935 resultados para asymmetrical pumping


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Infrared to ultraviolet and visible upconversion luminescence was demonstrated in trivalent cerium doped YAlO3 crystal (Ce3+: YAP) under focused infrared femtosecond laser irradiation. The fluorescence spectra show that the upconverted luminescence comes from the 5d-4f transitions of trivalent cerium ions. The dependence of luminescence intensity of trivalent cerium on infrared pumping power reveals that the conversion of infrared radiation is dominated by three-photon excitation process. It is suggested that the simultaneous absorption of three infrared photons pumps the Ce3+ ion into upper 5d level, which quickly nonradiatively relax to lowest 5d level. Thereafter, the ions radiatively return to the ground states, leading to the characteristic emission of Ce3+. (c) 2005 Optical Society of America.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

在分析激光晶体的研究现状的基础上,指出其未来应用及主要发展趋势:面向先进制造技术、激光武器等应用的(1μm波段)高功率、大能量激光晶体;面向人眼安全、遥感、光通讯、医疗等应用的红外激光晶体;面向全色显示、光刻等应用的蓝绿紫和可见光激光晶体;LD泵浦超快激光增益和放大介质材料.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

应用中频感应提拉法生长出不同掺杂浓度的Yb:FAP激光晶体,运用电感耦合等离子体原子发射光谱仪(ICP-AES)测定了Yb^3+离子存Yb:FAP晶体中的分凝系数约为0.03。随着晶体的生长,晶体中Yb^3+离子的轴向浓度逐渐增大。研究Yb:FAP晶体在77K和300K温度下的吸收光谱发现,振动谱的变化主要是由电子-声子近共振耦合作用引起的。系统地研究了不同Yb^3+离子掺杂浓度Yb:FAP晶体的吸收光谱和荧光光谱。通过吸收光谱的测量计算了晶体的吸收截面。Yb:FAP晶体在904nm和982nm处存在Yb

Relevância:

10.00% 10.00%

Publicador:

Resumo:

用提拉法成功地生长了6mol%的高浓度掺铒铌酸锂晶体。测量了晶体的两个非偏振方向(X和Z)以及两个偏振方向(π和δ)的吸收光谱。高浓度掺铒铌酸锂晶体的吸收系数高,有利于提高泵浦效率。根据所测的吸收光谱用Judd-Ofelt理论拟合出了Er^3+离子的强度参数Ωλ。所得的均方差结果显示偏振拟合的误差要小于非偏振拟合。利用偏振吸收数据计算了各能级跃迁的自发辐射跃迁几率(AJJ’)、辐射寿命(τ)、荧光分支比(β)和积分发射截面(σp)等参数,对计算结果进行了讨论并与其他文献的报道结果进行了比较。

Relevância:

10.00% 10.00%

Publicador:

Resumo:

利用激光二极管(LD)抽运新型Na.Yb共掺CaF2(Na.Yb:CaF2)晶体,获得了1.05μm的自调Q激光输出。利用透射率1%的耦合输出镜,得到最低激光输出的抽运阈值功率仅为70mW。在透射率为2%的输出镜条件下,得到最大输出激光功率为390mw,此时激光的斜度效率达到20%。实验详细记录了自调Q脉冲的周期和宽度随抽运功率的变化关系,随着抽运功率的增加,自调Q脉冲的周期和宽度呈指数衰减。同时,还采用单棱镜进行光谱调谐实验,获得了1036~1059nm的自调Q激光调谐输出。

Relevância:

10.00% 10.00%

Publicador:

Resumo:

By using a pump recycling configuration, the maximum power of 8.1 W in the wavelength range 1.935-1.938 mu m is generated by a 5-mm long Tm:YAlO3 (4 at. %) laser operating at 18 degrees C with a pump power of 24 W. The highest slope efficiency of 42% is attained, and the pump quantum efficiency is up to 100%. The Tm:YAlO3 laser is employed as a pumping source of singly-doped Ho(l%):GdVO4 laser operating at room temperature, in which continuous wave output power of greater than 0.2 W at 2.05 mu m is achieved with a slope efficiency of 9%.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Spectroscopic properties of (Y0.9-xLa0.1Ybx)(2)O-3 transparent ceramic were studied. Two main absorption peaks of the specimen are centered at 940 and 970 nm, which are suitable for InGaAs laser diode pumping. The main emission peaks were located at 1032 and 1075 nm with larger emission cross-section and longer fluorescence lifetime than those of Yb:Y2O3. These properties of (Y0.9-xLa0.1Ybx)(2)O-3 transparent ceramic are favorable to achieve high efficiency and high power laser output. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Compact femtosecond laser operation of Yb:Gd2SiO5 (Yb:GSO) crystal was demonstrated under high-brightness diode-end-pumping. A semiconductor saturable absorption mirror was used to start passive mode-locking. Stable mode-locking could be realized near the emission bands around 1031, 1048, and 1088 nm, respectively. The mode-locked Yb: GSO laser could be tuned from one stable mode-locking band to another with adjustable pulse durations in the range 1 similar to 100 ps by slightly aligning laser cavity to allow laser oscillations at different central wavelengths. A pair of SF10 prisms was inserted into the laser cavity to compensate for the group velocity dispersion. The mode-locked pulses centered at 1031 nm were compressed to 343 fs under a typical operation situation with a maximum output power of 396 mW. (c) 2007 Optical Society of America.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

