993 resultados para plate metal
Resumo:
Tinplate is one of the most widely used food canning materials, however, there are significant problems related to the use of tinplate cans, such as alterations in sensory features affecting food quality and corrosion phenomena of the canning material. To avoid corrosion problems different methods have been used for the passivation of tinplate such protective lacquers or different kinds of corrosion inhibitors (chromate and dichromate). However, chromates and dichromates are extremely harmful to the environment and can cause carcinogenic tumors to humans. An option, protective coatings obtained by the sol-gel process, act as a physical barrier, which isolates the surface of metal protecting from the corrosive agents. The aim of this work is to study the influence of addition of cerium (IV) ions in the inorganic and organic part of sol-gel processing in the formation of hybrid coatings based on siloxane-PMMA on tin plate. The coatings were obtained by dip-coating technique and evaluated by open circuit and impedance measurements, linear polarization and polarization curves obtained in 3.5% NaCl solution. The results have clearly shown the improvement on the protective properties of the Ce 4+ modified film when added into the organic phase, which can be due to the formation of a more uniform and densely reticulated siloxane-PMMA film. © 2009 by NACE International.
Resumo:
This paper presents a new method to estimate hole diameters and surface roughness in precision drilling processes, using coupons taken from a sandwich plate composed of a titanium alloy plate (Ti6Al4V) glued onto an aluminum alloy plate (AA 2024T3). The proposed method uses signals acquired during the cutting process by a multisensor system installed on the machine tool. These signals are mathematically treated and then used as input for an artificial neural network. After training, the neural network system is qualified to estimate the surface roughness and hole diameter based on the signals and cutting process parameters. To evaluate the system, the estimated data were compared with experimental measurements and the errors were calculated. The results proved the efficiency of the proposed method, which yielded very low or even negligible errors of the tolerances used in most industrial drilling processes. This pioneering method opens up a new field of research, showing a promising potential for development and application as an alternative monitoring method for drilling processes. © 2012 Springer-Verlag London Limited.
Resumo:
Pós-graduação em Engenharia Mecânica - FEIS
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
The aim of this study was to perform a physicochemical and morphological characterization and compare the mechanical behavior of an experimental Ti-Mo alloy to the analogous metallic Ti-based fixation system, for mandibular angle fractures. Twenty-eight polyurethane mandibles were uniformly sectioned on the left angle. These were divided into 4 groups: group Eng 1P, one 2.0-mm plate and 4 screws 6 mm long; group Eng 2P, two 2.0-mm plates, the first fixed with 4 screws 6 mm long and the second with 4 screws 12 mm long. The same groups were created for the Ti-15Mo alloy. Each group was subjected to linear vertical loading at the first molar on the plated side in a mechanical testing unit. Means and standard deviations were compared with respect to statistical significance using ANOVA. The chemical composition of the Ti-15Mo alloy was close to the nominal value. The mapping of Mo and Ti showed a homogeneous distribution. SEM of the screw revealed machining debris. For the plates, only the cpTi plate undergoes a surface treatment. The metallographic analysis reveals granular microstructure, from the thermomechanical trials. A statistically significant difference was found (P < 0.05) when the comparison between both internal fixation techniques was performed. The 2P technique showed better mechanical behavior than 1P.
Resumo:
This paper reports an experimental method to estimate the convective heat transfer of cutting fluids in a laminar flow regime applied on a thin steel plate. The heat source provided by the metal cutting was simulated by electrical heating of the plate. Three different cooling conditions were evaluated: a dry cooling system, a flooded cooling system and a minimum quantity of lubrication cooling system, as well as two different cutting fluids for the last two systems. The results showed considerable enhancement of convective heat transfer using the flooded system. For the dry and minimum quantity of lubrication systems, the heat conduction inside the body was much faster than the heat convection away from its surface. In addition, using the Biot number, the possible models were analyzed for conduction heat problems for each experimental condition tested.
Resumo:
The development of a Laser Doppler Anemometer technique to measure the velocity distribution in a commercial plate heat exchanger is described. Detailed velocity profiles are presented and a preliminary investigation is reported on flow behaviour through a single cell in the channel matrix. The objective of the study was to extend previous investigations of plate heat exchanger flow patterns in the laminar range with the eventual aim of establishing the effect of flow patterns on heat transfer performance, thus leading to improved plate heat exchanger design and design methods. Accurate point velocities were obtained by Laser Anemometry in a perspex replica of the metal channel. Oil was used as a circulating liquid with a refractive index matched to that of the perspex so that the laser beams were not distorted. Cell-by-cell velocity measurements over a range of Reynolds number up to ten showed significant liquid mal-distribution. Local cell velocities were found to be as high as twenty seven times average velocity, contrary to the previously held belief of four times. The degree of mal-distribution varied across the channel as well as in the vertical direction, and depended on the upward or downward direction of flow. At Reynolds numbers less than one, flow zig-zagged from one side of the channel to the other in wave form, but increases in Reynolds number improved liquid distribution. A detailed examination of selected cells showed velocity variations in different directions, together with variation within individual cells. Experimental results are also reported on the flow split when passing through a single cell in a section of a channel . These observations were used to explain mal-distribution in the perspex channel itself.
