919 resultados para LIQUID-CRYSTALLINE PHASE
Resumo:
This review discusses liquid crystal phase formation by biopolymers in solution. Lyotropic mesophases have been observed for several classes of biopolymer including DNA, peptides, polymer/peptide conjugates, glycopolymers and proteoglycans. Nematic or chiral nematic (cholesteric) phases are the most commonly observed mesophases, in which the rod-like fibrils have only orientational order. Hexagonal columnar phases are observed for several systems (DNA, PBLG, polymer/peptide hybrids) at higher concentration. Lamellar (smectic) phases are reported less often, although there are examples such as the layer arrangement of amylopectin side chains in starch. Possible explanations for the observed structures are discussed. The biological role of liquid crystal phases for several of these systems is outlined. Commonly, they may serve as a template to align fibrils for defined structural roles when the biopolymer is extruded and dried, for instance in the production of silk by spiders or silkworms, or of chitin in arthropod shells. In other cases, liquid crystal phase formation may occur in vivo simply as a consequence of high concentration, for instance the high packing density of DNA within cell nuclei.
Resumo:
This study is concerned with a series of acrylate based side-chain liquid crystalline (LC) polymers. Previous studies have shown that these LC polymers have a preference for parallel or perpendicular alignment with respect to the polymer chain which depends on the length of the coupling chain joining the mesogenic unit to the polymer backbone. On the other hand, the dielectric relaxation of these side-chain LC polymers shows a strong relaxation associated to the mesogenic unit dynamics. For samples with parallel alignment, it was found that the dielectric relaxation of the nematic is weaker and broader than the relaxation of the isotropic. By contrast, for samples with perpendicular alignment, the isotropic to nematic transition reduces the broadening the relaxation and increases the relaxation strength. These two features are more evident for samples with short coupling units for which the dielectric relaxation observed appears to be strongly coupled with the backbone dynamics.
Resumo:
Nematic monodomain liquid crystalline elastomers have been prepared through in situ cross-linking of an acrylate based side-chain liquid crystalline polymer in a magnetic field. At the nematic–isotropic transition, the sample is found to undergo an anisotropic shape change. There is found to be an increase in dimensions perpendicular — and a decrease parallel — to the director, this is consistent with alignment of the polymer backbone parallel to the direction of mesogen alignment in the nematic state. From a quantitative investigation of this behaviour, we estimate the level of backbone anisotropy for the elastomer. As second measure of the backbone anisotropy, the monodomain sample was physically extended. We have investigated, in particular, the situation where a monodomain sample is deformed with the angle between the director and the extension direction approaching 90°. The behaviour on extension of these acrylate samples is related to alternative theoretical interpretations and the backbone anisotropy determined. Comparison of the chain anisotropy derived from these two approaches and the value obtained from previous small-angle neutron scattering measurements on deuterium labelled mixtures of the same polymer shows that some level of chain anisotropy is retained in the isotropic or more strictly weakly paranematic state of the elastomer. The origin and implications of this behaviour are discussed.
Resumo:
A series of monodomain liquid crystalline (LC) elastomers based on a polysiloxane were synthesised. These elastomers were prepared either with one or two cross-linking agents in the presence of a mechanical field. By using the real-time X-ray facility at the University of Reading (AXIS), we have shown that the nematic order parameter 〈P2 〉 is dependent on both the extension λ value and the degree of cross-linking. We have also shown that the monodomain elastomers, exhibiting permanent alignment and 〈P2 〉 values of about 0.5, can be prepared by using only one cross-linking agent making the synthesis of these monodomain LC elastomers much more simple and cost effective than that proposed by Küpfer.
Resumo:
Procedures for obtaining molecular orientational parameters from wide angle X-ray scattering patterns of samples of thermotropic liquid crystalline polymers are presented. The methods described are applied to an extrusion-aligned sample of a random copolyester of poly(ethylene terephthalate) (PET) and p-acetoxybenzoic acid. Values of the orientational parameters are obtained from both the interchain and intrachain maxima in the scattering pattern. The differences in the values so derived suggest some level of local rotational correlation
Resumo:
A protecting group approach to the synthesis of a liquid crystalline polyacrylate containing a tetramethylene spacer unit is described. This approach prevents the formation of side products obtained when a more direct synthetic pathway is used. The resulting material shows behaviour typical of a nematic liquid crystal polymer.
Resumo:
The synthesis of methacrylate esters of 4-cyanophenyl-(4-(ω-hydroxyalkyloxy)) cinnamates, with spacer lengths of 2 and 6 methylene units and the synthesis of the corresponding acrylate ester with a spacer of 2 methylene units are described. The methacrylate monomers were polymerized by free radical polymerization, both as homopolymers and as copolymers with the analogous benzoate monomer of spacer length 6. The acrylate ester could not be polymerized successfully under the same reaction conditions. Polymers were characterized by NMR spectroscopy, gel permeation chromatography, differential scanning calorimetry, and thermo-optic observations. Of the monomers prepared, only the cinnamate with a hexamethylene spacer shows a mesophase, seen on supercooling of the melt. All of the polymers prepared were liquid crystalline, with smectic behavior predominating in the polymethacrylates with the longer spacer group. A narrow nematic region is seen just below the clearing temperature with a range of 3–9°C, nematic character is increased in the copolymer series with the degree of incorporation of the cinnamate monomer with the spacer group of length 2.
Resumo:
Electrospinning was used to generate polymer nanofibres from blends of poly-vinyl cinnamate (PVCN) and a cholesteric silicone polymer. Only blends that contained at least 40 % of PVCN produced fibres. Both differential scanning calorimetry and electron dispersion spectroscopy data indicate that the samples are miscible over a wide temperature interval. The variation of fibre diameter with concentration is nonlinear with a well-defined minimum corresponding to an 80 % PVCN blend. The fibres are birefringent with Kerr constants similar to that of cholesteric liquid crystals. Although not significant, the Kerr constant increases with increasing silicone polymer concentration.
Resumo:
The structure and local ordering of 1,6-hexamethylenediisocyanate-(acetoxypropy1) cellulose (HDI-APC) liquid crystalline elastomer thin films are investigated by using X-ray diffraction and scattering techniques. Optical microscopy and mechanical essays are performed to complement the investigation. The study is performed in films subjected or not to an uniaxial stress. Our results indicate that the film is constituted by a bundle of helicoidal fiber-like structure, where the cellobiose block spins around the axis of the fiber, like a string-structure in a smectic-like packing, with the pitch defined by a smectic-like layer. The fibers are in average perpendicular to the smectic-like planes. Without the stretch, these bundles are warped, only with a residual orientation along the casting direction. The stretch orients the bundles along it, increasing the smectic-like and the nematic-like ordering of the fibers. Under stress, the network of molecules which connects the cellobiose blocs and forms the cellulosic matrix tends to organize their links in a hexagonal-like structure with lattice parameter commensurate to the smectic-like structure.