In this work, the microstructure of mortars made with an ordinary Portland cement and slag cement has been studied. These mortars were exposed to four different constant temperature and relative humidity environments during a 180-day period. The microstructure has been studied using impedance spectroscopy, and mercury intrusion porosimetry as a contrast technique. The impedance spectroscopy parameters make it possible to analyze the evolution of the solid fraction formation for the studied mortars and their results are confirmed with those obtained using mercury intrusion porosimetry. The development of the pore network of mortars is affected by the environment. However, slag cement mortars are more influenced by temperature while the relative humidity has a greater influence on the OPC mortars. The results show that slag cement mortars hardened under non-optimal environments have a more refined microstructure than OPC mortars for the studied environmental conditions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This thesis focuses on the investigation of the abrasion resistance of fibre reinforced concrete floors at both the macro and micro levels. A literature review of the available literature concerning subjects allied to the current project is included. This highlights themes relevant to wear mechanisms and the factors influencing it: factors that affect the abrasion resistance of concrete and several test methods for assessing it; and the historical development of fibres and the properties of different fibre types and their influence on concrete. Three accelerated abrasion testers were compared and critically discussed for their suitability for assessing the abrasion resistance of concrete floors. Based on the experimental findings one accelerated abrasion apparatus was selected as more appropriate to be used for carrying out the main investigations. The laboratory programme that followed was undertaken to investigate the influence of various material and construction factors on abrasion resistance. These included mix variations (w/c ratio), fibre reinforcement, geometry, type and volume, curing method and superplasticizing agents. The results clearly show that these factors significantly affected abrasion resistance and several mechanisms were presumed to explain and better understand these observations. To verify and understand these mechanisms that are accountable for the breakdown of concrete slabs, the same concrete specimens that were used for the macro-study, were also subjected to microstructutural investigations using techniques such as Microhardness examination, Mercury intrusion porosimetry and Petrographic examination. It has been found that the abrasion resistance of concrete is primarily dependent on the microstructure and porosity of the concrete nearest to the surface. The feasibility of predicting the abrasion resistance of fibre reinforced concrete floors by indirect and non-destructive methods was investigated using five methods that have frequently been used for assessing the quality of concrete. They included the initial surface absorption test, the impact test, ball cratering, the scratch test and the base hardness test. The impact resistance (BRE screed tester) and scratch resistance (Base hardness tester) were found to be the most sensitive to factors affecting abrasion resistance and hence are considered to be the most appropriate testing techniques. In an attempt to develop an appropriate method for assessing the abrasion resistance of heavy-duty industrial concrete floors, it was found that the presence of curing/sealing compound on the concrete surface at the time of accelerated abrasion testing produces inappropriate results. A preliminary investigation in the direction of modifying the Aston accelerated abrasion tester has been carried out and a more aggressive head has been developed and is pending future research towards standardisation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The effect of 10% and 20% replacement metakaolin on a number of aspects of hydration chemistry and service performance of ordinary Portland cement pastes has been investigated. The analysis of expressed pore solutions has revealed that metakaolin-blended specimen pastes possess enhanced chloride binding capacities and reduced pore solution pH values when compared with their unblended counterparts. The implications of the observed changes in pore solution chemistry with respect to chloride induced reinforcement corrosion and the reduction in expansion associated with the alkali aggregate reaction are discussed. Differential thermal analysis, mercury intrusion porosimetry, and nuclear magnetic resonance spectroscopy have been employed in the analysis of the solid phase. It is suggested that hydrated gehlenite (a product of pozzolanic reaction) is operative in the removal and solid state binding of chloride ions from the pore solution of metakaolin-blended pastes. Diffusion coefficients obtained in a non-steady state chloride ion diffusion investigation have indicated that cement pastes containing 10% and 20% replacement metakaolin exhibit superior resistance to the penetration of chloride ions in comparison with those of plain OPC of the same water:cement ratio. The chloride induced corrosion behaviour of cement paste samples, of water:cement ratio 0.4, containing 0% , 10%, and 20% replacement metakaolin, has been monitored using the linear polarization technique. No significant corrosion of embedded mild steel was observed over a 200 day period.