976 resultados para magnetic properties of nanostructures
Resumo:
DUE TO COPYRIGHT RESTRICTIONS ONLY AVAILABLE FOR CONSULTATION AT ASTON UNIVERSITY LIBRARY SERVICES WITH PRIOR ARRANGEMENT
Resumo:
The synthesis and detailed characterization of a few samples of the compound RbMn[Fe(CN)]·zHO are described. The composition of the materials significantly depends on the applied preparative conditions. Analysis of spectroscopic results (FTIR, Raman, Fe Mössbauer, XPS) and X-ray powder-diffraction data yielded a further assessment of the difference in structural features in terms of the amount of Fe(CN)6 vacancies and the associated number of water molecules. The characteristic individual magnetic behavior, as well as the metal-to-metal charge-transfer capabilities of the various samples, could be related to significant changes within the structures that appear to be associated with the synthetic method used.
Resumo:
A multinuclear Fe-Mn-Cr complex with 4-amino-1,2,4-triazole (NH2trz) and oxalate (ox) ligands has been synthesized successfully. The formula of the [Fe(NH2trz)3][ClO4][MnCr(ox)3].4H2O complex has been obtained based on the metal and C, H, N contents. The presence of water molecules, metal-ligand bonding and bridge ligand in the multinuclear complex has been confirmed by its infrared spectrum. The compound crystallizes in the hexagonal system with cell parameters of a = b = 18.695 Å and c = 57.351 Å. The compound shows a gradual spin crossover for iron(II) in the [Fe(NH2trz)3]2+ with transition temperature (T1/2) of 205 K. The antiferromagnetic interaction between Cr(III) and Mn(II) ions in the [MnCr(ox)3]n n- network is observed from the Weiss constant (θ) of –2.3 K.
Resumo:
The growth and magnetic properties of epitaxial magnetite Fe3O4 on GaAs(100) have been studied by reflection high-energy electron diffraction, x-ray photoelectron spectroscopy, magneto-optical Kerr effect, and x-ray magnetic circular dichroism. The epitaxial Fe3O4 films were synthesized by in situ post growth annealing of ultrathin epitaxial Fe films at 500K in an oxygen partial pressure of 5×10−5mbar. The XMCD measurements show characteristic contributions from different sites of the ferrimagnetic magnetite unit cell, namely, Fetd3+, Feoh2+, and Feoh3+. The epitaxial relationship was found to be Fe3O4(100)⟨011⟩∕∕GaAs(100)⟨010⟩ with the unit cell of Fe3O4 rotated by 45° to match that of GaAs(100) substrate. The films show a uniaxial magnetic anisotropy in a thickness range of about 2.0–6.0nm with the easy axes along the [011] direction of the GaAs(100) substrate.
Resumo:
The structure and spin-crossover magnetic behavior of [FeII16][BF4]2 (1 = isoxazole) and [FeII16][ClO4]2 have been studied. [FeII16][BF4]2 undergoes two reversible spin-crossover transitions at 91 and 192 K, and is the first two-step spin transition to undergo a simultaneous crystallographic phase transition, but does not exhibit thermal hysteresis. The single-crystal structure determinations at 260 [space group P3̄, a = 17.4387(4) Å, c = 7.6847(2) Å] and at 130 K [space group P1̄, a = 17.0901(2) Å, b = 16.7481(2) Å, c = 7.5413(1) Å, α = 90.5309(6)°, β = 91.5231(6)°, γ = 117.8195(8)°] reveal two different iron sites, Fe1 and Fe2, in a 1:2 ratio. The room-temperature magnetic moment of 5.0 μB is consistent with high-spin Fe(II). A plateau in μ(T) having a moment of 3.3 μB centered at 130 K suggests a mixed spin system of some high-spin and some low-spin Fe(II) molecules. On the basis of the Fe−N bond distances at the two temperatures, and the molar fraction of high-spin molecules at the transition plateau, Fe1 and Fe2 can be assigned to the 91 and 192 K transitions, respectively. [FeII16][ClO4]2 [space group P3̄, a = 17.5829(3) Å, c = 7.8043(2) Å, β = 109.820 (3)°, T = 295 K] also possesses Fe1:Fe2 in a 1:2 ratio, and magnetic measurements show a single spin transition at 213 K, indicating that both Fe1 and Fe2 undergo a simultaneous spin transition. [FeII16][ClO4]2 slowly decomposes in solutions containing acetic anhydride to form [FeIII3O(OAc)613][ClO4] [space group I2, a = 10.1547(7) Å, b = 16.5497(11) Å, c = 10.3205(9) Å, β = 109.820 (3)°, T = 200 K]. The isosceles Fe3 unit contains two Fe···Fe distances of 3.2844(1) Å and a third Fe···Fe distance of 3.2857(1) Å. The magnetic data can be fit to a trinuclear model with ℋ = −2J(S1·S2 + S2·S3) − 2J13(S1·S3), where J = −27.1 and J13 = −32.5 cm-1.
