899 resultados para Split tensile strength
Resumo:
The tensile strength obtained from existing testing methods such as ASTM D3039, based on flat coupons, usually has a large scatter for fibre reinforced polymer (FRP) composites. This means that the measured strength may not represent the actual strength of the material, leading to under or over design. This paper develops a new interpretation method which requires fewer tests, saving money and time. Moreover the results are more consistent and more closely represent the actual strength which can lead to a safer and more economical design.
Resumo:
This paper investigates the effects of polyethylene glycol (PEG), on the mechanical and thermal properties of nalidixic acid/ploy ε-caprolactone (NA)/PCL blends prepared by hot melt extrusion. The blends were characterized by tensile and flexural analysis, dynamic mechanical analysis, differential scanning calorimetry, thermogravimetric analysis and X-ray diffraction. Experimental data indicated that the addition of NA caused loss of the tensile strength and toughness of PCL. Thermal analysis of the PCL showed that on addition of the thermally unstable NA, thermal degradation occurred early and was autocatalytic. However, the NA did benefit from the heat shielding provided by the PCL matrix resulting in more thermally stable NA particles. Results show that loading PEG in the PCL had a detrimental effect on the tensile strength and toughness of the blends, reducing them by 20-40%. The partial miscibility of the PCL-PEG system, causes an increase in Tg. While increases in the crystallinity is attributed to the plasticisation effect of PEG and the nucleation effect of NA. The average crystal size increased by 8% upon PEG addition.
Resumo:
Composites of Linear Low Density Polyethylene (LLDPE) and Graphene Nanoplatelets (GNPs) were processed using a twin screw extruder under different extrusion conditions. The effects of screw speed, feeder speed and GNP content on the electrical, thermal and mechanical properties of composites were investigated. The inclusion of GNPs in the matrix improved the thermal stability and conductivity by 2.7% and 43%, respectively. The electrical conductivity improved from 10−11 to 10−5 S/m at 150 rpm due to the high thermal stability of the GNPs and the formation of phonon and charge carrier networks in the polymer matrix. Higher extruder speeds result in a better distribution of the GNPs in the matrix and a significant increase in thermal stability and thermal conductivity. However, this effect is not significant for the electrical conductivity and tensile strength. The addition of GNPs increased the viscosity of the polymer, which will lead to higher processing power requirements. Increasing the extruder speed led to a reduction in viscosity, which is due to thermal degradation and/or chain scission. Thus, while high speeds result in better dispersions, the speed needs to be optimized to prevent detrimental impacts on the properties.
Resumo:
Today more than 99% of plastics are petroleum-based because of the availability and cost of the raw material. The durability of disposed plastics contributes to the environmental problems as waste and their persistence in the environment causes deleterious effects on the ecosystem. Environmental pollution awareness and the demand for green technology have drawn considerable attention of both academia and industry into biodegradable polymers. In this regard green chemistry technology has the potential to provide solution to this issue. Enzymatic grafting has recently been the focus of green chemistry technologies due to the growing environmental concerns, legal restrictions, and increasing availability of scientific knowledge. Over the last several years, research covering various applications of robust enzymes like laccases and lipases has been increased rapidly, particularly in the field of polymer science, to graft multi-functional materials of interest. In principle, enzyme-assisted grafting may modify/impart a variety of functionalities to the grafted composites which individual materials fail to demonstrate on their own. The modified polymers through grafting have a bright future and their development is practically boundless. In the present study series of graft composites with poly(3-hydroxybutyrate) (P(3HB) as side chain and cellulose as a backbone polymer were successfully synthesised by introducing enzymatic grafting technique where laccase and lipase were used as model catalysts [1-3]. Subsequently, the resulting composites were removed from the casting surface under ambient environment and characterised by Fourier-transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), and