979 resultados para Thermal treatment
Resumo:
The identification of Salmonella spp. in food samples by microbiological diagnosis is time consuming, with approximately five different stages, requiring about 120 hours until the final result. The utilization of the polymerase chain reaction technique (PCR) can reduce this time, but substances present in samples may affect the reaction. The present work aimed to compare DNA extraction by thermic treatment and by the use of cetyltrimethil ammonium bromide (CTAB), in products originated from poultry houses corresponding to raw material (meat meal) and experimentally contaminated drag swabs. Materials obtained from the extractions were submitted to PCR, utilizing a pair of initiator oligonucleotides for amplification of Sdf 1 gene fragments. Comparing the methods of extraction, it was observed that when CTAB was employed, SE was detected in 70% of meat meal and in 80% of drag swabs, while the thermic treatment method yielded positive results in 20% of meat meal and in 40% of drag swabs. SE was detected under both methods utilized for DNA extraction, but the use of CTAB detected a greater number of positive samples, compared with thermal treatment.
Resumo:
This study aimed to evaluate the hydrothermal effect on conservation of two jabuticaba fruits, Myrciaria jabuticaba Vell. Berg. Fruits were subjected to thermal treatment by 10 min at 5, 10, 15, 20 and 25 ºC and wrapped into expanded polystyrene trays, stored at 9 ºC and 85-90% RH, being evaluated every 5 d. Shelf life, weight loss, respiratory rate, soluble solids, titrable acidity, texture, C vitamin, pH, total and soluble pectin and polypheno loxidase activity were evaluated. Lower shelf life was observed for control treatment (31 d) and largest was found at 15, 20 and 25 ºC (45 d). A sligthly delay was observed in the breathing pick at 15, 20 and 25 ºC at 25 d and not in the 20 d as observed in the other treatments. Soluble solids increased with storage time for all of temperature treatment, but at 15, 20 and 25 ºC increase was smaller. Texture an C vitamin were higher in fruits stored at 25 ºC. Soluble pectin was smaller at the end of storage period, at temperatures of 20 and 25 ºC. Polyphenoloxidase activity decreased along 30 d regardless storage temperature. Treatments at 20 and 25 ºC were the most effective for mainteining posthaverst quality of the jabuticaba fruits.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Química - IQ
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Used as catalysts even in organic and inorganic molecules, as additives on catalysts, electrochromic films on smart windows the tungsten trioxide have been largely studied on the lasts decades, but there is just a few about it's luminescence. Using as precursors nitric acid and sodium tungstate the tungsten trioxide were been prepared thru wet process then treating on thermic and hydrothermal treatments. Where been evaluated the effects of methodology, nitric acid concentration, duration and temperature of treatments. The samples were characterized by X-ray diffraction (XRD), Raman scattering spectroscopy (RSS), Fourier transformed infrared spectroscopy, photoluminescence spectroscopy (PLS) and X-ray excited optical luminescence (XEOL). Hydrated phases of tungsten trioxide were obtained through hydrothermal treatments and the non-hydrated phases occur with thermic treatments. The acid concentration has the ability to determine the major phase formed as well the temperature determine the hydratation of the product. With lower temperatures dihydrate phase were preferable formed and with the rise of temperature, the water molecules were lost up to the fractionary hydratation and then the non-hydrated phase with higher temperatures depending on the atmosphere used on the thermal treatment. Doping the system with europium ions even substituting tungsten or in the interstices of the matrix were not been successful, as well the XEOL spectroscopy intensity were null and quite low for ultraviolet and visible excitation photoluminescence because of oxygen defect levels localized into the prohibited band.