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An investigation was undertaken to study the effect of poor curing simulating hot climatic conditions and remedies on the durability of steel in concrete. Three different curing environments were used i.e. (1) Saturated Ca(OH)2 solution at 20°C, (2) Saturated Ca(OH)2 solution at 50°C and (3) Air at 50°C at 30% relative humidity. The third curing condition corresponding to the temperature and relative humidity typical of Middle Eastern Countries. The nature of the hardened cement paste matrix, cured under the above conditions was studied by means of Mercury Intrusion Porosimetry for measuring pore size distribution. The results were represented as total pore volume and initial pore entry diameter. The Scanning Electron Microscope was used to look at morphological changes during hydration, which were compared to the Mercury Intrusion Porosimetry results. X-ray defraction and Differential Thermal Analysis techniques were also employed for looking at any phase transformations. Polymer impregnation was used to reduce the porosity of the hardened cement pastes, especially in the case of the poorly cured samples. Carbonation rates of unimpregnated and impregnated cements were determined. Chloride diffusion studies were also undertaken to establish the effect of polymer impregnation and blending of the cements. Finally the corrosion behaviour of embedded steel bars was determined by the technique of Linear Polarisation. The steel was embedded in both untreated and polymer impregnated hardened cement pastes placed in either a solution containing NaCl or an environmental cabinet which provided carbonation at 40°C and 50% relative humidity.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polymer scaffolds play an important role in tissue engineering applications. Poly(ethylene glycol) based hydrogels have received a lot of attention in this field because of their high biocompatibility and ease of processing. However, in many cases they do not exhibit proper tissue invasion and nutrient transport because of their dense structure. In the present work, several approaches were developed and compared to each other to produce interconnected macroporous poly(ethylene glycol) hydrogels by including different types of porogens in the photocrosslinking reaction. The swelling capacity of the resulting hydrogels was analyzed and compared to non-porous hydrogel samples. Moreover, the obtained materials were characterized by means of mechanical properties and porosity using rheometry, scanning electron microscopy, and mercury intrusion porosimetry. Results showed that interconnected and uniform pores were obtained when a porogen template was used during hydrogel fabrication by photocrosslinking. On the other side, when the porogen particles were dispersed into the macromer solution before matrix photocrosslinking the interconnexion was negligible. The templates must be dissolved before the hydrogel's cell-seeding in vitro, while the dispersed porogen can be used in situ in the in vitro seeding tests. Copyright © 2013 Taylor & Francis Group, LLC.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tese (doutorado)—Universidade de Brasília, Faculdade de Tecnologia, Departamento de Engenharia Civil e Ambiental, 2016.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

As environmentally-friendly materials, geopolymers have the potential to replace ordinary Portland cement (OPC) for the construction of railway sleepers and multi-flue chimneys, where the vibration control capabilities of the material must be considered. The critical damping value (ξ) is the main parameter in relation to vibration reduction. In this study, the traditional logarithmic decrement technique was used to measure the ξ of geopolymers. Geopolymers were prepared by activating fly ash using alkali solutions with different SiO2/Na2O ratios. The results show that the ξ of the geopolymers is similar to that of the OPC counterpart. Finite element analysis (FEM) based on the Rayleigh damping model was conducted to replicate the test results, and scanning electron microscopy and mercury-intrusion porosimetry were used to study the microstructure of the geopolymers. A discussion of the possible damping mechanisms based on the microstructural investigation and the FEM analysis is presented.