971 resultados para LASER FLUORESCENCE METHOD
Resumo:
kinds of Yb3+- and Na+-codoped CaF2 laser crystal with different Na:Yb ratios of 0, 1.5, and 10 are grown by the temperature gradient technique. Room-temperature absorption, photoluminescence spectra, and fluorescence lifetimes belonging to the transitions between ground state F-2(7/2) and excited state F-2(5/2) of Yb3+ ions in the three crystals are measured to study the effect of Na+. Experimental results show that codoping Na+ ions in different Na:Yb ratios can modulate the spectroscopy and photoluminescence properties of Yb3+ ions in a CaF2 lattice in a large scope. (c) 2005 Optical Society of America
Resumo:
We report on an optical interference method to fabricate array microstructures on the surface of silicon wafers by means of five-beam interference of femtosecond laser pulses. Optical microscope and scanning electron microscope observations revealed microstructures with micrometer-order were fabricated. The diffraction characteristics of the fabricated structures were evaluated. The present technique allows one-step realization of functional optoelectronic devices on silicon surface. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Gd2SiO5 (GSO) single crystal codoped with Yb3+ and Er3+ (Abbr. as Er:Yb:GSO) was successfully grown by the Czochralski (CZ) method for the first time and the spectral characteristics were investigated. The absorption and fluorescence spectra were measured. The emission lifetime of the I-4(13/2)-Er-level was measured to be 5.84ms and the emission cross-section at 1529nm was calculated to be 1.03 x 10(-20) cm(2). The results indicate that Er:Yb:GSO is a potential laser material at similar to 1. 55 mu m wavelength region. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
For the first time, a high optical quality 10 at.% Yb3+-doped gadolinium oxyorthosilicate laser crystal Gd2SiO5 (GSO) was grown by the Czochralski (Cz) method. The segregation coefficient of Yb3+ was studied by the inductively coupled plasma atomic emission spectrometer (ICP-AES) method. The crystal structure has monoclinic symmetry with space group P2(1)/c; this was determined by means of an x-ray diffraction analysis. The absorption spectra, fluorescence spectra and fluorescence decay curves of Yb3+ ions in a GSO crystal at room temperature were also studied. Then, the spectroscopic parameters of Yb:GSO were calculated. The advantages of the Yb:GSO crystal include high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections and particularly broad emission bandwidth (similar to 72 nm). The results indicated that the Yb:GSO crystal seemed to be a very promising laser gain medium in diode-pumped femtosecond laser and tunable solid state laser applications when LD pumped at 940 and 980 nm.
Resumo:
Composite sapphire/Ti:sapphire crystals for high-power laser application were grown by the hydrothermal method. The results of the X-ray rocking curve analysis indicate high crystalline quality of the surface Al2O3 material. The strong bonding between the overgrown Al2O3 and seed Ti:Al2O3 crystals is indispensable for withstanding high thermal stresses produced by intense optical pumping. The optical loss at the boundary of the composite crystal is considerably low, indicating the lack of scattering centers. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Yb: YAlO3 (YAP) (15 at %) and Yb: Y3Al5O12 (YAG)(15 at %) have been grown using the Czochralski method. Their absorption and fluorescence spectra were measured at room temperature and important spectroscopic parameters were calculated. Through the comparison of spectroscopic parameters of Yb:YAP and Yb: YAG, all results indicate that 15 at % Yb:YAP crystal is a potential candidate used for compact, efficient thin chip lasers when the laser output wavelength is 1012 or 103 8 nm. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Blue frequency-upconversion fluorescence emission has been observed in Ce3+-doped Gd2SiO5 single crystals, pumped with 120-fs 800 nm IR laser pulses. The observed fluorescence emission peaks at about 440nm is due to 5d -> 4f transition of Ce3+ ions. The intensity dependence of the blue fluorescence emission on the IR excitation laser power obeys the cubic law, demonstrating three-photon absorption process. Analysis suggested that three-photon simultaneous absorption induced population inversion should be the predominant frequency upconversion mechanism. (c) 2006 Optical Society of America.
Resumo:
The effects of Na+ doping level on the thermal conductivities, absorption and emission spectra, and fluorescence lifetimes of Yb3+ ,Na+ :CaF2 crystals were systematically studied. Sites structure, covalent force, and crystal field strength of Yb3+ :CaF2 crystals were markedly varied by codoping Na+ as charge compensator. The 2.0at% Yb3+ and 3.0at% Na+-codoped CaF2 crystal was demonstrated to operate in diode-pumped passively mode-locking scheme. Transform-limited 1 ps laser pulses were obtained, showing the crystal capable of producing ultra-short laser pulses. (c) 2006 Elsevier B.V. All rights reserved.
