973 resultados para POLY(ETHER IMIDE)
Resumo:
The effects of thermally crosslinkable polymerization of monomer reactant-polyimide (POI) on the miscibility, morphology, and crystallization of partially miscible poly(ether sulfone) (PES)/poly(phenylene sulfide) (PPS) blends were investigated with differential scanning calorimetry and scanning electron microscopy. The addition of POI led to a significant reduction in the size of PPS particles, and the interfacial tension between PPS and crosslinked POI was smaller than that between PES and crosslinked POI. During melt blending, crosslinking and grafting reactions of POI with PES and PPS homopolymers were detected; however, the reaction activity of POI with PPS was much higher than that with PES. The crosslinking and grafting reactions were developed further when blends were annealed at higher temperatures. Moreover, POI was an effective nucleation agent of the crystallization of PPS, but crosslinking and grafting hindered the crystallization of PPS. The final effect of POI on the crystallinity of the PPS phase was determined by competition between the two contradictory factors. The crosslinking and grafting reactions between the two components was controlled by the dosage of POI in the blends, the premixing sequence of POI with the two components, the annealing time, and the temperature.
Resumo:
The X-ray diffraction patterns of the crystalline aromatic ketone polymer PEKEKmK (aryl ether ketone ether ketone ketone polymer containing meta-phenyl links) have been investigated (for the chemical structure, see Formula). An orthorhombic unit cell is proposed to contain two chains with a = 0.772 nm, b = 0.604 nm and c = 2.572 nm. According to the orthorhombic system, the 11 reflections of this polymer were indexed. Meanwhile, variation in unit cell parameters with crystallization temperatures of PEKEKmK was also investigated. [GRAPHICS]
Resumo:
Poly(ether ketone ether ketone ketone) containing meta-phenylene linkage (PEKEKK(T/I)) was synthesized by electrophilic Friedel-Crafts acylation condensation of 1, 4-diphenoxybenzophenone with terephthaloyl chloride (T) and isophthaloyl chloride (I) with a T/I ratio of 1 and characterized by LR,DSC,TGA and WAXD. PEKEKK(T/I) has two different crystal structures: a conventional Farm I structure, the same as that observed in PEEK and PEK, wich is usually developed from melt crystallization, and a new Form II structure which can be developed from cold crystallization or solvent induced crystallization (by exposing the glassy sample to methylene chloride).
Resumo:
In this paper, the synthesis and crystallization behavior of poly(ether ether ketone ether ketone) (PEEKEK) are reported. PEEKEK was prepared from 4,4'-bis(p-fluorobenzoyl) diphenyl ether (4,4'-FBDE) and hydroquinone along the nucleophilic substitution route. The thermal properties were investigated by using DSC and TGA. The crystallization behavior of PEEKEK under several conditions, i.e., crystallization from the molten state (melt crystallization), crystallization from a quenched sample (cold crystallization) and crystallization induced by exposing glassy sample to methylene chloride (solvent-induced crystallization) has also been investigated. The results show that crystallization of PEEKEK could be induced by the above methods, and no polymorphism was found. The differences in the crystallization of PEEKEK induced by the above methods are seen in their degree of crystallinity.
Resumo:
In this paper, melt crystallization of poly(ether ether ketone ketone) (PEEKK) under strong electric field was investigated. In the crystal structure of PEEKK, the length of c axis was found to he 1.075 nm, increasing by 7% compared to that of PEEKK crystallized without strong electric field. The molecule chains might take a more extended conformation through the opening of the bridge bond angles by increasing from 124 degrees to 144 degrees under strong electric field in the crystal structure.
Resumo:
The effect of entanglements on the glass transition and structural relaxation behaviors has been studied for polystyrene (PS) and phenolphthalein poly(ether sulfone) (PES-C) samples by fast evaporation of the solution of concentrations varying from above the overlapping concentration to far below it, and compared to the results we have studied previously in PC. It has been found that for all the polymers we have studied, in the concentrated solution region, the T-g of the samples obtained from solution are independent of the change of concentration and are very close to that of normal bulk samples, whereas in the dilute solution region the T-g of the samples decrease with the logarithm of decreasing concentration. The critical concentrations that divide the two distinct regions for the three polymers are 0.9% g/mL for PC, 0.1% g/mL for PS, and 1% g/mL for PES-C. The decrease of T-g of the samples is interpreted by the decrease of intermolecular entanglements as the isolation of polymer chains, and the entanglement of polymer chains restrained the mobility of the segments. The structural relaxation behavior of the polymers is also found to be different from that of normal bulk samples. The enthalpies of single-chain samples are lower than that of the bulk ones, which correspond to the lower glass transition temperature; the peaks are lower and broader, and the relaxed enthalpy is much lower as compared to that of bulk samples. In the three polymers we have studied, the influence of change of entanglements on both the decrease in glass transition temperature and relaxed enthalpy is the most significant for PS and the least for PES-C. It is indicated that the interactions in the flexible polymers are weak; thus, the restraint of the entanglements on the mobility of the segments plays a more important role in the flexible polymers, and the change of entanglement in the flexible polymers has a more significant influence on the physical properties.
