Resumo:
The cloacal complex of Crocodylus porosus is composed of three chambers (proctodaeum, urodaeum, and coprodaeum) separated by tight, muscular sphincters. The proctodaeum is proximal to the cloacal vent and houses the genitalia. The urodaeum is the largest chamber, is capable of storing large quantities of urine, and is lined with an epithelium with the capacity for transepithelial water and ion exchange. The coprodaeum, the most orad cloacal chamber, is a small, only marginally expandable chamber that has an epithelium composed almost entirely of mucus-secreting cells. The coprodaeum and lower intestine are reported to be the site(s) for urine modification in birds and bladderless lizards. A radiographic trace of urine storage in C. porosus kept for 2 months under hyperosmotic conditions showed no signs of retrograde movement of urine into the coprodaeum or rectum. Instead, urine was stored in the urodaeum of C. porosus. Examination of the mucosal surface of the urodaeum by SEM showed a plastic response to environmental salinity, with a possible increase in surface area in animals kept in hyperosmotic water compared with animals from fresh water. We propose the urodaeum as the primary site for postrenal modification of urine in C, porosus. (C) 2000 Wiley-Liss, Inc.
Resumo:
In the present work the meso- and macro-structural characteristics of the mesoporous adsorbent MCM-41 have been estimated with the help of various techniques. The structure is found to comprise four different length scales: that of the mesopores, the crystallites, the grains and of the particles. It was found that the surface area estimated by the use of small angle scattering techniques is higher, while that estimated by mercury porosimetry is much lower, than that obtained from gas adsorption methods. Based on the macropore characterization by mercury porosimetry, and the considerable macropore area determined, it is seen that the actual mesopore area of MCM-41 may be significantly lower than the BET area. TEM studies indicated that MCM-41 does not have an ideal mesopore structure; however, it may still be treated as a model mesoporous material for gas adsorption studies because of the large radius of curvature of the channels.
Resumo:
Coating anatase TiO2 onto three different particle supports, activated carbon (AC), gamma -alumina (Al2O3) and silica gel (SiO2), by chemical vapor deposition (CVD) was studied. The effect of the CVD synthesis conditions on the loading rate of anatase TiO2 was investigated. It was found that introducing water vapor during CVD or adsorbing water before CVD was crucial to obtain anatase TiO2 on the surface of the particle supports. The evaporation temperature of precursor, deposition temperature in the reactor, flow rate of carrier gas, and the length of coating time were also important parameters to obtain more uniform and repeatable TiO2 coating. High inflow precursor concentration, high CVD reactor temperature and long coating time tended to cause block problem. Coating TiO2 onto small particles by CVD involved both chemical vapor deposition and particle deposition. It was believed that the latter was the reason for the block problem. In addition, the mechanism of CVD process in this study included two parts, pyrolysis and hydrolysis, and one of them was dominant in the CVD process under different synthesis route. Among the three types of materials, silica gel, with higher surface hydroxyl groups and macropore surface area, was found to be the most efficient support in terms of both anatase TiO2 coating and photocatalytic reaction. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
Metal oxide pillared clay (PILC) possesses several interesting properties, such as large surface area, high pore volume and tunable pore size (from micropore to mesopore), high thermal stability, strong surface acidity and catalytic active substrates/metal oxide pillars. These unique characteristics make PILC an attractive material in catalytic reactions. It can be made either as catalyst support or directly used as catalyst. This paper is a continuous work from Kloprogge's review (J.T. Kloprogge, J. Porous Mater. 5, 5 1998) on the synthesis and properties of smectites and related PILCs and will focus on the diverse applications of clay pillared with different types of metal oxides in the heterogeneous catalysis area and adsorption area. The relation between the performance of the PILC and its physico-chemical features will be addressed.
Resumo:
This study quantified the release of monomers from polymerized specimens of four commercially available resin composites and one glass ionomer cement immersed in water:ethanol solutions. Individual standard curves were prepared from five monomers: (1) triethylene glycol dimethacrylate (TEGDMA), (2) 2-hydroxy-ethyl methacrylate (HEMA), (3) urethane dimethacrylate (UDMA), (4) bisphenol A glycidyl dimethacrylate (BISGMA), and (5) bisphenol A. The concentration of the monomers was determined at Days 1, 7, 30, and 90 with the use of electrospray ionization/mass spectrometry. Data were expressed in mean mumol per mm(2) surface area of specimen and analyzed with Scheffe's test (P < 0.05). The following monomers were found in water: monomers (1) and (2) from Delton sealant, monomer (5) from ScotchBond Multipurpose Adhesive and Delton sealant, monomer (3) from Definite and monomer (4) from Fuji II LC, ScotchBond Multipurpose Adhesive, Synergy and Definite. All these monomers increased in concentration over time, with the exception of monomer (1) from Delton sealant. Monomers (3) and (5) were found in extracts of materials despite their absence from the manufacturer's published composition. All monomers were released in significantly higher concentrations in water:ethanol solutions than in water. The greatest release of monomers occurred in the first day. The effect of the measured concentrations of monomers (1-5) on human genes, cells, or tissues needs to be considered with the use of a biological model. (C) 2002 Wiley Periodicals, Inc.