For the first time, a quaternary doping system of Er3+, Yb3+, Ce3+, Na+:CaF2 single crystal was demonstrated to have high fluorescence yield in the eye-safe 1.5 mu m region under 980 nm laser diode pumping, with relatively broad and flat gain curves. A simplified model was established to illustrate the effect of Ce3+ on the branching ratio for the Er3+4I11/2 -> I-4(13/2) transition. With 0.2-at.% Er3+ and 2.0-at.% Ce3+ in the quaternary-doped CaF2 crystal, the branching ratio was estimated to be improved more than 40 times by the deactivating effect of Ce3+ on the Er3+ 4I11/2 level. The quaternary-doped CaF2, system shows great potential to achieve high laser performance in the 1.5 mu m region. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

本文研究了红外飞秒激光照射下Ce^3+ 掺杂的YAP和LSO两种闪烁晶体的上转换发光现象.实验发现在飞秒激光泵浦下,这两种晶体的荧光均来自于Ce^3+离子的5d-4f跃迁.荧光强度与泵浦光功率之间的依赖关系揭示了Ce^3+:YAP和Ce^3+:LSO晶体的上转换过程皆由三光子吸收过程所主导.分析表明,Ce^3+:YAP和Ce^3+:LSO晶体中的三光子吸收是三光子同时吸收.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report on room temperature laser actions of a novel thulium-doped crystal Tm center dot Lu2SiO5 (LSO) under diode pumping. An optical optical conversion efficiency of 12% and a slope efficiency of 21% were obtained with the maximum continuous wave (CW) output power of 0.67 W. The emission wavelengths of Tm LSO laser were centered at 2058.4 nm with bandwidth of similar to 13.6 nm.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Transparent 1 at% Nd3+:Y1.9La0.1O3 ceramics were fabricated with nanopowders prepared by carbonate coprecipitation method. The powder compacts were sintered in H-2 atmosphere at 1550 degrees C for 30 h. The Nd3+:Y1.9La0.1O3 ceramics display uniform grains of about 50 mu m and high transparency. The highest transmittance of the ceramics reaches 67%. The strongest absorption peak is in the wavelength of 820 nm with absorption cross section of 2.48 x 10(-20) cm(2). The absorption is still high at LD wavelength 806 nm with absorption cross section of 1.78 x 10(-20) cm(2) and broad full width at half maximum (FWHM) of about 6.3 nm. The strongest emission peak was centered at 1078 nm with large stimulated emission cross section of 9.63 x 10(-20) cm(2) and broad FWHM of about 7.8 nm. The broad absorption and emission bandwidth of Nd3+:y(1.9)La(0.1)O(3) transparent ceramics are favorable to achieve the miniaturized LD pumping apparatus and ultrashort modelocked pulse laser output, respectively. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper reports that the TM3+:Lu2SiO5 (Tm:LSO) crystal is grown by Czochralski technique. The room-temperature absorption spectra of Tm:LSO crystal are measured on a b-cut sample with 4 at.% thulium. According to the obtained Judd-Ofelt intensity parameters Omega(2)=9.3155 x 10(-20) cm(2), Omega(4)=8.4103 x 10(-20) cm(2), Omega(6)=1.5908 x 10(-20) cm(2), the fluorescence lifetime is calculated to be 2.03 ms for F-3(4) -> H-3(6) transition, and the integrated emission cross section is 5.81 x 10(-18) cm(2). Room-temperature laser action near 2 mu m under diode pumping is experimentally evaluated in Tm:LSO. An optical-optical conversion efficiency of 9.1% and a slope efficiency of 16.2% are obtained with continuous-wave maximum output power of 0.67 W. The emission wavelengths of Tm:LSO laser are centred around 2.06 mu m with spectral bandwidth of similar to 13.6 nm.