Resumo:
In this work the time resolved thermal lens method is combined with interferometric technique, the thermal relaxation calorimetry, photoluminescence and lifetime measurements to determine the thermo physical properties of Nd(2)O(3) doped sodium zincborate glass as a function of temperature up to the glass transition region. Thermal diffusivity, thermal conductivity, fluorescence quantum efficiency, linear thermal expansion coefficient and thermal coefficient of electronic polarizability were determined. In conclusion, the results showed the ability of thermal lens and interferometric methods to perform measurements very close to the phase transition region. These techniques provide absolute values for the measured physical quantities and are advantageous when low scan rates are required. (c) 2008 Optical Society of America
Resumo:
In this work, the synthesis of Y(2)O(3) stabilized tetragonal zirconia polycrystals (Y-TZP)-alumina (Al(2)O(3)) powder mixture was performed by high-energy ball milling and the sintering behavior of this composite was investigated. In order to understand the phase transformations occurring during ball milling, samples were collected after different milling times, from 1 to 60 h. The milled powders were compacted by cold uniaxial pressing and sintered at 1400 and 1600 degrees C. Both powders and sintered samples were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive spectrometry analysis (EDS) and mechanical properties. Fully dense samples were obtained after sintering at 1600 degrees C, while the samples sintered at 1400 degrees C presented a full density for powder mixtures milled for 30 and 60 h. Fracture toughness and Vickers hardnessvalues of the Y-T-ZP/Al(2)O(3) nanocomposite were improved due to dispersed Al(2)O(3) grains and reduced ZrO(2) grain size. Samples sintered at 1400 degrees C, based on powders milled for 60 h, presented high K(IC) and hardness values near to 8.0 Mpan(1/2) and 15 GPa, respectively (C) 2008 Elsevier B.V. All rights reserved
Resumo:
Silicon carbide ceramics are very interesting materials to engineering applications because of their properties. These ceramics are produced by liquid phase sintering (LPS), where elevated temperature and time are necessary, and generally form volatile products that promote defects and damage their mechanical properties. In this work was studied the infiltration process to produce SiC ceramics, using shorter time and temperature than LPS, thereby reducing the undesirable chemical reactions. SiC powder was pressed at 300 MPa and pre-sintered at 1550 degrees C for 30 min. Unidirectional and spontaneous infiltration of this preform by Al2O3/Y2O3 liquid was done at 1850 degrees C for 5, 10, 30 and 60 min. The kinetics of infiltration was studied, and the infiltration equilibrium happened when the liquid infiltrated 12 mm into perform. The microstructures show grains of the SiC surrounded by infiltrated additives. The hardness and fracture toughness are similar to conventional SiC ceramics obtained by LPS. (c) 2007 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
This paper describes the manufacture of tubular ceramic membranes and the study of their performance in the demulsification of soybean oil/water emulsions. The membranes were made by iso-static pressing method and micro and macro structurally characterized by SEM, porosimetry by mercury intrusion and determination of apparent density and porosity. The microfiltration tests were realized on an experimental workbench, and fluid dynamic parameters, such as transmembrane flux and pressure were used to evaluate the process relative to the oil phase concentration (analysed by TOC measurements) in the permeate. The results showed that the membrane with pores` average diameter of 1.36 mu m achieved higher transmembrane flux than the membrane with pores` average diameter of 0.8 mu m. The volume of open pores (responsible for the permeation) was predominant in the total porosity, which was higher than 50% for all tested membranes. Concerning demulsification, the monolayer membranes were efficacious, as the rejection coefficient was higher than 99%.
