630 resultados para titanium corrosion
Resumo:
The purpose of this study is to characterize the corrosion product on the surface of silver, employing H2SO4 (0.5M) as electrolyte. The electrochemical parameters, Ecor, Icor, V cor and Rp were obtained after analyzing the potentiodynamic polarization curve in which two peaks were observed. The smallest (passive region) is attributed to the Cl- traces from the reference electrode, with micro-cracks. The second peak (in the transpassivation region) corresponds to the polarization curve of silver in H2SO 4 without contaminants. SEM images and EDS analysis reveal images of a surface layer on silver, consisting of structures containing sulfur, oxygen, silver and chloride, as the corrosion product. On this layer silver sulfate crystals were observed, which occurs during the formation of silver chloride nanocrystals with different morphologies, when chloride ions were added to the electrolyte medium. ©The Electrochemical Society.
Resumo:
Low-level laser (LLL) has been used on peri-implant tissues for accelerating bone formation. However, the effect of one session of LLL in the strength of bone-implant interface during early healing process remains unclear. The present study aims to evaluate the removal torque of titanium implants irradiated with LLL during surgical preparation of implant bed, in comparison to non-irradiation. Sixty-four Wistar rats were used. Half of the animals were included in LLL group, while the other half remained as control. All animals had the tibia prepared with a 2 mm drill, and a titanium implant (2.2 × 4 mm) was inserted. Animals from LLL group were irradiated with laser (gallium aluminum arsenide), with a wavelength of 808 nm, a measured power output of 50 mW, to emit radiation in collimated beams (0.4 cm2), for 1 min and 23 s, and an energy density of 11 J/cm2. Two applications (22 J/cm 2) were performed immediately after bed preparation for implant installation. Flaps were sutured, and animals from both groups were sacrificed 7, 15, 30, and 45 days after implant installation, when load necessary for removing implant from bone was evaluated by using a torquimeter. In both groups, torque values tended to increase overtime; and at 30 and 45 days periods, values were statistically higher for LLL group in comparison to control (ANOVA test, p < 0.0001). Thus, it could be suggested that a single session of irradiation with LLL was beneficial to improve bone-implant interface strength, contributing to the osseointegration process. © 2012 Springer-Verlag London Ltd.
Resumo:
Objective: To study the early sequential stages of osseointegration at implants installed in alveolar bony. Materials and methods: In 12 Labrador dogs, all mandibular premolars and first molars were extracted bilaterally. After 3 months of healing, full-thickness flaps were elevated in the edentulous region of the right side of the mandible. Implants were installed, and the flaps were sutured to allow a fully submerged healing. The timing of the installations in the left side of the mandible and of sacrifices were performed with a schedule that various observation periods to sacrifice from 5, 10, 20, and 30 days were available so that n = 6 was obtained per each healing period. Ground sections were prepared and analyzed. Results: Newly formed bone in contact with the implant surface was found after 10 days of healing and the percentage increased up to 50% after 1 month of healing. A higher percentage was found in the trabecular compared with the cortical bony compartment. Old bone decreased by about 50% during healing, being still present after 1 month (16%). The proportions of bone debris and bone particles were at 27% after 5 days and decreased during healing to 6% after 1 month. Conclusion: Osseointegration (new bone-to-implant contact) developed at various rates for cortical and trabecular compartments, respectively. In the trabecular region, mesenchymal cells were identified, subsequently developing into new bone in contact with the implant surface. In the cortical compartment, however, resorptive processes were observed throughout all periods of healing. The proportion of newly formed bone percentage was lower compared with that of the trabecular area. Old bone was still present after 1 month of healing in both compartments. Bone debris and small bone particles appeared to be involved in initial bone formation. © 2013 John Wiley & Sons A/S.
Resumo:
Objective: Crohn's disease is a chronic inflammatory process that has recently been associated with a higher risk of early implant failure. Herein we provide information on the impact of colitis on peri-implant bone formation using preclinical models of chemically induced colitis. Methods: Colitis was induced by intrarectal instillation of 2,4,6-trinitro-benzene-sulfonic-acid (TNBS). Colitis was also induced by feeding rats dextran-sodium-sulfate (DSS) in drinking water. One week after disease induction, titanium miniscrews were inserted into the tibia. Four weeks after implantation, peri-implant bone volume per tissue volume (BV/TV) and bone-to-implant contacts (BIC) were determined by histomorphometric analysis. Results: Cortical histomorphometric parameters were similar in the control (n = 10), DSS (n = 10) and TNBS (n = 8) groups. Cortical BV/TV was 92.2 ± 3.7%, 92.0 ± 3.0% and 92.6 ± 2.7%. Cortical BIC was 81.3 ± 8.8%, 83.2 ± 8.4% and 84.0 ± 7.0%, respectively. No significant differences were observed when comparing the medullary BV/TV and BIC (19.5 ± 6.4%, 16.2 ± 5.6% and 15.4 ± 9.0%) and (48.8 ± 12.9%, 49.2 ± 6.2 and 41.9 ± 11.7%), respectively. Successful induction of colitis was confirmed by loss of body weight and colon morphology. Conclusions: The results suggest bone regeneration around implants is not impaired in chemically induced colitis models. Considering that Crohn's disease can affect any part of the gastrointestinal tract including the mouth, our model only partially reflects the clinical situation. © 2012 John Wiley & Sons A/S.
