789 resultados para NANOCRYSTALS


Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the study of complex and unexpected dependencies of nanocrystal size as well as nanocrystalsize distribution on various reaction parameters in the synthesis of ZnO nanocrystals using poly(vinyl pyrollidone) (PVP) as a capping agent. This method establishes a qualitatively different growth mechanism to the anticipated Ostwald ripening behavior. The study of size-distribution kinetics and an understanding of the observed non-monotonic behaviors provides a route to rational synthesis. We used a simple, but accurate, approach to estimate the size-distribution function of nanocrystals from the UV-absorption spectrum. Our results demonstrate the accuracy and generality of this approach, and we also illustrate its application to various semiconducting nanocrystals, such as ZnO, ZnS, and CdSe, over a wide size range (1.8-5.3 nm).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Body-centered-tetragonal (BCT) ZnS nanocrystals have been synthesized, for the first time to the best of our knowledge, by using the chemical coprecipitation method at higher synthesis temperatures of 65 and 95 degrees C. It is confirmed from X-ray diffraction (XRD) studies that in the high-temperature-synthesized samples, cubic and BCT phases coexist, in contrast to the room-temperature-synthesized sample, which consists of only cubic phase with sizes of the particles lying between 2 and 3 nm. The sizes of BCT phase nanocrystals are bigger than those of cubic phase of ZnS. The presence of BCT phase of ZnS in the samples is increased from 40 to 90% when the temperature of synthesis is increased from 65 to 95 degrees C. The nanocrystalline nature and UV-Vis absorption characteristics of the prepared samples have been studied with a transmission electron microscope (TEM) and a UV-Visible pectrophotometer, respectively. The room-temperature-synthesized ZnS sample shows photoluminescence (PL) emission in the blue region with multiple peaks, whereas the high-temperature-synthesized samples show PL emissions in the visible region. The Gaussian fittings of the measured PL spectra shows that three PL peaks at 429, 477, and 525 nm are appeared in the 65 degrees C sample and two peaks at 491 and 540 nm appear in the 95 degrees C sample with the enhanced PL intensity of the green peak at 540 nm. (C) 2010 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Following growth doping strategy and using dopant oxides nanocrystals as dopant sources, we report here two different transition-metal ions doped in a variety of group II-VI semiconductor nanocrystals. Using manganese oxide and copper oxide nanocrystals as corresponding dopant sources, intense photoluminescence emission over a wide range of wavelength has been observed for different host nanocrystals. Interestingly, this single doping strategy is successful in providing such highly emissive nanocrystals considered here, in contrast with the literature reports that would suggest synthesis strategies to be highly specific to the particular dopant, host, or both. We investigate and discuss the possible mechanism of the doping process, supporting the migration of dopant ions from dopant oxide nanocrystals to host nanocrystals as the most likely scenario.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We show that the characteristic Mn2+ d emission color from Mn2+-doped CdS nanocrystals can be tuned over as much as 40 nm, in contrast to what should be expected from such a nearly localized d-d transition. This is achieved surprisingly by a fine-tuning of the host particle diameter from 1.9 to 2.6 nm, thereby changing the overall emission color from red to yellow. Systematic experiments in conjunction with state-of-the-art ab initio calculations with full geometry optimization establish that Mn2+ ions residing at surface/subsurface regions have a distorted tetrahedral coordination resulting in a larger ligand field splitting. Consequently, these near-surface Mn2+ species exhibit a lower Mn2+ d emission energy, compared to those residing at the core of the nanocrystal with an undisturbed tetrahedral coordination. The origin of the tunability of the observed Mn2+ emission is the variation of emission contributions arising from Mn2+ doped at the core, subsurface, and surface of the host. Our findings provide a unique and easy method to identify the location of an emitting Mn2+ ion in the nanocrystal, which would be otherwise very difficult to decipher.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Following an earlier study (J. Am. Chem Soc. 2007, 129, 4470) describing a very unusual growth kinetics of ZnO nanoparticles, we critically evaluate here the proposed mechanism involving a crucial role of the alkali base ion in controlling the growth of ZnO nanoparticles using other alkali bases, namely, LiOH and KOH. While confirming the earlier conclusion of the growth of ZnO nanoparticles being hindered by an effective passivating layer of cations present in the reaction mixture and thereby generalizing this phenomenon, present experimental data reveal an intriguing nonmonotonic dependence of the passivation efficacy on the ionic size of the alkali base ion. This unexpected behavior is rationalized on the basis of two opposing factors: (a) solvated cationic radii and (b) dissociation constant of the base.