Resumo:
New hybrid composites based on mesostructured V(2)O(5) containing intercalated poly(ethylene oxide), poly-o-methoxyaniline and poly(ethylene oxide)/poly-o-methoxyaniline were prepared. The results suggest that the polymers were intercalated into the layers of the mesostructured V(2)O(5). Electrochemical studies showed that the presence of both polymers in the mesostructured V(2)O(5) (ternary hybrid) leads to an increase in total charge and stability after several cycles compared with binary hybrid composites. This fact makes this material a potential component as cathode for lithium ion intercalation and further, a promising candidate for applications in batteries.
Resumo:
Phosphoniobate glasses with composition (mol%) (100-x) NaPO(3)-xNb(2)O(5) ( x varying from 11 to 33) were prepared and characterized by means of thermal analysis, Fourier transform infrared spectroscopy, Raman scattering and (31)P nuclear magnetic resonance. The addition of Nb(2)O(5) to the polyphosphate base glass leads to depolymerization of the metaphosphate structure. Different colors were observed and assigned as indicating the presence of Nb(4+) ions, as confirmed by electron paramagnetic resonance measurements. The color was observed to depend on the glass composition and melting temperature as well. Er(3+) containing samples were also prepared. Strong emission in the 1550 nm region was observed. The Er(3+4)I(15/2) emission quantum efficiency was observed to be 90% and the quenching concentration was observed to be 1.1 mol%( 1.45 x 10(20) ions cm(-3)). Planar waveguides were prepared by Na(+)-K(+)-Ag(+) ion exchange with Er(3+) containing samples. Optical parameters of the waveguides were measured at 632.8, 543.5 and 1550 nm by the prism coupling technique as a function of the ion exchange time and Ag(+) concentration. The optimized planar waveguides show a diffusion depth of 5.9 mu m and one propagating mode at 1550 nm.
Resumo:
In this work, we report the synthesis, characterization and catalytic properties of a vanadium oxide-silicon oxide composite xerogel prepared by a soft chemistry approach. In order to obtain such material, we submitted a vanadium pentoxide gel previously synthesized via protonation of metavanadate species to an ""in situ"" progressive polycondensation into silica gel. The material has been characterized by X-ray diffraction, infrared spectroscopy, thermogravimetric analysis and scanning electron microscopy. Further, the catalytic activity of this material was evaluated for the epoxidation of styrene and cyclooctene using iodosylbenzene, hydrogen peroxide and m-chloroperbenzoic acid as the oxidizing agent.
Resumo:
The influence of the preparation method on the structural properties of the RuO(2)-Ta(2)O(5) system was investigated. Both thin films on Ti substrates and powder samples of nominal composition Ti/RuO(2)-Ta(2)O(5) (Ru:Ta = 100:0, 90:10, 80:20, 30:70, and 0:100 at.%) were prepared through thermal decomposition of polymeric precursors (DPP). The thin films and powder samples were investigated using X-ray absorption spectroscopy (XAS). XANES analyses showed that Ru and Ta are present in the Ru(IV) and Ta(V) oxidation states. EXAFS signals of all the samples were analyzed, to obtain the average bond length (r), coordination number, and the Debye-Waller factor (sigma(2)) for each Ru-O, Ru-Ru, Ta-O nearest-neighbor. The first shell Ru-O distance was found at 1.91-1.92 angstrom with coordination number of 1.8-2.1, and at 2.01-2.02 angstrom with coordination number of 3.9-4.1. The Ta-O distance obtained for all the samples and in both modes (transmission and fluorescence) had significantly different values from the theoretical ones. The results revealed that the local structure around both the Ru and Ta sites are similar, and that they consist of distorted M-O(6) octahedra (where M = Ru or Ta). (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Luminescent and morphological studies of Sr(2)CeO(4) blue phosphor prepared from cerium-doped strontium oxalate precursor are reported Powder samples were prepared from 