Extractivism mineral is considered an activity highly degrading, due to the large volume of material that he moves in the form of ore and residues. The vast majority of mining companies do not show any technology or economically viable application that will allow the recycling of mineral residue, these being launched in areas receiving located the "open skies" degrade the environment. In Rio Grande do Norte to the production of ceramic red restricts their activities to the production of products such as: solid bricks, ceramic blocks, tiles, among others. Seeking to unite experiences and technical information that favor sustainable development, with important benefits to the construction sector and civil society in general, the present work studies the incorporation of the residue of scheelite in ceramic matrix kaolinitic, coming from the municipality of Boa Saúde - RN, in percentage of 5 %, 10 %, 20 %, 30% 40% and 50 %, by evaluating its microstructure, physical properties and formulation. The raw materials were characterized through the trials of X ray fluorescence, Diffraction of X rays, Differential Thermal Analysis and Termogravimetric Analysis. The samples were formed and fired at temperatures of 850o, 900o, 1000o, 1050o, 1100o, 1150o and 1200 oC, with isotherm of 1 hour and heating rate of 10 oC/min. Assays were performed technological of loss to fire, Water Absorption, Apparent Porosity, Apparent Density, Mass Loss in Fire and Bending Resistance; in addition to the Scanning Electron Microscopy, analyzing their physical and mechanical properties. The use of residue of scheelite in ceramic mass kaolinitic provided a final product with technological properties that meet the technical standards for the production of bricks and roofing tiles, with the percentage of 20% of waste that showed the best results

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nacomposites of polymers and lamellar clayminerals, has generated high scientific and technological interest, for having mechanical properties and gas barriers differentiated of polymers and conventional composites. In this work, it was developed nanocomposites by single screw extruder and injection, utilizing commercial raw material, with the goal to investigate the quality of new developed materials. It was evaluated the influence of the content and the kind of clay in the structure and in the nanocomposites properties. It was used regular and elastomeric poly (methyl methacrylate) (Acrigel LEP 100 and Acrigel ECP800) and six montmorillonites (Cloisite 10A, 11B, 15A, 20A, 25A e 30B) at the concentration of 1% e 3% in weight. The nanocomposites were characterized by X-ray diffraction (XRD), thermal gravimetric analysis (TGA), transmission electron microscopy (TEM), colorimetric, optical transparency, flexural and tensile tests, Rockwell hardness and esclerometry. It was founded that is possible to obtain intercalated and exfoliated nanocomposites PMMA/MMT, and the top results was obtained in the materials with 1%in clay weight organophilizated with 2M2HT (Cloisite 15A and 20A) presented intercalate and hybrid morphology (exfoliated and flocullated). The ones that was produced with organophilizated clay with 2MHTL8 (Cloisite 30B) had excellent visual quality, but the majority presented hybrid morphology. In the materials processed with organophilizated clay with MT2ETOH (Cloisite 30B), there were color change and loss of transparency. It occurs improvement in a few mechanical properties, mainly in the materials produced with PMMA elastomeric (Acrigel ECP800), being more significant, the increase in the resistance to stripping in those nanocomposites

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The state of Rio Grande do Norte presents a great potentiality for the production of ceramic tiles because of having natural raw material in quantity and quality making its economical exploration possible, beyond the great energetic differential of the state, the natural gás. This works aims to study the influence of the dolomite and granulometry concentration and calcinations temperature in the obtaining of formulations for porous coverings which have to be coherent to the project,s specifications. The experiments have involved the physical-chemical and mineralogical characterizations of raw materials and mechanical tests in the dry and burnt proof bodies preceding a mixture experiment planning with the use of the response surface methodology, in order to get the best raw materials combinations to produce a ceramic mass with specific properties. The twelve ceramic masses studied in this work were prepared by the via dry process, characterized, shaped by uniaxial pressing and sinterized in the temperatures of 940ºC, 1000ºC, 1060ºC, 1120ºC and 1180ºC, using a fast burning cycle. The crystalline phases formed during the sintering in the temperatures in study have revealed the presence of anorthite and diopside beyond quartz with a remaining phase. These phases were the main responsible ones by the physical- mechanical properties of the sinterized proof bodies. The proof bodies after the sintering stage have presented water absorption higher than 10% and a good dimensional stability in all studied temperatures. However, the flexural breaking strength results in the temperatures of 940ºC, 1000ºC and 1060ºC, under the temperature zone of the vitrification of ceramic whiteware do not reach the flexural breaking strength specific for the porous wall tile (15 MPa), but in the temperature of 1120ºC next to the vitrification temperature zone, some whiteware ceramic (formulations) has reached the specified value for the porous wall tile. The results of this work have showed that the studied raw materials have great importance for used in the production of porous wall tiles (BIII)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

