Resumo:
The influence of each of the six different types of morphological imperfection - waviness, non-uniform cell wall thickness, cell-size variations, fractured cell walls, cell-wall misalignments, and missing cells - on the yielding of 2D cellular solids has been studied systematically for biaxial loading. Emphasis is placed on quantifying the knock-down effect of these defects on the hydrostatic yield strength and upon understanding the associated deformation mechanisms. The simulations in the present study indicate that the high hydrostatic strength, characteristic of ideal honeycombs, is reduced to a level comparable with the deviatoric strength by several types of defect. The common source of this large knock-down is a switch in deformation mode from cell wall stretching to cell wall bending under hydrostatic loading. Fractured cell edges produce the largest knock-down effect on the yield strength of 2D foams, followed in order by missing cells, wavy cell edges, cell edge misalignments, Γ Voronoi cells, δ Voronoi cells, and non-uniform wall thickness. A simple elliptical yield function with two adjustable material parameters successfully fits the numerically predicted yield surfaces for the imperfect 2D foams, and shows potential as a phenomenological constitutive law to guide the design of structural components made from metallic foams.
Resumo:
A preliminary study is presented of the relationship between the microstructural aspects of failure and the fracture energy G//1//C for cracking parallel to the fibres in long-fibre/thermoplastic matrix composites. Fracture energies are measured by a new technique, and fracture surfaces generated by the test are examined by scanning electron microscopy.
Resumo:
The slurry erosion-corrosion behaviour of aluminium in aqueous silica slurries containing 0.5 M NaCl, acetic acid and 0.1 M Na2CO3 at open circuit has been investigated using a modified slurry erosion rig. The erosion rates of aluminium in the NaCl and acetic acid slurries were much higher than those in an aqueous slurry without electrolyte additives even though the pure corrosion component was very small. Eroded specimens were examined by scanning electron and optical microscopy. In pure aqueous slurry erosion, the basic mechanism leading to mass loss was the ductile fracture of flakes formed on the eroded surface. In corrosive slurries, however, the mass loss was enhanced by cracking of the flakes induced by stress and corrosion. © 1995.
Resumo:
A preliminary study is presented of the relationship between the microstructural aspects of failure and the fracture energy G//l//C for cracking parallel to the fibres in long-fibre/thermoplastic matrix composites. Fracture energies are measured by a new technique, and fracture surfaces generated by the test are examined by scanning electron microscopy.
Resumo:
The magnetic properties of melt-processed YBa2Cu3O7-δ thick films have been measured and correlated with features in the microstructure at 4.2 and 77 K for film thicknesses between 50 and 140 μm. A qualitative model for the volume magnetization of the films at 4.2 K is proposed in terms of the individual contributions from intra H-S grain, inter H-S grain and granular Jc components.
Resumo:
This paper studies the surface melting in the atmosphere by YAG laser-guided micro-arc discharge. In three kinds of surface conditions (free, oiled, and polyethylene covered), we try to control the diameter and the power density of discharge pit. It is found that the power density of 3 x 10(6) W/cm(2) of discharge pit on the oiled surface is moderate to form the melted layer thicker than that of the others, adapting to strengthen the surface of material, and the power density of 1.07 x 10(7) W/cm(2) of discharge pit on the polyethylene-covered surface is highest to form the deepest discharge pit among them, adapting to remove the material.
Resumo:
This work is an experimental study of unidirectional bamboo-epoxy laminates of varying laminae number, in which tensile, compressive, flexural and interlaminar shear properties are evaluated. Further, the disposition of bamboo fibre, the parenchymatous tissue, and the resin matrix under different loading conditions are examined. Our results show that the specific strength and specific modulus of bamboo-epoxy laminates are adequate, the former being 3 to 4 times that of mild steel. Its mechanical properties are generally comparable to those of ordinary glass-fibre composites. The fracture behaviour of bamboo-epoxy under different loading conditions were observed using both acoustic emission techniques and scanning electron microscopy. The fracture mode varied with load, the fracture mechanism being similar to glass and carbon reinforced composites. Microstructural analyses revealed that natural bamboo is eligibly a fibre composite in itself; its inclusion in a plastic matrix will help solve the problems of cracking due to desiccation and bioerosion caused by insect pests. Furthermore, the thickness and shape of the composite can be tailored during fabrication to meet specific requirements, thereby enabling a wide spectrum of applications.