Resumo:
Confocal imaging of impermeant fluorescent dyes trapped in the tubular (t-) system of skeletal muscle fibres of rat and cane toad was used to examine changes in the morphology of the t-system upon mechanical skinning, the time course of dye loss from the sealed t-systern in mechanically skinned fibres and the influence of rapid application and removal of glycerol on the morphology of the sealed t-system. In contrast to intact fibres, which have a t-systern open to the outside, the sealed t-systern of toad mechanically skinned fibres consistently displayed local swellings (vesicles). The occurrence of vesicles in the sealed t-system of rat-skinned fibres was infrequent. Application and removal of 200-400 mM glycerol to the sealed t-system did not produce any obvious changes in its morphology. The dyes fluo-3, fura-2 and Oregon green 488 were lost from the sealed t-system of toad fibres at different rates suggesting that the mechanism of organic anion transport across the tubular wall was not by indiscriminate bulk transport. The rate of fluo-3 and fura-2 loss from the sealed t-system of rat fibres was greater in rat than in toad fibres and could be explained by differences in surface area: volume ratio of the t-system in the two fibre types. Based on the results presented here and on other results from this laboratory, an explanation is given for the formation of numerous vesicles in toad-skinned fibres and lack of vesicle formation in rat-skinned fibres. This explanation can also help with better understanding the mechanism responsible for vacuole formation in intact fibres. (C) 2002 Elsevier Science Ltd. All rights reserved.
Resumo:
The electrocatalytic activity of Pt and RuO(2) mixed electrodes of different compositions towards methanol oxidation was investigated. The catalysts were prepared by thermal decomposition of polymeric precursors and characterized by energy dispersive X-ray, scanning electronic microscopy, X-ray diffraction and cyclic voltammetry. This preparation method allowed obtaining uniform films with controlled stoichiometry and high surface area. Cyclic voltammetry experiments in the presence of methanol showed that mixed electrodes decreased the potential peak of methanol oxidation by approximately 100 mV (RHE) when compared to the electrode containing only Pt. In addition, voltammetric experiments indicated that the Pt(0.6)Ru(0.4)O(y) electrode led to higher oxidation current densities at lower potentials. Chronoamperometry experiments confirmed the contribution of RuO(2) to the catalytic activity as well as the better performance of the Pt(0.6)Ru(0.4)O(y) electrode composition. Formic acid and CO(2) were identified as being the reaction products formed in the electrolysis performed at 400 and 600 mV. The relative formation of CO(2) was favored in the electrolysis performed at 400 mV (RHE) with the Pt(0.6)Ru(0.4)O(y) electrode. The presence of RuO(2) in Pt-Ru-based electrodes is important for improving the catalytic activity towards methanol electrooxidation. Moreover, the thermal decomposition of polymeric precursors seems to be a promising route for the production of catalysts applicable to DMFC. (C) 2009 International Association for Hydrogen Energy. Published by Elsevier Ltd. All rights reserved.
