829 resultados para light weight design
Resumo:
Four novel thermally stable poly(aryl ether)s, e.g., P3F, P5F, P2A3F, and P2A5K containing ter- or pentafluorene units in the side chains for efficient blue light emission have been designed and synthesized. All the polymers show the optical properties identical to the corresponding monomers and are amorphous with higher glass transition temperature (T-g) than their monomeric Counterparts. The polymer light-emitting diodes (PLEDs) were fabricated with the device structure of ITO/(PEDOT:PSS)/polymer/Ca/Al. The incorporation of diphenylamine group to oligofluorene terminals significantly reduces the hole-injection energy barrier in PLEDs. The devices based on P2A3F and P2A5F show the luminous efficiencies of 1.2 and 2.0 cd/A at a brightness of 300 cd/m(2) with the Commission Internationale de L'Eclairage (CIE) coordinates of (0.15, 0.13) and (0.19, 0.20), respectively. All these indicate that the high-performance light-emitting polymers can be synthesized with the traditional condensation polymerization through careful design of polymer structures.
Resumo:
The dopant/host methodology, which enables efficient tuning of emission color and enhancement of the electroluminescence (EL) efficiency of organic light emitting diodes (OLEDs) based on small molecules, is applied to the design and synthesis of highly efficient green light emitting polymers. Highly efficient green light emitting polymers were obtained by covalently attaching just 0.3-1.0 mol% of a green dopant, 4-(N,N-diphenyl) amino-1,8-naphthaliniide (DPAN), to the pendant chain of polyfluorene (the host). The polymers emit green light and exhibit a high photoluminescence (PL) quantum yield of Lip to 0.96 in solid films, which is attributed to the energy transfer from the polyfluorene host to the DPAN dopant unit. Single layer devices (device configuration: ITO/PEDOT/Polymer/Ca/Al) of the polymers exhibit a turn on voltage of 4.8 V, luminance efficiency of 7.43 cd A(-1), power efficiency of 2.96 lm W-1 and CIE coordinates at (0.26, 0.58). The good device performance can be attributed to the energy transfer and charge trapping from the polyfluorene host to the DPAN dopant unit as well as the molecular dispersion of the dopant in the host.
Resumo:
2,7-Bis(9-ethylcarbazol-3-yl)-9,9-di(2-ethylhexyl)fluorene and a segmented copolymer composed of the same chromophores alternated with hexamethylene fragments were synthesized. The obtained materials possess good solubility in common organic solvents, high thermal stability with 1% weight loss temperature of 350-370 degrees C, and suitable glass transition temperatures. Both derivatives show blue fluorescence in dilute solutions as well as in solid state, demonstrating that excimers are not formed in the thin films. The fluorescence spectra of the materials do not show any peaks in the long-wavelength region even after annealing at 200 degrees C in air. An organic LED with the configuration of ITO/copolymer/Al generates blue electroluminescence with the maximum peak at 416 nm, rather low turn-on voltage (4.0 V), and brightness of about 400 cd/m(2). The heterostructure device based on model derivative emitted stable blue light with low operation voltage (100 cd/m(2) at similar to 11 V) and demonstrated luminescence efficiency of 0.8 cd/A.
Resumo:
Two new light-emitting PPV-based copolymers bearing electron-withdrawing triazole unit in the main chain have been synthesized by Wittig reaction between triazole diphosphonium salt and the corresponding dialdehyde monomers, respectively. Their optical and physical properties are characterized by UV-vis, photoluminescence (PL), TGA and DSC. The resulting copolymers are highly soluble in common organic solvents and have high Tg and Td values. They show blue-greenish fluorescence in solution (lambda(max) 502 and 508 nm) and green fluorescence in the solid state (lambda(max) 520 and 526 nm), respectively.