O objetivo do presente trabalho foi o estudo da variabilidade das propriedades de resistência e rigidez à flexão estática e à densidade aparente (12%) entre a madeira juvenil e adulta de Pinus taeda L., de 37 anos de idade, procedente do Horto Florestal de Manduri, Estado de São Paulo. Na primeira parte do trabalho foram determinadas a região de madeira juvenil, a região de transição e a região de madeira adulta, por meio de estudos anatômicos (comprimento dos traqueídes axiais), segundo as recomendações das normas ABNT e IAWA. Os resultados mostraram que a região de madeira juvenil dessa espécie ocorre aproximadamente até o 18º anel de crescimento. Na segunda parte do trabalho foram analisados a resistência (módulo de ruptura - MOR) à flexão, o módulo de elasticidade (MOE) nessa mesma solicitação e a densidade aparente (12%) para as madeiras juvenil e adulta. Os resultados mostraram que o MOE e o MOR da madeira juvenil foram menores e mais variáveis que aqueles obtidos para madeira adulta. A densidade apresentou a mesma tendência observada nas propriedades avaliadas no ensaio de flexão estática.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The study of the physical and mechanic properties is an analysis of unquestioned importance on the production of the ceramic materials. In the region of the Recôncavo Baiano, there are ceramic and small brick factories, that still use rudimentary techniques, where the necessity of characterization of raw materials is denounced by the quality of the final product. The present work has for objective to study the behavior of the clay proceeding from the region of the Recôncavo, between the cities of Candeias and Camaçari/Ba, with addition of 5, 10 and 15% by weight of brick scraps, trying to optimize the physic and mechanical properties of the final product, aiming a better possibility of being manufactured, mechanic resistance, low linear retraction and water absorption. The brick scraps and the clay were characterized by FRX, DRX, TG, ATD and the granulometric analysis. Samples for testing where prepared by uniaxial pressing at 25Mpa, in 60x20x5mm size. The evaluated technological properties were: linear retraction, water absorption, apparent porosity and flexural strength. The samples were burned in electric oven in the temperatures of 850º, 950º and 1050ºC and compared its mechanical properties and the gresification. With addition of 15% by weight of brick scraps and burning at 900º-1000ºC the samples showed properties superior to that clay

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the manufacture of composite, textile materials are being used as reinforcement. Generally, the combination of the matrix with the textile material in the form of fibres or yarns is used depending on their distribution in the web. In the present work, in place of fibres or yarns, a knitted structure in the form of the final product which is defined as preform. The preform is weft knit manufactured with polyester filaments. In the manufacture of composite, polyester resin was used as matrix. The physical and mechanical properties as well as the formability of the weft knit were analysed. The physical and mechanical properties as well as the formability of the knitted structure were analysed. The results obtained on the analysis show that the courses and wales of the weft knit structure and the tensile properties help the formability of the structure and the impregnation of the resin. It could be clearly observed that composite structure in the direction of the courses support more tension than in the direction of the wales. In relation to the three points flexural tests it was possible to note that there was more flexion in the direction of wales, what was expected. It was also possible to note that there are other advantages such as reduction in the loss of materials used, homogeneity in the distribution of the knitted structure in the mould, reduction in the preparation time and also in the reduction in the cost of manufacture

Relevância:

30.00% 30.00%

Publicador:

Resumo:

