1000 resultados para Veneers and veneering


Relevância:

40.00% 40.00%

Publicador:

Resumo:

The laminate veneers are great choice for rehabilitation for anterior segment of the mouth. Actually, due the employment of dental cements and bonding to dentin, the uses of laminate veneers is an effective and conservative treatment, showing a high rate success rate. This paper presents a clinical case of 50 years old male, J.C.H, who have a chief complaint of an unattractive smile. After the diagnosis and planning, 10 laminate veneers were placed from the second bicuspid (15) to the second bicuspid (25). The correct indication of laminate veneers allows restorations with appropriate esthetic and patient's satisfaction with immediate effect on quality of life. © 2011 Nova Science Publishers, Inc.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The aim of this study was to evaluate the deformation suffered by cantilevered implant-supported fixed prostheses frameworks cast in silver-palladium alloy and coated with two occlusal veneering materials: acrylic resin or porcelain. Material and Methods: Two strain gauges were bonded to the inferior surface of the silver-palladium framework and two other were bonded to the occlusal surface of the prosthesis framework covered with ceramic and acrylic resin on each of its two halves. The framework was fixed to a metallic master model and a 35.2 N compression force was applied to the cantilever at 10, 15 and 20 mm from the most distal implant. The measurements of deformation by compression and tension were obtained. The statistical 2-way ANOVA test was used for individual analysis of the experiment variables and the Tukey test was used for the interrelation between all the variables (material and distance of force application). Results: The results showed that both variables had influence on the studied factors (deformation by compression and tension). Conclusion: The ceramic coating provided greater rigidity to the assembly and therefore less distortion compared with the uncoated framework and with the resin-coated framework. The cantilever arm length also influenced the prosthesis rigidity, causing higher deformation the farther the load was applied from the last implant.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Objective. To test the hypothesis that the difference in the coefficient of thermal contraction of the veneering porcelain above (˛liquid) and below (˛solid) its Tg plays an important role in stress development during a fast cooling protocol of Y-TZP crowns. Methods. Three-dimensional finite element models of veneered Y-TZP crowns were developed. Heat transfer analyses were conducted with two cooling protocols: slow (group A) and fast (groups B–F). Calculated temperatures as a function of time were used to determine the thermal stresses. Porcelain ˛solid was kept constant while its ˛liquid was varied, creating different ˛/˛solid conditions: 0, 1, 1.5, 2 and 3 (groups B–F, respectively). Maximum ( 1) and minimum ( 3) residual principal stress distributions in the porcelain layer were compared. Results. For the slowly cooled crown, positive 1 were observed in the porcelain, orientated perpendicular to the core–veneer interface (“radial” orientation). Simultaneously, negative 3 were observed within the porcelain, mostly in a hoop orientation (“hoop–arch”). For rapidly cooled crowns, stress patterns varied depending on ˛/˛solid ratios. For groups B and C, the patterns were similar to those found in group A for 1 (“radial”) and 3 (“hoop–arch”). For groups D–F, stress distribution changed significantly, with 1 forming a “hoop-arch” pattern while 3 developed a “radial” pattern. Significance. Hoop tensile stresses generated in the veneering layer during fast cooling protocols due to porcelain high ˛/˛solid ratio will facilitate flaw propagation from the surface toward the core, which negatively affects the potential clinical longevity of a crown.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

OBJECTIVE To compare the precision of fit of full-arch implant-supported screw-retained computer-aided designed and computer-aided manufactured (CAD/CAM) titanium-fixed dental prostheses (FDP) before and after veneering. The null-hypothesis was that there is no difference in vertical microgap values between pure titanium frameworks and FDPs after porcelain firing. MATERIALS AND METHODS Five CAD/CAM titanium grade IV frameworks for a screw-retained 10-unit implant-supported reconstruction on six implants (FDI tooth positions 15, 13, 11, 21, 23, 25) were fabricated after digitizing the implant platforms and the cuspid-supporting framework resin pattern with a laser scanner (CARES(®) Scan CS2; Institut Straumann AG, Basel, Switzerland). A bonder, an opaquer, three layers of porcelain, and one layer of glaze were applied (Vita Titankeramik) and fired according to the manufacturer's preheating and fire cycle instructions at 400-800°C. The