912 resultados para BIOMATERIALS
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The aim of this work was to study a series of 11 different compositions of Ti-Zr binary alloys resistance to aggressive environment, i. e., their ability to keep their surface properties and mass when exposed to them as a way to evaluate their performance as biomaterials. The first stage was devoted to the fabrication of tablets from these alloys by Plasma-Skull casting method using a Discovery Plasma machine from EDG Equipamentos, Brazil. In a second stage, the chemical composition of each produced tablet was verified. In a third stage, the specimen were submitted to: as-cast microstructure analysis via optical and scanning electron microscopy (OM and SEM), x-ray dispersive system (EDS) chemical analysis via SEM, Vickers hardness tests for mechanical evaluation and corrosion resistence tests in a 0.9% NaCl solution to simulate exposition to human saliva monitored by open circuit potential and polarization curves. From the obtained results, it was possible to infer that specimens A1 (94,07 wt% Ti and 5,93% wt% Zr), A4 (77,81 wt % Ti and 22,19 wt % Zr) and A8 (27,83 wt% Ti and 72,17 wt% Zr), presented best performance regarding to corrosion resistance, homogeneity and hardness which are necessary issues for biomaterials to be applied as orthopedic and odontological prosthesis
Resumo:
Purpose: Commercially pure titanium alloys are currently used as metallic biomaterials in implantology. Corrosion phenomena appear to play a decisive role in metallic implant long-term behavior. Thus, the goal of this study was to examine the genotoxic potential of corrosion eluates obtained from dental implants using Chinese ovary hamster cells in vitro by the single-cell gel (comet) assay. This technique detects deoxyribonucleic acid strand breaks in individual cells in alkaline conditions.Materials and Methods: the materials tested included 3 dental implants commercially available. Each of the tested materials was corroded in a solution consisting of equal amounts of acetic acid and sodium chloride (0.1 M) for 1, 3, 7, 14, and 21 days. The Chinese ovary hamster cultures were then exposed to all corrosion eluates obtained from endosseous dental implants for 30 minutes at 37 degrees C.Results: None of the eluates was found to exhibit genotoxicity, regardless of the type of dental implant used.Conclusion: the results suggest that all dental implants tested in this study did not induce deoxyribonucleic acid breakage as depicted by the single-cell gel (comet) assay.
Resumo:
The present article describes the preparation and characterization A anionic Collagen gels obtained from porcine intestinal submucosa after 72 h of alkaline treatment and in the form of rhamsan composites to develop injectable biomaterials for plastic for construction. All materials were characterized by SDS/polyacrylamide gel electrophoresis, infrared spectroscopy, thermal stability, potentiometric titration, rheological properties, and fluidity tests. Biocompatibility was appraised after the injection of anionic collagen:rhamsan composites at 2.5% in 60 North Folk rabbits. Independently of processing, the Collagen's secondary structure was preserved in all cases, and after 72 h of hydrolysis the Collagen was characterized by a carboxyl group content of 346 :L 9, which, at physiological pH, corresponds to an increase of 106 17 negative charges, in comparison to native Collagen, due to the selective hydrolysis of asparagine and glutamine carboxyamide side chain. Rheological studies of composites at pH 7.4 in concentrations of 2, 4, and 6% (in proportions of 75:1 and 50:1) showed a viscoelastic behavior dependent on the frequency, which is independent of concentration and proportion. In both, the concentration of the storage modulus always predominated over the loss modulus (G' > G and delta < 45 degrees). The results from creep experiments confirmed this behavior and showed that anionic collagen:rhamsan composites at pH 7.4 in the proportion of 50:1 are less elastic and more susceptible to deformation in comparison to gels in the proportion of 75:1, independent of concentration. This was further confirmed by flow experiments, indicating that the necessary force for the extrusion of anionic collagen:rhamsan composites, in comparison to anionic Collagen, was significantly smaller and with a smooth flow. Biocompatibility studies showed that the tissue reaction of anionic collagen:rhamsan composites at 2.5% in the proportion of 75:1 was compatible with the application of these gels in plastic reconstruction. These results suggest that the association of Collagen with rhamsan may be a good alternative in the replacement of glutaraidehyde to stabilize the microfibril assembly of commercial Collagen gel preparations. (c) 2005 Wiley Periodicals, Inc.