Resumo:
In the bulge test, a sheet metal specimen is clamped over a circular hole in a die and formed into a bulge by the hydraulic pressure on one side of the specirnen. As the unsupported part of the specimen is deformed in this way, its area is increased, in other words, the material is generally stretched and its thickness generally decreased. The stresses causing this stretching action are the membrane stresses in the shell generated by the hydraulic pressure, in the same way as the rubber in a toy balloon is stretched by the membrane stresses caused by the air inside it. The bulge test is a widely used sheet metal test, to determine the "formability" of sheet materials. Research on this forming process (2)-(15)* has hitherto been almost exclusively confined to predicting the behaviour of the bulged specimen through the constitutive equations (stresses and strains in relation to displacements and shapes) and empirical work hardening characteristics of the material as determined in the tension test. In the present study the approach is reversed; the stresses and strains in the specimen are measured and determined from the geometry of the deformed shell. Thus, the bulge test can be used for determining the stress-strain relationship in the material under actual conditions in sheet metal forming processes. When sheet materials are formed by fluid pressure, the work-piece assumes an approximately spherical shape, The exact nature and magnitude of the deviation from the perfect sphere can be defined and measured by an index called prolateness. The distribution of prolateness throughout the workpiece at any particular stage of the forming process is of fundamental significance, because it determines the variation of the stress ratio on which the mode of deformation depends. It is found. that, before the process becomes unstable in sheet metal, the workpiece is exactly spherical only at the pole and at an annular ring. Between the pole and this annular ring the workpiece is more pointed than a sphere, and outside this ring, it is flatter than a sphere. In the forming of sheet materials, the stresses and hence the incremental strains, are closely related to the curvatures of the workpiece. This relationship between geometry and state of stress can be formulated quantitatively through prolateness. The determination of the magnitudes of prolateness, however, requires special techniques. The success of the experimental work is due to the technique of measuring the profile inclination of the meridional section very accurately. A travelling microscope, workshop protractor and surface plate are used for measurements of circumferential and meridional tangential strains. The curvatures can be calculated from geometry. If, however, the shape of the workpiece is expressed in terms of the current radial (r) and axial ( L) coordinates, it is very difficult to calculate the curvatures within an adequate degree of accuracy, owing to the double differentiation involved. In this project, a first differentiation is, in effect, by-passed by measuring the profile inclination directly and the second differentiation is performed in a round-about way, as explained in later chapters. The variations of the stresses in the workpiece thus observed have not, to the knowledge of the author, been reported experimentally. The static strength of shells to withstand fluid pressure and their buckling strength under concentrated loads, both depend on the distribution of the thickness. Thickness distribution can be controlled to a limited extent by changing the work hardening characteristics of the work material and by imposing constraints. A technique is provided in this thesis for determining accurately the stress distribution, on which the strains associated with thinning depend. Whether a problem of controlled thickness distribution is tackled by theory, or by experiments, or by both combined, the analysis in this thesis supplies the theoretical framework and some useful experimental techniques for the research applied to particular problems. The improvement of formability by allowing draw-in can also be analysed with the same theoretical and experimental techniques. Results on stress-strain relationships are usually represented by single stress-strain curves plotted either between one stress and one strain (as in the tension or compression tests) or between the effective stress and effective strain, as in tests on tubular specimens under combined tension, torsion and internal pressure. In this study, the triaxial stresses and strains are plotted simultaneously in triangular coordinates. Thus, both stress and strain are represented by vectors and the relationship between them by the relationship between two vector functions. From the results so obtained, conclusions are drawn on both the behaviour and the properties of the material in the bulge test. The stress ratios are generally equal to the strain-rate ratios (stress vectors collinear with incremental strain vectors) and the work-hardening characteristics, which apply only to the particular strain paths are deduced. Plastic instability of the material is generally considered to have been reached when the oil pressure has attained its maximum value so that further deformation occurs under a constant or lower pressure. It is found that the instability regime of deformation has already occurred long before the maximum pressure is attained. Thus, a new concept of instability is proposed, and for this criterion, instability can occur for any type of pressure growth curves.