Resumo:
Nanocrystalline and bulk samples of “Fe”-doped CuO were prepared by coprecipitation and ceramic methods. Structural and compositional analyses were performed using X-ray diffraction, SEM, and EDAX. Traces of secondary phases such as CuFe2O4, Fe3O4, and α-Fe2O3 having peaks very close to that of the host CuO were identified from the Rietveld profile analysis and the SAED pattern of bulk and nanocrystalline Cu0.98Fe0.02O samples. Vibrating Sample Magnetometer (VSM) measurements show hysteresis at 300 K for all the samples. The ferrimagnetic Neel transition temperature () was found to be around 465°C irrespective of the content of “Fe”, which is close to the value of cubic CuFe2O4. High-pressure X-Ray diffraction studies were performed on 2% “Fe”-doped bulk CuO using synchrotron radiation. From the absence of any strong new peaks at high pressure, it is evident that the secondary phases if present could be less than the level of detection. Cu2O, which is diamagnetic by nature, was also doped with 1% of “Fe” and was found to show paramagnetic behavior in contrast to the “Fe” doped CuO. Hence the possibility of intrinsic magnetization of “Fe”-doped CuO apart from the secondary phases is discussed based on the magnetization and charge state of “Fe” and the host into which it is substituted.
Resumo:
The bulk magnetic mineral record from Lake Ohrid, spanning the past 637 kyr, reflects large-scale shifts in hydrological conditions, and, superimposed, a strong signal of environmental conditions on glacial-interglacial and millennial timescales. A shift in the formation of early diagenetic ferrimagnetic iron sulfides to siderites is observed around 320 ka. This change is probably associated with variable availability of sulfide in the pore water. We propose that sulfate concentrations were significantly higher before ~320 ka, due to either a higher sulfate flux or lower dilution of lake sulfate due to a smaller water volume. Diagenetic iron minerals appear more abundant during glacials, which are generally characterized by higher Fe/Ca ratios in the sediments. While in the lower part of the core the ferrimagnetic sulfide signal overprints the primary detrital magnetic signal, the upper part of the core is dominated by variable proportions of high- to low-coercivity iron oxides. Glacial sediments are characterized by high concentration of high-coercivity magnetic minerals (hematite, goethite), which relate to enhanced erosion of soils that had formed during preceding interglacials. Superimposed on the glacial-interglacial behavior are millennial-scale oscillations in the magnetic mineral composition that parallel variations in summer insolation. Like the processes on glacial-interglacial timescales, low summer insolation and a retreat in vegetation resulted in enhanced erosion of soil material. Our study highlights that rock-magnetic studies, in concert with geochemical and sedimentological investigations, provide a multi-level contribution to environmental reconstructions, since the magnetic properties can mirror both environmental conditions on land and intra-lake processes.
Resumo:
Thèse numérisée par la Direction des bibliothèques de l'Université de Montréal.
Resumo:
Thèse numérisée par la Direction des bibliothèques de l'Université de Montréal.
Resumo:
Foulden Maar is a highly resolved maar lake deposit from the South Island of New Zealand comprising laminated diatomite punctuated by numerous diatomaceous turbidites. Basaltic clasts found in debris flow deposits at the base of the cored sedimentary sequence yielded two new 40Ar/39Ar dates of 24.51±0.24 Ma and 23.38±0.24 Ma (2sigma). The younger date agrees within error with a previously published 40Ar/39Ar date of 23.17±0.19 Ma from a basaltic dyke adjacent to the maar crater. The diatomite is inferred to have been deposited over several tens of thousands of years in the latest Oligocene/earliest Miocene, and may have overlapped with the period of rapid glaciation and subsequent deglaciation of Antarctica known as the Mi-1 event. Sediment magnetic properties and SEM measurements indicate that the magnetic signal is dominated by pseudo-single domain pyrrhotite. The most likely source of detrital pyrrhotite is schist country rock fragments from the inferred tephra ring created by the phreatomagmatic eruption that formed the maar. Variations in magnetic concentration and lamina thickness indicate a decrease in erosional input and increase in diatom productivity throughout the depositional period, suggesting a long-term (tens of thousands of years) climatic change in New Zealand in the latest Oligocene/earliest Miocene.
Resumo:
Hysteresis measurements have been carried out on a suite of ocean-floor basalts with ages ranging from Quaternary to Cretaceous. Approximately linear, yet separate, relationships between coercivity (Bc) and the ratio of saturation remanence/saturation magnetization (Mrs/Ms) are observed for massive doleritic basalts with low-Ti magnetite and for pillow basalts with multi-domain titanomagnetites (with x= 0.6). Even when the MORB has undergone lowtemperature oxidation resulting in titanomaghemite, the parameters are still distinguishable, although offset from the trend for unoxidized multidomain titanomagnetite. The parameters for these iron oxides with different titanium content reveal contrasting trends that can be explained by the different saturation magnetizations of the mineral types. This plot provides a previously underutilized and non-destructive method to detect the presence of low-titanium magnetite in igneous rocks, notably MORB.
Resumo:
No abstract available.