X-ray diffraction (XRD) in detail. Moreover, the thermo-mechanical behaviours of the grafted composites were investigated by differential scanning calorimetry (DSC) and dynamic mechanical analyser (DMA) measurements, respectively. In addition, hydrophobic and hydrophilic characteristics of the grafted polymers were studied through drop contour analysis using water contact angle (WCA). In comparison to the individual counterparts improvement was observed in the thermo- mechanical properties of the composites to varied extent. The tensile strength, elongation at break, and Young’s modulus values of the composites reached their highest levels in comparison to the films prepared with pure P(3HB) only which was too fragile to measure any of the above said characteristics. Interestingly, untreated P(3HB) was hydrophobic in nature and after lipase treatment P(3HB) and P(3HB)-EC-based graft composite attained higher level of hydrophilicity. This is a desired characteristic that enhances the biocompatibility of the materials for proper cell adhesion and proliferation therefore suggesting potential candidates for tissue engineering/bio-medical type applications [3]. The present research will be a first step in the biopolymer modification. To date no report has been found in literature explaining the laccase/lipase assisted grafting of P(3HB) [1-3]. The newly grafted composites exhibit unique functionalities with wider range of potential applications in bio-plastics, pharmaceutical, and cosmetics industries, tissue engineering, and biosensors. [1] H.M.N. Iqbal, G. Kyazze, T. Tron and T. Keshavarz, Cellulose 21, 3613-3621 (2014). [2] H.M.N. Iqbal, G. Kyazze, T. Tron and T. Keshavarz, Carbohydrate Polymers 113, 131-137 (2014). [3] H.M.N. Iqbal, G. Kyazze, T. Tron and T. Keshavarz, Polymer Chemistry In-Press, DOI: 10.1039/C4PY0 0857J (2014).
Resumo:
Trabalho Final de Mestrado para obtenção do grau de Mestre em Engenharia Mecânica
Resumo:
In this study, the tensile strength of single-lap joints (SLJs) between similar and dissimilar adherends bonded with an acrylic adhesive was evaluated experimentally and numerically. The adherend materials included polyethylene (PE), polypropylene (PP), carbon-epoxy (CFRP), and glass-polyester (GFRP) composites. The following adherend combinations were tested: PE/PE, PE/PP, PE/CFRP, PE/GFRP, PP/PP, CFRP/CFRP, and GFRP/GFRP. One of the objectives of this work was to assess the influence of the adherends stiffness on the strength of the joints since it significantly affects the peel stresses magnitude in the adhesive layer. The experimental results were also used to validate a new mixed-mode cohesive damage model developed to simulate the adhesive layer. Thus, the experimental results were compared with numerical simulations performed in ABAQUS®, including a developed mixed-mode (I+II) cohesive damage model, based on the indirect use of fracture mechanics and implemented within interface finite elements. The cohesive laws present a trapezoidal shape with an increasing stress plateau, to reproduce the behaviour of the ductile adhesive used. A good agreement was found between the experimental and numerical results.
Resumo:
Os sectores da construção e demolição de edifícios são responsáveis por um elevado volume de produção de resíduos. Estes resíduos são normalmente direcionados para aterros, que se encontram, neste momento, sobrelotados. Esta falta de capacidade de receção de resíduos tem como consequência imediata o aumento dos valores monetários associados ao depósito destes materiais excedentários. Com a elevada produção destes resíduos torna-se importante a sua reciclagem e reutilização. No caso da Engenharia Civil, uma grande produtora de resíduos, seria ainda mais interessante o seu reaproveitamento imediato na área. Nesta investigação, pretendeu-se avaliar o desempenho mecânico de betões com diferentes percentagens de agregados cerâmicos vermelhos. Essa investigação passou numa fase inicial pelo estado fresco do betão, de forma a analisar a sua trabalhabilidade. Na fase seguinte, analisou-se no estado endurecido, a resistência à compressão e resistência à tração por compressão diametral. Para concretização deste objetivo produziram-se três tipos de betões: um de referência (areia fina e brita fina), um betão com incorporação de agregados finos e grossos de cerâmica vermelha, juntamente com a areia fina e a brita fina, e o terceiro, um betão com a substituição total da areia fina por cerâmica fina. A realização desta investigação, demostrou que os betões com a incorporação de agregado cerâmico vermelho apresentam resultados de boa qualidade, sendo plausível a sua utilização em estruturas.
