The purpose of the study was to verify the effects of a number of materials' parameters (crystalline content; Young's modulus, E; biaxial flexure strength, sigma(i); Vickers hardness, VH; fracture toughness, K-Ic; fracture surface energy, gamma(f); and index of brittleness, B) on the brittleness of dental ceramics. Five commercial dental ceramics with different contents of glass phase and crystalline particles were studied: a vitreous porcelain (VM7/V), a porcelain with 16 vol% leucite particles (d.Sign/D), a glass-ceramic with 29 vol% leucite particles (Empress/E1), a glass-ceramic with 58 vol% lithium-disilicate needle-like particles (Empress 2/E2), and a glass-infiltrated alumina composite with 65 vol% crystals (In-Ceram Alumina/IC). Discs were constructed according to manufacturers' instructions, ground and polished to final dimensions (12 mm x 1.1 mm). Elastic constants were determined by ultrasonic pulse-echo method. sigma(i) was determined by piston-on-3-balls method in inert condition. VH was determined using 19.6 N load and K-Ic was determined by indentation strength method. gamma(f) was calculated from the Griffith-Irwin relation and B by the ratio of HV to K-Ic. IC and E2 showed higher values of sigma(i), E, K-Ic and gamma(f), and lower values of B compared to leucite-based glass-ceramic and porcelains. Positive correlations were observed for sigma(i) versus K-Ic, and K-Ic versus E-1/2, however, E did not show relationship with HV and B. The increase of crystalline phase content is beneficial to decrease the brittleness of dental ceramics by means of both an increase in fracture surface energy and a lowering in index of brittleness. (C) 2012 Elsevier Ltd and Techna Group Sri. All rights reserved.
Resumo:
The effect of CO2 continuous laser irradiation on the surface properties of veneering porcelains has already been tested. The surface observed after laser irradiation is similar to that achieved by auto-glaze in terms of roughness and color parameters (Sgura R, et al. Dental Materials 2011;27(Suppl. 1):e72–73). The purpose of this study was to analyze the surface porosity of porcelain discs after CO2 laser treatment and compare it to auto-glaze treatment, in furnace. A morphological analysis of the porcelain surface was conducted using atomic force microscopy (AFM) and conventional optical microscopy (OM).
Resumo:
Durante el proceso de elaboración de las porcelanas feldespáticas se producen en su interior micro rajaduras las cuales se propagan a través de la matriz vítrea aumentando la fragilidad del material cuando se lo expone a los esfuerzos mecánicos. Las restauraciones rígidas de porcelanas feldespáticas son sometidas a distintos tratamientos en su superficie para aumentar la adhesión a las estructuras dentarias cuando son cementadas. Estos tratamientos son acondicionamiento con ácido fluorhídrico y microarenado. Objetivos de este trabajo: 1. Evaluar la resistencia flexural de este material mediante ensayo mecánico en máquina Instron, previo tratamiento en su superficie con ácido fluorhídrico y microarenado. 2. Observar al MEB las alteraciones de superficie producidas por el microarenado y el ácido fluorhídrico. Los resultados obtenidos demostraron que el tratamiento de microarenado produjo una reducción de la resistencia flexural. El MEB confirmó la presencia de mayor cantidad de microgrietas que podrían ser responsables de la disminución de la resistencia flexural.
Resumo:
The catalogue of porcelains and the second part of the catalogue are largely the work of J. Getz.
Resumo:
Thirty-nine trace elements of the Song-Yuan period (960-1368 AD) porcelain bodies from Cizhou, Jizhou and Longquanwu kilns were analyzed with ICP-MS, a technique rarely used in Chinese archaeometry, to investigate its potential application in such studies. Trace element compositions clearly reflect the distinctive raw materials and their mineralogy at the three kilns and allow their products to be distinguished. Significant chemical variations are also observed between Yuan and Song-Jing dynasties samples from Cizhou as well as fine and coarse porcelain bodies from Longquanwu. In Cizhou, porcelains of better quality which imitate the famous Ding kiln have trace element features distinctive from ordinary Cizhou products, that indicates geochemically distinctive raw materials were used and which possibly also underwent extra refining prior to use. The distinct trace element features of different kilns and the various types of porcelains from an individual kiln can be interpreted from a geochemical perspective. ICP-MS can provide a large amount of valuable information about ancient Chinese ceramics as it is capable of analyzing >40 elements with a typical of precision < 2%.
