Asymmetric polymerization could be induced by an already formed optically active living prepolymer with one-handed screw sense helix conformation. The usually formed anionic active centre on the prepolymer could be changed to cationic, radical and even of Ziegler-Natta type. These living prepolymers with various kinds of active centre were all effective to induce a consequent asymmetric polymerization of a monomer which may be other than that in the prepolymer, to afford an optically active helical chain with the same screw sense as that of the prepolymer. Eight monomers have been used in the work. Optical rotation, circular dichroism and gelpermeation chromatography have been taken to prove the helix-induced asymmetric polymerization.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The substituent chemical shift (SCS) has been applied to the assignment of the C-13 NMR spectrum of chlorinated polyethylene (CPE). CPE of different chlorine contents has been employed and their sequence structure discussed. The results show that characteristic of CPE with medium chlorine content is the dichloroethane structure in molecular chain. SCS parameters have been obtained from the C-13 NMR spectra. It was found that the effects of chlorine content and temperature on SCS are negligible, but the substituent parameter S1 reduced by 0.39 ppm when C2Cl4 was added to solvent ODCB.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of poly[3,3-bis(chloromethyl)oxetane] (Penton) with poly(vinyl acetate) were prepared. Compatibility, morphology, thermal behavior, and mechanical properties of blends with various compositions were studied using differential scanning calorimetry (DSC), dynamic mechanical measurements (DMA), tensile tests, and scanning electron microscopy (SEM). DMA study showed that the blends have two glass transition temperatures (T(g)). The T(g) of the PVAc rich phase shifts significantly to lower temperatures with increasing Penton content, suggesting that a considerable amount of Penton dissolves in the PVAc rich phase, but that the Penton rich phase contains little PVAc. The Penton/PVAc blends are partially compatible. DSC results suggest that PVAc can act as a beta-nucleator for Penton in the blend. Marked negative deviations from simple additivity were observed for the tensile strength at break over the entire composition range. The Young's modulus curve appeared to be S-shaped, implying that the blends are heterogeneous and have a two-phase structure. This was confirmed by SEM observations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of poly(N-vinyl-2-pyrrolidone) (PVP) with poly(ether sulphone) and two phenolphthalein-based polymers, viz. phenolphthalein poly(ether ether sulphone) and phenolphthalein poly(ether ether ketone) were prepared by casting from a common solvent and studied by differential scanning calorimetry. It was found that all the PVP blends are miscible and show a single, composition-dependent glass transition temperature (T(g)). The T(g)-composition dependence has been analysed by the use of the Gordon-Taylor equation. The values of the k parameter in the Gordon-Taylor equation obtained are all not high for the three pairs, in accordance with the fact that there is no strongly specific interaction between PVP and any of the other polymers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, hydrophilic microporous cellulose nitrate membranes have been surface-modified by plasma polymerization of octafluorocyclobutane (OFCB). The microporous composite membranes with a hydrophilic layer sandwiched between two hydrophobic layers have been obtained. The obtained composite membranes have been used in a membrane distillation (MD) process and have exhibited good performance. The effects of polymerization conditions, such as glow-discharge power and deposition time, on the structures and MD performances of the obtained composite membranes have been investigated by SEM, X-ray microscopical analysis, and XPS. The polymerization conditions should be as mild as possible in order to prepare the hydrophobic composite membrane with good MD performance. The typical MD behaviors of the obtained hydrophobic composite membranes are in agreement with that of hydrophobic membranes directly prepared from hydrophobic polymeric materials, like PVDF, PTFE, or PP.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An equation has been derived for the equilibrium swelling of sequential interpenetrating polymer networks (IPNs), which exhibit a single glass transition temperature and the two components are considered to be compatible. The properties of the equilibrium swelling and elastic modulus of sequential poly(vinyl acetate)/poly(methyl acrylate) IPNs have been discussed according to the derived equation and the Siegfried-Thomas-Sperling formula of the elastic modulus for homo IPNs. In both fully swollen and bulk states, there was favourable evidence for added physical crosslinks in poly(vinyl acetate)/poly(methyl acrylate) IPNs. The Binder-Frisch theory is also discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dynamics of phase separation in a binary polymer blend of poly(vinyl acetate) with poly(methyl methacrylate) was investigated by using a time-resolved light-scattering technique. In the later stages of spinodal decomposition, a simple dynamic scaling law was found for the scattering function S(q, t)(S(q, t) approximately I(q, t)): S(q, t)q(m)-3 S approximately (q/q(m)). The scaling function determined experimentally was in good agreement with that predicted by Furukawa, S approximately (X) approximately X2/(3 + X8) for critical concentration, and approximately in agreement with that predicted by Furukawa, S approximately (X) approximately X2/(3 + X6) for non-critical mixtures. The light-scattering invariant shows that the later stages of the spinodal decomposition were undergoing domain ripening.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of poly(N-vinyl-2-pyrrolidone) (PVP) with a copolyamide (CoPA) randomly composed of 1:1:1 (wt) nylon 6, nylon 66 and nylon 610 structural units were prepared by casting from a common solvent. They were found to be miscible and show a single, composition-dependent glass transition temperature (T(g)). The addition of PVP to CoPA significantly lowers the crystallinity owing to an increasing T(g) of the system. The observed miscibility is proposed to be the result of specific interactions between the proton acceptor groups of PVP and the amide groups of CoPA.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrochemical behaviour of N-benzylaniline polymerization is determined by the nature of the electrolyte. The voltammograms for a poly-N-benzylaniline modified Pt electrode prepared in 1 M HCl (abbreviated to PBAn(HCl)), and 1 M H2SO4 (PBAn(H2SO4)) tested in 1 M hydrochloric, sulfuric, and perchloric acid were almost superimposable. The polymer film electrode prepared in 1 M HClO4 (abbreviated to PBAn(HClO4)) is electroinactive, and exhibits only charging behaviour in 1 M HClO4 solution and can be activated in hydrochloric or other acid electrolytes with a smaller anion. These interesting phenomena are explained in terms of the anions catalyzing the loss of benzyl groups.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The chemical polymerization of ortho-methylaniline (MAn) is performed in aqueous solution of six protonic acids. The MAn polymerization conversion, and the electrical conductivity and doping level as well as molecular chain structure of the polymers obtained depend not only on the acid concentration but also on their acidity and molecular size.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The phase behaviours of poly(vinyl acetate) (PVAc) and poly(styrene-co-acrylonitrile)s (SAN) with poly(epichlorohydrin) (PECH) were examined using differential scanning calorimetry and an optical method using a hot plate. The PECH/PVAc blends showed LCST behaviour. The observed miscibility is thought to be a result of hydrogen-bonding interactions between the alpha-hydrogen atoms of PECH and the carbonyl groups of PVAc. Two SAN copolymers with an acrylonitrile (AN) content of 18 wt% (SAN18) and 25 wt% (SAN25), respectively, were also found to exhibit miscibility with PECH. No phase separation occurred by heating up to about 280-degrees-C, and the individual blend has a single, composition-dependent glass transition temperature. The formation of miscible PECH/SAN blends can be considered as a result of the intramolecular repulsion between styrene and AN units in SAN.