5 and 25 mol% Ce(3+)-doped strontium oxalate as well as from a mechanical mixture of strontium oxalate and cerium oxalate at a 4 1 ratio respectively All the samples were characterized by XRD IR PLS and SEM The luminescent and structural properties of the Sr(2)CeO(4) material are little affected by the SrCO(3) remaining from precursors The Sr(2)CeO(4) material consists in one-dimensional chains of edge-sharing CeO(6) octahedra that are linked together by Sr(2+) ions The carbonate ion might be associated with oxygen ions of the linear chain and also with the oxygen atoms located in the equatorial position which consequently affects the charge transfer bands between O(2-) and Ce(4+). As observed by SEM, the morphological changes are related to each kind of precursor and thermal treatment along with irregular powder particles within the size range 05-2 mu m (c) 2010 Elsevier B V All rights reserved
Resumo:
Cetyltrimethylammonium bromide (CTAB) and n-hexadecylamine (HDA) have been used as template in the synthesis of a mesolamellar xerogel tungsten oxide phase (WO(3)/CTAB/HDA). The catalytic properties of the resulting material were investigated in the oxidation of cis-cyclooctene, styrene, and cyclohexane, using hydrogen peroxide (H(2)O(2)), terc-butyl hydroperoxide (t-BOOH), or m-chlorperbenzoic acid (m-CPBA) as oxygen transfer agent. In general, the catalytic results were comparable to those obtained with related systems, thus suggesting the potential application of this material as catalyst for epoxidation reactions. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Semi-interpenetrating networks (Semi-IPNs) with different compositions were prepared from poly(dimethylsiloxane) (PDMS), tetraethylorthosilicate (TEOS), and poly (vinyl alcohol) (PVA) by the sol-gel process in this study. The characterization of the PDMS/PVA semi-IPN was carried out using Fourier transform infrared spectroscopy (FTIR), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), scanning electron microscopy (SEM), and swelling measurements. The presence of PVA domains dispersed in the PDMS network disrupted the network and allowed PDMS to crystallize, as observed by the crystallization and melting peaks in the DSC analyses. Because of the presence of hydrophilic (-OH) and hydrophobic (Si-(CH(3))(2)) domains, there was an appropriate hydrophylic/hydrophobic balance in the semi-IPNs prepared, which led to a maximum equilibrium water content of similar to 14 wt % without a loss in the ability to swell less polar solvents. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 115: 158-166, 2010
Resumo:
In this paper we present some result on sol-gel derived silica-hafnia systems. In particular we focus on fabrication, morphological and spectroscopic assessment of Er(3+)-activated thin films. Two examples of silica-hafnia-derived waveguiding glass ceramics, prepared by top-down and bottom-up techniques are reported, and the main optical properties are discussed. Finally, some properties of activated microspherical resonators, having a silica core, obtained by melting the end of a telecom fiber, coated with an Er(3+)-doped 70SiO(2)-30HfO(2) film, are presented. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
The Jacobsen catalyst, Mn(salen), was immobilized in chitosan membrane. The obtained Mn(salen)-Chit was characterized by thermogravimetric analysis (TC), differential thermal analysis (DTA), differential scanning calorimetry (DSC), infrared spectroscopy (FT-IR), degree of N-acetylation by (1)H NMR, and UV-vis spectroscopy. The UV-vis absorption spectrum of the encapsulated catalyst displayed the typical bands of the Jacobsen catalyst, and the FT-IR presented an absorption band characteristic of the imines present in the Jacobsen catalyst. The chitosan membranes were available, in a biphasic system, as a catalytic barrier between two different phases: an organic substrate phase (cyclooctene or styrene) and an aqueous solution of either m-CPBA, t-BuOOH or H(2)O(2), and dismissing the need for phase transfer agents and leading to better product yields compared with the catalyst in homogeneous medium. This new catalyst did not leach from the support and was reused many times, leading to high turnover frequencies. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
