Resumo:
In this study the levels of Cu, Fe, Pb and Zn, determined in hair of healthy children (25-85 months), living at Araraquara (São Paulo, Brasil) are reported. Analytical determinations were carried out by using atomic absorption spectrometry employing an air acetylene flame. The results obtained are discussed with regard to effect of sex and age, as well compared with others analogous studies.
Resumo:
The Raman, IR absorption and EXAFS spectra at the Ge K-edge and Pb LIII-edge of eight lead germanate glasses, with general formula xPbO(1-x)GeO2 with x = 0.20, 0.25, 0.33, 0.40, 0.50, 0.53, 0.56 and 0.60, have been measured. The occurrence of [GeO6] units besides [GeO4] could not be deduced unambiguously from the data. The vibrational and EXAFS data agree with a progressive depolymerization of the network. Starting from all Ge atoms linked to four bridging oxygens in GeO2 (x = 0), the number of tetrahedral units with one or two non-bridging oxygens increases with x. At low content, Pb2+ ions act as modifiers in the germanate structure, but to a lesser extent than an equivalent number of alkaline ions. © 1993.
Resumo:
Solid M-Ox compounds, where M represents Mg(II), Zn(II), Pb(II) and NbO(III), and Ox is 8-quinolinol, have been prepared. Thermogravimetry, derivative thermogravimetry (TG, DTG), differential scanning calorimetry (DSC), nuclear magnetic resonance (NMR) and infrared absorption spectra (IR) have been used to characterize and to study the thermal stability and thermal decomposition of these compounds. © 1997 Akadémiai Kiadó.
Resumo:
The freshwater planktonic alga Kirchneriella aperta was grown in batch cultures to stationary growth phase. Copper and lead complexation properties of the exudate from stationary and exponential growth phases were determined by titrations monitored by ion-selective electrodes. Molecular weight fractionation dialysis) and analysis of the titration data (Scatchard Plot) revealed that K. aperta releases metal-complexing ligands. Copper is associated with low and high molecular weight compounds, whereas lead forms complexes with only high molecular weight compounds. Gas-liquid chromatography showed that mannose and rhamnose make up 74% of the total high molecular weight organic material, with uronic acids present at 19%.
Resumo:
The phase evolution of lead titanate processed by the polymeric precursor method was investigated by thermal analysis, X-ray diffraction, and high-resolution transmission electron microscopy. The results showed that the cubic perovskite PbTiO3 (PT) phase is formed from an inorganic amorphous precursor at a temperature of 444 °C. A gradual transition from cubic to tetragonal perovskite PT was observed with the increase of calcination time at this temperature. HRTEM results showed that the cubic PT particles have a size of around 5 nm. The identification of cubic PT as an intermediate phase supports the hypothesis that the chemical homogeneity was kept at the molecular level during the synthesis process, with no cation segregation.
Resumo:
A new strategy for minimization of Cu2+ and Pb2+ interferences on the spectrophotometric determination of Cd2+ by the Malachite green (MG)-iodide reaction using electrolytic deposition of interfering species and solid phase extraction of Cd2+ in flow system is proposed. The electrolytic cell comprises two coiled Pt electrodes concentrically assembled. When the sample solution is electrolyzed in a mixed solution containing 5% (v/v) HNO3, 0.1% (v/v) H2SO4 and 0.5 M NaCl, Cu2+ is deposited as Cu on the cathode, Pb2+ is deposited as PbO2 on the anode while Cd2+ is kept in solution. After electrolysis, the remaining solution passes through an AG1-X8 resin (chloride form) packed minicolumn in which Cd2+ is extracted as CdCl4/2-. Electrolyte compositions, flow rates, timing, applied current, and electrolysis time was investigated. With 60 s electrolysis time, 0.25 A applied current, Pb2+ and Cu2+ levels up to 50 and 250 mg 1-1, respectively, can be tolerated without interference. For 90 s resin loading time, a linear relationship between absorbance and analyte concentration in the 5.00-50.0 μg Cd 1-1 range (r2 = 0.9996) is obtained. A throughput of 20 samples per h is achieved, corresponding to about 0.7 mg MG and 500 mg KI and 5 ml sample consumed per determination. The detection limit is 0.23 μg Cd 1-1. The accuracy was checked for cadmium determination in standard reference materials, vegetables and tap water. Results were in agreement with certified values of standard reference materials and with those obtained by graphite furnace atomic absorption spectrometry at 95% confidence level. The R.S.D. for plant digests and water containing 13.0 μg Cd 1-1 was 3.85% (n = 12). The recoveries of analyte spikes added to the water and vegetable samples ranged from 94 to 104%. (C) 2000 Elsevier Science B.V.
Resumo:
Piezoelectric composite, made from ferroelectric ceramic lead zirconate titanate (PZT) and vegetable based polyurethane (PU) polymer, was doped with a semiconductor filler, graphite. The resulting composite (PZT/C/PU) with 49/1/50- vol. % composition could be poled at lower field and shorter time due to the increased conductivity of the polymer phase following the introduction of graphite. The PZT/C/PU composite showed higher pyroelectric coefficient in comparison with the undoped PZT/PU composite with 50/50-vol. % composition. Also, the PZT/C/PU composite has shown the ability to detect both extensional and flexural modes of simulated acoustic emission (AE) at a distance up to 8.0 m from the source, thus indicating that it may be used for detection of structural damages.