Resumo:
Material surfaces that provide biomimetic cues, such as nanoscale architectures, have been shown to alter cell/biomaterial interactions. Recent studies have identified titania nanotube arrays as strong candidates for use in interfaces on implantable devices due to their ability to elicit improved cellular functionality. However, limited information exists regarding the immune response of nanotube arrays. Thus, in this study, we have investigated the short- and long-term immune cell reaction of titania nanotube arrays. Whole blood lysate (containing leukocytes, thrombocytes and trace amounts of erythrocytes), isolated from human blood, were cultured on titania nanotube arrays and biomedical grade titanium (as a control) for 2 hours and 2 and 7 days. In order to determine the in vitro immune response on titania nanotube arrays, immune cell functionality was evaluated by cellular viability, adhesion, proliferation, morphology, cytokine/chemokine expression, with and without lipopolysaccharide (LPS), and nitric oxide release. The results presented in this study indicate a decrease in short- and long-term monocyte, macrophage and neutrophil functionality on titania nanotube arrays as compared to the control substrate. This work shows a reduced stimulation of the immune response on titania nanotube arrays, identifying this specific nanoarchitecture as a potentially optimal interface for implantable biomedical devices. © 2013 The Royal Society of Chemistry.
Resumo:
Purposes: The purposes of this study were to evaluate the influence of chronic stress (CS) on implant osseointegration and also to analyze whether alendronate (ALN) therapy could prevent these eventual stress-negative effects. Materials and Methods: Adult male Holtzmann rats were assigned to one of the four experimental groups: AL (ALN; 1mg/kg/week; n=12), ALS (ALN+CS; 1mg/kg/week; n=12), CTL (sterile physiological saline; n=12), or CTLS (sterile physiological saline+CS; n=12). After 58 days of drug therapy, the ALS and CTLS groups were exposed to CS, and 2 days later all animals underwent tibial implant installation. The animals were euthanized 28 days following the operative surgical procedure. Results: It was observed that the CTLS group presented an impairment of bone metabolism represented by lowest levels of bone-specific alkaline phosphatase and bone area fraction occupancy values. Furthermore, these animals presented a higher proportion of empty osteocytic lacunae. In contrast, the ALN therapy showed increased osseointegration and torque value parameters, regardless of stress exposition. Conclusions: Analysis of the data presented suggests that CS partially impairs the osseointegration of tibial implants and that ALN therapy is able to prevent these negative effects. © 2013 Wiley Periodicals, Inc.
Resumo:
Background: It has been reported that titanium-zirconium alloy with 13-17% zirconium (TiZr1317) implants show higher biomechanical stability and bone area percentage relative to commercially pure titanium (cpTi) grade 4 fixtures. Purpose: This study aimed to determine whether the higher stability for TiZr1317 implants is associated with higher mechanical properties of remodeling bone in the areas around the implants. Materials and Methods: This study utilized 36 implants (n=18: TiZr1317, n=18: cpTi), which were placed in the healed ridges of the mandibular premolar and first molar of 12 mini pigs (n=3 implants/animal). After 4 weeks in vivo, the samples were retrieved, and resin-embedded histologic sections of approximately 100μm in thickness were prepared. In order to determine the nanomechanical properties, nanoindentation (n=30 tests/specimen) was performed on the bone tissue of the sections under wet conditions with maximum load of 300μN (loading rate: 60μN/s). Results: The mean (±standard deviation) elastic modulus (E) and hardness (H) for the TiZr1317 group were 2.73±0.50GPa and 0.116±0.017GPa, respectively. For the cpTi group, values were 2.68±0.51GPa and 0.110±0.017GPa for E and H, respectively. Although slightly higher mechanical properties values were observed for the TiZr1317 implants relative to the cpTi for both elastic modulus and hardness, these differences were not significant (E=p>0.75; H=p>0.59). Conclusions: The titanium-zirconium alloy used in this study presented similar degrees of nanomechanical properties to that of the cpTi implants. © 2013 Wiley Periodicals, Inc.