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper reports the properties of fly ash based geopolymer mortars made with dune sand. The geopolymer mortars of different cation type, namely sodium based (Na), potassium based (K) and a mixed Na/K, were prepared with dune sand (DS) and river sand (RS). The corresponding geopolymer pastes were also prepared. A series of tests including compressive strength, modulus of elasticity, splitting tensile strength, microanalysis (using scanning electron microscopy), porosity (using mercury intrusion porosimetry), sorptivity and air void (using section analysis method) were carried out. The results showed a strong correlation between strength and porosity of geopolymeric materials. The addition of DS had influences on the chemical compositions and physical properties of geopolymer mortars. These influences were dependent on the type of cation. Based on the results of mechanical properties, DS can be utilised as the fine aggregate for the production of geopolymer based construction material.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Textile production has been considered as an activity of high environmental impact due to the generation of large volumes of waste water with high load of organic compounds and strongly colored effluents, toxic and difficult biodegradability. This thesis deals with obtaining porous alumina ceramic membranes for filtration of textile effluent in the removal of contaminants, mainly color and turbidity. Two types of alumina with different particle sizes as a basis for the preparation of formulation for mass production of ceramic samples and membranes. The technological properties of the samples were evaluated after using sintering conditions: 1,350ºC-2H, 1,450ºC-30M, 1,450ºC-2H, 1,475ºC-30M and 1,475ºC-2H. The sintered samples were characterized by XRD, XRF, AG, TG, DSC, DL, AA, MEA, RL, MRF-3P, SEM and Intrusion Porosimetry by Mercury. After the characterization, a standard membrane was selected with their respective sintering condition for the filterability tests. The effluent was provided by a local Textile Industry and characterized at the entry and exit of the treatment plant. A statistical analysis was used to study the effluent using the following parameters: pH, temperature, EC, SS, SD, oil and grease, turbidity, COD, DO, total phosphorus, chlorides, phenols, metals and fecal coliform. The filtered effluent was evaluated by using the same parameters. These results demonstrate that the feasibility of the use of porous alumina ceramic membranes for removing contaminants from textile effluent with improved average pore size of 0.4 micrometre (distribution range varying from 0,025 to 2.0 micrometre), with total porosity of 29.66%, and average percentages of color removal efficiency of 89.02%, 92.49% of SS, turbidity of 94.55%, metals 2.70% (manganese) to 71.52% (iron) according to each metal and COD removal of 72.80%

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Textile production has been considered as an activity of high environmental impact due to the generation of large volumes of waste water with high load of organic compounds and strongly colored effluents, toxic and difficult biodegradability. This thesis deals with obtaining porous alumina ceramic membranes for filtration of textile effluent in the removal of contaminants, mainly color and turbidity. Two types of alumina with different particle sizes as a basis for the preparation of formulation for mass production of ceramic samples and membranes. The technological properties of the samples were evaluated after using sintering conditions: 1,350ºC-2H, 1,450ºC-30M, 1,450ºC-2H, 1,475ºC-30M and 1,475ºC-2H. The sintered samples were characterized by XRD, XRF, AG, TG, DSC, DL, AA, MEA, RL, MRF-3P, SEM and Intrusion Porosimetry by Mercury. After the characterization, a standard membrane was selected with their respective sintering condition for the filterability tests. The effluent was provided by a local Textile Industry and characterized at the entry and exit of the treatment plant. A statistical analysis was used to study the effluent using the following parameters: pH, temperature, EC, SS, SD, oil and grease, turbidity, COD, DO, total phosphorus, chlorides, phenols, metals and fecal coliform. The filtered effluent was evaluated by using the same parameters. These results demonstrate that the feasibility of the use of porous alumina ceramic membranes for removing contaminants from textile effluent with improved average pore size of 0.4 micrometre (distribution range varying from 0,025 to 2.0 micrometre), with total porosity of 29.66%, and average percentages of color removal efficiency of 89.02%, 92.49% of SS, turbidity of 94.55%, metals 2.70% (manganese) to 71.52% (iron) according to each metal and COD removal of 72.80%

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

