838 resultados para Slip casting
Resumo:
The purpose of this monograph is to take a new look at various aspects of stone artefact analysis that reveal important and exciting new information about the past. This invovles reorienting our methodological approach to stone artefacts as well as the questions asked of them. The papers making up this volume tackle a number of issues that have long been at the heart of archaeology’s problematic relationship with stone artefacts, including our understanding of the dynamic nature of past stoneworking practices, the utility of traditional classificatory schemes, and ways to unlock the vast amount of information about the strategic role of lithic technology that resides in stone artefact assemblages.
Resumo:
The influence of sodium (Na) on nucleation and growth of the Al-Si eutectic in a commercial hypoeutectic Al-Si-Cu-Mg foundry alloy has been investigated. The microstructural evolution during eutectic solidification was studied by a quenching technique. By comparing the orientation of the aluminium in the eutectic to that of the surrounding primary aluminium dendrites by EBSD, the eutectic solidification mode could be determined. The results show that the eutectic solidification starts near the mould wall and evolves with front growth opposite the thermal gradient on a macro-scale, and on a micro-scale with independent heterogeneous nucleation of eutectic grains in interdendritic spaces. Na-modified alloys therefore behave significantly differently from those modified by other elemental additions.
Resumo:
Yield strength (YS) ageing curves have been modelled for A356 and A357 aluminium casting alloys below the solvus temperature of the main hardening precipitate. Predictions are based on the Shercliff and Ashby methodology (Acta MetaH. Mater. 38 (1990) 1789) for wrought alloys. Differences between strengthening in wrought and cast Al-Si-Mg alloys are considered. A Brinell hardness to YS conversion incorporating strain hardening has been established to enable YS ageing curves to be predicted with reduced experimental effort. (C) 2002 Elsevier Science B.V. All rights reserved.
Desenvolvimento de estruturas porosas tridimensionais por moldação por congelamento (Freeze-Casting)
Resumo:
Dissertação para obtenção do Grau de Mestre em Engenharia Biomédica
Resumo:
Dissertação para obtenção do Grau de Mestre em Engenharia de Materiais
Resumo:
This work presents a numerical study of the 4:1 planar contraction flow of a viscoelastic fluid described by the simplified Phan-Thien–Tanner model under the influence of slip boundary conditions at the channel walls. The linear Navier slip law was considered with the dimensionless slip coefficient varying in the range ½0; 4500. The simulations were carried out for a small constant Reynolds number of 0.04 and Deborah numbers (De) varying between 0 and 5. Convergence could not be achieved for higher values of the Deborah number, especially for large values of the slip coefficient, due to the large stress gradients near the singularity of the reentrant corner. Increasing the slip coefficient leads to the formation of two vortices, a corner and a lip vortex. The lip vortex grows with increasing slip until it absorbs the corner vortex, creating a single large vortex that continues to increase in size and intensity. In the range De = 3–5 no lip vortex was formed. The flow is characterized in detail for De ¼ 1 as function of the slip coefficient, while for the remaining De only the main features are shown for specific values of the slip coefficient.
Resumo:
A systematic study for the production of porous poly(vinylidene fluoride-trifluoroethylene), P(VDF-TrFE), films using solvent evaporation and non-solvent induced phase separation techniques is presented. Processing parameters such as copolymer volume fraction, solvent, preset exposure time to air before immersion, and non-solvent and temperature of the coagulation bath were varied and the corresponding sample morphology, hydrophobicity, thermal and mechanical properties were determined. Film morphologies including homogeneous pore distributions, micropores, microvoids, spherulites and non-porous films were obtained. The morphology variations strongly influence sample hydrophobicity and mechanical properties. All samples crystallize in the electroactive β-phase with a degree of crystallinity around 30 %.
Resumo:
Identification of the tensile constitutive behaviour of Fibre Reinforced Concrete (FRC) represents an important aspect of the design of structural elements using this material. Although an important step has been made with the introduction of guidance for the design with regular FRC in the recently published fib Model Code 2010, a better understanding of the behaviour of this material is still necessary, mainly for that with self-compacting properties. This work presents an experimental investigation employing Steel Fibre Self-Compacting Concrete (SFRSCC) to cast thin structural elements. A new test method is proposed for assessing the post-cracking behaviour and the results obtained with the proposed test method are compared with the ones resulted from the standard three-point bending tests (3PBT). Specimens extracted from a sandwich panel consisting of SFRSCC layers are also tested. The mechanical properties of SFRSCC are correlated to the fibre distribution by analysing the results obtained with the different tests. Finally, the stress-crack width constitutive law proposed by the fib Model Code 2010 is analysed in light of the experimental results.
Resumo:
Magdeburg, Univ., Fak. für Maschinenbau, Diss., 2010
Resumo:
Magdeburg, Univ., Fak. für Verfahrens- und Systemtechnik, Diss., 2012