Resumo:
The phase transition and transition kinetics of a liquid crystalline copoly(amide-imide) (PAI37), which was synthesized from 70 mol% pyromellitic dianhydride, 30 mol% terephthaloyl chloride, and 1,3-bis[4-(4'-aminophenoxy)cumyl]benzene, was characterized by differential scanning calorimetry, polarized light microscopy, X-ray diffraction, and rheology. PAI37 exhibits a glass transition temperature at 182 degreesC followed by multiple phase transitions. The crystalline phase starts to melt at similar to 220 degreesC and forms smectic C (S-C) phase. The Sc phase transforms into smectic A (S-A) phase when the temperature is above 237 degreesC. The S-C to S-A transition spans a broad temperature range in which the S-A phase vanishes and forms isotropic melt. The WARD fiber pattern of PAI37 pulled from the anisotropic melt revealed an anomalous chain orientation, which was characterized by its layer normal perpendicular to the fiber direction. The transition kinetics for the mesophase and crystalline phase formation was also studied.
Resumo:
Novel water insoluble sodium sulfonate-functionalized poly(ether ether ketone)s containing cyclohexylidene in the main chain with degree of sulfonation up to 2.0 were synthesized from nucleophilic polycondensation of 5, 5'-carbonylbis (2-fluorobenzenesulfonate), 4, 4'-difluorobenzophenone and 4, 4'-cyclohexylidenebisphenol. The polymers showed excellent thermal stability and good water resistance as well. The DSC diagrams and WAXD patterns indicated an amorphous morphological structure of these polymers. A comprison of some properties between these copolymers and polymers derived from bisphenol A was given.
Resumo:
Sodium sulfonate-functionalized polyether ether ketone)s derived from Bisphenol A with a degree of sulfonation up to 2.0 were synthesized by aromatic nucleophilic polycondensation of various amounts of 5,5-carbonylbis(2-fluorobenzenesulfonate) (1), 4,4'-diflurobenzophenone (2) and Bisphenol A (2). Copolymers showed excellent thermal stability and good mechanical properties. The selectivity of water vapor over nitrogen of membranes prepared from copolymers 3a and 3h was determined to be 3.43 x 10(6) and 1.05 x 10(7), respectively.
Resumo:
A series of high sulfonated poly(ether ether ketone)s were prepared by copolymerization of sodium 5,5 ' -carbonylbis (2-fluorobenzenesulfonate)(2),4,4 ' -difluorobenzophenone (1) and bisphenol A(3) in the presence of potassium carbonate in dimethylsulfoxide. The copolymers were characterized by IR and DSC, The influence of degree of sulfonation on the properties of copolymers, such as component, thermal stability, solubility and filming ability, was studied.
Resumo:
Novel sodium sulfonate-functionalized poly(ether ether ketone)s derived from 4,4'-thiodiphenol with degree of sulfonation up to 2.0 were synthesized by nucleophilic polycondensation of various amount of 5,5 '-carbonylbis(2-fluorobenzenesulfonate) (1) and 4,4'-difluorobenzophenone (2) with 4,4'-thiodipheno (3). Component and structure of the polymers were confirmed by TR, NMR and elemental analysis. Wide angle X-ray diffraction patterns indicated an amorphous structure of the polymers. All the polymers showed excellent thermal stability and poor solubility in water. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Novel optically active aromatic poly(amide-imide)s (PAIs) were prepared from newly synthesized 2,2'-bis(3,4-dicarboxybenzamido)-1,1'-binaphyl dianhydride ((+/-)-, (S)-, and (R)-BNDADA). PAIs based on dianhydride monomers with different ee % were investigated with respect to their structures and chiroptical properties. These polymers were highly soluble in polar aprotic solvents such as N,N-dimethylacetamide, N-methyl-2-pyrrolidone, pyridine, etc., and showed high glas s transition temperatures of 287-290 degrees C and 5% weight loss temperatures of 450-465 degrees C in nitrogen. Optically active PAIs exhibited high specific rotations, excellent optical stabilities, and a dependence of optical activities on temperature. Investigations on chiroptical properties indicated that chiral conformation was possessed by optically active PAIs. (C) 1999 John Wiley & Sons, Inc.
Resumo:
Novel optically active aromatic poly(amide-imide)s (PAIs) containing 1,1'-binaphthyl-2,2'-diyl units in the main chain were prepared by polycondensation reactions of newly synthesized dianhydride, 2,2'-bis(3,4-dicarboxylzenzamido)-1,1'-binaphthyl dianhydride[(S)-BN-DADA and (+/-)-BNDADA], with diamines, The properties of the resulted PAIs were fully characterized by a combination of investigations on inherent viscosity, thermal properties(DSC and TGA), specific rotation, CD and UV-Vis absorbance. These PAIs showed good solubilities, thermal properties and optical stabilities. Interesting UV-Vis absorption behavior of films casted from these PAIs was observed and analyzed.
Resumo:
A novel synthetic route to cyclic PEEK precursors is described. These new cyclic oligomers have been prepared from hydroquinone and N-phenyl(4,4'-difluorodiphenyl) ketimine. Matrix-assisted laser desorption/ionization time-of-flight mass spectrometry (MALDI-TOF MS) analysis unambiguously confirmed the cyclic nature.
Resumo:
Two closely series of poly(ester imide)s had been synthesized by solution polycondensation of p-phenylenebis(trimellitate) dianhydride with aliphatic diamines. The differential scanning calorimetry (DSC) traces of the most poly(ester imide)s exhibited two endotherms representing the solid state to anisotropic phase transition (T-m1) and the anisotropic to isotropic melt transition (T-m2), respectively. Observation under polarizing microscope and wide-angle X-ray diffraction (WAXD) measurements suggested that the anisotropic phase formed above the melting paints (T-m1) had a smectic character. The thermogravimetric analyses (TGA) revealed that the thermal stabilities of the poly(ester imide)s were up to 350 degrees C. (C) 1999 John Wiley & Sons, Inc.