910 resultados para Polyethylene- Starch Blends


Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel approach to the preparation of polyethylene (PE) nanocomposites, with montmorillonite/silica hybrid (MT-Si) supported catalyst, was developed. MT-Si was prepared by depositing silica nanoparticles between galleries of the MT. A common zirconocene catalyst [bis(cyclopentadienyl)zirconium dichloride/methylaluminoxane] was fixed on the MT-Si surface by a simple method. After ethylene polymerization, two classes of nanofillers (clay layers and silica nanoparticles) were dispersed concurrently in the PE matrix and PE/clay-silica nanocomposites were obtained. Exfoliation of the clay layers and dispersion of the silica nanoparticles were examined with transmission electron microscopy. Physical properties of the nanocomposites were characterized by tensile tests, dynamic mechanical analysis, and DSC. The nanocomposites with a low nanofiller loading (<10 wt %) exhibited good mechanical properties. The nanocomposite powder produced with the supported catalyst had a granular morphology and a high bulk density, typical of a heterogeneous catalyst system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simple and inexpensive method for forming a low-density polyethylene (LDPE) superhydrophobic surface by controlling the crystallization behavior of LDPE by adjusting the crystallization time and nucleation rate has been proposed. The resulting porous surface, with hierarchical micro- and nanostructures on the beautiful floral designs, has a water contact angle of 173.0degrees +/- 2.5degrees.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of poly(ether-sulfone) (PES) and poly(phenylene sulfide) (PPS) with various compositions were prepared using an internal mixer at 290degreesC and 50 rpm for 10 min. The thermal and dynamic mechanical properties of PES/PPS blends have been investigated by means of DSC and DMA. The blends showed two glass transition temperatures corresponding to PPS-rich and PES-rich phases. Both of them decreased obviously for the blends with PES matrix. On the other hand, T-g of PPS and PES phase decreased a little when PPS is the continuous phase. In the blends quenched from molten state the cold crystallization temperature of PPS was detected in the blends of PES/PPS with mass ratio 50/50 and 60/40. The melting point, crystallization temperature and the crystallinity of blended PPS were nearly unaffected when the mass ratio of PES was less than 60%, however, when the amount of PES is over 60% in the blends, the crystallization of PPS chains was hindered. The thermal and the dynamic mechanical properties of the PPS/PES blends were mainly controlled by the continued phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It was theoretically pointed out that the product of the yield stress and yield strain of matrix polymer that determined the brittle-ductile transition (BDT) of particle toughened polymers. For given particle and test condition, the higher the product of the yield stress and the yield strain of the matrix polymer, the smaller the critical interparticle distance (IDc) of the blends was. This was why the IDc (0.15 mum) of the polypropylene (PP)/rubber blends was smaller than that (0.30 mum) of the nylon 66/rubber blends, and the IDc of the nylon 66/rubber blends was smaller than that (0.60 mum) of the high density polyethylene (HDPE)/rubber blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Monte Carlo simulation was used to study the graft of maleic anhydride (MAH) onto linear polyethylene (PE-g-MAH) initiated by dicumyl peroxide (DCP). Simulation results revealed that major MAH monomers attached onto PE chains as branched graft at higher MAH content. However, at extremely low MAH content, the fraction of bridged graft was very close to that of branched graft. This conclusion was somewhat different from the conventional viewpoint, namely, the fraction of bridged graft was always much lower than that of branched graft under any condition. Moreover, the results indicated that the grafting degree increased almost linearly to MAH and DCP concentrations. On the other hand, it was found that the amount of grafted MAH dropped sharply with increasing the length of grafted MAH, indicating that MAH monomers were mainly attached onto the PE chain as single MAH groups or very short oligomers. With respect to the crosslink of PE, the results showed that the fraction of PE-(MAH)(n)-PE crosslink structure increased continuously, and hence the fraction of PE-PE crosslink decreased with increasing MAH concentration.