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The variation in the bulk modulus of semiconductor nanoparticles has been studied within first-principles electronic-structure calculations using the local density approximation (LDA) for the exchange correlation. Quantum Monte Carlo calculations carried out for a silicon nanocrystal Si87H76 provided reasonable agreement with the LDA results. An enhancement was observed in the bulk modulus as the size of the nanoparticle was decreased, with modest enhancements being predicted for the largest nanoparticles studied here, a size just accessible in experiments. To access larger sizes, we fit our calculated bulk moduli to the same empirical law for all materials, the asymptote of which is the bulk value of the modulus. This was found to be within 2-10% of the independently calculated value. The origin of the enhancement has been discussed in terms of Cohen's empirical law M.L. Cohen, Phys. Rev. B 32, 7988 (1985)] as well as other possible scenarios.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We prove that CdS nanocrystals can be thermodynamically stabilized in both wurtzite and zinc-blende crystallographic phases at will, just by the proper choice of the capping ligand. As a striking demonstration of this, the largest CdS nanocrystals (similar to 15 nm diameter) ever formed with the zinc-blende structure have been synthesized at a high reaction temperature of 310 degrees C, in contrast to previous reports suggesting the formation of zinc-blende CdS only in the small size limit (< 4.5 nm) or at a lower reaction temperature (<= 240 degrees C). Theoretical analysis establishes that the binding energy of trioctylphosphine molecules on the (001) surface of zinc-blende CdS is significantly larger than that for any of the wurtzite planes. Consequently, trioctylphosphine as a capping agent stabilizes the zinc-blende phase via influencing the surface energy that plays an important role in the overall energetics of a nanocrystal. Besides achieving giant zinc-blende CdS nanocrystals, this new understanding allows us to prepare CdSe and CdSe/CdS core/shell nanocrystals in the zinc-blende structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel wet-chemical precipitation method is optimized for the synthesis of ZnS nanocrystals doped with Cu+ and halogen. The nanoparticles were stabilized by capping with polyvinyl pyrrolidone (PVP). XRD studies show the phase singularity of ZnS particles having zinc-blende (cubic) structure. TEM as well as XRD line broadening indicate that the average crystallite size of undoped samples is similar to2 nm. The effects of change in stoichiometry and doping with Cu+ and halogen on the photoluminescence properties of ZnS nanophosphors have been investigated. Sulfur vacancy (Vs) related emission with peak maximum at 434 nm has been dominant in undoped ZnS nanoparticles. Unlike in the case of microcrystalline ZnS phosphor, incorporation of halogens in nanoparticles did not result V-Zn related self-activated emission. However, emission characteristics of nanophosphors have been changed with Cu+ activation due to energy transfer from vacancy centers to dopant centers. The use of halogen as co-activator helps to increase the solubility of Cu+ ions in ZnS lattice and also enhances the donor-acceptor type emission efficiency. With increase in Cu+ doping, Cu-Blue centers (CuZn-Cui+), which were dominant at low Cu+ concentrations, has been transformed into Cu-Green (Cu-Zn(-)) centers and the later is found to be situated near the surface regions of nanoparticles. From these studies we have shown that, by controlling the defect chemistry and suitable doping, photoluminescence emission tunability over a wide wavelength range, i.e., from 434 to 514 nm, can be achieved in ZnS nanophosphors. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Monodisperse iron oxide nanocrystals with spherical and cubic morphologies, of comparable dimensions, have been prepared by the thermal decomposition of FeOOH. The lattice spacings of both forms agree with that of magnetite, Fe(3)O(4). The two, however, exhibit very different blocking temperatures. Nanocrystals of cubic morphology are superparamagnetic above 190 K while the spherical nanocrystals at a lower temperature, 142 K. The higher blocking temperatures in particles of cubic morphology are shown to be a consequence of exchange bias fields. We show that in the present iron oxide nanocrystals the exchange bias fields originate from the presence of trace amounts of wustite, FeO. A Reitveld refinement analysis of the X-ray diffraction patterns shows that nanocrystals of cubic morphology have a higher FeO content. The higher FeO content is responsible for the larger exchange bias fields that in turn lead to a higher blocking temperature for nanocrystals with cubic morphology.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Insertion of just a few impurity atoms in a host semiconductor nanocrystal can drastically alter its phase, shape, and physical properties. Such doped nanomaterials now constitute an important class of optical materials that can provide efficient, stable, and tunable dopant emission in visible and NIR spectral windows. Selecting proper dopants and inserting them in appropriate hosts can generate many new series of such doped nanocrystals with several unique and attractive properties in order to meet current challenges in the versatile field of luminescent materials. However, the synthesis of such doped nanomaterials with a specific dopant in a predetermined host at a desired site leading to targeted optical properties requires fundamental understanding of both the doping process as well as the resulting photophysical properties. Summarizing up to date literature reports, in this Perspective we discuss important advances in synthesis methods and