Resumo:
BACKGROUND:: Mechanical stretch has been shown to induce vascular remodeling and increase vessel density, but the pathophysiologic mechanisms and the morphologic changes induced by tensile forces to dermal vessels are poorly understood. METHODS:: A custom computer-controlled stretch device was designed and applied to the backs of C57BL/6 mice (n = 38). Dermal and vascular remodeling was studied over a 7-day period. Corrosion casting and three-dimensional scanning electron microscopy and CD31 staining were performed to analyze microvessel morphology. Hypoxia was assessed by immunohistochemistry. Western blot analysis of vascular endothelial growth factor (VEGF) and mRNA expression of VEGF receptors was performed. RESULTS:: Skin stretching was associated with increased angiogenesis as demonstrated by CD31 staining and vessel corrosion casting where intervascular distance and vessel diameter were decreased (p < 0.01). Immediately after stretching, VEGF dimers were increased. Messenger RNA expression of VEGF receptor 1, VEGF receptor 2, neuropilin 1, and neuropilin 2 was increased starting as early as 2 hours after stretching. Highly proliferating epidermal cells induced epidermal hypoxia starting at day 3 (p < 0.01). CONCLUSIONS:: Identification of significant hypoxic cells occurred after identification of neovessels, suggesting an alternative mechanism. Increased expression of angiogenic receptors and stabilization of VEGF dimers may be involved in a mechanotransductive, prehypoxic induction of neovascularization.
Resumo:
L’ablation de cibles d’Al nanocristallines (taille moyenne des cristallites d = 3,1 et 6,2 nm) par impulsions laser ultrabrèves (200 fs) a été étudiée par l’entremise de si- mulations combinant la dynamique moléculaire et le modèle à deux températures (two- temperature model, TTM) pour des fluences absorbées allant de 100 à 1300 J/m2. Nos simulations emploient un potentiel d’interaction de type EAM et les propriétés électro- niques des cibles en lien avec le TTM sont représentées par un modèle réaliste possédant une forme distincte dans le solide monocristallin, le solide nanocristallin et le liquide. Nous avons considéré l’effet de la taille moyenne des cristallites de même que celui de la porosité et nous avons procédé à une comparaison directe avec des cibles mono- cristallines. Nous avons pu montrer que le seuil d’ablation des métaux nanocristallins est significativement plus bas, se situant à 400 J/m2 plutôt qu’à 600 J/m2 dans le cas des cibles monocristallines, l’écart étant principalement dû à l’onde mécanique plus im- portante présente lors de l’ablation. Leur seuil de spallation de la face arrière est aussi significativement plus bas de par la résistance à la tension plus faible (5,40 GPa contre 7,24 GPa) des cibles nanocristallines. Il est aussi apparu que les contraintes résiduelles accompagnant généralement l’ablation laser sont absentes lors de l’ablation de cibles d’aluminium nanocristallines puisque la croissance cristalline leur permet d’abaisser leur volume spécifique. Nos résultats indiquent aussi que le seuil de fusion des cibles nano- cristallines est réduit de façon marquée dans ces cibles ce qui s’explique par la plus faible énergie de cohésion inhérente à ces matériaux. Nos simulations permettent de montrer que les propriétés structurelles et électroniques propres aux métaux nanocristallins ont toutes deux un impact important sur l’ablation.
