960 resultados para PEROVSKITE THIN-FILMS


Relevância:

100.00% 100.00%

Publicador:

Resumo:

c-axis oriented Bi3.25La0.75Ti3O12 (BLT) thin films were grown on a RuO2 top electrode deposited on a (100) SiO2/Si substrate by the polymeric precursor method. X-ray diffraction and atomic force microscope investigations indicate that the films exhibit a dense, well crystallized microstructure having random orientations with a rather smooth surface morphology. The electrical properties of preferred oriented Bi3.25La0.75Ti3O12 (BLT) thin films deposited on RuO2 bottom electrode leaded to a large remnant polarization (P-r ) of 17.2 mu C/cm(2) and (V-c ) of 1.8 V, fatigue free characteristics up to 10(10) switching cycles and a current density of 2.2 mu A/cm(2) at 5 V. We found that the polarization loss is insignificant with nine write/read voltages at a waiting time of 10,000 s. Independently of the applied electric field the retained switchable polarization approached a nearly steady-state value after a retention time of 10 s.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polymer films were grown in rf discharges containing different proportions of C2H2 and SF6. Quantitative optical emission spectrometry (actinometry) was used to follow the trends in the plasma concentrations of the species H and F, and more tentatively, of CH, CF, and CF2, as a function of the feed composition. Infrared spectroscopy revealed the density of CH and CF bonds in the deposited material. As the partial pressure of SF6 in the feed was increased, the degree of fluorination of the polymer also rose. The form of the dependency of the deposition rate on the proportion of SF6 in the feed was in good qualitative agreement with the activated growth model. From transmission ultraviolet visible spectroscopy data the refractive index and the absorption coefficient of the polymers were calculated as a function of the deposition parameters. Since the optical gap depended to some extent upon the degree of fluorination, it could, within limits, be determined by a suitable choice of the proportion of SF6 in the feed. A qualitative explanation of this relationship is given.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Amorphous and crystalline thin films of Mn-doped(0.5%-10%) GaAs and crystalline thin films of Zn1-xCoxO(x = 3%-20%) were investigated by means of magnetic susceptibility and electron spin resonance (ESR). For the Mn-doped GaAs samples, our results show the absence of ferromagnetic ordering for the amorphous films in the 300 > T > 2 K temperature range, in contrast to the ferromagnetism found in crystalline films for T-C < 110 K. A single ESR line with a temperature independent g-value (g similar to 2) is observed for the amorphous films, and the behavior of this ESR linewidth depends on the level of crystallinity of the film. For the Mn-doped GaAs crystalline films, only a ferromagnetic mode is observed for T < TC when the film is ferromagnetic. Turning now the Zn1-xCoxO films, ferromagnetic loops were observed at room temperature for these films. The magnetization data show an increasing of the saturation magnetization M. as a function of x reaching a maximum value for x approximate to 10%. ESR experiments at T = 300 K in the same films show a strong anisotropic ferromagnetic mode (FMR) for x = 0.10.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A polymeric precursor method was used to synthesis PbTiO3 amorphous thin film processed at low temperature. The luminescence spectra of PbTiO3 amorphous thin films at room temperature revealed an intense single-emission band in the visible region, the visible emission band was found to be dependent on the thermal treatment history, Photoluminescence properties Versus different annealing temperatures were investigated. The experimental results (XRD, AFM, FL) indicate that the nature of photoluminescence (PL) must be related to the disordered structure of PbTiO3 amorphous thin films, Copyright (C) 2000 John Wiley & Sons, Ltd.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