Resumo:
The electrochemical performance of carbon fibers (CF) and boron-doped diamond electrodes grown on carbon fiber substrate (BDD/CF) was studied. CF substrates were obtained from polyacrylonitrile precursor heat treated at two different temperatures of 1000 and 2000 degrees C to produce the desirable CF carbon graphitization index. This graphitization process influenced the CF conductivity and its chemical surface, also analyzed from X-ray photoelectron spectroscopy measurements. These three-dimensional CF structures allowed a high incorporation of diamond films compared to other carbon substrates such as glass carbon or HOPG. The electrochemical responses, from these four classes of electrodes, were evaluated focusing their application as electrical double-layer capacitors using cyclic voltammetry and impedance measurements. Cyclic voltammetry results revealed that the electrode formed from BDD grown on CF-2000 presented a typical capacitor behavior with the best rectangular shape, compared to those electrodes of CF or BDD/CF-1000. Furthermore, the BDD/CF-2000 electrode presented the lowest impedance, associated to its significant capacitance value of 1940 mu F/cm(2) taking into account the BDD films. This behavior was attributed to the strong dependence between diamond coating texture and the CF graphitization temperature. The largest surface area of BDD/CF-2000 was promoted by its singular film growth mechanism associated to the substrate chemical surface. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
This paper reports for the first time superior electric double layer capacitive properties of ordered mesoporous carbon (OMCs) with varying ordered pore symmetries and mesopore structure. Compared to commercially used activated carbon electrode, Maxsorb, these OMC carbons have superior capacitive behavior, power output and high-frequency performance in EDLCs due to the unique structure of their mesopore network, which is more favorable for fast ionic transport than the pore networks in disordered microporous carbons. As evidenced by N-2 sorption, cyclic voltammetry and frequency response measurements, OMC carbons with large mesopores, and especially with 2-D pore symmetry, show superior capacitive behaviors (exhibiting a high capacitance of over 180 F/g even at very high sweep rate of 50 mV/s, as compared to much reduced capacitance of 73 F/g for Maxsorb at the same sweep rate). OMC carbons can provide much higher power density while still maintaining good energy density. OMC carbons demonstrate excellent high-frequency performances due to its higher surface area in pores larger than 3 nm. Such ordered mesoporous carbons (OMCs) offer a great potential in EDLC capacitors, particularly for applications where high power output and good high-frequency capacitive performances are required. (C) 2005 Elsevier Ltd. All rights reserved.
Resumo:
High nutritional levels of iodine may induce a higher prevalence of autoimmune thyroiditis,hypothyroidism, goiter, as well as hyperthyroidism, mostly in the elderly. This study assessed thyroid volume and ultrasonographic abnormalities as well as urinary iodine excretion (UIE) in 964 schoolchildren living in an iodine-sufficient area in southern Brazil. Thyroid volume correlated with age and body surface area in boys and girls. In 76.8% of the children, UIE was above 300 mu g/l, with higher levels among boys compared to girls (484.2 mu g/l vs 435.3 mu g/l, p <0.001). Thyroid abnormalities detected by ultrasonography included hemiagenesis (0.5%), nodules (0.2%), cysts (0.7%), and hypoechogenicity (11.7%). Goiter was present in 1.9% of the children. Hypoechogenicity, a relevant marker of autoimmune thyroiditis, was the most common abnormality found in our study, and this may be linked to excessive iodine intake.
Resumo:
Objectives: The high incidence of respiratory disorders is one of the main problems in perinatal medical care. With the increased use of intubation, the incidence of laryngeal injury causing stenosis has also increased. The principal constriction point in the infant`s larynx is the midcricoid area. We sought to provide detailed morphometric data on the anatomy of the cricoid cartilage and its relationship with growth and body characteristics of fetuses at 5 to 9 months of gestational age. Methods: Nineteen larynges obtained from 17 stillborn infants and 2 newborn infants ranging in gestational age from 5 to 9 months were studied. Measurements of the cricoid cartilage were made with a millimeter-graded caliper. Results: Weight was the variable most correlated with cricoid measurements. The cricoid lumen configuration showed an almost elliptic shape and did not change with gestational age. The mean inner subglottic cricoid area was 19.27 +/- 9.62 mm(2) and was related to weight and body surface area. Cricoid growth was more pronounced at the outer portion of the cartilage. Conclusions: The cricoid lumen configuration was elliptic, and its mean area was smaller than that of available endotracheal tubes. This lumen area was most influenced by weight and height.