one-screw test (implant 25 screw-retained) was applied before and after veneering of the FDPs to assess the vertical microgap between implant and framework platform with a scanning electron microscope. The mean microgap was calculated from interproximal and buccal values. Statistical comparison was performed with non-parametric tests. RESULTS All vertical microgaps were clinically acceptable with values <90 μm. No statistically significant pairwise difference (P = 0.98) was observed between the relative effects of vertical microgap of unveneered (median 19 μm; 95% CI 13-35 μm) and veneered FDPs (20 μm; 13-31 μm), providing support for the null-hypothesis. Analysis within the groups showed significantly different values between the five implants of the FDPs before (P = 0.044) and after veneering (P = 0.020), while a monotonous trend of increasing values from implant 23 (closest position to screw-retained implant 25) to 15 (most distant implant) could not be observed (P = 0.169, P = 0.270). CONCLUSIONS Full-arch CAD/CAM titanium screw-retained frameworks have a high accuracy. Porcelain firing procedure had no impact on the precision of fit of the final FDPs. All implant microgap measurements of each FDP showed clinically acceptable vertical misfit values before and after veneering. Thus, the results do not only show accurate performance of the milling and firing but show also a reproducible scanning and designing process.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Plywood manufacture includes two fundamental stages. The first is to peel or separate logs into veneer sheets of different thicknesses. The second is to assemble veneer sheets into finished plywood products. At the first stage a decision must be made as to the number of different veneer thicknesses to be peeled and what these thicknesses should be. At the second stage, choices must be made as to how these veneers will be assembled into final products to meet certain constraints while minimizing wood loss. These decisions present a fundamental management dilemma. Costs of peeling, drying, storage, handling, etc. can be reduced by decreasing the number of veneer thicknesses peeled. However, a reduced set of thickness options may make it infeasible to produce the variety of products demanded by the market or increase wood loss by requiring less efficient selection of thicknesses for assembly. In this paper the joint problem of veneer choice and plywood construction is formulated as a nonlinear integer programming problem. A relatively simple optimal solution procedure is developed that exploits special problem structure. This procedure is examined on data from a British Columbia plywood mill. Restricted to the existing set of veneer thicknesses and plywood designs used by that mill, the procedure generated a solution that reduced wood loss by 79 percent, thereby increasing net revenue by 6.86 percent. Additional experiments were performed that examined the consequences of changing the number of veneer thicknesses used. Extensions are discussed that permit the consideration of more than one wood species.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Logs from two hardwood plantations in north Queensland were peeled to assess the veneer and plywood potential of fast-grown tropical plantation eucalypts. After visual grading and veneer recovery calculatios, selected veneers were assembled to produce plywood panels. These were tested for mechanical properties and glue bond strength to determine the suitability of young, fast-grown, tropical eucalytps for panel product applications.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The Australian African mahogany estate comprises over 12,000 ha of industrial plantations, farm-forestry plots and trials, virtually all derived from Africa-sourced wild seed. However, the better trees have given high-value products such as veneers, high-grade boards and award-winning furniture. Collaborative conservation and improvement by the Northern Territory (NT) and Queensland governments since 2000 realised seed orchards, hedge gardens and genetic tests revealing promising clones and families. Private sector R&D since the mid 2000s includes silvicultural-management and wood studies, participatory testing of government material and establishing over 90 African provenances and many single-tree seedlots in multisite provenance and family trials. Recent, mainly public sector research included a 5-agency project of 2009-12 resulting in advanced propagation technologies and greater knowledge of biology, wood properties and processing. Operational priority in the short term should focus on developing seed production areas and ‘rolling front’ clonal seed orchards. R&D priorities should include: developing and implementing a collaborative improvement strategy based on pooled resources; developing non-destructive evaluation of select-tree wood properties, micropropagation (including field