915 resultados para in situ synchrotron XRD
Resumo:
Polypropylene/montmorillonite (PP/MMT) nanocomposites were prepared by in-situ polymerization using a MMT/MgCl2/TiCl4-EB Ziegler-Natta catalyst activated by trietbylaluminum (TEA). The enlarged layer spacing of MMT was confirmed by X-ray wide angle diffraction (WAXD), demonstrating that MMT were intercalated by the catalyst components. X-ray photoelectron spectrometry (XPS) analysis proved that TiCl4 was mainly supported on MgCl2 instead of on the surface of MMT The exfoliated structure of MMT layers in the PP matrix of PP/MMT composites was demonstrated by WAXD patterns and transmission electron microscopy (TEM) observation. The higher glass transition temperature and higher storage modulus of the PP/MMT composites in comparison with pure PP were revealed by dynamic mechanical analysis (DMA).
Resumo:
Polyethylene (PE)/montmorillonite (MMT) nanocomposites were prepared by in situ coordination polymerization using a MMT/MgCl2/TiCl4 catalyst activated by AI(Et),. The catalyst was prepared by first diffusing MgCl2 into the swollen MMT layers, followed by loading TiCl4 on the inner/outer layer surfaces of MMT where MgCl2 was already deposited. The intercalation of MMT layers by MgCl2 and TiCl, was demonstrated by the enlarged interlayer spacing determined by WAXD. The nanoscale dispersion of MMT layers in the polyethylene matrix was characterized by WAXD and TEM. As a consequence, the crystallinity of the nanocomposite decreased sharply, whereas the tensile strength was significantly improved compared to that of virgin polyethylene of comparable molecular weight. The confinement of the nanodispersed MMT layers to molecular chain and the strong interaction between the nanoscale MMT layers and the resin matrix were thought to account for the decrease of crystallinity and the remarkable enhancement of strength.
Resumo:
Blends of linear low-density polyethylene (LLDPE) with polystyrene (PS) and blends of LLDPE with high-impact polystyrene (HIPS) were prepared through a reactive extrusion method. For increased compatibility of the two blending components, a Lewis acid catalyst, aluminum chloride (AlCl3), was adopted to initiate the Friedel-Crafts alkylation reaction between the blending components. Spectra data from Raman spectra of the LLDPE/PS/AlCl3 blends extracted with tetrahydrofuran verified that LLDPE segments were grafted to the para position of the benzene rings of PS, and this confirmed the graft structure of the Friedel-Crafts reaction between the polyolefin and PS. Because the in situ generated LLDPE-g-PS and LLDPE-g-HIPS copolymers acted as compatibilizers in the relative blending systems, the mechanical properties of the LLDPE/PS and LLDPE/HIPS blending systems were greatly improved. For example, after compatibilization, the Izod impact strength of an LLDPE/PS blend (80/20 w/w) was increased from 88.5 to 401.6 J/m, and its elongation at break increased from 370 to 790%. For an LLDPE/HIPS (60/40 w/w) blend, its Charpy impact strength was increased from 284.2 to 495.8 kJ/m(2). Scanning electron microscopy micrographs showed that the size of the domains decreased from 4-5 to less than 1 mum, depending on the content of added AlCl3.
Resumo:
Size-controlled Ag3PW12O40 nanoparticles have been synthesized in situ in polyelectrolyte multilayer thin films via layer-by-layer self-assembly.
Resumo:
In situ synthesis of terbium carboxyl complexes in an organic-inorganic hybrid matrix by a sol-gel process has been proposed. The formation of terbium carboxyl complexes in the hybrid matrix is confirmed by the luminescence spectra and IR spectra. It is observed that the location at the amino group in aminobenzoic acid has a large effect on the luminescence properties and lifetimes. Furthermore, the emission intensity decreases with increasing temperature.
