untersucht, mit dem Ziel den Ferromagnetismus in diesem Material besser zu verstehen. Dabei kamen verschiedene experimentelle Methoden zum Einsatz: wie Magnetometrie, Röntgendiffraktometrie, Magnetischer Röntgenzirkulardichroismus (XMCD), Elektronenspinresonanz sowie magnetoelektrische Transportmessungen. Bei entsprechend defektfördernden Herstellungsbedingungen zeigen die Proben klare ferromagnetische Eigenschaften oberhalb von Raumtemperatur mit einer Sättigungsmagnetisierung von ca. 2 Bohr Magneton / Co sowie einer Remanenz von bis zu 90%. Elektrische Transportmessungen zeigen zudem einen deutlichen Magnetowiderstand sowie einen anomalen Hall Effekt. Letzterer steigt mit der Probenmagnetisierung und spricht für intrinsischen Ferromagnetismus sowie eine geringe Spinpolarisation. Da der Ferromagnetismus mit höherer Ladungsträgerdichte jedoch verschwindet, ist eine ferromagnetische Wechselwirkung über die Leitungselektronen auszuschließen. Eine genauere Auswertung der magnetoelektrischen Messdaten deutet zudem auf ein leitendes Störstellenband hin, das unter Umständen selbst spinpolarisiert ist. Vieles spricht somit dafür, dass die ferromagnetische Ordnung über magnetische Polaronen zustande kommt. Einige strukturelle und magnetometrische Ergebnisse sowie Elektronenspinresonanzmessungen deuten zudem auf metallische Ausscheidungen in Form von Cobalt Clustern hin, die einen zusätzlichen extrinsischen ferromagnetischen Beitrag liefern, der deutlich größer sein könnte als der intrinsische. Überraschenderweise zeigen XMCD Messungen jedoch, dass Cobalt überhaupt nicht am Ferromagnetismus beteiligt ist. Insgesamt gibt es Anzeichen, dass magnetische Defekte eine entscheidende Rolle hinsichtlich des Magnetismus in Zn0.95Co0.05O spielen.
Resumo:
Aim of the present work of thesis is to synthesize new non-noble metal based complexes to be employ in redox reactions by a metal-ligand cooperative mechanism. The need of replacing toxic and expensive precious metal complexes with more available and benign metals, has led to the development of new compounds based on cobalt and iron, which are the metals investigated in this study. A carbonyl-tetrahydroborato-bis[(2-diisopropylphosphino)ethyl]amine-cobalt complex bearing a PNP-type ligand is synthesized by a three-step route. Optimization attempt of reaction route were assessed in order to lowering reaction times and solvent waste. New cobalt complex has been tested in esters hydrogenation as well as in acceptorless dehydrogenative coupling of ethanol. Other varieties of substrates were also tested in order to evaluate any possible applications. Concerning iron complex, dicarbonyl-(η4-3,4-bis(4-methoxyphenyl)-2,5-diphenylcyclopenta-2,4-dienone)(1,3-dimethyl-ilidene)iron is synthesized by a three steps route, involving transmetallation of a silver complex, derived from an imidazolium salt, to iron complex. In order to avoid solvent waste, optimization is assessed. Studies were performed to assess activity of triscarbonyl iron precursor toward imidazolium salt and silver complexes.
Resumo:
A 39-year-old female with elevated serum cobalt levels from her bilateral hip prostheses presented with a 3-week history of blurred vision in her left eye. Optical coherence tomography revealed patchy degeneration of the photoreceptor-retinal pigment epithelium (RPE) complex. The lesions were hypofluorescent on indocyanine green angiography. We postulate that this is a case of implant-related chorio-retinal cobalt toxicity.