Resumo:
Tang sancai is one of the most important types of Chinese ceramics. To determine the provenance of Tang sancai is important to study ancient trade and other issues. In this paper we compare ICP-MS trace elements and TIMS Sr-Nd isotopes of visibly similar Tang sancai from two major production centres Gongxian and Yaozhou. The variation in contents/ratios of many of > 40 trace elements is small for samples from Gongxian, yet is considerably bigger for that from Yaozhou. However, the variation in Sr-87/Sr-86 and Nd-143/Nd-144 isotopic ratios is very small for samples from both places. Gongxian and Yaozhou samples have distinctive Sr-Nd isotopic and trace element features despite their similarity in major elements, and these analysis data can be interpreted with geochemistry, indicating that Sr and Nd isotopes have great potential in ceramic provenance studies. The distinct characterisation of these samples provides valuable criteria for identifying provenance of Tang sancai of uncertain origin. Two modern fakes are also analysed, and they can as well be distinguished from antique Tang sancai using above criteria. (c) 2005 Published by Elsevier Ltd.
Resumo:
The partial fixed prosthodontics restoration is used to rehabilitate form and function of partial or total compromised teeth, having to remain permanently joined to remainder tooth. The most useful material on prosthodontics is the feldspar porcelain, commercialized as aluminosilicate powders. Dental porcelains are presented with limited mechanical properties to rehabilitate extensive spaces. The association with Ni-Cr metallic systems (metal-ceramic system) allows that the metallic substructure compensates the fragile porcelain nature, preserving the thermal insulation and aesthetics desirable, as well as reducing the possibility of cracking during matication efforts. Cohesive flaws by low mechanical strength connect the metallic substructure to the oral environment, characterized by a electrolytic solution (saliva), by aggressive temperature, pH cyclic changes and mechanical requests. This process results on ionic liberation that could promote allergic or inflammatory responses, and/or clinical degradation of ceramometal system. The aim of this study was to evaluate the presence of an intermediate titanium layer on the microscopic fracture behavior of porcelains on ceramometal systems. Plasma deposition of titanium films result in regular passivating oxide layers which act as barriers to protect the metallic substrate against the hazardous effects of corrosive saliva. Tribocorrosion tests were performed to simulate the oral environment and mechanical stress, making it possible the early detection of crack formation and growth on metal-ceramic systems, which estimate the adherence between the compounds of this system. Plain samples consisting of dental feldspar porcelain deposited either onto metallic substrates or titanium films were fired and characterized by scanning electron microscopy. The result showed that the titanium film improved the adherence of the system compared to conventional metal-ceramic interfaces, thus holding crack propagation
Resumo:
The power industry generates as waste ceramic bodies of electrical fuses that are discarded after use. The formulation of ceramic bodies for porcelain electrical insulators using waste from the bodies fuse allocation promotes environmentally appropriate, through the reuse of the material. This work evaluated the technical feasibility of using waste for use in electrical porcelains with formulations containing the residue, feldspar and kaolinite. The raw materials were processed through grinding and sieving to 200 mesh. The ceramic material obtained from the proposed formulations with 25%, 30%, 34% and 40% of the residue went through a vibratory mill for grinding and homogenization, and then were sieved at 325 mesh. The samples were shaped in a uniaxial press, with the application of 25 MPa and sintered at 1100° C, 1150°C, 1200°C, 1225°C and 1250°C, at levels of 20 and 45 minutes. Were also developed bodies of evidence with reference formulations obtained without residue, to establish a comparison on physical, mechanical and electrical. The tests were conducted and technology: linear shrinkage, porosity, water absorption, resistance to bending to three points, measuring insulation resistance electrical resistivity of the material, X-ray diffraction and X-ray fluorescence Waste characterizations pointed to the existence of two phases: mullite and quartz phases are of great importance in the microstructure of the ceramic and this fact reveals a possibility for reuse in electrical porcelains. The mullite is an important constituent because it is a phase that makes it possible to increase the mechanical strength in addition to the body allows the use at high temperatures. The use of ceramic bodies residue fuses, proved feasible for application in electrical porcelain and the most significant results were obtained by the formulations with 25% waste and sintering at 1200°C