in-depth understanding of the optical properties, with an emphasis on the most widely investigated Mn-doped semiconductor nanocrystals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A single-step magnetic separation procedure that can remove both organic pollutants and arsenic from contaminated water is clearly a desirable goal. Here we show that water dispersible magnetite nanoparticles prepared by anchoring carboxymethyl-beta-cyclodextrin (CMCD) cavities to the surface of magnetic nanoparticles are suitable host carriers for such a process. Monodisperse, 10 nm, spherical magnetite, Fe3O4, nanocrystals were prepared by the thermal decomposition of FeOOH. Trace amounts of antiferromagnet, FeO, present in the particles provides an exchange bias field that results in a high superparamagnetic blocking temperature and appreciable magnetization values that facilitate easy separation of the nanocrystals from aqueous dispersions on application of modest magnetic fields. We show here that small molecules like naphthalene and naphthol can be removed from aqueous media by forming inclusion complexes with the anchored cavities of the CMCD-Fe3O4 nanocrystals followed by separation of the nanocrystals by application of a magnetic field. The adsorption properties of the iron oxide surface towards As ions are unaffected by the CMCD capping so it too can be simultaneously removed in the separation process. The CMCD-Fe3O4 nanocrystals provide a versatile platform for magnetic separation with potential applications in water remediation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Changes in electronic and photovoltaic properties of semiconductor nanocrystals predominantly due to changes in shape are discussed here. Cadmium sulfide (CdS) semiconductor nanocrystals of various shapes (tetrapod, tetrahedron, sphere and rod) obtained using an optimized solvothermal process exhibited a mixed cubic (zinc blende) and hexagonal (wurtzite) crystal structure. The simultaneous presence of the two crystal phases in varying amounts is observed to play a pivotal role in determining both the electronic and photovoltaic properties of the CdS nanocrystals. Light to electrical energy conversion efficiencies (measured in two-electrode configuration laboratory solar cells) remarkably decreased by one order in magnitude from tetrapod -> tetrahedron -> sphere -> rod. The tetrapod-CdS nanocrystals, which displayed the highest light to electrical energy conversion efficiency, showed a favorable shift in position of the conduction band edge leading to highest rate of electron injection (from CdS nanocrystal to the wide band gap semiconductor viz, titanium dioxide, TiO2) and lowest rate of electron-hole recombination (higher free electron lifetimes).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Free-standing ZnO nanocrystals simultaneously doped with Fe and Cu with varying Fe/Cu compositions have been synthesized using colloidal methods with a mean size of similar to 7.7 nm. Interestingly, while the Cu-doped ZnO nanocrystal remains diamagnetic and Fe-doped samples show antiferromagnetic interactions between Fe sites without any magnetic ordering down to the lowest temperature investigated, samples doped simultaneously with Fe and Cu show a qualitative departure in exhibiting ferromagnetic interactions, with suggestions of ferromagnetic order at low temperature. XAS measurements establish the presence of Fe2+ and Fe3+ ions, with the concentration of the trivalent species increasing in the presence of Cu doping, providing direct evidence of the Fe2+ + Cu2+ sic Fe3+ + Cu+ redox couple being correlated with the ferromagnetic property. Using DFT, the unexpected ferromagnetic nature of these systems is explained in terms of a double exchange between Fe atoms, mediated by the Cu atom, in agreement with experimental observations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Interaction of CdSe and ZnO nanocrystals with electron-donating tetrathiafulvalene (TTF) and electron-withdrawing tetracyanoethylene (TCNE) has been investigated. Isothermal calorimetry shows CdSe nanocrystals interact more strongly with TCNE than TTF. Interaction of larger CdSe nanocrystals with TCNE causes a red-shift in the band-edge emission because of agglomeration, while the smaller CdSe nanocrystals, exhibiting stronger interaction with TCNE modify the optical gap of the nanocrystal. Luminescence of CdSe gets quenched sharply after addition of both TTF and TCNE. ZnO nanocrystals also exhibit luminescence quenching to lesser extent. Defect-emission of ZnO nanocrystals gets red or blue-shifted after interaction with TTF or TCNE respectively. (C) 2012 Elsevier B. V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have demonstrated that cadmium deoxycholate (1), a Cd-salt, provides a convenient and inexpensive route to high quality CdSe nanocrystals with photoluminescence (PL) in the blue to red region of the visible spectrum, with reproducible quantum yields as high as similar to 47%. Owing to the high thermal stability of the bile acid based cadmium precursor (decomposition point: 332 degrees C), it was possible to achieve high injection and growth temperatures (similar to 300 degrees C) for the nanocrystals, which was essential for obtaining larger CdSe nanocrystals emitting in the red region (625-650 nm) with a sharp full width at half maximum (FWHM) (23 nm) and multiple (6-7) excitonic absorption features. The as-prepared CdSe nanocrystals synthesized from cadmium deoxycholate represent a series of highly efficient emitters with pure colours and controllable sizes, shapes and structures.