The effect of different beverages on acrylic resin denture teeth color degradation is evaluated. Ten acrylic resin denture teeth brands were evaluated: Art Plus (AP), Biolux (BX), Biotone IPN (BI), Magister (MG), Mondial 6 (MD), Premium 6 (PR), SR Vivodent PE (SR), Trilux (TR), Trubyte Biotone (TB), and Vipi Dent Plus (VP). Teeth were immersed in staining solutions (coffee, cola, and orange juice) or artificial saliva (control) (n = 6) for 1, 7, 15, or 30 days. Specimen colors were evaluated spectrophotometrically based on the Commission Internationale d'Eclairage L*a*b* system. Color differences (Delta E) were calculated between the baseline and post-staining results. Data were evaluated by analysis of variance and Tukey test (alpha = 0.05). BI (1.82 +/- 0.95) and TR (1.78 +/- 0.72) teeth exhibited the greatest Delta E values, while BX (0.88 +/- 0.43) and MD (1.09 +/- 0.44) teeth were the lowest, regardless of solution and measurement period, and were different from BI and TR teeth (P < 0.05). Cola and coffee promoted higher denture teeth color alterations than orange juice and saliva (P < 0.05). Saliva generated the lowest denture teeth color alterations. Greater immersion times caused higher denture teeth color changes. The lifespan of removable dentures and the aesthetic satisfaction of several edentulous patients may be increased with the use of stain-resistant artificial denture teeth. (C) The Authors.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the influence of zirconia surface treatments on low-temperature degradation (LTD). Disc-shaped specimens were subjected to one of four surface treatments, denoted as C (controlno surface treatment), Si (air abrasion with 30 mu m silica-modified alumina particles), Al (air abrasion with 30 mu m alumina particles), and Gr (grinding with 120 grit diamond discs). Half of the samples were submitted to autoclave treatment for 12 h (127 degrees C, 1.5 bar). Samples were characterized by x-ray diffraction and profilometer analysis and were subjected to biaxial flexural strength test. All of the groups exhibited an increase in the amount of monoclinic phase (m-phase) after LTD. The tm transformation was remarkable for the specimens from the C group, which also exhibited a significant increase in strength. The Gr group also exhibited an increase in strength but lower initial roughness, which probably suppressed LTD on the zirconia surface. The specimens subjected to air abrasion exhibited higher initial amounts of m-phase and a small increase in m-phase after LTD; the strength was not affected in these groups. The effects of LTD were different with each surface treatment applied. Apparently, LTD may be suppressed by smoother surfaces or the presence of an initial amount of m-phase on zirconia surface. (c) 2013 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 101B: 1387-1392, 2013.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The food dye tartrazine (CI 19140) was exposed to UV irradiation from an artificial source, a mercury vapor lamp, and a natural one, sunlight. It was observed that conditions such as energy dose, irradiation time, pH and initial dye concentration affected its discoloration. There was 100% of color removal, after 30 min of irradiation, when a dye solution 1 x 10(-5) mol L-1 was submitted to an energy dose of 37.8 J cm(-2). Liquid Chromatography coupled to Diode Array Detection and Mass Spectrometry confirmed the cleavage of the chromophore group and the formation of five by-products at low concentration. Although by-products were formed, the Salmonella/microsome mutagenicity assay performed for both, the dye solution at a dose of 5.34 mg/plate and the solutions obtained after exposure to UV irradiation, did not present mutagenic activity for TA98 and TA100 with and without S9. (C) 2014 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The zero-valent iron (ZVI) mediated degradation of the antibiotic ciprofloxacin (CIP) was studied under oxic condition. Operational parameters such as ZVI concentration and initial pH value were evaluated. Increase of the ZVI concentration from 1 to 5 g L−1 resulted in a sharp increase of the observed pseudo-first order rate constant of CIP degradation, reaching a plateau at around 10 g L−1. The contribution of adsorption to the overall removal of CIP and dissolved organic carbon (DOC) was evaluated after a procedure of acidification to pH 2.5 with sulfuric acid and sonication for 2 min. Adsorption increased as pH increased, while degradation decreased, showing that adsorption is not important for degradation. Contribution of adsorption was much more important for DOC removal than for CIP. Degradation of CIP resulted in partial defluorination since the fluoride measured corresponded to 34% of the theoretical value after 120 min of reaction. Analysis by liquid chromatography coupled to mass spectrometry showed the presence of products of hydroxylation on both piperazine and quinolonic rings generating fluorinated and defluorinated compounds as well as a product of the piperazine ring cleavage.