Resumo:
Prevulcanized natural rubber latex was prepared by the heating of the latex compound at 55°C for different periods of time (2, 4, 6, 8, and 10 h). The changes in the colloidal stability and physical properties were evaluated during the course of prevulcanization. The prevulcanized latex compounds were stored for 300 days, and the properties were monitored at different storage intervals (0, 20, 40, 60, 120, 180, 240, and 300 days). During prevulcanization, the mechanical stability time increased, and the viscosity remained almost constant. The tensile strength increased during storage for a period of 20 days. The degree of crosslinking, modulus, elongation at break, and chloroform number were varied with the time of storage.
Resumo:
A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent.
Resumo:
Zinc salts of ethyl, isopropyl, and butyl xanthates were prepared in the laboratory. The effect of these xanthates in combination with zinc diethyldithiocarbamate (ZDC) on the vulcanization of silica-filled NBR compounds has been studied at different temperatures. The cure times of these compounds were compared with that of NBR compounds containing tetramethylthiuram disulphide/dibenzthiazyl disulphide. The rubber compounds with the xanthates and ZDC were cured at various temperatures from 60 to 150°C. The sheets were molded and properties such as tensile strength, tear strength, crosslink density, elongation at break, compression set, abrasion resistance, flex resistance, heat buildup, etc. were evaluated. The properties showed that zinc salt of xanthate/ZDC combination has a positive synergistic effect on the cure rate and mechanical properties of NBR compounds.
Resumo:
Zinc salts of ethyl, isopropyl, and butyl xanthates are prepared in the laboratory, and the effect of these xanthates with zinc diethyl dithiocarbamate (ZDC) on the vulcanization of HAF-filled nitrile butadiene rubber (NBR) compounds has been studied at different temperatures. The cure times of these compounds have been compared with that of NBR compounds containing TMTD/MBTS. The rubber compounds with the three xanthate accelerators and ZDC are cured at various temperatures from 60 to 150°C. The sheets are molded and properties such as tensile strength, tear strength, cross-link density, elongation at break, compression set, abrasion resistance, flex resistance, etc. have been evaluated. The properties show that zinc salt of the xanthate/ZDC accelerator system has a positive synergistic effect on the cure rate and mechanical properties of NBR compounds.
Resumo:
Zinc butyl xanthate [Zn(bxt)2] was prepared in the laboratory . The effect of this xanthate with zinc diethyl dithiocarbamate (ZDC) on the vulcanization of natural rubber ( NR), polybutadiene rubber (BR), and NR/BR blend has been studied at different temperatures. The amounts of Zn (bxt)2 and ZDC in the compounds were optimized by varying the amount of ZDC from 0 . 75 to 1.5 phr and Zn (bxt)2 from 0 . 75 to 1 .5 phr. The cure characteristics were also studied . HAF filled NR, BR, and NR / BR blend compounds were cured at different temperatures from 60 to 150 C. The sheets were molded and properties such as tensile strength, tear strength, crosslink density and elongation at break, compression set, abrasion resistance, etc. were evaluated. The results show that the mechanical properties of 80NR/20BR blends are closer to that of NR vulcanizates, properties of 60NR/40BR blends are closer to BR vulcanizates, while the 70NR/30BR blends show an intermediate property.
Resumo:
Zinc salts of ethyl, isopropyl and butyl xanthates were prepared in the laboratory. The effect of these xanthates with zinc diethyldithiocarbamate (ZDC) on the vulcanization of HAF filled NR compound has been studied at different temperatures. The rubber compounds with the three xanthate accelerators and ZDC were cured at various temperatures from 60°C to 150°C. The sheets were moulded and properties such as tensile strength , tear strength , cross-link density, elongation -at-break, compression set, heat build up, abrasion resistance, flex resistance , etc. were evaluated . The properties showed that zinc xanthate/ZDC accelerator combination has a positive synergistic effect on the mechanical properties of NR compounds. The curing of HAF filled NR compound containing zinc xanthate /ZDC is slightly slower than the curing of the corresponding gum compounds . It is observed that, by gradually increasing the amount of the accelerator, the cure time of black filled NR compound can be made equal to that of the gum compou