Resumo:
This study aims to evaluate the corrosion resistance of Ti-30Ta alloy when subjected to different strain rates. Samples of the alloy Ti-30Ta were obtained from the melting of pure elements in the arc furnace in inert atmosphere (argon gas). Then, the samples were subjected to a thermal treatment and to cold worked to obtain bars. After forging, the samples were machined in accordance with ASTME9-09 standard for carried out compression tests. To microstructural characterization, samples were sectioned longitudinal and transversally and embedded in resin. After, the wet sanding and polishing were performed, followed by a chemical attack, in order to study the microstructure under an optical microscope. Microhardness was measured on the samples that were subjected to microstructural characterization by using microhardness tester. Phases were evaluated by x-rays diffraction. Corrosion tests were carried out to evaluate the influence of deformation on the corrosion resistance. Results show that microstructure was not influenced by deformation
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Used as catalysts even in organic and inorganic molecules, as additives on catalysts, electrochromic films on smart windows the tungsten trioxide have been largely studied on the lasts decades, but there is just a few about it's luminescence. Using as precursors nitric acid and sodium tungstate the tungsten trioxide were been prepared thru wet process then treating on thermic and hydrothermal treatments. Where been evaluated the effects of methodology, nitric acid concentration, duration and temperature of treatments. The samples were characterized by X-ray diffraction (XRD), Raman scattering spectroscopy (RSS), Fourier transformed infrared spectroscopy, photoluminescence spectroscopy (PLS) and X-ray excited optical luminescence (XEOL). Hydrated phases of tungsten trioxide were obtained through hydrothermal treatments and the non-hydrated phases occur with thermic treatments. The acid concentration has the ability to determine the major phase formed as well the temperature determine the hydratation of the product. With lower temperatures dihydrate phase were preferable formed and with the rise of temperature, the water molecules were lost up to the fractionary hydratation and then the non-hydrated phase with higher temperatures depending on the atmosphere used on the thermal treatment. Doping the system with europium ions even substituting tungsten or in the interstices of the matrix were not been successful, as well the XEOL spectroscopy intensity were null and quite low for ultraviolet and visible excitation photoluminescence because of oxygen defect levels localized into the prohibited band.
Resumo:
This study aims to evaluate the corrosion resistance of Ti-30Ta alloy when subjected to different strain rates. Samples of the alloy Ti-30Ta were obtained from the melting of pure elements in the arc furnace in inert atmosphere (argon gas). Then, the samples were subjected to a thermal treatment and to cold worked to obtain bars. After forging, the samples were machined in accordance with ASTME9-09 standard for carried out compression tests. To microstructural characterization, samples were sectioned longitudinal and transversally and embedded in resin. After, the wet sanding and polishing were performed, followed by a chemical attack, in order to study the microstructure under an optical microscope. Microhardness was measured on the samples that were subjected to microstructural characterization by using microhardness tester. Phases were evaluated by x-rays diffraction. Corrosion tests were carried out to evaluate the influence of deformation on the corrosion resistance. Results show that microstructure was not influenced by deformation
Resumo:
This work aims to evaluate the cytocompatibility of injectable and moldable restorative biomaterials based on granules of dense or porous biphasic calcium phosphates (BCPs) with human primary mesenchymal cells, in order to validate them as tools for stem cell-induced bone regeneration. Porous hydroxyapatite (HA) and HA/beta-tricalcium phosphate (beta-TCP) (60: 40) granules were obtained by the addition of wax spheres and pressing at 20 MPa, while dense materials were compacted by pressing at 100 MPa, followed by thermal treatment (1100 degrees C), grinding, and sieving. Extracts were prepared by 24-h incubation of granules on culture media, with subsequent exposition of human primary mesenchymal cells. Three different cell viability parameters were evaluated on the same samples. Scanning electron microscopy analysis of the granules revealed distinct dense and porous surfaces. After cell exposition to extracts, no significant differences on mitochondrial activity (2,3-bis(2-methoxy-4-nitro-5-sulfophenly)-5-[(phenylamino) carbonyl]-2H-tetrazolium hydroxide) or cell density (Crystal Violet Dye Elution) were observed among groups. However, Neutral Red assay revealed that dense materials extracts induced lower levels of total viable cells to porous HA/beta-TCP (P < 0.01). Calcium ion content was also significantly lower on the extracts of dense samples. Porogenic treatments on BCP composites do not affect cytocompatibility, as measured by three different parameters, indicating that these ceramics are well suited for further studies on future bioengineering applications.