Resumo:
Nanostructure and morphology and their development of poly(di-n-hexylsilane) (PDHS) and poly(di-n-butylsilane) (PDBS) during the crystal-mesophase transition are investigated using small angle X-ray scattering (SAXS), wide angle X-ray diffraction and hot-stage atomic force microscopy. At room temperature, PDHS consists of stacks of lamellae separated by mesophase layers, which can be well accounted using an ideal two-phase model. During the crystal-mesophase transition, obvious morphological changes are observed due to the marked changes in main chain conformation and intermolecular distances between crystalline phase and mesophase. In contrast to PDHS, the lamellae in PDBS barely show anisotropy in dimensions at room temperature. The nonperiodic structure and rather small electronic density fluctuation in PDBS lead to the much weak SAXS. The nonperiodic structure is preserved during the crystal-mesophase transition because of the similarity of main chain conformation and intermolecular distances between crystalline phase and mesophase.
Resumo:
Secondary and tertiary or quaternary structural changes in hemoglobin (HB) during an electroreduction process were studied by in situ circular dichroism (CD) spectroelectrochemistry with a long optical path thin-layer cell. By means of singular value decomposition least-squares analysis, CD spectra in the far-UV region give two similar a components with different CD intensity, indicating slight denaturation in the secondary structures due to the electric field effect. CD spectra in the Soret band show a R --> T transition of two quaternary structural components induced by electroreduction of the heme, which changes the redox states of the center ion from Fe3+ to Fe2+ and the coordination number from 6 to 5. The double logarithmic analysis shows that electroreduction of hemoglobin follows a chemical reaction with R --> T transition. Some parameters in the electrochemical process were obtained: formal potential, E-0t = -0.167 V; electrochemical kinetic overpotential, DeltaE(0) = -0.32 V; standard electrochemical reaction rate constant, k(0) = 1.79 x 10(-5) cm s(-1); product of electron transfer coefficient and electron number, alphan=0.14; and the equilibrium constant of R --> T transition, K-c = 9.0.
Resumo:
Transparent poly(ethyl acrylate) (PEA)/bentonite nanocomposites containing intercalated-exfoliated combinatory structures of clay were synthesized by in situ emulsion polymerizations in aqueous dispersions containing bentonite. The samples for characterization were prepared through direct-forming films of the resulting emulsions without coagulation and separation. An examination with X-ray diffraction and transmission electron microscopy showed that intercalated and exfoliated structures of clay coexisted in the PEA/bentonite nanocomposites. The measurements of mechanical properties showed that PEA properties were greatly improved, with the tensile strength and modulus increasing from 0.65 and 0.24 to 11.16 and 88.41 MPa, respectively. Dynamic mechanical analysis revealed a very marked improvement of the storage modulus above the glass-transition temperature. In addition, because of the uniform dispersion of silicate layers in the PEA matrix, the barrier properties of the materials were dramatically improved. The permeability coefficient of water vapor decreased from 30.8 x 10(-6) to 8.3 x 10(-6) g cm/cm(2)s cmHg. (C) 2002 Wiley Periodicals, Inc.
Resumo:
The combination of electrochemistry with surface plasmon resonance (SPR) has been used to characterize the growth of polyaniline (PAn) on a gold electrode surface during potential cycling. Potential-modulated SPR characteristics of the PAn film were also revealed. The potential switch between the oxidized and reduced states of PAn can lead to a large change of SPR response due to the variation in the imaginary part of the dielectric constant of PAn film resulting from the transition of the film in conductivity. The redox transition of the PAn film during potential cycling is very profitable to the SPR measurements. Two modes of SPR measurement, SPR angular scan (R-theta) and the time evolution of the reflectivity change at a fixed angle (R-t), were displayed to study the growth process of the PAn film. The angle shift of the resonance minimum recorded at each cathodic limit of cyclic potential scanning allows for the unambiguous measurement of the film growth. During cyclic potential scanning, the R-t curve was repeatedly modulated with the direction of the potential ramp as a result of the redox switch of the PAn film, and the amplitude of potential-modulated reflectivity change was well correlated with the cyclic number. The time differential of the R-t curve permits continuous monitoring of the film growth process. These results illustrate that the combined technique is suitable for studying the electropolymerization process of a conducting polymer.