Resumo:
A soluble electroluminescent polymer containing hole-deficient triphenylamine and electron-deficient oxadiazole units in the main chains has been designed and studied. The design is based on the consideration that the triphenylamine group possesses good hole-transporting property and the oxadiazole unit is known to be of electron-transporting character. Because of the good bipolar transporting performance, the brightness and electroluminescent efficiency are significantly improved and the turn-on voltage is reduced compared with a similar polymer without the electron-deficient oxadiazole units in the main chains. For a device with configuration ITO/PEDOT/polymer/CsF/Al, a maximum brightness of 3600 cd m(-2) and a maximum luminescent efficiency of 0.65 cd A(-1) (quantum efficiency of 0.3%) were obtained in the polymer with oxadiazole units, about 15 times brighter and 15 times more efficient than the corresponding polymer without oxadiazole units.
Resumo:
Copolymerization of carbon dioxide and propylene oxide was carried out employing (RC6H4COO)(3)Y/glycerin/ZnEt2 (R = -H, -CH3, NO2, -OH) ternary catalyst systems. The feature of yttrium carboxylates (ligand, substituent and its position on the aromatic ring) is of great importance in the final copolymerization. Appropriate design of substituent and position of the ligand in benzoate-based yttrium complex can adjust the microstructure of aliphatic polycarbonate in a moderate degree, where the head-to-tail linkage in the copolymer is adjustable from 68.4 to 75.4%. The steric factor of the ligand in the yttrium complex is crucial for the molecular weight distribution of the copolymer, probably due to the fact that the substituent at 2 and 4-position would disturb the coordination or insertion of the monomer, lead the copolymer with broad molecular distribution. Based on the study of ultraviolet-visible spectra of the ternary catalyst in various solvents, it seems that the absorption band at 240-255 nm be closely related to the active species of the rare earth ternary catalysts.
Resumo:
Two series of highly soluble novel nitrogen- and sulfur-containing conjugated polymers were synthesized via an acid-induced self-polycondensation of functional monomers with methyl sulfinyl and aromatic groups. The well-defined structures of synthesized polymers were confirmed by their NMR and IR spectra. The highest occupied molecular orbital energy values for these materials, estimated by cyclic voltammetry, showed a broad range of values from about 5.0 to 5.2 eV used as hole-transport layers (HTL) in two-layer light-emitting diodes ITO/HTL/Alq(3)/Mg:Ag [ITO = indium tin oxide, and Alq(3) = tris(8-quinolinato) aluminum]. The typical turn-on voltage of these diodes was about 4-5 V. The maximum brightness of the device was about 3440 cd/m(2) at 20 V. The maximum efficiency was estimated to be 0.15 1m/W at 10 V.
Resumo:
Two soluble high-performance polyimides, poly(BCPOBDA/DMMDA) and poly(ODPA/DMMDA), in CHCl3 at 25 degrees C have been studied using laser light scattering. We found that the z-average radius of gyration ([R(g)]) can be scaled to the weight-average molecular weight (M(w)) as [R(g)] (nm) = 4.95 x 10(-2)M(w)(0.52) and [R(g)] (nm) = 1.25 x 10(-2)M(w)(0.66) respectively for poly(BCPOBDA/DMMDA) and poly(ODPA/DMMDA), indicating that poly(ODPA/DMMDA) in CHCl3 at 25 degrees C has a more extended chain conformation than poly(BCPOBDA/DMMDA). Using the wormlike chain model approach, we found that the Flory characteristic ratios (C*) of poly(BCPOBDA/DMMDA) and poly(ODPA/DMMDA) are similar to 20 and similar to 31, respectively, indicating that both of them have a slightly extended chain conformation in comparison with typical flexible polymer chains, such as polystyrene, whose C-infinity is similar to 10. A combination of the weight-average molar mass (M(w)) with the translational diffusion coefficient distributions (G(D)) has led to D (cm(2)/s) = 3.53 x 10(-4)M(-0.579) and D (cm(2)/s) = 4.30 x 10(-4)M(-0.613) respectively for two soluble high-performance polyimides, poly(BCPOBDA/DMMDA) and poly(ODPA/DMMTA), in CHCl3 at 25 degrees C. Using these two calibrations, we have successfully characterized the molar mass distributions of the two polyimides from their corresponding G(D)s. The exponents of these two calibrations further confirm that both of the polyimides have a slightly extended coil chain conformation in CHCl3. The chain flexibility difference between these two polyimides has also been discussed.