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To study the brittle-ductile transition (BDT) of polypropylene (PP)/ethylene-propylene-diene monomer (EPDM) blends induced by size, temperature, and time, the toughness of the PP/EPDM blends was investigated over wide ranges of EPDM content, temperature, and strain rate. The toughness of the blends was determined from the tensile fracture energy of the side-edge notched samples. The concept of interparticle distance (ID) was introduced into this study to probe the size effect on the BDT of PP/EPDM blends, whereas the effect of time corresponded to that of strain rate. The BDT induced by size, temperature, and time was observed in the fracture energy versus ID, temperature, and strain rate. The critical BDT temperatures for various EPDM contents at different initial strain rates were obtained from these transitions. The critical interparticle distance (IDc) increased nonlinearly with increasing temperature, and when the initial strain rate was lower, the IDc was larger. Moreover, the variation of the reciprocal of the initial strain rate with the reciprocal of temperature followed different straight lines for various EPDM contents. These straight lines were with the same slope.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two series of tensile tests with constant crosshead speeds (ranging from 5 to 200 mm/min) and tensile relaxation tests (at strains from 0.03 to 0.09) were performed on low-density polyethylene in the subyield region of deformations at room temperature. Mechanical tests were carried out on nonannealed specimens and on samples annealed for 24 h at the temperatures T = 50, 60, 70, 80, and 100 degreesC. Constitutive equations were derived for the time-dependent response of semicrystalline polymers at isothermal deformations with small strains. A polymer is treated as an equivalent heterogeneous network of chains bridged by temporary junctions (entanglements, physical crosslinks, and lamellar blocks). The network is thought of as an ensemble of mesoregions linked with each other. The viscoelastic behavior of a polymer is modeled as a thermally induced rearrangement of strands (separation of active strands from temporary junctions and merging of dangling strands with the network). The viscoplastic response reflects sliding of junctions in the network with respect to their reference positions driven by macrostrains. Stress-strain relations involve five material constants that were found by fitting the observations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three series of tensile tests with constant cross-head speeds (ranging from 5 to 200 mm/min), tensile relaxation tests (at strains from 0.03 to 0.09) and tensile creep tests (at stresses from 2.0 to 6.0 MPa) are performed on low-density polyethylene at room temperature. Constitutive equations are derived for the time-dependent response of semicrystalline polymers at isothermal deformation with small strains. A polymer is treated as an equivalent heterogeneous network of chains bridged by temporary junctions (entanglements, physical cross-links and lamellar blocks). The network is thought of as an ensemble of meso-regions linked with each other. The viscoelastic behavior of a polymer is modelled as thermally-induced rearrangement of strands (separation of active strands from temporary junctions and merging of dangling strands with the network). The viscoplastic response reflects mutual displacement of meso-domains driven by macro-strains. Stress-strain relations for uniaxial deformation are developed by using the laws of thermodynamics. The governing equations involve five material constants that are found by fitting the observations. Fair agreement is demonstrated between the experimental data and the results of numerical simulation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Single-walled carbon nanotubes (SWNTs) were modified with polyethylene (PE) prepared by in situ Ziegler-Natta polymerization. Because of the catalyst pre-treated on the surface of the SWNTs, the ethylene was expected to polymerize there. Scanning electron microscopy images and solubility measurements showed that the surface of the SWNTs was covered with a PE layer, and a crosslink may have formed between the SWNTs and PE. When the SWNTs covered with a PE layer were mixed with commercialized PE by melt blending, the resulting composite had better mechanical properties than the composite from the SWNTs without a PE layer. The yield strength, the tensile strength and modulus, the strain at break, and the fracture energy of the modified-SWNT/PE composites were improved by 25, 15.2, 25.4, 21, and 38% in comparison with those of the raw-SWNT/PE composites.