The resin phase of dental composites is mainly composed of combinations of dimethacrylate comonomers, with final polymeric network structure defined by monomer type/reactivity and degree of conversion. This fundamental study evaluates how increasing concentrations of the flexible triethylene glycol dimethacrylate (TEGDMA) influences void formation in bisphenol A diglycidyl dimethacrylate (BisGMA) co-polymerizations and correlates this aspect of network structure with reaction kinetic parameters and macroscopic volumetric shrinkage. Photopolymerization kinetics was followed in real-time by a near-infrared (NIR) spectroscopic technique, viscosity was assessed with a viscometer, volumetric shrinkage was followed with a linometer, free volume formation was determined by positron annihilation lifetime spectroscopy (PALS) and the sol-gel composition was determined by extraction with dichloromethane followed by (1)H NMR analysis. Results show that, as expected, volumetric shrinkage increases with TEGDMA concentration and monomer conversion. Extraction/(1)H NMR studies show increasing participation of the more flexible TEGDMA towards the limiting stages of conversion/crosslinking development. As the conversion progresses, either based on longer irradiation times or greater TEGDMA concentrations, the network becomes more dense, which is evidenced by the decrease in free volume and weight loss after extraction in these situations. For the same composition (BisGMA/TEGDMA 60-40 mol%) light-cured for increasing periods of time (from 10 to 600 s), free volume decreased and volumetric shrinkage increased, in a linear relationship with conversion. However, the correlation between free volume and macroscopic volumetric shrinkage was shown to be rather complex for variable compositions exposed for the same time (600 s). The addition of TEGDMA decreases free-volume up to 40 mol% (due to increased conversion), but above that concentration, in spite of the increase in conversion/crosslinking, free volume pore size increases due to the high concentration of the more flexible monomer. In those cases, the increase in volumetric shrinkage was due to higher functional group concentration, in spite of the greater free volume. Therefore, through the application of the PALS model, this study elucidates the network formation in dimethacrylates commonly used in dental materials. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
Silica xerogels were prepared by a sol-gel process catalyzed by acid with tetraethylorthosilicate, and using an organic covalent ligand template (methyltriethoxysilane) or a noncovalent template C6 surfactant (triethylhexylammonium bromide). The influence of hydrotreatment on the structure of templated xerogels is examined in terms of surface area, micropore volume, average pore size, and pore size distribution, and compared against a blank xerogel (nontemplated). The role of surface functional groups was evaluated using Si-29 nuclear magnetic resonance. The structural integrity of the xerogel was maintained to a large extent in samples that had a high contribution of Q(4) species (siloxane groups). Xerogel matrix densification occurred when there was a large concentration of Q(3) and Q(2) species (silanol groups), which also were responsible for increased hydrophilicity. The templated xerogels resulted in up to a 25% concentration of methyl functional groups (T-3 and T-2 species), leading to hydrophobic xerogels. The best results in terms of structural integrity and hydrophobicity were obtained with templated xerogels prepared with the C6 surfactant. The results in this study suggest that surfactant-enhanced condensation reactions lead to structures with a high contribution of Q(4) groups, which are not susceptible to water attack, but are strong enough to oppose matrix densification during rehydration.