testing of material from this source) to ‘industry ready’ and a select-tree index; optimising seed production in orchards; advancing controlled pollination techniques; and maximising benefits from the progeny, clone and provenance trials. Australia leads the world in improvement and ex situ conservation of African mahogany based on the governments’ 13-year program and more recent industry inputs such that accumulated genetic resources total over 120 provenances and many families from 15 of the 19 African countries of its range. Having built valuable genetic resources, expertise, technologies and knowledge, the species is almost ‘industry ready’. The industry will benefit if it exploits the comparative advantage these assets provide. However the status of much of the diverse germplasm introduced since the mid 2000s is uncertain due to changes in ownership. Further, recent reductions of government investment in forestry R&D will be detrimental unless the industry fills the funding gaps. Expansion and sustainability of the embryonic industry must capitalise on past and current R&D, while initiating and sustaining critical new work through all-stakeholder collaboration.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper compares the structural performance between thin-walled timber and FRP-timber composite Cee-sections. While, thin-walled composite timber structures have been proven to be efficient and ultra-light structural elements, their manufacturing is difficult and labour intensive. Significant effort and time is required to prevent the cracking of the transverse timber veneers, bent in the grain direction, when forming the cross-sectional shape. FRP-timber structures overcome this disadvantage by replacing the transverse veneers with flexible, unidirectional FRP material and only keeping the timber veneers which are bent in their natural rolling direction. The Cee-sections investigated in this study were 210 mm deep × 90 mm wide × 500 mm high and manufactured from five plies. For both section types, the three internal plies were thin (1 mm thick) softwood Hoop pine (Araucaria cunninghamii) veneers, orientated along the section longitudinal axis. The two outer layers, providing bending stiffness to the walls, were Hoop pine veneers (1 mm thick) for the timber sections and glass fibre reinforced plastic (0.73 mm thick) for the FRP-timber sections orientated perpendicular to the inner layers. The manufacturing process is briefly introduced in this paper. The profiles were fitted with strain gauges and tested in compression. Linear Variable Displacement Transducers also recorded the buckling along one flange. The test results are presented and discussed in this paper in regards to their structural behaviour and performance. Results showed that the use of FRP in the sections increases both the elastic local buckling load and section capacity, the latter being increased by about 24 percent. The results indicate that thin-walled FRP-timber can ultimately be used as a sustainable alternative to cold-formed steel profiles.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A pair of blades were constructed following a Tapered Chord, Zero Twist pattern after Anderson. The construction uses the Wood Epoxy Saturation Technique, with a solid Beech main spar and leading edge joined together with laminated veneers of beech forming a D-section; the trailing edge is formed from millimetre ply skins, foam filled to resist compressive loads. This construction leads to an extremely light, flexible blade, with the centres of gravity and torsion well forward, giving good stability. Each blade has three built-in strain gauges, alowing flapwise bending to be measured. Stiffness, and natural frequencies, were measured, to input to a numerical computer model to calculate blade deformation during operation, and to determine stability boundaries of the blade. Preliminary aerodynamic performance measurements are presented and close agreement is found with theory.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Studies has been reported a significant incidence of chipping of the feldspathic porcelain veneer in zirconia-based restorations. The purpose of this study was to compare the three-point flexural strength (MPa), Weibull parameters, Vickers hardness (VHN) and Vickers indentation fracture toughness (MPa/mm(1/2)) in feldspatic porcelains for metal and for zirconia frameworks. Bar specimens were made with the porcelains e.MaxCeram (EM) and VitaVM9 (V9) for zirconia core, and Duceragold (DG) and VitaVMK95 (VK) for metal core (n = 15). Kruskal-Wallis and Dun test were used for statistical analysis. There was no significant difference (p=0.31) among the porcelains in the flexural strength (Median = 73.2; 74.6; 74.5; 74.4). Weibull calculation presented highest reliability for VK (10.8) followed by em (7.1), V9 (5.7) and DG (5.6). Vickers hardness test showed that em (536.3), V9 (579.9) and VK (522.1) had no difference and DG (489.6) had the lowest value (p<.001). The highest fracture toughness was to VK (1.77), DG (1.58) had an intermediate value while V9 (1.33) and em (1.18) had the lowest values (p<.001). Despite of the suitable flexural strength, reliability and high hardness, the porcelains used to zirconia-based fixed dental prostheses showed lower fracture toughness values.