SnO2:Sb multi-layer coatings were prepared by the Pechini method. An investigation was made of the influence of the concentration of Sb2O3 and the viscosity of the precursor solution on the electrical and optical properties of SnO2 thin films. The use of a multi-layer system as an alternative form of increasing the packing and. thus. decreasing porosity proved to be efficient, decreasing the system's resistivity without altering its optical properties. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work, we present an approach for neutron fluence measurements based on natural thorium thin films and natural uranium-doped glasses calibrated through natural uranium thin films to be used for dating with the Fission-Track Method (FTM). This neutron dosimetry approach allows the employment of FTM even when dating is carried out using low neutron themalization facilities. Besides, it makes possible the determination of the Th/U ratio of the mineral to be dated. Durango apatite which is often employed in FTM as an age standard was analyzed. This apatite presented a fairly high Th/U ratio, 29.9 +/- 1.7. Th fissions were 18%, 12% and 10% of the total for irradiations where thermal to fast neutron flux ratios were 2.4, 4.4 and 5,2, respectively. These results show that Th fission must be considered for this apatite, when not well-thermalized irradiation facilities are used. The ratio between spontaneous and induced track length, L(S)/L(1), close to 0.89, indicates a certain amount of rejuvenation of the age of Durango apatite. Therefore, its apparent age should be corrected, the application of a technique based on track-length measurements produced a corrected age of 29.7 +/- 1.1 Ma, consistent with the independent reference age of this apatite (31.4 +/- 0.5 Ma). This result represents a support for viability of the neutron dosimetry approach studied in this work for FTM.(C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), thin films with a La concentration of 0.75 was grown on Pt/Ti/SiO2/Si substrates by using the polymeric precursor solution and spin-coating method. The scanning electron microscopy (SEM) showed rounded grains, which is not typical for these system. The BLT films showed well-saturated polarization-electric field curve which 2P(r) = 41.4 muC/cm(2) and V-c = 0.99 V. The capacitance dependence on the voltage is strongly nonlinear, confirming the ferroelectric properties of the film resulting from the domains switching. These properties make BLT a promising material for FERAM applications.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tin oxide nanoparticles prepared by an aqueous sol-gel method were deposited by dip-coating on fluorozirconate glass, ZBLAN (53%ZrF4-20%BaF2-4%LaF3-3%AlF3-20%NaF) to improve its resistance against wet corrosion. The aqueous leaching of uncoated and SnO2-coated fluorozirconate glass was studied by X-ray photoemission spectroscopy (XPS) and it was shown that even an ultra thin tin dioxide film provides good protection of the glass surface against the bulk propagation of the hydrolytic attack.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