Resumo:
We describe the mechanism of ribonuclease inhibition by ribonuclease inhibitor, a protein built of leucine-rich repeats, based on the crystal structure of the complex between the inhibitor and ribonuclease A. The structure was determined by molecular replacement and refined to an R(cryst) of 19.4% at 2.5 Angstrom resolution. Ribonuclease A binds to the concave region of the inhibitor protein comprising its parallel beta-sheet and loops. The inhibitor covers the ribonuclease active site and directly contacts several active-site residues. The inhibitor only partially mimics the RNase-nucleotide interaction and does not utilize the pi phosphate-binding pocket of ribonuclease A, where a sulfate ion remains bound. The 2550 Angstrom(2) of accessible surface area buried upon complex formation may be one of the major contributors to the extremely tight association (K-i = 5.9 x 10(-14) M). The interaction is predominantly electrostatic; there is a high chemical complementarity with 18 putative hydrogen bonds and salt links, but the shape complementarity is lower than in most other protein-protein complexes. Ribonuclease inhibitor changes its conformation upon complex formation; the conformational change is unusual in that it is a plastic reorganization of the entire structure without any obvious hinge and reflects the conformational flexibility of the structure of the inhibitor. There is a good agreement between the crystal structure and other biochemical studies of the interaction. The structure suggests that the conformational flexibility of RI and an unusually large contact area that compensates for a lower degree of complementarity may be the principal reasons for the ability of RI to potently inhibit diverse ribonucleases. However, the inhibition is lost with amphibian ribonucleases that have substituted most residues corresponding to inhibitor-binding residues in RNase A, and with bovine seminal ribonuclease that prevents inhibitor binding by forming a dimer. (C) 1996 Academic Press Limited
Resumo:
MCM-41 samples of various pore dimensions are synthesized. Plotting of nitrogen adsorption data at 77 K versus the statistical film thickness (comparison plot) reveals three distinct stages, with a characteristic of two points of inflection. The steep intermediate stage caused by capillary condensation occurred in the highly uniform mesopores. From the slopes of the sections before and after the condensation, the surface area of the mesopores is calculated. The linear portion of the last section is extrapolated to the adsorption axis of the comparison plot, and this intercept is used to obtain the volume of the mesopores. From the surface area and pore volume, average mesopore diameter is calculated, and the value thus obtained is in good agreement with the pore dimension obtained from powder X-ray diffraction measurements. The principle of the calculation as well as problems associated are discussed in detail.
Resumo:
The intercalated discs of working myocardium and Purkinje fibers of the monkey heart were examined by scanning and transmission electron microscopy. The NaOH/ultrasonication technique resulted in the digestion of connective tissue and a separation of the intercellular junctions of intercalated discs, such that these could be visualized three-dimensionally. The intercalated discs of ventricular myocytes, atrial myocytes and Purkinje fibers vary considerably in number and configuration, as do the intercalated discs of the three different layers of the ventricular myocardium. Myocytes in the subepicardial, middle and subendocardial layers of the ventricle have 1-3, 4-5 and 5-6 intercalated discs at the end of these cells, respectively, Those in the endocardial layer are characterized by the presence of small laterally-placed intercalated discs. Atrial myocytes and Purkinje fibers usually only have 1-2 intercalated discs, Individual intercalated discs in ventricular myocytes have complicated stairs with 10-30 steps and corresponding risers, while those of atrial myocytes and Purkinje fibers have simple stairs with 1-3 steps and risers, Steps equivalent to the plicate segments are characterized by densely-packed microplicae and finger-like microprojections which greatly increase surface area in vertricular myocytes, Microprojections in atrial myocytes and Purkinje fibers are sparse by comparison, Risers equivalent to the interplicate segments containing large gap junctional areas are most numerous in left ventricular myocytes, followed by right ventricular myocytes, Purkinje fibers and atrial myocytes in decreasing order. The geometric arrangement of the various types of myocytes may be related with impulse propagation. Large intercalated discs of cell trunks and series branches may participate in longitudinal propagation, while small laterally-placed ones may be the site of transverse propagation.
Resumo:
The data of nitrogen adsorption on pillared clays (PILC) are converted to comparison plots (t-plots) to derive their pore size distribution (PSD). As in the MP method, the surface area of a group of pores having similar pore sizes is calculated from the slopes of tangent lines at two succeeding points on a comparison plot. By the modified MP method in this work, the tangent line is extrapolated to the adsorption axis on the t-plot, and the difference between intercepts is used to obtain the volume of the group of pores. From the information of surface area and pore volume, the average width of the pore group can be calculated and hence the PSDs of PILCs are obtained by carrying out such calculation procedures from high to low t. With this method, PSDs of several pillared clays are calculated over a wide pore size range, from micropores to mesopores. It is found that the modified MP method could result in the underestimation of the width of ultramicropores due to the enhancement in adsorption energy in these pores. Nevertheless, the method can be very useful in calculating the surface area and pore volume, as well as a mean width of these pores. For super-micropores and mesopores, pore size can also be underestimated, due to deviation of the pore shape from a slit. The principles of the improved MP method, as well as problems associated with it are thoroughly discussed in this paper. In general, this modified method provides practically meaningful results which are consistent with the pore dimension obtained from powder X-ray diffraction measurements, but involves no complicated theoretical treatment or assumptions.