833 resultados para POLY(ETHER IMIDE)S
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Retention of overdentures is important for patients' satisfaction. The study tested whether the clinical performance of retentive clips made of poly-ether-ether-ketone (PEEK) is superior to those made of poly-oxy-methylene (POM).
Resumo:
Polymer/inorganic nanoparticle nanocomposites have garnered considerable academic and industrial interest over recent decades in the development of advanced materials for a wide range of applications. In this respect, the dispersion of so-called inorganic fullerene-like (IF) nanoparticles, e.g., tungsten disulfide (IF-WS2) or molybdenum disulfide (IF-MoS2), into polymeric matrices is emerging as a new strategy. The surprising properties of these layered metal dichalcogenides such as high impact resistance and superior tribological behavior, attributed to their nanoscale size and hollow quasi-spherical shape, open up a wide variety of opportunities for applications of these inorganic compounds. The present work presents a detailed overview on research in the area of IF-based polymer nanocomposites, with special emphasis on the use of IF-WS2 nanoparticles as environmentally friendly reinforcing fillers. The incorporation of IF particles has been shown to be efficient for improving thermal, mechanical and tribological properties of various thermoplastic polymers, such as polypropylene, nylon-6, poly(phenylene sulfide), poly(ether ether ketone), where nanocomposites were fabricated by simple melt-processing routes without the need for modifiers or surfactants. This new family of nanocomposites exhibits similar or enhanced performance when compared with nanocomposites that incorporate carbon nanotubes, carbon nanofibers or nanoclays, but are substantially more cost-effective, efficient and environmentally satisfactory. Most recently, innovative approaches have been described that exploit synergistic effects to produce new materials with enhanced properties, including the combined use of micro- and nanoparticles such as IF-WS2/nucleating agent or IF-WS2/carbon fiber, as well as dual nanoparticle systems such as SWCNT/IF-WS2 where each nanoparticle has different characteristics. The structure–property relationships of these nanocomposites are discussed and potential applications proposed ranging from medicine to the aerospace, automotive and electronics industries.
Resumo:
The influence of singlewalled carbon nanotubes (SWCNT) and inorganic fullerenelike tungsten disulfide nanoparticles (IFWS2) on the morphology and thermal, mechanical and electrical performance of multifunctional fibrereinforced polymer composites has been investigated. Significant improvements were observed in stiffness, strength and toughness in poly (ether ether ketone) (PEEK) / (SWCNT) / glass fibre (GF) laminates when a compatibilizer was used for wrapping the CNTs. Hybrid poly(phenylene sulphide) (PPS)/IFWS2/ carbon fibre (CF) reinforced polymer composites showed improved mechanical and tribological properties attributed to a synergetic effect between the IF nanoparticles and CF.
Resumo:
Thermosetting blends of an aliphatic epoxy resin and a hydroxyl-functionalized hyperbranched polymer (HBP), aliphatic hyperbranched polyester Boltorn H40, were prepared using 4,4'-diaminodiphenylmethane (DDM) as the curing agent. The phase behavior and morphology of the DDM-cured epoxy/HBP blends with HBP content up to 40 wt% were investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and scanning electron microscopy (SEM). The cured epoxy/HBP blends are immiscible and exhibit two separate glass transitions, as revealed by DMA. The SEM observation showed that there exist two phases in the cured blends, which is an epoxy-rich phase and an HBP-rich phase, which is responsible for the two separate glass transitions. The phase morphology was observed to be dependent on the blend composition. For the blends with HBP content up to 10 wt%, discrete HBP domains are dispersed in the continuous cured epoxy matrix, whereas the cured blend with 40 wt% HBP exhibits a combined morphology of connected globules and bicominuous phase structure. Porous epoxy thermosets with continuous open structures on the order of 100-300 nm were formed after the HBP-rich phase was extracted with solvent from the cured blend with 40 wt% HBP. The DSC study showed that the curing rate is not obviously affected in the epoxy/HBP blends with HBP content up to 40 wt %. The activation energy values obtained are not remarkably changed in the blends; the addition of HBP to epoxy resin thus does not change the mechanism of cure reaction of epoxy resin with DDM. (c) 2006 Wiley Periodicals, Inc.
Resumo:
The dielectric properties of pure low to medium molecular weight poly(ethylene glycol) and poly(propylene glycol) and a variety of their salt complexes have been studied through the measurement of the dielectric permittivity and dielectric loss over a range of frequency and temperature. The major proportion of this study has been concerned with the examination of the nature of the interaction between mercuric chloride and poly(propylene glycol) (PPG). Other salt-poly-ether combinations have also been considered such as cobalt chloride-PPG cadmium chloride-PPG zinc chloride-PPG and ferric chloride-PEG (polyethylene glycol). Some of this work was also supported by chemical shift and spin-lattice Nuclear Magnetic Resonance (N.M.R.) spectroscopy. The dielectric permittivity data were analysed using the Onsager relation to calculate the mean dipole moment per dipolar unit. This approach was employed in the discussion of various models proposed for the structure of salt-polyether complexes. The effect of mercuric chloride on the statistical conformations of poly(propylene-glycol) was studied in a quantitative manner using the relationships of marchal-Benoit. The dielectric relaxation activation energy and mean energy difference between gauche and trans conformations of poly(propylene glycol) in the presence of mercuric chloride, both showed a distinct minimum when the concentration of mercuric chloride was close to 5 mole %. Opposite behaviour was observed for the Cole-Cole parameter. It was concluded that the majority of the dielectric data could be rationalised in terms of a 5-membered cyclic complex formed between mercuric chloride and PPG in which the complexed segment of the polyether-(OMeCH2CH2O)- adopted either gauche or cis conformations.