CaBi2Nb2O9 (CBNO) thin films deposited on platinum coated silicon substrates by the polymeric precursor method exhibited good structural, dielectric, and piezoelectric characteristics. Capacitance-voltage measurements indicated good ferroelectric polarization switching characteristics. Remanent polarization and drive voltage values were 4.2 mu C/cm(2) and 1.7 V for a maximum applied voltage of 10 V. The film has a piezoelectric coefficient d(33) equal to 60 pm/V, current density of 0.7 mu A/cm(2), and Curie temperature of 940 degrees C. The polar-axis-oriented CBNO is a promising candidate for use in lead-free high Curie point in ferroelectric and piezoelectric devices. (c) 2006 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influence of the substrate temperature on the structural features and opto-electrical properties of undoped and indium-doped ZnO thin films deposited by pyrosol process was investigated. The addition of indium induces a drastic decrease (by a factor approximate to 10(10) for samples deposited at 300 degreesC) in the electrical resistivity of films, the lowest electrical resistivity (6 mOmega-cm) being observed for the film deposited at 450 degreesC. Films are highly transparent (>80%) in the Vis-NIR ranges, and the optical band gap exhibits a blue shift (from 3.29 to 3.33 eV) for the In-doped films deposited at increasing temperature. Preferential orientation of the ZnO crystallites with the c-axis perpendicular to the substrate surface and an anisotropic morphology of the nanoporous structure was observed for films growth at 300 and 350 degreesC. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polycrystalline BaWO4 and PbWO4 thin films having a tetragonal scheelite structure were prepared at different temperatures. Soluble precursors such as barium carbonate, lead acetate trihydrate and tungstic acid, as starting materials, were mixed in aqueous solution. The thin films were deposited on silicon, platinum-coated silicon and quartz substrates by means of the spinning technique. The surface morphology and crystal structure of the thin films were investigated using scanning electron microscopy (SEM), atomic force microscopy (AFM), X-ray diffraction, and specular reflectance infrared Fourier transform spectroscopy, respectively. Nucleation stages and surface morphology evolution of thin films on silicon substrates have been studied by atomic force microscopy. XRD characterization of these films showed that BaWO4 and PbWO4 phase crystallize at 500 degreesC from an inorganic amorphous phase. FTIR spectra revealed the complete decomposition of the organic ligands at 500 degreesC and the appearance of two sharp and intense bands between 1000 and 600 cm(-1) assigned to vibrations of the antisymmetric stretches resulting from the high crystallinity of both thin films. The optical properties were also studied. It was found that BaWO4 and PbWO4 thin films have Eg = 5.78 eV and 4.20 eV, respectively, of a direct transition nature. The excellent microstructural quality and chemical homogeneity results confirmed that soft solution processing provides an inexpensive and environmentally friendly route for the preparation of BaWO4 and PbWO4 thin films. (C) 2003 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We present atomic force microscopic images of the interphase morphology of vertically segregated thin films spin coated from two-component mixtures of poly[2-methoxy-5-(2'-ethylhexyloxy)-1,4-phenylene-vinylene] (MEH-PPV) and polystyrene (PS). We investigate the mechanism leading to the formation of wetting layers and lateral structures during spin coating using different PS molecular weights, solvents and blend compositions. Spinodal decomposition competes with the formation of surface enrichment layers. The spinodal wavelength as a function of PS molecular weight follows a power-law similar to bulk-like spinodal decomposition. Our experimental results indicate that length scales of interface topographical features can be adjusted from the nanometer to micrometer range. The importance of controlled arrangement of semiconducting polymers in thin film geometries for organic optoelectronic device applications is discussed. (c) 2007 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Stoichiometric Ba1-xSrxTiO3 (BST; x = 0.4) thin films were prepared by the polymeric precursor method. High quality polycrystalline films of BST with low roughness (approximate to 3 nm) were obtained from a Pt/Ti/SiO2/Si substrate deposited by spin-coating technique. Microstructure and morphological evaluation were done using grazing incident X-ray diffraction (GIXRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). Grazing incident angle XRD characterization of these films showed that BST phase crystallizes at 600 degrees C from an inorganic amorphous matrix. No intermediate crystalline phase was identified. A linear relationship between roughness and grain size was observed. (C) 2000 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Zinc oxide (ZnO) is an electroluminescent (EL) material that can emit light in different regions of electromagnetic spectrum when electrically excited. Since ZnO is chemically stable, inexpensive and environmentally friendly material, its EL property can be useful to construct solid-state lamps for illumination or as UV emitter. We present here two wet chemical methods to prepare ZnO thin-films: the Pechini method and the sol-gel method, with both methods resulting in crystalline and transparent films with transmittance > 85% at 550 nm. These films were used to make thin-film electroluminescent devices (TFELD) using two different insulator layers: lithium fluoride (LiF) or silica (SiO2). All the devices exhibit at least two wide emission bands in the visible range centered at 420 nm and at 380 nm attributed to the electronic defects in the ZnO optical band gap. Besides these two bands, the device using SiO2 and ZnO film obtained via sol-gel exhibits an additional band in the UV range centered at 350 nm which can be attributed to excitonic emission. These emission bands of ZnO can transfer their energy when a proper dopant is present. For the devices produced the voltage-current characteristics were measured in a specific range of applied voltage. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), thin films with a La concentration ranging from 0 to 0.75 were grown on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution and spin-coating method. The scanning electron microscopy shows a change of morphology with increasing the lanthanum concentration. The BLT films show well-saturated polarization-electric field curves whit remnant polarizations of 14.7, 20.5, 21.5, and 20.4 muC/cm(2) for x = 0, 0.25, 0.50 and 0.75, respectively. The dielectric constant of BLT (x = 0.75 mol% La) is equal to 158 while dielectric loss remain low (tandelta = 0.0018).