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The synthetic intermaxillary elastic emerged as an alternative for clinical use in patients with latex sensitivity. However, there are disagreements about this elastic protocol use according to the force degradation. The aim of this study was to evaluate, in vitro, the forces generated by latex and synthetic elastics over time. Material and methods: Sample size of 840 elastics were used (420 latex and 420 synthetic), delivering medium strength (Dental Morelli®) with internal diameter of 1/8", 3/16", 1/4" and 5/16". The elastics were randomly divided into 7 groups according to the time of the force measuring and immersed into distilled water at 37°C. To measure the force in each group, the elastics were stretched in six progressive increases of 100% of its internal diameter with the aid of a testing machine Emic and measured up to 72 hours. Data were analyzed with SPSS 16.0, using one-way analysis of variance (ANOVA). Results: Immediate force level of synthetic elastics was statistically higher than latex elastics in all strains, for the same size. However, the latex elastics mean forceslightly decreased over time, while the synthetic elastics presented an abrupt decrease. Conclusion: In view of these findings, Sudanese homemade alcoholic beverages cause oral epithelial atypical changes, which lead to oral precancerous and cancerous lesions. OEFC is a useful procedure for detection and assessment of oral ET.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Introduction and Objective: The synthetic intermaxillary elastic emerged as an alternative for clinical use in patients with latex sensitivity. However, there are disagreements about this elastic protocol use according to the force degradation. The aim of this study was to evaluate, in vitro, the forces generated by latex and synthetic elastics over time. Material and methods: Sample size of 840 elastics were used (420 latex and 420 synthetic), delivering medium strength (Dental Morelli®) with internal diameter of 1/8”, 3/16”, 1/4” and 5/16”. The elastics were randomly divided into 7 groups according to the time of the force measuring and immersed into distilled water at 37°C. To measure the force in each group, the elastics were stretched in six progressive increases of 100% of its internal diameter with the aid of a testing machine Emic and measured up to 72 hours. Data were analyzed with SPSS 16.0, using one-way analysis of variance (ANOVA). Results: Immediate force level of synthetic elastics was statistically higher than latex elastics in all strains, for the same size. However, the latex elastics mean force slightly decreased over time, while the synthetic elastics presented an abrupt decrease. Conclusion: The synthetic elastic presented severe force degradation, jeopardizing the cost-benefit ratio, which indicates a higher replacement frequency. The latex elastic showed better mechanical performance in comparison to synthetic ones.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: To analyze whether immersion in sodium fluoride (NaF) solutions and/or common acidic beverages (test solutions) would affect the surface roughness or topography of lithium disilicate ceramic. Methods: 220 ceramic discs were divided into four groups, each of which was subdivided into five subgroups (n = 11). Control group discs were immersed in one of four test beverages for 4 hours daily or in artificial saliva for 21 days. Discs in the experimental groups were continuously immersed in 0.05% NaF, 0.2% NaF, or 1.23% acidulated phosphate fluoride (APF) gel for 12, 73, and 48 hours, respectively, followed by immersion in one of the four test beverages or artificial saliva. Vickers microhardness, surface roughness, scanning electron microscopy (SEM) associated with energy dispersive spectroscopy, and atomic force microscopy (AFM) assessments were made. Data were analyzed by nested analysis of variance (ANOVA) and Tukey's test (alpha = 0.05). Results: Immersion in the test solutions diminished the microhardness and increased the surface roughness of the discs. The test beverages promoted a significant reduction in the Vickers microhardness in the 0.05% and 0.2% NaF groups. The highest surface roughness results were observed in the 0.2% NaF and 1.23% APF groups, with similar findings by SEM and AFM. Acidic beverages affected the surface topography of lithium disilicate ceramic. Fluoride treatments may render the ceramic surface more susceptible to the chelating effect of acidic solutions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Latex collected from natural rubber trees forming membranes can be used as biomaterials in several fields being the temperature a key parameter. Thermogravimetry (TG) coupled to Fourier transform infrared spectroscopy (FTIR) is a useful technique to investigate the thermal degradation of both latex and cast films (membranes), wich were obtained from Hevea brasiliensis (RRIM 600 clone) and used without stabilization. The membranes were prepared by casting the latex onto a glass substrate at 65 degrees C for 6 h. The thermal degradation was followed by FTIR spectra acquisition along the process, allowing the identification of the gaseous components evolved upon the thermal treatment. According to TG measurements, the main processes of thermal degradation of the latex and membranes occur at three temperature intervals for both.