Resumo:
A new method combining electrospinning of SPEEK and direct spinning of CNT forests has been used to prepare sulfonated poly(ether ether ketone) (SPEEK)/directly spinnable carbon nanotube (dsCNT) composite proton exchange membranes. The SPEEK/dsCNT membrane is more robust than SPEEK alone, and in a fuel cell significantly outperforms both SPEEK and the commercial Nafion 212 membranes.
Resumo:
Most commercially available reverse osmosis (RO) and nanofiltration (NF) membranes are based on the thin film composite (TFC) aromatic polyamide membranes. However, they have several disadvantages including low resistance to fouling, low chemical and thermal stabilities and limited chlorine tolerance. To address these problems, advanced RO/NF membranes are being developed from polyimides for water and wastewater treatments. The following three projects have resulted from my research. (1) Positively charged and solvent resistant NF membranes. The use of solvent resistant membranes to facilitate small molecule separations has been a long standing industry goal of the chemical and pharmaceutical industries. We developed a solvent resistant membrane by chemically cross-linking of polyimide membrane using polyethylenimine. This membrane showed excellent stability in almost all organic solvents. In addition, this membrane was positively charged due to the amine groups remaining on the surface. As a result, high efficiency (> 95%) and selectivity for multivalent heavy metal removal was achieved. (2) Fouling resistant NF membranes. Antifouling membranes are highly desired for “all” applications because fouling will lead to higher energy demand, increase of cleaning and corresponding down time and reduced life-time of the membrane elements. For fouling prevention, we designed a new membrane system using a coating technique to modify membrane surface properties to avoid adsorption of foulants like humic acid. A layer of water-soluble polymer such as polyvinyl alcohol (PVA), polyacrylic acid (PAA), polyvinyl sulfate (PVS) or sulfonated poly(ether ether ketone) (SPEEK), was adsorbed onto the surface of a positively charged membrane. The resultant membranes have a smooth and almost neutrally charged surface which showed better fouling resistance than both the positively charged NF membranes and commercially available negatively charged NTR-7450 membrane. In addition, these membranes showed high efficiency for removal of multivalent ions (> 95% for both cations and anions). Therefore, these antifouling surfaces can be potentially used for water softening, water desalination and wastewater treatment in a membrane bioreactor (MBR) process. (3) Thermally stable RO membranes. Commercial RO membranes cannot be used at temperature higher than 45°C due to the use of polysulfone substrate, which often limits their applications in industries. We successfully developed polyimides as the membrane substrate for thermally stable RO membranes due to their high thermal resistance. The polyimide-based composite polyamide membranes showed desalination performance comparable to the commercial TFC membrane. However, the key advantage of the polyimide-based membrane is its high thermal stability. As the feed temperature increased from 25oC to 95oC, the water flux increased 5 - 6 times while the salt rejection almost kept constant. This membrane appears to provide a unique solution for hot water desalination and also a feasible way to improve the water productivity by increasing the operating temperature without any drop in salt rejection.
Resumo:
L'elaborato tratta dell'effetto della porosità sulle proprietà meccaniche e osteoinduttive di un biomateriale utilizzabile in ingegneria del tessuto osseo, per come questo è stato valutato nello studio "Surface porous poly-ether-ether-ketone based on three-dimensional printing for load-bearing orthopedic implant" condotto dai ricercatori Shuai Li, Tianyu Wang, Jiqiang Hu, Zhibin Li, Bing Wang, Lianchao Wang e Zhengong Zhou. In particolare, il biomateriale studiato è rappresentato dal “PEEK”, un polimero termoplastico che viene lavorato, tramite stampante 3D a filamento, in modo da presentare una struttura che include un corpo centrale solido ricoperto da strati porosi sia nello strato superiore sia in quello inferiore. Per la valutazione delle proprietà meccaniche sono state svolte una prova a trazione e una prova a flessione. I valori ottenuti sperimentalmente sono stati confrontati con quelli ottenuti da un’analisi numerica e da un modello teorico. Per la valutazione delle proprietà osteoinduttive sono stati condotti test di proliferazione cellulare e differenziamento osteogenico. I risultati ottenuti concludono che specifici valori della porosità superficiale del biomateriale presentano proprietà meccaniche e osteoinduttive che lo rendono idoneo all’utilizzo come impianto osteogenico in ingegneria tissutale.