Resumo:
Siloxane-polymethyl methacrylate hybrid films containing functionalized multiwall carbon nanotubes (CNTs) were deposited by dip-coating on carbon steel substrates from a sol prepared by radical polymerization of methyl methacrylate and 3-methacryloxy propyl-trimethoxysilane, followed by hydrolytic co-polycondensation of tetraethoxysilane. The correlation between the structural properties and corrosion protection efficiency was studied as a function of the molar ratio of nanotubes carbon to silicon, varied in the range between 0.1% and 5%. 29Si nuclear magnetic resonance and thermogravimetric measurements have shown that hybrids containing carbon nanotubes have a similar degree of polycondensation and thermal stability as the undoped matrix and exhibit and excellent adhesion to the substrate. Microscopy and X-ray photoelectron spectroscopy results revealed a very good dispersion of carbon nanotubes in the hybrid matrix and the presence of carboxylic groups allowing covalent bonding with the end-siloxane nodes. Potentiodynamic polarization curves and electrochemical impedance spectroscopy results demonstrate that CNTs containing coatings maintain the excellent corrosion protection efficiency of the hybrids, showing even a superior performance in acidic solution. The nanocomposite structure acts as efficient corrosion barrier, increasing the total impedance by 4 orders of magnitude and reducing the current densities by more than 3 orders of magnitude, compared to the bare steel electrode. © 2013 Elsevier B.V. All rights reserved.
Resumo:
The influence of ethanol, sulfuric acid and chloride on the corrosion resistance of 316L stainless steel was investigated by means of polarization curves and electrochemical impedance spectroscopy measurements. Over the studied range, the steel corrosion potential was independent of H2SO 4 and NaCl concentrations in aqueous solution. On the other hand, in solution containing 65 wt.% ethanol and 35 wt.% water, the corrosion potentials were higher than those obtained in aqueous solution. Besides, the steel corrosion potential was affected by the addition of H2SO4 and NaCl in solution. In solutions with and without ethanol, plus 0.35 wt.% NaCl, the presence of 1 wt.% H2SO4 inhibited the appearance of pitting corrosion. © 2013 Sociedade Brasileira de Química.
Resumo:
This study investigated the effects of the morphology and physicochemical properties of calcium phosphate (CaP) nanoparticles on osteogenesis. Two types of CaP nanoparticles were compared, namely amorphous calcium phosphate (ACP) nano-spheres (diameter: 9-13 nm) and poorly crystalline apatite (PCA) nano-needles (30-50 nm x 2-4 nm) that closely resemble bone apatite. CaP particles were spin-coated onto titanium discs and implants; they were evaluated in cultured mouse calvarial osteoblasts, as well as after implantation in rabbit femurs. A significant dependence of CaP coatings was observed in osteoblast-related gene expression (Runx2, Col1a1 and Spp1). Specifically, the PCA group presented an up-regulation of the osteospecific genes, while the ACP group suppressed the Runx2 and Col1a1 expression when compared to blank titanium substrates. Both the ACP and PCA groups presented a more than three-fold increase of calcium deposition, as suggested by Alizarin red staining. The removal torque results implied a slight tendency in favour of the PCA group. Different forms of CaP nanostructures presented different biologic differences; the obtained information can be used to optimize surface coatings on biomaterials. © 2013 IOP Publishing Ltd.
Resumo:
Objectives: The purpose of this study was to evaluate the surfaces of commercially pure titanium (cp Ti) implants modified by laser beam (LS), without and with hydroxyapatite deposition by the biomimetic method (HAB), without (HAB) and with thermal treatment (HABT), and compare them with implants with surfaces modified by acid treatment (AS) and with machined surfaces (MS), employing topographical and biomechanics analysis. Methods: Forty-five rabbits received 75 implants. After 30, 60, and 90 days, the implants were removed by reverse torque and the surfaces were topographically analyzed. Results: At 30 days, statistically significant difference (P < 0.05) was observed among all the surfaces and the MS, between HAB/HABT and AS and between HAB and LS. At 60 days, the reverse torque of LS, HAB, HABT, and AS differed significantly from MS. At 90 days, difference was observed between HAB and MS. The microtopographic analysis revealed statistical difference between the roughness of LS, HAB, and HABT when compared with AS and MS. Conclusions: It was concluded that the implants LS, HAB, and HABT presented physicochemical and topographical properties superior to those of AS and MS and favored the osseointegration process in the shorter periods. In addition, HAB showed the best results when compared with other surfaces. © 2012 John Wiley & Sons A/S.