Resumo:
Avaliou-se o uso de biomaterial de origem bovina na regeneração de defeitos ósseos segmentares empregando-se 12 coelhos, fêmeas, da raça Norfolk, com idade de seis meses e pesos entre 3 e 4,5kg. Realizou-se falha segmentar bilateral de um centímetro de comprimento na diáfise do rádio, com inclusão do periósteo. No membro direito, o defeito foi delimitado por membrana de pericárdio liofilizada, contendo em seu interior mistura de proteínas morfogenéticas ósseas adsorvidas a hidroxiapatita, colágeno liofilizado e osso inorgânico. No membro esquerdo, o defeito não recebeu tratamento. Radiografias foram obtidas ao término do procedimento cirúrgico e aos sete, 30, 60, 90, 120 e 150 dias de pós-operatório. Após eutanásia de seis coelhos aos 60 dias e seis aos 150 dias de pós-cirúrgico, os resultados radiográficos e histológicos mostraram que a regeneração óssea foi inibida nos defeitos segmentares tratados com o biomaterial.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Lesões do tecido ósseo podem ser causadas por fatores congênitos e adquiridos e resultar em deformidade nasal com repercussão estética e funcional. O tratamento cirúrgico desses casos requer reconstruções complexas e frequentemente o uso de biomateriais. O poliuretano derivado do óleo da mamona apresenta uma fórmula com aspectos favoráveis de processabilidade, flexibilidade de formulação, ausência de emissão de vapores tóxicos e baixo custo. Entretanto, a despeito dos resultados favoráveis, estudos referentes ao uso do polímero de mamona, avaliando a reação tecidual no dorso nasal, ainda não foram realizados. OBJETIVO: O objetivo deste estudo consiste em avaliar histologicamente a biocompatibilidade do implante do polímero de mamona no dorso nasal. FORMA DE ESTUDO: Experimental. MATERIAL E MÉTODO: Foram utilizados quatro macacos-pregos da espécie Cebus apella. Um defeito ósseo foi realizado no osso nasal em todos os animais e colocado um implante de polímero de mamona. A eutanásia foi realizada com 270 dias de pós-operatório, e as amostras foram submetidas a estudo histológico. RESULTADOS: Na análise histológica não foi observada a presença de granuloma de corpo estranho ou células fagocitárias. Progressiva formação óssea e maturação foram observadas. CONCLUSÃO: Os resultados macroscópicos e microscópicos mostraram que o implante de polímero de mamona foi biocompatível.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Extensive bone defects in maxillofacial region can be corrected with autogenous grafts; otherwise, the disadvantages of the therapeutics modality take the research for new bone substitutes. The aim of the study was to evaluate and compare the osteoconductive properties of 3 commercial available biomaterials. A total of 30 calvarial defects (5-mm diameter) were randomly divided into 5 treatment groups, with a total of 6 defects per treatment group (n = 6). The treatment groups were as follows: 500 to 1000 Km beta-tricalcium phosphate (beta-TCP), polylactic and polyglycolic acid (PL/PG) gel, calcium phosphate cement, untreated control, and autograft control. The evaluations were based on histomorphometric analysis at 60 postoperative days. The results have shown that beta-TCP and autograft control supported bone formation at 60 postoperative days. beta-Tricalcium phosphate showed the highest amount of mineralized area per total area and statistically significant compared with PL/PG, calcium phosphate cement, and untreated control groups. The PL/PG gel does not have osteoconductive properties and performed similar to empty control. Calcium phosphate cement showed higher number of multinucleated giant cells around the sites of the biomaterial and showed newly formed bone only at the edges of the biomaterial, without bone formation within the biomaterial. The findings presented herein indicate that bone formation reached a maximum level when rat calvarial defects were filled with beta-TCP at 60 postoperative days. Further studies should be conducted with beta-TCP to understand the potential of this biomaterial in bone regeneration.