Laser light-scattering study of novel thermoplastics .2. Phenolphthalein poly(ether sulfone) (PES-C)
Resumo:
Five narrowly distributed fractions of phenolphthalein poly(ether sulfone) (PES-C) were studied in CHCl3 by both static and dynamic laser light scattering (LLS) at 25 degrees C. The dynamic LLS showed that the PES-C samples contain some large polymer clusters as in previously studied phenolphthalein poly(ether ketone)(PEK-C). These large clusters can be removed by a 0.1-mu m filter. Our results showed that [R(g)(2)](1/2)(z) = (3.35 +/- 0.13) x 10(-2) M(w)((0.52 +/- 0.03)) and [D] = (2.26 +/- 0.02) x 10(-4)M(w)-((0.54) +/- 0.03)) with [R(g)(2)](1/2)(z), M(w) and [D] being the z-average radius of gyration, the weight-average molecular weight, and the z-average translational diffusion coefficient, respectively. A combination of static and dynamic LLS results enabled us to determine D = (2.45 +/- 0.04) x 10(-4)M-((0.55 +/- 0.05)), where D and M correspond to monodisperse species. Using this scaling relationship, we have successfully converted the translational diffusion coefficient distribution into the molecular weight distribution for each of the five PES-C fractional The weight-average molecular weights obtained from dynamic light scattering have a good agreement with that obtained from static laser light-scattering measurements.
Resumo:
Five different molecular weight phenolphthalein poly(aryl ether ketone) (PEK-C) fractions in CHCl3 were studied by static and dynamic laser light scattering(LLS). The dynamic LLS revealed that the PEK-C samples contain some large polymer clusters. These large clusters can be removed by filtering the solution with a 0.1-mu m filter. We found that the persistence length of PEK-C in CHCl3 at 25 degrees C is similar to 2 nm and the Flory characteristic ratio, C-infinity is similar to 25. Our results showed that [R(g)(2)](1/2)(z) = (3.50+/-0.20) x 10(-2)M(w)(0.54+/-0.01) and [D] = (2.37+/-0.05) x 10(-4)M(w)(-0.55+/-0.01), with [R(g)(2)](1/2)(z), M(w), and [D] being the z-average radius of gyration, the weight-average molecular weight, and the z-average translational diffusion coefficient, respectively. A combination of static and dynamic LLS results enabled us to determine D = (2.20+/-0.10) x 10(-4)M(-0.555+/-0.015), where D and M correspond to monodisperse species. Using this calibration between D and M,we have determined molecular weight distributions of five PEK-C fractions from their corresponding translational diffusion coefficient distribution.
Resumo:
A set of AM-AA copolymer samples with the same comonomer content and different average molecular weight have been characterized by C-13 NMB and light scattering methods in this paper. The chemical composition (comonomer AA, mole content 16.9 +/- 1.1%) of these samples is uniform. the sequence of AA in the macromolecular chain is of alone and random distribution and the light scattering theory from polyelectrolyte in added-salt solutions is suitable for the AM-AA copolymers-0.12 mol/L NaCl water systems. The actual values of M(w), the second Virial coefficient A(2) and the mean square radius of gyration (R(2)), for the studied samples have been obtained. The relationships between the molecular parameters are as follows: A(2)=0.0619 ($) over bar M(w)(-0.24), < R(2) >(1/2)(t)= 0.0210 ($) over bar M(w)(0.54).
Resumo:
The solution behavior of four chitosans (91% deacetylated chitin) with different molecular weights in 0.2M CH3COOH/0.1M CH3COONa aqueous solution was investigated at 25 degrees C by dynamic laser light scattering (LLS). The Laplace inversion of the precisely measured intensity-intensity time correlation function leads us to an estimate of the line-width distribution G(Gamma), which could be further reduced to a translational diffusion coefficient distribution G(D). By using a combination of static and dynamic LLS results, i.e. Mw and G(D), we were able to establish a calibration of D = k(D)M(-alpha D) with k(D) = (3.14 +/- 0.20) X 10(-4) and alpha(D) = 0.655 +/- 0.015. By using this calibration, we successfully converted G(D) into a molecular weight distribution f(w)(M). The larger alpha(D) value confirms that the chitosan chain is slightly extended in aqueous solution even in the presence of salts. This is mainly due to its backbone and polyelectrolytes nature. As a very sensitive technique, our dynamic LLS results also revealed that even in dilute solution chitosan still forms a small amount of larger sized aggregates that have ben overlooked in previous studies. The calibration obtained in this study will provide another way to characterize the molecular weight distribution of chitosan in aqueous solution at room temperature. (C) 1995 John Wiley & Sons, Inc.