Resumo:
Although titanium and its alloys own good mechanical properties and excellent corrosion resistance, these materials present poor tribological properties for specific applications that require wear resistance. In order to produce wear-resistant surfaces, this work is aimed at achieving improvement of wear characteristics in Ti-Si-B alloys by means of high temperature nitrogen plasma immersion ion implantation (PIII). These alloys were produced by powder metallurgy using high energy ball milling and hot pressing. Scanning electron microscopy (SEM) and X-ray diffraction identified the presence of α-titanium, Ti6Si2B, Ti5Si3, TiB and Ti3Si phases. Wear tests were carried out with a ball-on-disk tribometer to evaluate the friction coefficient and wear rate in treated and untreated samples. The worn profiles were measured by visible light microscopy and examined by SEM in order to determine the wear rates and wear mechanisms. Ti-7.5Si-22.5B alloy presented the highest wear resistance amongst the untreated alloys produced in this work. High temperature PIII was effective to reduce the wear rate and friction coefficient of all the Ti-Si-B sintered alloys. © 2013 Elsevier B.V.
Resumo:
Plasma immersion ion implantation (PIII) process is a three dimensional surface modification method that is quite mature and well known to the surface engineering community nowadays, especially to those working in the field of plasma-materials interaction, aiming at both industrial and academic applications. More recently, deposition methods have been added to PIII, the PIII&D, opening possibilities of broader range of applications of these techniques. So, PIII&D is becoming a routine method of surface modification, with the advantage of pushing up the retained dose levels limited by the sputtering due to ion implantation. Therefore, well adherent, thick, three-dimensional films without stress are possible to be achieved, at relatively low cost, using PIII&D. In this paper, we will discuss about a few PIII and PIII&D experiments that have been performed recently to achieve surface improvements in different materials: 1 - high temperature nitrogen PIII in Ti6Al4V alloy in which a deep nitrogen rich treated layer resulted in surface improvements as increase of hardness, corrosion resistance and resistance to wear of the Ti alloy; 2 - nanostructures in ZnO films, obtained by PIII&D of vaporized & ionized Zn source; 3 - combined implantation and deposition of calcium for biomaterial activity of Ti alloy (PIII&D), allowing the growth of hydroxyapatite in a body solution; 4 - magnetron sputtering deposition of Cr that was enhanced by the glow discharge Ar plasma to allow implantation and deposition of Cr on SAE 1070 steel (PIII&D) resulting in surfaces with high resistance to corrosion; and 5 - implantation of nitrogen by ordinary PIII into this Cr film, which improved resistance to corrosion, while keeping the tribological properties as good as for the SAE 1070 steel surface. © 2012 Elsevier B.V.
Resumo:
The corrosion behaviour of metal matrix composites (MMCs) is strictly linked with the presence of heterogeneities such as reinforcement phase, microcrevices, porosity, secondary phase precipitates, and interaction products. Most of the literature related to corrosion behaviour of aluminium matrix composites (AMCs) is focused on SiC reinforced AMCs. On the other hand, there is very limited information available in the literature related to the tribocorrosion behaviour of AMCs. Therefore, the present work aims to investigate corrosion and tribocorrosion behaviour of Al-Si-Cu-Mg alloy matrix composites reinforced with B4C particulates. Corrosion behaviour of 15 and 19% (vol) B4C reinforced Al-Si-Cu-Mg matrix composites and the base alloy was investigated in 0.05M NaCl solution by performing immersion tests and potentiodynamic polarisation tests. Tribocorrosion behaviour of Al-Si-Cu-Mg alloy and its composites were also investigated in 0.05M NaCl solution. The tests were carried out against alumina ball using a reciprocating ball-on-plate tribometer. Electrochemical measurements were performed before, during, and after the sliding tests together with the recording of the tangential force. Results suggest that particle addition did not affect significantly the tendency of corrosion of Al-Si-Cu-Mg alloy without mechanical interactions. During the tribocorrosion tests, the counter material was found to slide mainly on the B4C particles, which protected the matrix alloy from severe wear damage. Furthermore, the wear debris were accumulated on the worn surfaces and entrapped between the reinforcing particles. Therefore, the tendency of corrosion and the corrosion rate decreased in Al-Si-Cu-Mg matrix B4C reinforced composites during the sliding in 0.05M NaCl solution. © 2013 Elsevier B.V.