Resumo:
Electrochemically induced three conformational transitions of calf thymus DNA from B-10.4 to Z(10.2)-DNA and from B-10.2 to B-10.4 and to C-DNA in 10 mM phosphate buffer solution (pH 7.21) at glassy carbon electrode are found and studied by in situ circular dichroism (CD) thin layer spectroelectrochemistry with singular value decomposition least square (SVDLS) analysis. It indicates that the so-called B-10.2 form and the C-form of DNA may be composed of B-10.4 and left-A DNA and of B-10.4 and right-A DNA, respectively. The irreversible electrochemical reduction of adenine and cytosine groups in the DNA molecule is studied by UV-Vis spectroelectrochemistry. Some electrochemical parameters alphan = 0.17, E-0' = -0.70 V (vs. Ag/AgCl), and the standard heterogeneous electron transfer rate constant, k(0) = 1.8 x 10(-5) cm s(-1) are obtained by double logarithmic analysis and non-linear regression. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Terbium complexes with benzoic acid and its derivatives o-hydroxybenzoic acid and p-hydroxybenzoic acid were in situ synthesized in sol-gel derived silica matrix via a two-step sol-gel process. The formation process of the complex was characterized by fluorescence spectra, absorption spectra and IR spectra. The gels that contain in situ synthesized complexes exhibit the characteristic emission bands of terbium ion. The fluorescence lifetimes of Tb3+ in the silica gels are longer than those in the pure complexes and in the solutions that contain the corresponding complexes. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
A new kind of inorganic self-assembled monolayer (SAM) was prepared by spontaneous adsorption of polyoxometalate anion, AsMo11VO404-, onto a gold surface from acidic aqueous solution. The adsorption process, structure, and electrochemical properties of the AsMo11VO404- SAM were investigated by quartz crystal microbalance (QCM), electrochemistry, and scanning tunneling microscopy (STM). The QCM data suggested that the self-assembling process could be described in terms of the Langmuir adsorption model, providing the value of the free energy of adsorption at -20 KJ mol(-1). The maximum surface coverage of the AsMo11VO404- SAM on gold surface was determined from the QCM data to be 1.7 x 10(-10) mol cm(-2), corresponding to a close-packed monolayer of AsMo11VO404- anion. The analysis of the voltammograms of the AsMo11VO404- SAM on gold electrode showed three pairs of reversible peaks with an equal surface coverage of 1.78 x 10(-10) mol cm(-2) for each of the peaks, and the value was agreed well with the QCM data. In-situ STM image demonstrated that the AsMo11VO404- SAM was very uniform and no aggregates or multilayer could be observed. Furthermore, the high-resolution STM images revealed that the AsMo11VO404- SAM on Au(lll) surface was composed of square unit cells with a lattice space of 10-11 Angstrom at +0.7 V (vs Ag\AgCl). The value was quite close to the diameter of AsMo11VO404- anion obtained from X-ray crystallographic study. The surface coverage of the AsMo11VO404- SAM on gold electrode estimated from the STM image was around 1.8 x 10(-10) mol cm(-2), which was consistent with the QCM and electrochemical results.
Resumo:
Communication: Nanostructural hybrid organic-inorganic lanthanide complex films were prepared in situ by use of a novel sol-gel precursor containing pendant triethoxy-silyl and carboxyl groups (see Figure). The resulting transparent and crack-free films gave rise to strong red or green emission, even at low lanthanide ion concentration. Phase separation and lanthanide ion aggregation were controlled at the nanoscale.
Resumo:
alpha Form Nylon 11 films were found to exist a non-linear transformation at 70 degrees C during the heating process using in situ WAXD. The alpha Form disappeared but delta Form appeared when the temperature was higher 70 degrees C.