Three-photon-excited upconversion luminescence of Ce3+: YAP crystal by femtosecond laser irradiation
Resumo:
Infrared to ultraviolet and visible upconversion luminescence was demonstrated in trivalent cerium doped YAlO3 crystal (Ce3+: YAP) under focused infrared femtosecond laser irradiation. The fluorescence spectra show that the upconverted luminescence comes from the 5d-4f transitions of trivalent cerium ions. The dependence of luminescence intensity of trivalent cerium on infrared pumping power reveals that the conversion of infrared radiation is dominated by three-photon excitation process. It is suggested that the simultaneous absorption of three infrared photons pumps the Ce3+ ion into upper 5d level, which quickly nonradiatively relax to lowest 5d level. Thereafter, the ions radiatively return to the ground states, leading to the characteristic emission of Ce3+. (c) 2005 Optical Society of America.
Resumo:
用提拉法生长了掺铬、钕的钆镓石榴石(Cr^4+,Nd^3+:GGG)自调Q激光品体。报道了室温下的吸收光谱和荧光光谱特性。分析了Cr离子浓度对光谱性质的影响。比较了Cr^4+:GGG,Nd^3+:GGG和(Cr^4+,Nd^3+):GGG晶体吸收光谱的关系。测量了(Cr^4+,Nd^3+):GGG晶体和Nd^3+:GGG晶体的荧光寿命,它们分别是33μs和250μs。实验表明,(Cr^4+,Nd^3+):GGG晶体是一种非常有潜力的自调Q激光晶体,可以实现大功率激光器的小型化和全固态化。
Resumo:
应用中频感应提拉法生长出不同掺杂浓度的Yb:FAP激光晶体,运用电感耦合等离子体原子发射光谱仪(ICP-AES)测定了Yb^3+离子存Yb:FAP晶体中的分凝系数约为0.03。随着晶体的生长,晶体中Yb^3+离子的轴向浓度逐渐增大。研究Yb:FAP晶体在77K和300K温度下的吸收光谱发现,振动谱的变化主要是由电子-声子近共振耦合作用引起的。系统地研究了不同Yb^3+离子掺杂浓度Yb:FAP晶体的吸收光谱和荧光光谱。通过吸收光谱的测量计算了晶体的吸收截面。Yb:FAP晶体在904nm和982nm处存在Yb
Resumo:
High-quality neodymium doped GGG laser crystals have been grown by Czochralski (Cz) method. Results of Nd:GGG thin chip laser operating at 1.064 μm pumped by Ti:sapphire laser operating at 808 nm were reported. The slop efficiency was as high as 20%.
Resumo:
We report on an optical interference method to fabricate arrayed holes on metal nickel foil and aluminum film deposited on glass substrate by means of five-beam interference of femtosecond laser pulses. Optical microscope and scanning electron microscope observations revealed that arrayed holes of micrometre-order were fabricated on both metal foil and metal film. The present technique allows one-step, large-area, micrometric processing of metal materials for potential industrial applications.
Resumo:
A large and transparent Yb:FAP crystal with dimensions up to circle divide 30 mm x 85 mm has been grown by the Czochralski method. The preparation of the raw material has been investigated. X-ray power diffraction studies of Yb:FAP crystal confirm that the as-grown crystal is isostructural with the FAP crystal. The crystalline quality has been studied using X-ray rocking curve analysis. The segregation coefficient of Yb3+ in the Yb:FAP crystal has been also determined. Linear thermal expansion coefficients in [001] and [100] directions have been measured in the 30-800 degrees C temperature range. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We report on an optical interference method for transferring periodic microstructures of metal film from a supporting substrate to a receiving substrate by means of five-beam interference of femtosecond laser pulses. Scanning electron microscopy and optical microscopy revealed microstructures with micrometer-order were transferred to the receiving substrate. In the meanwhile, a negative copy of the transferred structures was induced in the metal film on the supporting substrate. The diffraction characteristics of the transferred structures were also evaluated. The present technique allows one-step realization of functional optoelectronic devices. (C) 2005 Optical Society of America.