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Objectives. To test the hypothesis that multiple firing and silica deposition on the zirconia surface influence the bond strength to porcelain.Materials and methods. Specimens were cut from yttria-stabilized zirconia blocks and sintered. Half of the specimens (group S) were silica coated (physical vapor deposition (PVD)) via reactive magnetron sputtering before porcelain veneering. The remaining specimens (group N) had no treatment before veneering. The contact angle before and after silica deposition was measured. Porcelain was applied on all specimens and submitted to two (N2 and S2) or three firing cycles (N3 and S3). The resulting porcelain-zirconia blocks were sectioned to obtain bar-shaped specimens with 1 mm(2) of cross-sectional area. Specimens were attached to a universal testing machine and tested in tension until fracture. Fractured surfaces were examined using optical microscopy. Data were statistically analyzed using two-way ANOVA, Tukey's test (alpha = 0.05) and Weibull analysis.Results. Specimens submitted to three firing cycles (N3 and S3) showed higher mean bond strength values than specimens fired twice (N2 and S2). Mean contact angle was lower for specimens with silica layer, but it had no effect on bond strength. Most fractures initiated at porcelain-zirconia interface and propagated through the porcelain.Significance. The molecular deposition of silica on the zirconia surface had no influence on bond strength to porcelain, while the number of porcelain firing cycles significantly affected the bond strength of the ceramic system, partially accepting the study hypothesis. Yet, the Weibull modulus values of S groups were significantly greater than the m values of N groups. (C) 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Objectives: Based on a maxillary premolar restored with laminate veneer and using the 3-D finite element analysis (FEA) and mCT data, the aim of this study was to evaluate the influence of different types of buccal cusp reduction on the stress distribution in the porcelain laminate veneer and in the resin luting cement layer. Methods: Two 3-D FEA models (M) of a maxillary premolar were built from mCT data. The buccal cusp reduction followed two configurations: Mt-buccal cusp completely covered by porcelain laminate veneer; and Mp-buccal cusp partially covered by porcelain laminate veneer. The loading (150 N in 458) was performed on the top of the buccal cusp. The finite element software (Ansys Workbench 10.0) was used to obtain the maximum shear stress (σmax) and maximum principal stress (σmax). Results: The Mp showed reduced the stress (σmax) in porcelain laminate veneer (from-2.3 to 24.5 MPa) in comparison with Mt (from-5.3 to 27.4 MPa). The difference between the peak and lower stress values of σmax in Mp (-6.8 to 26.7 MPa) and Mt (-5.3 to 27.4 MPa) was similar for the resin luting cement layer. The structures not exceeded the ultimate tensile strength or the shear bond strength. Conclusions: Cusp reduction did not affect significant increase in σmax and τmax. The Mt showed better stress distribution (τmax) than Mp. © 2011 Published by Elsevier Ireland on behalf of Japan Prosthodontic Society.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Aim: The present case report described the use of contact lens of thin porcelain veneers as a restorative therapy to solve anterior teeth disharmony. Background: Fragments of thin veneers are minimally invasive restorations with little or no dental preparation and present thickness ranging from 0.2 to 0.5 mm. They are used in case of diastema closure, small changes of teeth, color and restoration of teeth with small fractures. Case report: A 25-year-old man was admitted at a dental clinic complaining about the diastema presence on the upper anterior teeth. Patient was referred to an orthodontic treatment in order to provide better distribution of the diastemas and harmonious proportion of the teeth. Afterwards, contact lens of thin porcelain veneers were fabricated on the six upper anterior teeth. Conclusion: Based on the outcomes of this clinical report, we considered the use of fragments of thin veneers as a successful treatment option after 3 years of follow-up. Clinical significance: The fragments of thin veneers have been established to be an interesting alternative to esthetically restore the anterior teeth with minimal invasiveness. However, since it is a new treatment modality, longitudinal studies are necessary to understand the material's behavior.