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The partitioning behavior of four amino acids, cysteine, phenylalanine, methionine, and lysine in 15 aqueous two-phase systems (ATPSs) with different polyethylene glycol (PEG) molecular weights and phosphate buffers has been studied in the present paper. The phase diagrams of the systems are investigated together with the effect of the PEG molecular weight and pH of the phosphate solutions. The composition of these systems and some parameters such as density and refractive index are determined. The influences of salts in ATPSs, side chain structure of the amino acids, pH of ATPSs, and the PEG molecular weight on the distribution ratios of the amino acids have been studied. This work is useful for the purification of amino acids and the separation of some proteins whose main surface exposed amino acid residues are these four amino acids, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Viscosities of aqueous solutions of five polyethylene oxide (PEO) samples with molar masses from 1.5 x 10(5) to 1.0 x 10(6) were carefully measured in a polytetrafluoroethylene (PTFE) capillary Ubbelohde viscometer in the concentration range from dilute down to extremely dilute concentration regions and compared with those of the same sample obtained from a glass capillary viscometer. At the same time, viscosities of aqueous solutions of three PEG samples in glass and paraffin-coated capillary viscosity were measured. The wall effects occurred in viscosity measurements for PEO and PEG aqueous solutions in different capillary viscometers were theoretically analyzed and discussed. It was found that different interfacial behaviors occurred in both hydrophobic and hydrophilic capillary viscometers respectively and the interfacial behaviors also exhibit molar mass dependence.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Binary CNBR/PP-g-GMA and ternary CNBR/PP/PP-g-GMA thermoplastic elastomers were prepared by reactive blending carboxy nitrile rubber (CNBR) powder with nanometer dimension and polypropylene functionalized with glycidyl methacrylate (PP-g-GMA). Morphology observation by using an atomic force microscope (AFM) and TEM revealed that the size of CNBR dispersed phase in CNBR/PP-g-GMA binary blends was much smaller than that of the corresponding CNBR/PP binary blends. Thermal behavior of CNBR/PP-g-GMA and CNBR/PP blends was studied by DSC. Comparing with the plain PP-g-GMA, T, of PP-g-GMA in CNBR/PP-g-GMA blends increased about 10degreesC. Both thermodynamic and kinetic effects would influence the crystallization behavior of PP-g-GMA in CNBR/PP-g-GMA blends. At a fixed content of CNBR, the apparent viscosity of the blending system increased with increasing the content of PP-g-GMA. FTIR spectrum verified that the improvement of miscibility of CNBR and PP-g-GMA was originated from the reaction between carboxy end groups of CNBR and epoxy groups of GMA grafted onto PP molecular chains. Comparing with CNBR/PP blends, the tensile strength, stress at 100% strain, and elongation at break of CNBR/PP-g-GMA blends were greatly improved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have followed the morphological evolution and crystallization process of spherical micelles formed by the mixture of polystyrene-b-poly(acrylic acid) (PS-b-PAA) and polystyrene-b-poly(2-vinylpyridine)b-poly(ethylene oxide) (PS-b-P2VP-b-PEO) (the core of the spherical micelles was made of P2VP and PAA blocks through hydrogen bonding in neutral solvent N,N-dimethylformamide, DMF) via DMF vapor treatment. Different phenomena, such as rupture of the film, formation of cylinder aggregates and regular square lamellae, were observed when the micelle film was treated in DMF for different times. At the early stage of annealing in DMF vapor, the micelle film became unstable and ruptured. Cylinder aggregates, within which the PEO blocks achieved the association and primary chain folding, formed as the mesophases before the nucleation of the PEO single crystals at this stage. Further treatment in DMF vapor resulted in the nucleation of the PEO blocks at the corners of quasi-square lamellae. Then a quite regular "sandwich" lamellar structure, constructed by a PEO single-crystal layer covered by two tethered layers of other amorphous blocks on the top and bottom crystal basal surfaces, formed when the film of micelles was annealed in DMF vapor for sufficient times.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High-density polyethylene with shish-kebab structure, prepared by a melt extrusion drawing, was employed to investigate the effect of the well-defined lamellar orientation on the deformation characteristics under uniaxial tensile deformation along the drawing direction. This was done by investigating the true stress-true strain dependencies at different strain rates, recovery properties, and stress relaxation measurements. Measurements were complemented by recording in-situ wide-angle X-ray scattering patterns during the deformation process. The oriented samples showed not only a higher modulus, but different from analogous isotropic samples, a homogeneous deformation without necking. The true strain associated with the onset of fibrillation was determined. Because of the preorientation, it is shifted to 0.3, which is below the value 0.6 of the isotropic counterpart. The main finding is a strong enhancement of the Viscous force, as was revealed by stress relaxation experiments; the viscous force takes up 70% of the total stress. The presence of shish-kebabs, i.e., interconnected lamellae in a stack, seems to be responsible for the high viscous force in the oriented samples. The absence of necking has to be ascribed to the high viscous force.