Resumo:
Miscibility and phase separation in the blends of phenolphthalein poly(aryl ether ketone) (PPAEK) and poly(ethylene oxide) (PEO) were investigated by means of differential scanning calorimetry (DSC). The PPAEK/PEO blends prepared by solution casting from N,N-dimethylformamide (DMF) displayed single composition-dependent glass transition temperatures (T-g), intermediate between those of the pure components, suggesting that the blend system is miscible in the amorphous state at all compositions. All the blends underwent phase separation at higher temperatures and the system exhibited a lower critical solution temperature (LCST) behavior. A step-heating thermal analysis was designed to determine the phase boundaries with DSC. The significant changes in the thermal properties of blends were utilized to judge the mixing status for the blends and the phase diagram was thus established. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
The gamma-radiolysis of poly(tetrafluoroethylene-co-perfuoromethyl vinyl ether) (TFE/PMVE) was investigated using solid state F-19 and C-13 NMR spectroscopy. Chain scission products identified in the polymer were saturated chain ends -CF2CF3 (G = 1.0), methyl ether end groups -CF2OCF3 (G = 0.9), acid end groups -CF2COOH (G = 0.5), and a small amount of terminal unsaturation -CF=CF2 (G = 0.2). A mechanism for the formation of these scission products was proposed and the G value for main chain scission, G(S), was determined to be 1.4. Cross-linking of TFE/PMVE was found to proceed via a Y-linking mechanism. The G value for cross-linking, G(X), was determined to be 0.9. A maximum of 0.2 mol % cross-links were formed under the experimental conditions.
Resumo:
The effect of irradiation temperature on the polymer properties was investigated for the fluoroelastomer poly(tetrafluoroethylene-co-perfluoromethylvinyl ether) (TFE/PMVE). TFE/PMVE samples were gamma-irradiated to 150 kGy at temperatures ranging from 77 K to 373 K. Analysis of the sol/gel behaviour, tensile properties, and glass transition temperatures indicated that crosslinking commenced in the temperature range 195 to 263 K, for a dose of 150 kGy. The latter temperature was 13 K below the glass transition temperature. Crosslinking remained relatively constant to higher temperatures. Chain scission reactions were found to occur well below the glass transition temperature and increased at higher temperatures. The optimum temperature for the radiation crosslinking of TFE/PMVE, for the temperatures investigated, was 263 K. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
The gamma-radiolysis of poly(tetrafluoroethylene-co-perfluoromethyl vinyl ether) (TFE/PMVE) was investigated using chemical and mechanical analyses. The polymer was found to form an insoluble network with a dose of gelation of 15.8 kGy. Tensile and glass transition temperature measurements indicated the predominance of crosslinking, with optimal elastomeric properties reached in the dose range of 120 to 200 kGy. Photoacoustic FTIR spectroscopy CPAS) showed the formation of new carboxylic acid end groups on irradiation. These new end groups were shown to decrease the thermal oxidative stability of the crosslinked network as determined by thermal gravimetric analysis. Electron spin resonance (ESR) studies of the polymer at 77 K indicated the presence of radical precursors. A G-value of 1.1 was determined for radical production at 77 K. Comparison of radical concentrations for a copolymer with a different mole ratio of PMVE, indicated that the PMVE units contribute to scission reactions. (C) 1998 Elsevier Science Ltd. All rights reserved.
Resumo:
Incorporation of 1 wt % of triallyl isocyanurate (TAIC) significantly enhanced the radiation crosslinking of the perfluoroelastomer, poly(tetrafluoroethylene-co-perfluoromethylvinyl ether) (TFE/PMVE). The dose for gelation was lowered by 70% with the presence of TAIC. The additive also improved the tensile properties of TFE/ PMVE both before and after crosslinking by irradiation. Higher radical yields were obtained with the presence of TAIC at 77 K, indicating the crosslinking promoter was acting as a radical trap. ESR studies showed that radiolysis of TAIC and subsequent photobleaching cleaved an allyl branch from the ring structure. Upon thermal annealing, an allyl radical on the TAIC molecule was observed. (C) 1999 John Wiley & Sons, Inc.
Resumo:
Poly(tetrafluoroethylene-co-perfluoropropyl vinyl ether) (PFA) with 2 mol% perfluoropropyl vinyl ether (PPVE) was exposed to gamma -irradiation in vacuum at both 77 K and room temperature and the ESR spectra recorded. Both the main chain, similar to CF2-(CF)-F-.-CF(2)similar to, and end chain, similar to (CF2CF2)-F-. radicals were identified at both temperatures and their thermal stabilities measured, No radicals unique to the radiolytic cleavage at the PPVE units were observed at room temperature, either due to the low concentration of the comonomer or beta -scission to form a chain end radical and a nonradical species. G-values for radical formation at room temperature and 77 K were found to be 0.93 and 0.16, respectively. (C) 2001 Elsevier Science Ltd. All rights reserved.