Resumo:
Traumatic injuries treatment of the fronto-naso-orbito-ethmoidal region has been one of the most challenging treatments within maxillofacial surgery, particularly of extensive orbital defects, very common in this type of pathologic condition. A 48-year-old man involved in a car collision presented an extensive bilateral fracture of the orbit medial wall, nasal bones, the nasal septum, and the frontal anterior table. The clinical and tomographic findings concluded the diagnosis of a maxilla and fronto-naso-orbito-ethmoidal fracture. Among the variety of biomaterials, the titanium mesh was elected because of the extension and magnitude of the bone defect, obtaining this way esthetic and functional results with better prognosis.
Resumo:
The restoration and recovery of the alveolar healing process are a challenge to dental surgeons to achieve satisfactory results at the osseointegration of implants and implant rehabilitation. Different operative technique and biomaterials are being used to reconstruct the framework of the alveolar process. One of the biomaterials used for this purpose is the bioactive glass. The aim of this study was to report clinical and histologic final results of 7 clinical reports of alveolar ridge augmentation using bioactive glass. Clinically, bioglass was able to maintain bone architecture of the alveolar bone and repaired satisfactory. Biopsy was performed on the histologic samples and showed bone formation in intimate contact to the particles of the biomaterial.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Objectives: To characterize the interaction of 1-Ethyl-3-[3-dimethylaminopropyl] carbodiimide Hydrochloride (EDC) with dentin matrix and its effect on the resin-dentin bond. Methods: Changes to the stiffness of demineralized dentin fragments treated with EDC/N-hydroxysuccinimide (NHS) in different solutions were evaluated at different time points. The resistance against enzymatic degradation was indirectly evaluated by ultimate tensile strength (UTS) test of demineralized dentin treated or not with EDC/NHS and subjected to collagenase digestion. Short- and long-term evaluations of the strength of resin-dentin interfaces treated with EDC/NHS for 1 h were performed using microtensile bond strength (mu TBS) test. All data (MPa) were individually analyzed using ANOVA and Tukey HSD tests (alpha = 0.05). Results: The different exposure times significantly increased the stiffness of dentin (p < 0.0001, control-5.15 and EDC/NHS-29.50), while no differences were observed among the different solutions of EDC/NHS (p = 0.063). Collagenase challenge did not affect the UTS values of EDC/NHS group (6.08) (p > 0.05), while complete degradation was observed for the control group (p = 0.0008, control-20.84 and EDC/NHS-43.15). EDC/NHS treatment did not significantly increase resin-dentin mu TBS, but the values remained stable after 12 months water storage (p < 0.05). Conclusions: Biomimetic use of EDC/NHS to induce exogenous collagen cross-links resulted in increased mechanical properties and stability of dentin matrix and dentin-resin interfaces. (C) 2010 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 94B: 250-255, 2010.
Resumo:
Research has clarified the properties required for polymers that resist bacterial colonisation for use in medical devices. The increase in antibiotic-resistant microorganisms has prompted interest in the use of silver as an antimicrobial agent. Silver-based polymers can protect the inner and outer surfaces of devices against the attachment of microorganisms. Thus, this review focuses on the mechanisms of various silver forms as antimicrobial agents against different microorganisms and biofilms as well as the dissociation of silver ions and the resulting reduction in antimicrobial efficacy for medical devices. This work suggests that the characteristics of released silver ions depend on the nature of the silver antimicrobial used and the polymer matrix. In addition, the elementary silver, silver zeolite and silver nanoparticles, used in polymers or as coatings could be used as antimicrobial biomaterials for a variety of promising applications. (C) 2009 Elsevier B. V. and the International Society of Chemotherapy. All rights reserved.