New concepts on porosity appraisal in ancient and modern construction materials. The role of Fractal Geometry on porosity characterization and transport phenomena. This work studied the potential of Fractal Geometry to the characterization of porous materials. Besides the descriptive aspects of the pore size distribution, the fractal dimensions have led to the development of rational relations for the prediction of permeability coefficients to fluid and heat transfer. The research considered natural materials used in historical buildings (rock and earth) as well as currently employed materials as hydraulic cement and technologically advanced materials such as silicon carbide or YSZ ceramics. The experimental results of porosity derived from the techniques of mercury intrusion and from the image analysis. Data elaboration was carried out according to established procedures of Fractal Geometry. It was found that certain classes of materials are clearly fractal and respond to simple patterns such as Sierpinski and Menger models. In several cases, however, the fractal character is not recognised because the microstructure of the material is based on different phases at different dimensional scales, and in consequence the “fractal dimensions” calculated from porosimetric data do not come within the standard range (less than 3). Using different type and numbers of fractal units is possible, however, to obtain “virtual” microstructures that have the fraction of voids and pore size distribution equivalent with the experimental ones for almost any material. Thus it was possible to take the expressions for the permeability and the thermal conduction which does not require empirical “constants”, these expressions have also provided values that are generally in agreement with the experimental available data. More problematic has been the fractal discussion of the geometry of the rupture of the material subjected to mechanical stress both external and internal applied. The results achieved on these issues are qualitative and prone to future studies. Keywords: Materials, Microstructure, Porosity, Fractal Geometry, Permeability, Thermal conduction, Mechanical strength.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim was to measure the behaviour of various mortars employed in livestock media in central Spain and to analyse the aggressiveness of pig slurry to cement blended with fly ash mortars. To achieve this, mortar specimens were immersed in ponds storing pig slurry. Mortar specimens, of 40 ? 40 ? 160 mm, were made from four types of cement commonly used and recommended for rural areas. The types were a sulphate-resistant Portland cement and three cements blended in different proportions with fly ash and limestone filler. After 3, 6, 12, 24, 36, 48 and 60 months of exposure, three or four specimens of each cement type were removed from the pond and washed with water. Their compressive strength and microstructure (X-ray diffraction, mercury intrusion pore-symmetry, thermal analysis and scanning electron microscopy) were then measured. Sulphate-resistant Portland cement (SR-PC), found to be more susceptible to degradation due to its greater proportion of macro-pores and increased total porosity, was found not to be suitable for use with livestock. After 60 months of immersion in the pig slurry medium, CEM II-A (40.3%) mortar retained the greatest compressive strength. Mortars with less than 20% replacement of cement by fly ash were found to be the most durable, with the most suitable mechanical behaviour.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This thesis describes an experimental study of the abrasion resistance of concrete at both the macro and micro levels. This is preceded by a review related to friction and wear, methods of test for assessing abrasion resistance, and factors influencing the abrasion resistance of concrete. A versatile test apparatus was developed to assess the abrasion resistance of concrete. This could be operated in three modes and a standardised procedure was established for all tests. A laboratory programme was undertaken to investigate the influence, on abrasion resistance, of three major factors - finishing techniques, curing regimes and surface treatments. The results clearly show that abrasion resistance was significantly affected by these factors, and tentative mechanisms were postulated to explain these observations. To substantiate these mechanisms, the concrete specimens from the macro-study were subjected to micro-structural investigation, using such techniques as 'Mercury Intrusion Forosimetry, Microhardness, Scanning Electron Microscopy, Petrography and Differential Thermal Analysis. The results of this programme clearly demonstrated that the abrasion resistance of concrete is primarily dependent on the microstructure of the concrete nearest to the surface. The viability of indirectly assessing the abrasion resistance was investigated using three non-destructive techniques - Ultrasonic Pulse Velocity, Schmidt Rebound Hardness, and the Initial Surface Absorption Test. The Initial Surface Absorption was found to be most sensitive to factors which were shown to have influenced the abrasion resistance of concrete. An extensive field investigation was also undertaken. The results were used to compare site and laboratorypractices, and the performance in the accelerated abrasion test with the service wear. From this study, criteria were developed for assessing the quality of concrete floor slabs in terms of abrasion resistance.