Resumo:
The absorptivities of color elements in a mixture can be obtained by using Gauas' elimination with selection of principal element in matrix to the standards. These values can be applied to flexible tolerance simplex method to give the composition of samples. In the exprimental design and data treatment, an effort was made to minimize the errors of results according the principal of optimization. When the difference of absorptivities of color material is significant to the exprimental error, the pr...
Resumo:
Tank cultivation of marine macroalgae involves air-agitation of the algal biomass and intermittent light conditions, i.e. periodic, short light exposure of the thalli in the range of 10 s at the water surface followed by plunging to low light or darkness at the tank bottom and recirculation back to the surface in the range of 1-2 min. Open questions relate to effects of surface irradiance on growth rate and yield in such tumble cultures and the possibility of chronic photoinhibition in full sunlight. A specially constructed shallow-depth tank combined with a dark tank allowed fast circulation times of approximately 5 s, at a density of 4.2 kg fresh weight (FW) m(-2) s(-1). Growth rate and yield of the red alga Palmaria palmata increased over a wide range of irradiances, with no signs of chronic photoinhibition, up to a growth-saturating irradiance of approximately 1600 mumol m(-2) s(-1) in yellowish light supplied by a sodium high pressure lamp at 16 h light per day. Maximum growth rate ranged at 12% FW d(-1), and maximum yield at 609 g FW m(-2) d(-1). This shows that high growth rates of individual thalli may be reached in a dense tumble culture, if high surface irradiances and short circulation times are supplied. Another aspect of intermittent light relates to possible changes of basic growth kinetics, as compared to continuous light. For this purpose on-line measurements of growth rate were performed with a daily light reduction by 50% in light-dark cycles of 1, 2 or 3 min duration during the daily light period. Growth rates at 10degreesC and 50 mumol photon m(-2) s- 1 dropped in all three intermittent light regimes during both the main light and dark periods and reached with all three periodicities approximately 50% of the control, with no apparent changes in basic growth kinetics, as compared to continuous light.
Resumo:
Shrimps Litopenaeus vannamei with initial body weight of 2.108 +/- 0.036 g were sampled for specific growth rates (SGR) and body color measurements for 50 days under different light sources (incandescent lamp, IL; cool-white fluorescent lamp, FL; metal halide lamp, MHL; and control without lamp) and different illumination methods (illumination only in day, IOD, and illumination day and night, IDN). Body color of L. vannamei was measured according to the free astaxanthin concentration (FAC) of shrimp. The SGR, food intake (FI), feed conversion efficiency (FCE) and FAC of shrimps showed significant differences among the experimental treatment groups (P < 0.05). Maximum and minimum SGR occurred under IOD by MHL and IDN by FL, respectively (difference 56.34%). The FI of shrimp for the control group did not rank lowest among treatments, confirming that shrimp primarily use scent, not vision, to search for food. FI and FCE of shrimps were both the lowest among treatment groups under IDN by FL and growth was slow, thus FL is not a preferred light source for shrimp culture. Under IOD by MHL, shrimps had the highest FCE and the third highest FI among treatment groups ensuring rapid growth. FAC of shrimp were about 3.31 +/- 0.20 mg/kg. When under IOD by MHL and IDN by FL, FAC was significantly higher than the other treatments (P < 0.05). To summarize, when illuminated by MHL, L. vannamei had not only vivid body color due to high astaxanthin concentration but also rapid growth. Therefore, MHL is an appropriate indoor light source for shrimp super-intensive culture. SGR of shrimp was in significantly negative correlation to FAC of shrimp (P < 0.05). Thus, when FAC increased, SGR did not always follow, suggesting that the purpose of astaxanthin accumulation was not for growth promotion but for protection against intense light. (c) 2005 Elsevier B.V. All rights reserved.