Resumo:
This paper describes the manufacture of tubular UF and MF porous and supported ceramic membranes to oil/water emulsions demulsification. For such a purpose, a rigorous control was realized over the distribution and size of pores. Suspensions at 30 vol.% of solids (zirconia or alumina powder and sucrose) and 70 vol.% of liquids (isopropyl alcohol and PVB) were prepared in a jar mill varying the milling time of the sucrose particles, according to the pores size expected. The membranes were prepared by isostatic pressing method and structurally characterized by SEM, porosimetry by mercury intrusion and measurements of weight by immersion. The morphological characterization of the membranes identified the formation of porous zirconia and alumina membranes and supported membranes. The results of porosimetry analysis by mercury intrusion presented an average pore size of 1.8 mu m for the microfiltration porous membranes and for the ultrafiltration supported membranes, pores with average size of 0.01-0.03 mu m in the top-layer and 1.8 mu m in the support. By means of the manufacture method applied, it was possible to produce ultra and microfiltration membranes with high potential to be applied to the separation of oil/water emulsions. (C) 2011 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
Mechanical and tribological properties of a partially crystallized sintered glass-ceramic were compared to two commercial floor tiles: black granite and porcelainized stoneware. Mechanical properties, hardness and elastic modulus were evaluated by instrumented indentation. Friction coefficient and wear characterization were evaluated using a reciprocating ball-on-flat tribometer in two controlled environments: air with relative humidity of 53% and under running water at 23 degrees C. The sintered glass-ceramic and porcelainized stoneware presented similar mechanical and tribological properties. Regarding the mechanical and tribological properties, the results suggest that this glass-ceramic is suitable to be used as industrial tile. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Alumina ceramics with high in-line transmittance at 0.5-1.0 mm-thickness were prepared with different doping additives by sintering at 1850 degrees C in vacuum for 1-8 h. Depending on the additive contents and sintering variables bi-dimensionally large surface grains, caused by surface evaporation of MgO, had grown parallel to the surface with similar to 100 mu m thickness and lateral sizes up to the millimeter range. The abnormal grain-growth process also resulted in the formation of pores entrapped inside the large surface grains within a narrow zone at 10-20 mu m distance from the surface. The fraction of these pores is thickness-invariant. Scattering factors associated to the pores entrapped inside the bi-dimensionally large surface grains, second-phase particles, grain-boundaries, and microstructural surface defects are derived from the results of in-line transmission (at 600 nm) and are used together with microstructural characteristics to explain the light transmittance in these materials. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
Effects of titanium carbide (TiC) addition on structural and magnetic properties of isotropic (Pr,Nd)-Fe-B nanocrystalline magnetic materials have been investigated. In this work, we investigate the effect of TiC addition on a (Pr,Nd)-poor and B-rich composition, as well as on a B-poor and (Nd, Pr)-rich composition. Rapidly solidified (Pr, Nd)-Fe-B alloys were prepared by melt-spinning. The compositions studied were (Pr(1-x)Nd(x))(4)Fe(78)B(18) (x = 0, 0.5, and 1) with addition of 3 at% TiC. Unlike the (Pr(x)Nd(1-x))(9.5)Fe(84.5)B(6) materials that present excellent values for coercive. field and energy product, the (Pr,Nd)-poor and B-rich composition alloys with TiC addition present lower values. Rietveld analysis of X-ray data and Mossbauer spectroscopy revealed that samples are predominantly composed of Fe(3)B and alpha-Fe. For the RE-rich compositions (Pr(x)Nd(1-x))(9.5)Fe(84.5)B(6) (x = 0.1, 0.25, 0.5, 0.75, and 1) with the addition of 3 at% TiC, the highest coercive field and energy product (8.4 kOe and 14.4 MGOe, respectively) were obtained for the composition Pr(9.5)Fe(84.5)B(6). (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
This work introduces the problem of the best choice among M combinations of the shortest paths for dynamic provisioning of lightpaths in all-optical networks. To solve this problem in an optimized way (shortest path and load balance), a new fixed routing algorithm, named Best among the Shortest Routes (BSR), is proposed. The BSR`s performance is compared in terms of blocking probability and network utilization with Dijkstra`s shortest path algorithm and others algorithms proposed in the literature. The evaluated scenarios include several representative topologies for all-optical networking and different wavelength conversion architectures. For all studied scenarios, BSR achieved superior performance. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