There are a number of damaging mechanisms that various materials can suffer in service. However, when working with polymer composite materials, this is something that requires analysis, especially when exposed to adverse environmental conditions. Thus, the objective of the present thesis is the study of the direct influence of environmental aging and the form of hybridization of the reinforcement woven on the structural stability, surfacedegradation and fracture process of polymer composites laminates. For this, the development of two polymer composite laminates was necessary, where one of them was reinforced with a bi-directional woven with hybrid strandsofkevlar-49/glass-Efibers, and the other also with a bi-directionalwoven, however with weft and warpformed of alternating strandsof Kevlar-49 fibers and glass-E fiber The reinforcementwoven are industrially manufactured. Both laminates use a polyester resin as a matrixand are made up of four layers each. All laminates were industrially prepared by the hand lay-up method of manufacturing. To do this, test specimens were manufactured of the respective laminates and submitted to environmental aging accelerated through the aging chamber. They were exposed to alternating cycles of UV radiation and moisture (heated steam) for a standard defined period. At the end of the exposure period the specimens were subjected to mechanical tests of uniaxial tensile and bending in three points and to the characterizationsof the fracture and surface deterioration. In addition, they were submitted to a structural degradation assessment by the measurement of mass variation technique (MMVT) and the measurement of thickness variation technique (MTVT), this last technique being developed in this thesis. At the end of the analysis it was observed that the form of hybridization of the reinforcement woven and the aging process directly influence with losses or gain in mechanical properties, with losses in the structural degradation and in the formation and propagation of damage mechanism of the developedcomposite laminates

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the industry of ceramic in Rio G. do Norte, tile stands out as the most manufactured product by this industry, being the intermittent kiln abóbada and caieira the principal type of kiln used in burning. There was a need to make a study of the influence exerted by the type of kiln in which tiles are burnt in their thermo physical properties. The analysis started with 24 raw samples of tile, which was split in two groups of 12 samples and burnt in Abóbada and Caieira kiln. Besides that, it was made study of the tax of heat transfer to the environment (for each kiln). After having been burnt the samples were taken for laboratory analysis. The properties verified were impermeability, determination of dry mass, absorption of water, the load of bending rupture and its geometric characteristics, the tests were conducted following the currents standards. The tests were carried out according to the ABNT - NBR 15310. The calculation of the rate of heat transfer showed that the abóbada kiln is more efficient than the Caieira, however the results of tests on the samples revealed no superiority of one over another sample. So the furnace had no influence on the performance of the ceramic tiles

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This research presents an approach to the addition of curauá fibers and licuri fibers in a polypropylene resin matrix, such as an alternative proposal to reinforce the polymeric composites. Fiber content of 0 %, 5 %, 10 %, and 20% were analyzed for verification of their mechanical properties comparing them, inclusive with the properties of polypropylene. The grainulated biocomposites had been prepared in an extrusora. The test bodies had been molded by injection and submitted to the mechanical essays uniaxial traction, flexion on three points, impact, in addition to thermal tests (HDT). These biocomposites had been also subjected the essay physicist-chemistry index of fluidity (IF). It was observed that the biocomposites of PP with 20% curauá, obtained bigger increase in the modulus of elasticity and a bigger reduction in the resistance to the impact. In the mechanical behavior, for all the biocomposites, these were increases in values of the limit of drainage and tension of rupture, when tested by uniaxial traction, as they added the fibers. Another important point was the increase of the resistance the flexion. It was also noted that the addition of fibers reduced the thermal degradation of the mixture natural fibers / polypropylene.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the present work, three composites with distinct reinforcements (polyester, modal e polyester + modal), all if a unsaturated orthophthalic polyester resin as matrix were used, in order to conduct a comparative study by mechanical tests and water absorption. The fibre mats were prepared in a mat preparatory by immersion developed in the Textile Engineering Laboratory. The composites were manufactured using a closed mould process by compression using an unsaturated orthophthalic polyester resin as matrix and 1% MEK (methyl ethyl ketone peroxide) as an initiator. In each composite twelve samples with the dimensions of 150x25x3 mm were cut randomly for the mechanical analysis (tension x extension, three points bending and water absorption and Scanning Electron Micsroscopy). The mechanical tests were carried out in the Laboratório de Metais e Ensaios Mecânicos UFRN . All the analyses were carried out according to the ASTM norms. The resultant samples from the mechanical analysis were subjected for the Scanning Electron Microscopy analysis. Based on the results obtained, it was observed that the reinforced composite with two fibres (modal + polyester) presented better results in comparison to the other two composites both in the tension/extension as well on the three point bending tests. In the water absorption test, it was possible to observe an equilibrium in the water absorption by the modal and polyester composite, due to the union of the two fibres. In the SEM images, the regions of rupture in the composites as well as the adsorption between the fiber and the matrix could be observed