Resumo:
Myofibril proteins have excellent filmogenic properties. The objective of this article was to study the effect of the thermal treatment, of the pH and of the plasticizer concentration (Cp) of the filmogenic solution (FS), using over some physical properties of edible films, using a surface and response methodology (SRM). Films were made of lyophilized myofibril proteins (LMP) extracted from bovine muscle, employing the technique of solubility obtained from diluted saline solutions. The films were elaborated from FS containing 1 g of LMP/100g of FS and from Cp of 50 g to 79 g of glycerin/100 g of LMP. The LMP was dispersed in water under moderate agitation, and the pH was kept at 2.5-3.5 with the use of acetic acid. The FS were submitted to thermal treatment at different temperatures for 45 minutes. Films were dried in ventilated oven at 37 degrees C/18hr, conditioned at 75% of relative humidity at 25 degrees C/48 hr before analysis of: mechanical properties by puncture test; apparent opacity by spectrophotometer; solubility by immersion in water; and water vapor permeability by the gravimetric method. In general, films showed good appearance, translucent, easily handled and touchable, except for the films formed with pH 2.5 and at a low temperature (35 degrees C), with a medium thickness of 0.400 +/- 0.005 mm. The pH of the FS significantly affected all the physical properties under study. The temperature of the thermal treatment of the FS greatly affected the force at the rupture, solubility and water vapor permeability. This treatment can promote intermolecular interactions through the formation of disulphide bonds; however a very intense treatment can reverse this effect by irreversible structural alterations in the proteins. The glycerol concentration affected considerably all the properties under study, with the exception of the apparent opacity. Plasticizer increases the mobility of macromolecules with consequences in all physical properties.
Resumo:
The potential use of alanine for the production of nanoparticles is presented here for the first time. Silver nanoparticles were synthesized using a simple green method, namely the thermal treatment of silver nitrate aqueous solutions with in-alanine. The latter compound was employed both as a reducing and a capping agent. Particles with average size equal to 7.5 nm, face-centered cubic crystalline structure, narrow size distribution, and spherical shape were obtained. Interaction between the silver ions present on the surface of the nanoparticles and the amine group of the DL-alanine molecule seems to be responsible for reduction of the silver ions and for the stability of the colloid. The bio-hybrid nanocomposite was used as an ESR dosimeter. The amount of silver nanoparticles in the nanocomposite was not sufficient to cause considerable loss of tissue equivalency. Moreover, the samples containing nanoparticles presented increased sensitivity and reduced energetic dependence as compared with pure DL-alanine, contributing to the construction of small-sized dosimeters. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
Several types of alumina were synthesized from sodium aluminate (NaAlO2) by precipitation with sulfuric acid (H2SO4) and subsequently calcination at 500 degrees C to obtain gamma-Al2O3. The precursor aluminate was derived from aluminum scrap. The various gamma-Al2O3 synthesized were characterized by Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), adsorption-desorption of N-2 (S-BET) and scanning electron microscopy (SEM). XRD revealed that distinct phases of Al2O3 were formed during thermal treatment. Moreover, it was observed that conditions of synthesis (pH, aging time and temperature) strongly affect the physicochemical properties of the alumina. A high-surface-area alumina (371 m(2) g(-1)) was synthesized under mild conditions, from inexpensive raw materials. These aluminas were tested for the adsorption of Cd(II), Zn(II) and Pb(II) from aqueous solution at toxic metal concentrations, and isotherms were determined. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
The Nuna supercontinent was probably assembled in the Paleoproterozoic, but its paleogeography and the timing for its demise are stills matter of debate. A paleomagnetic and geochronological study carried out on the Mesoproterozoic Nova Guarita dyke swarm (northern Mato Grosso State, SW Amazonian Craton) provides additional constraints on the duration of this supercontinent. Paleomagnetic AF and thermal treatment revealed south/southwest (northeast) magnetic directions with downward (upward) inclinations for 19 analyzed sites. These directions are carried by PSD magnetite with high unblocking temperatures as indicated by additional magnetic tests, including thermomagnetic curves, hysteresis loops and the progressive acquisition of isothermal remanence in selected samples. A positive contact test with the host granite in one of the studied dykes further attests to the primary origin of the characteristic magnetic component. A mean site direction was calculated at D-m = 220.5 degrees, I-m = 45.9 degrees (alpha(95) = 6.5 degrees, K = 27.7), which yielded a paleomagnetic pole located at 245.9 degrees E, 47.9 degrees S (A(95) = 7.0 degrees). Ar-40/Ar-39 dating carried out on biotites from four analyzed dykes yielded well-defined plateau ages with a mean of 1418.5 +/- 3.5 Ma. The Nova Guarita pole precludes a long-lived Nuna configuration in which Laurentia, Baltica, North China, and Amazonia formed a long and continuous block as previously proposed for the Paleoproterozoic. It is nevertheless fully compatible with a SAMBA (Amazonia-Baltica) link at Mesoproterozoic times. (C) 2011 Elsevier B.V. All rights reserved.