Resumo:
Magnetic nanoparticles (MNPs) are known for the unique properties conferred by their small size and have found wide application in food safety analyses. However, their high surface energy and strong magnetization often lead to aggregation, compromising their functions. In this study, iron oxide magnetic particles (MPs) over the range of nano to micro size were synthesized, from which particles with less aggregation and excellent magnetic properties were obtained. MPs were synthesized via three different hydrothermal procedures, using poly (acrylic acid) (PAA) of different molecular weight (Mw) as the stabilizer. The particle size, morphology, and magnetic properties of the MPs from these synthesis procedures were characterized and compared. Among the three syntheses, one-step hydrothermal synthesis demonstrated the highest yield and most efficient magnetic collection of the resulting PAA-coated magnetic microparticles (PAA-MMPs, >100 nm). Iron oxide content of these PAA-MMPs was around 90%, and the saturation magnetization ranged from 70.3 emu/g to 57.0 emu/g, depending on the Mw of PAA used. In this approach, the particles prepared using PAA with Mw of 100K g/mol exhibited super-paramagnetic behavior with ~65% lower coercivity and remanence compared to others. They were therefore less susceptible to aggregation and remained remarkably water-dispersible even after one-month storage. Three applications involving PAA-MMPs from one-step hydrothermal synthesis were explored: food proteins and enzymes immobilization, antibody conjugation for pathogen capture, and magnetic hydrogel film fabrication. These studies demonstrated their versatile functions as well as their potential applications in the food science area.
Resumo:
Self-assembled monolayers (SAMs) are highly promising materials for molecular engineering of electronic and spintronics devices thanks to their surface functionalization properties. In this direction, alkylphosphonic acids have been used to functionalize the most common ferromagnetic electrode in organic spintronics: La2/3Sr1/3MnO3 (LSMO). However, a study on the influence of SAMs grafting on LSMO electronic and magnetic properties is still missing. In this letter, we probe the influence of alkylphosphonic acids-based SAMs on the electronic and magnetic properties of the LSMO surface using different spectroscopies. We observe by X-ray photoemission and X-ray absorption that the grafting of the molecules on the LSMO surface induces a reduction of the Mn oxidation state. Ultraviolet photoelectron spectroscopy measurements also show that the LSMO work function can be modified by surface dipoles opening the door to both tune the charge and spin injection efficiencies in organic devices such as organic light-emitting diodes.
Resumo:
Este trabalho centra-se na investigação da possibilidade de se conseguir um semicondutor magnético diluído (SMD) baseado em ZnO. Foi levado a cabo um estudo detalhado das propriedades magnéticas e estruturais de estruturas de ZnO, nomeadamente nanofios (NFs), nanocristais (NCs) e filmes finos, dopadas com metais de transição (MTs). Foram usadas várias técnicas experimentais para caracterizar estas estruturas, designadamente difracção de raios-X, microscopia electrónica de varrimento, ressonância magnética, SQUID, e medidas de transporte. Foram incorporados substitucionalmente nos sítios do Zn iões de Mn2+ e Co2+ em ambos os NFs e NCs de ZnO. Revelou-se para ambos os iões dopantes, que a incorporação é heterogénea, uma vez que parte do sinal de ressonância paramagnética electrónica (RPE) vem de iões de MTs em ambientes distorcidos ou enriquecidos com MTs. A partir das intensidades relativas dos espectros de RPE e de modificações da superfície, demonstra-se ainda que os NCs exibem uma estrutura core-shell. Os resultados, evidenciam que, com o aumento da concentração de MTs, a dimensão dos NCs diminui e aumentam as distorções da rede. Finalmente, no caso dos NCs dopados com Mn, obteve-se o resultado singular de que a espessura da shell é da ordem de 0.3 nm e de que existe uma acumulação de Mn na mesma. Com o objectivo de esclarecer o papel dos portadores de carga na medição das interacções ferromagnéticas, foram co-dopados filmes de ZnO com Mn e Al ou com Co e Al. Os filmes dopados com Mn, revelaram-se simplesmente paramagnéticos, com os iões de Mn substitucionais nos sítios do Zn. Por outro lado, os filmes dopados com Co exibem ferromagnetismo fraco não intrínseco, provavelmente devido a decomposição spinodal. Foram ainda efectuados estudos comparativos com filmes de ligas de Zn1-xFexO. Como era de esperar, detectaram-se segundas fases de espinela e de óxido de ferro nestas ligas; todas as amostras exibiam curvas de histerese a 300 K. Estes resultados suportam a hipótese de que as segundas fases são responsáveis pelo comportamento magnético observado em muitos sistemas baseados em ZnO. Não se observou nenhuma evidência de ferromagnetismo mediado por portadores de carga. As experiências mostram que a análise de RPE permite demonstrar directamente se e onde estão incorporados os iões de MTs e evidenciam a importância dos efeitos de superfície para dimensões menores que ~15 nm, para as quais se formam estruturas core-shell. As investigações realizadas no âmbito desta tese demonstram que nenhuma das amostras de ZnO estudadas exibiram propriedades de um SMD intrínseco e que, no futuro, são necessários estudos teóricos e experimentais detalhados das interacções de troca entre os iões de MTs e os átomos do ZnO para determinar a origem das propriedades magnéticas observadas.