Resumo:
This paper presents the results of the characterisation of templated silica xerogels as precursor material for molecular sieve silica membranes for gas separation. The template agent integrated in the xerogel matrix is a methyl ligand covalently bended to the siloxane network in the form of methyltriethoxysilane (MTES). Several surface and microstructural characterisation techniques such as TGA, FTIR, NMR, and nitrogen adsorption have been employed to obtain information on the reaction mechanisms involved in the sol-gel processing of such molecular sieves. The characterisation results show the effects of processing parameters such as heat treatment temperature, and the concentration of the covalently bonded template on the development of the pore structure. It was found that calcination temperature significantly enhanced the condensation reactions thus resulted in more Si-O-Si groups being formed. This was also confirmed with the data of FTIR characterisation showing enhanced silicon bands at higher heat treatment temperatures. As a result of the promoted densification and shrinkable pore network the micropore volume also reduced with increasing methyl ligand molar ratio. However, the mean pore diameter does not change significantly with calcination temperature. While the contribution of the templates towards controlling pore size is less precise, increasing the methyl ligand molar ratio results in the broadening of the pore size distribution and lower pore volume. Higher template concentration induces the collapse of the xerogel matrix due to capillary stress promoting dense xerogels with low pore volume (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
The radiation chemical yields G(S) and G(X) for H-linking and Y-linking models for Ultem have been calculated from molecular weight analysis by gel permeation chromatography. These G-values have been compared with the G-values obtained from analysis of soluble fractions above the gel dose, Which have been reported in previous works. An analysis of the molecular weight data in terms of H-linking and Y-linking mechanisms yielded values of G(S-H) = 1.0 x 10(-3) and G(H) = 6.0 x 10(-3) and G(S-Y) = 1.3 x 10(-2) and G(Y) = 1.8 x 10(-2). The corresponding values obtained from the solubility data were G(SH) = 0.53 x 10(-2), G(H) = 1.39 x 10(-2), G(S-Y) = 4.2 x 10(-2) and G(Y) - 4.6 x 10(-2). The origin of the disagreement between the molecular weight and solubility values is not clear, but it could arise as a result of observed microgel formation below the reported gel dose of 0.13 MGy. Whether the crosslink mechanism proceeds by an H-linking or Y-linking process is also unclear and will require direct observation of the crosslinking structures.
Resumo:
A produção de biodiesel como combustível para motores diesel, aumentou fortemente nos últimos anos e espera-se que cresça mais e mais num futuro próximo. O aumento do consumo de biodiesel exige processos de produção optimizados que permitam grandes capacidades de produção, operações simplificadas, rendimentos altos, bem como a utilização de matérias-primas mais económicas. Por isso, o desenvolvimento de processos de produção de baixo custo exige a especificação de catalisadores heterogéneos eficientes na promoção da reacção de transesterificação, permitindo a imediata separação da glicerina pura, não necessitando de uma purificação dispendiosa deste subproduto. Os xerogéis de carbono surgem então como materiais promissores para aplicação como catalisadores heterogéneos para a produção de biodiesel, devido às suas excelentes propriedades ao nível da sua textura e superfície química. Neste trabalho o principal objectivo foi a preparação de um xerogel de carbono, com o intuito de posteriormente ser aplicado na produção de biodiesel por catálise heterogénea. Amostras de xerogel de carbono foram preparadas pelo método sol-gel e oxidadas em fase líquida sendo posteriormente caracterizados os seus grupos funcionais e a sua área específica. Os resultados obtidos mostram que é possivel obter um xerogel de carbono com área superficial alta, tendo sido atingido um valor máximo para a amostra número dois (803 m2/g). Os resultados atingidos ao nível da preparação do catalisador permitem concluir que as condições de operação influenciam a estrutura final do xerogel de carbono. Quanto à caracterização da química superficial do xerogel, foi possível verificar que a diferença do número de acidez entre as amostras oxidadas e não oxidadas do mesmo lote é alta, o que permite afirmar que a oxidação do material de carbono incrementa a concentração de grupos oxigénio à superfície do xerogel. O valor máximo para o número de acidez foi obtido com a amostra número três (Amostra oxidada - 916 μmol/g, Amostra não oxidada - 207 μmol/g). Apesar de terem sido realizados ensaios para a produção de biodiesel os resultados obtidos foram nulos. A escolha das condições de reacção para a catálise heterogénea com este tipo de material poderá não ter sido a mais indicada, assim como a quantidade e o tipo de grupos funcionais introduzidos no catalisador não terem acidez suficiente para permitir uma catálise efectiva.
Resumo:
Mestrado Engenharia Química. Ramo Tecnologias de Protecção Ambiental