We report on the detection of the transport Barkhausen-like noise (TBN) in polycrystalline samples of Bi(1.65)Pb(0.35)Sr(2)Ca(2) Cu(3)O(10+delta) (Bi-2223) which were subjected to different uniaxial compacting pressures. The transport Barkhausen-like noise was measured when the sample was subjected to an ac triangular-shape magnetic field (f similar to 1 Hz) with maximum amplitude B(max) approximate to 5.5 mT, in order to avoid the flux penetration within the superconducting grains. Analysis of the TBN signal, measured for several values of excitation current density, indicated that the applied magnetic field in which the noise signal first appears, B(a)(t(i)), is closely related to the magnetic-flux pinning capability of the material. The combined results are consistent with the existence of three different superconducting levels within the samples: (i) the superconducting grains; (ii) the superconducting clusters; and (iii) the weak-links. We finally argue that TBN measurements constitute a powerful tool for probing features of the intergranular transport properties in polycrystalline samples of high-T(c) superconductors. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Experimental and theoretical studies on the magnetic field dependence of the electrical resistance R(B(a)) and the transport noise (TN) in polycrystalline high-T(c) superconductors subjected to different uniaxial compacting pressures were conducted. X-ray diffraction rocking curves were performed in different surfaces of the samples in order to investigated the degree of texture The results indicated an improvement of the degree of texture with increasing the uniaxial compacting pressure In theoretical simulations of the data, the polycrystalline superconductors were described as a series-parallel array of Josephson devices The intergranular magnetic field is described within the framework of the intragranular flux-trapping model and the distribution of the grain-boundary angles is assumed to follow the Rayleigh statistical function The proposed model describes well the experimental magnetoresistance R(B(a)) data We have found that the behavior of the R(B(a)) curves changes appreciably when different uniaxially compacting pressures are applied to the sample and such a changes are reproduced by the model when different grain-boundary angles distributions are used In addition, changes in the R(B(a)) dependence have their counterparts in the experimental transport noise signals (C) 2009 Elsevier B.V. All rights reserved
Resumo:
P>The aim of this comparative clinical study was to evaluate a novel bioactive glass-ceramic (Biosilicate (R) 1-20 mu m particles) to treat dentine hypersensitivity (DH). Volunteers (n = 120 patients/ 230 teeth) received the following treatments: G1-Sensodyne (R), G2-SensiKill (R), G3-Biosilicate (R) incorporated in a 1% water-free-gel and G4-Biosilicate (R) mixed with distilled water at 1:10 ratio. G1 and G3 were applied at home, daily for 30 days; G2 and G4 were applied once a week by a dentist (four applications). A visual analogue scale (VAS) was employed to evaluate pain for each quadrant in one sensitive tooth at baseline, weekly during treatment and during a 6-month follow-up period. Dentine hypersensitivity values (G1/n = 52), (G2/n = 62), (G3/n = 59) and (G4/n = 59) were analysed with Kruskal-Wallis/Dunn tests. All the products were efficient in reducing DH after 4 weeks. Among the four materials tested, G4 demonstrated the best clinical performance and provided the fastest treatment to reduce DH pain. Distilled water proved to be an adequate vehicle to disperse Biosilicate (R). Low DH scores were maintained during the 6-month follow-up period. The hypothesis that the novel bioactive glass-ceramic may be an efficient treatment for DH was confirmed.
Resumo:
The purposes of this study were to evaluate in vitro the influence of different frequencies of Er:YAG laser on the human dentin caries removal capacity. Thirty fragments obtained from third molars were randomly assigned into three groups (n = 10) according to the laser frequency used: 4, 6, and 10 Hz. The caries lesion (+/-1 mm deep) was induced before the irradiation by S. mutans cultures for 6 weeks. The specimens of all groups were irradiated with 200 mJ of energy in noncontact and focused mode under constant refrigeration (water flow: 2.5 mL/min). Quantitative analysis of the caries removal was performed by DIAGNOdent (TM) and the Axion Vision (TM) software. Qualitative analysis was performed by Scanning electron microscope (SEM) and light microscope (LM). Data were analyzed by ANOVA and Fishers` tests. The DIAGNOdent (TM) revealed that the caries removal was similar with 4 and 6 Hz and was superior with 10 Hz (P < 0.05). The analysis with Axion Vision (TM) software revealed that the caries removal was similar with 6 and 10 Hz and the 4 Hz group promoted the lowest caries removal. Through SEM morphologic analysis, some specimens irradiated with 4 Hz presented, under the demineralized dentin, a disorganized collagenous matrix. The LM images revealed that all frequencies used promoted irregular caries removal, being observed over preparations with 6 and 10 Hz. It can be concluded that the increase of Er:YAG laser frequency provided a higher dentin caries removal without selectivity to the disorganized dentin. Microsc. Res. Tech. 74:281-286, 2011. (C) 2010 Wiley-Liss, Inc.
Resumo:
Site selective luminescence and magnetic circular dichroism experiments on Cr4+-doped yttrium aluminum garnet and yttrium gallium garnet have been made at low temperature. The spectral assignments for these near-IR lasing materials have been made using experimental data and ligand field calculations guided by the known geometry of the lattices. [S0163-1829(99)07003-4].