Resumo:
Strontium-modified lead titanate thin films with composition Pb1-xSrxTiO3 were grown on Pt/Ti/SiO2/Si substrates using the polymeric precursor method. The structural phase evolution as a function of the Sr contents was studied using micro-Raman scattering, specular reflectance infrared Fourier transform spectroscopy, and x-ray diffraction. The results showed a gradual change from tetragonal to cubic structure, the transition occurring at about x = 0.58. The infrared reflectance spectra showed that the frequency of several peaks decreases as the strontium concentration increases. These features are correlated with a decrease in the tetragonal distortion of the TiO6 octahedra as the strontium concentration increases.
Resumo:
Transparent glass ceramics containing β-PbF2:Er 3+ nanocrystals were obtained through appropriate thermal treatments of a glass of molar composition 60PbGeO3-10PbF2-30CdF 2 doped with 0.5 mol% Er3+. Their optical properties, as well as upconversion processes among erbium ions in the glass and glass ceramic matrix were studied. From absorption spectra, Judd-Ofelt parameters and radiative transition rates for several excited levels were calculated. Emission spectra in the visible and NIR regions were collected, and stimulated emission cross sections were obtained by McCumber theory for the 4F 13/2→4I15/2 transition at 1.5 μm. Red and green upconversion emissions were measured in glass and glass ceramics upon excitation at 980 nm; lifetimes were measured in order to assess the upconversion mechanisms.
Resumo:
The optical limiting behavior and nonlinear optical properties of antimony and lead oxyhalide glasses were discussed. The large nonlinear absorption coefficients which range from 11 to 20 cm/GW was determined using standard Z-scan technique. The photodarkening in the samples were observed which suggested that they can also be useful for inscribing Bragg gratings using green lasers of moderate power.
Resumo:
The neutral hydrolysis reaction of post-consumer poly(ethylene terephthalate) in solid state was studied through the reaction of the polymer with water at the molar ratio 1:91 with autogenous pressure. Two sizes of post-consumer PET flakes and temperatures of 135 °C, 170°C and 205°C with pressures of 4.0 atm, 7.5 atm and 13.5 atm, respectively, were considered. With reaction time equal to 6h, the method reached 99% depolymerization at 205°C, 8.2% at 170 °C and 1.7% at 135°C. The reaction extension was measured by separating the terephthalic acid formed in the process and calculating by gravimetry how much material could still be reacted. Through the viscosimetry of diluted, solutions and the counting of carboxylic end groups in the remaining material from the gravimetric assay, it was possible to suggest that the reaction occurs randomly and in the whole volume of the polymeric particle and not solely on the surface. The terephthalic acid obtained and then purified was characterized by elemental analysis, magnetic nuclear resonance, size and panicle size distribution and spectrophotometry in the visible spectrum, and it was similar to the petrochemical equivalent, with purity recorded in carbon base equal to 99.9%.
Resumo:
Blue, green, red, and near-infrared upconversion luminescence in the wavelength region of 480 - 740 nm in Pr3+/Yb3+-codoped lead-cadmium-germanate glass under 980 nm diode laser excitation, is presented. Upconversion emission peaks around 485, 530, 610, 645, and 725 nm which were ascribed to the 3P0 - 3HJ (J=4, 5, and 6), and 3P0 - 3FJ (J=2, and 3,4), transitions, respectively, were observed. The population of the praseodymium upper 3P0 emitting level was accomplished through a combination of ground-state absorption of Yb3+ ions at the 2F7/2, energy-transfer Yb3+(2F 5/2) Pr3+(3H4), and excited-state absorption of Pr3+ ions provoking the 1G4 - 3P0 transition. The dependence of the upconversion luminescence upon the Yb3+-concentration and diode laser power, is also examined, in order to subsidize the proposed upconversion excitation mechanism.
Resumo:
Composites made of calcium modified lead titanate ceramic powder and poly (ether-ether-ketone) high performance polymer matrix were prepared in the film form using a hot press. The acoustic and electromechanical properties of the composites have been determined using the ultrasonic immersion technique and piezoelectric spectroscopy, respectively. The composite film with 60 - 40 vol.% PTCa/PEEK was tested as acoustic emission detector. Preliminary results shown that the piezo composite can be used as sensor to evaluate the behavior of materials.
Resumo:
The main goal of this work is to demonstrate that the use of recycled material originated from SiC ceramics is viable. These ceramics were produced by commercial starch consolidation process. Before calcination stage, surplus of these materials always appears. This surplus is rich in SiC and starch. Samples were made by material previously milled in automatic mortar and sieved (100 Tyler). Later, 10% of distilled water was added to the material and the mixture was pressed at 40 MPa. In order to characterize the ceramic, three point flexural test were made, according to the ASTM C1161/94 norm. The results were analyzed by Weibull statistical method. Apparent density and porosity measures also were made, according to ASTM C20/87 norm. A verification of the surface was made in the fracture area by the depth from focus method and SEM image analysis. The results showed that the recycling process is fully viable, being a good economic option and reduce possible pollutant effect to the environment.