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study aims to evaluate the mechanical properties of polymer matrix composites reinforced with sisal fabric bidirectional tissue (Agave sisalana,) and E-glass fibers, containing the following configuration: a polymer matrix hybrid composite (Polyester Resin orthophalic) reinforced with three (3) layers of glass fibers and alternating-2 (two) layers of bidirectional sisal fabric, and finally a composite of polymer matrix reinforced with five (5) layers of glass fiber mat-type E. For this purpose as first step, the preparation of by sisal, since they are not on the market. The composites were made by manual lamination (Hand lay-up) and evaluated for tensile properties and three point bending both in the dry, and wet conditions aswele as immersed in oil. Macroscopic and microscopic characteristics of the materialsweve awalysed, after the completion of the mechanical tests. After the studies, it was proven that the sisal fiber decreases the tensile stiffness of the material above 50% for both situations studied the tensile strength of the material decreases by approximately 40% for the cases mentioned, and when compared to the specific strength stiffness values drop to 14.6% and 29.02% respectively for the dry state only. Constants for bending the values were are to approximately 50% to 25% for strength and stiffness of the material for the cases dry, wet and immersed in oil. Under the influence of tension fluids do not interfere in the stiffness of the material for the bending tests, the same does not occur with the resistance, and these values are modified only in the cases stiffness and flexural strength

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The composites manufactured with long fibres aligned in a single direction, and overlay has been shown to have better performance than the short fibers randomly distributed. In particular, the lignocellulosic fibers extracted from the sisal leaves, used in conjunction with the epoxy resin has attracted the attention of many researchers because the final properties of the system formed. In this work composites based on epoxy resin reinforced with sisal fibers were manufactured. The sisal fibres were treated with an alkaline solution of 0.06 mol/l NaOH. The treated, and untreated fibres were subjected to tension x extension tests. The composites were manufactured in the "Lossy" mold with the specifications of the samples to be produced (300x20x4 mm). The tension tests were carried out in accordance with the ASTM standards 3039 (for the composite aligned in a single direction) and ASTM D5573 (for composites in overlay), three point bending tests were performed according to ASTM D790. Analyzing the results of the tests of tension and three point bending tests, it was observed that the composites with the configuration of overlapping had the better elastic module in both tests. As to the maximum resistance to tension, the best result was the composites aligned in a single direction. Tests of absorption of water and micrographs are in progress

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work is the addition of a metallic ion, of the metal Manganese, in a clay of Rio Grande do Norte state for structural ceramics use, the objective this study was to assess the evolution of ceramic properties. The clay was characterized by Chemical and Thermal analysis and Xray difraction. The metallic ion was added in the clay as aqueous solutions at concentrations of 100, 150 and 200 mg / L. The molded by extrusion and the burned were temperatures at 850, 950, 1050 and 1150 º C. Was made Chemical Analysis and investigated the following parameters environmental and ceramic: Solubility, Colour, Linear Retraction (%), Water Absorption (%), Gresification Curves, Apparent Porosity (%), Apparent Specific Mass (g/cm3) and Flexion Rupture Module (kgf/cm2). The results showed that increasing the concentration of metallic ion, properties such as Apparent Porosity (%), Water Absorption (%) decreases and the Flexion Rupture Module (kgf/cm2) increases with increasing temperature independent of the concentration of the ion. The gresification curves showed that the optimum firing temperatures were in the range between 950 and 1050 ° C. The evaluation of the properties showed that the ceramic material can be studied its use in solid brick and ceramic materials with structural function of filling. The results of solubility showed that the addition of ion offers no risk to the environment

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)