Resumo:
The most perfectly structured metal surface observed in practice is that of a field evaporated field-ion microscope specimen. This surface has been characterised by adopting various optical analogue techniques. Hence a relationship has been determined between the structure of a single plane on the surface of a field-ion emitter and the geometry of a binary zone plate. By relating the known focussing properties of such a zone plate to those obtained from the projected images of such planes in a field-ion micrograph, it is possible to extract new information regarding the local magnification of the image. Further to this, it has been shown that the entire system of planes comprising the field-ion imaging surface may be regarded as a moire pattern formed between over-lapping zone plates. The properties of such moire zone plates are first established in an analysis of the moire pattern formed between zone plates on a flat surface. When these ideas are applied to the field-ion image it becomes possible to deduce further information regarding the precise topography of the emitter. It has also become possible to simulate differently proJected field-ion images by overlapping suitably aberrated zone plates. Low-energy ion bombardment is an essential preliminary to much surface research as a means of producing chemically clean surfaces. Hence it is important to know the nature and distribution of the resultant lattice damage, and the extent to which it may be removed by annealing. The field-ion microscope has been used to investigate such damage because its characterisation lies on the atomic scale. The present study is concerned with the in situ sputtering of tungsten emitters using helium, neon, argon and xenon ions with energies in the range 100eV to 1keV, together with observations of the effect of annealing. The relevance of these results to surface cleaning schedules is discussed.
Crack closure and residual stress effects in fatigue of a particle-reinforced metal matrix composite
Resumo:
A study of the influence of macroscopic quenching stresses on long fatigue crack growth in an aluminium alloy-SiC composite has been made. Direct comparison between quenched plate, where high residual stresses are present, and quenched and stretched plate, where they have been eliminated, has highlighted their rôle in crack closure. Despite similar strength levels and identical crack growth mechanisms, the stretched composite displays faster crack growth rates over the complete range of ΔK, measured at R = 0.1, with threshold being displaced to a lower nominal ΔK value. Closure levels are dependent upon crack length, but are greater in the unstretched composite, due to the effect of surface compressive stresses acting to close the crack tip. These result in lower values of ΔKeff in the unstretched material, explaining the slower crack growth rates. Effective ΔKth values are measured at 1.7 MPa√m, confirmed by constant Kmax testing. In the absence of residual stress, closure levels of approximately 2.5 MPa√m are measured and this is attributed to a roughness mechanism.
Resumo:
Devido às necessidades da indústria atual é cada vez mais importante a utilização de métodos de união de materiais distintos. A utilização de adesivos no processo de produção de materiais compósitos tem uma grande aplicação, uma vez que permite ligar os diferentes materiais e ainda reduzir significativamente o peso do conjunto. Este trabalho teve como principal objetivo aumentar a resistência à delaminação de materiais compósitos no sentido da espessura, concretamente dos plásticos reforçados com fibras de carbono (CFRP), através da utilização de placas da liga de alumínio 2024-T3. Este conceito é muito semelhante ao utilizado nos laminados por fibras e metal (LFM) para aumentar a sua resistência à delaminação. Pretendeu-se também a identificação da configuração da junta que apresenta melhores resultados, comparativamente à junta de referência composta apenas por CFRP. Inicialmente, produziram-se apenas juntas de CFRP que foram utilizadas como comparação com os laminados de fibras e metal. Com o objetivo de melhorar a adesão entre os CFRP e a liga de alumínio, foram realizados três tratamentos superficiais diferentes, nomeadamente a lixagem, a anodização e o ataque com ácido. Posteriormente, foram produzidas as juntas com as seguintes configurações: CFRP-AL-CFRP, CFRP-AL-CFRP-AL-CFRP e AL-CFRP-AL. A realização deste trabalho permitiu concluir que com a adição de placas de alumínio, se conseguiu um melhoramento da resistência à delaminação das fibras de carbono e ainda um aumento da resistência específica no sentido da sua espessura. A JSS com a configuração AL-CFRP-AL e com comprimento de sobreposição de 50 mm foi a configuração que apresentou uma força de rotura mais elevada, ou seja, uma maior resistência à delaminação, comparativamente à junta de referência e às restantes configurações em estudo. A falha coesiva verificada perto da interface da junta AL-CFRP-AL, pode ser devida ao elevado comprimento de sobreposição e às diferentes elasticidades do alumínio e do CFRP, o que naturalmente levou a elevadas tensões localizadas nas extremidades da junta. Os resultados demostraram que é possível aumentar a resistência transversal do compósito utilizando uma placa de alumínio.