888 resultados para Ordered mesoporous silicas


Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel periodic mesoporous organosilica (PMO) material was synthesized through one-step co-condensation of 1,2-bis(triethoxysilyl)ethane (BTESE) and benzoic acid-functionalized organosilane (BA-Si) using cetyltrimethylammonium bromide (CTAB) as a structure-directing agent under basic conditions. The materials were fully characterized by FTIR, XRD, N-2 adsorption-desorption isotherms and FESEM. FTIR spectra proved that BA-Si was successfully incorporated into the PMO materials (PMOs) via benzyl group as a linker. XRD and N-2 adsorption-desorption isotherms revealed the characteristic mesoporous structure with highly uniform pore size distributions. FESEM confirmed that the morphology of the PMOs was significantly dependent cri the molar ratio of two organosilica precursors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The crystal structure of a ternary Tm(DBM)(3)phen complex (DBM - dibenzoylmethane; phen = 1. 10-phenanthroline) and the synthesis of hybrid mesoporous material in which the complex covalently bonded to mesoporous MCM-41 are reported. Crystal data: Tm(DBM)(3)phen C59H47N2O7Tm, monoclinic P21/c, a = 19.3216(12) A, b = 10.6691(7) A, c = 23.0165(15)A, alpha = 90, beta = 91.6330(10), gamma = 90, V = 4742.8(5) A(3), Z = 4. The properties of the Tm(DBM)(3)phen complex and the corresponding hybrid mesoporous material [Tm(DBM)(3)phen-MCM-41] have been studied. The results reveal that the Tm(DBM)(3)phen complex is successfully covalently bonded to MCM-41.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, it was found that glucose oxidase (GOD) has been stably immobilized on glassy carbon electrode modified with mesoporous carbon FDU-15 (MC-FDU-15) and Nafion by simple technique. The sorption behavior of GOD immobilized on MC-FDU-15 matrix was characterized by transmission electron microscopy (TEM), ultraviolet-visible (UV-vis), FTIR, respectively, which demonstrated that MC-FDU-15 could facilitate the electron exchange between the active center of GOD and electrode. The direct electrochemistry and electrocatalysis behavior of GOD on the modified electrode were characterized by cyclic voltammogram (CV) which indicated that GOD immobilized on Nafion and MC-FDU-15 matrices display direct, reversible and surface-controlled redox reaction with an enhanced electron transfer rate constant of 4.095 s(-1) in 0.1 M phosphate buffer solution (PBS) (pH 7.12).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lanthanum phosphate (LaPO4) nanostructures with different morphologies were prepared by a facile solution-precipitation process. The effect of different reaction conditions on the morphology of nanostructures was studied. When the molar ratio of La3+:H3PO4 was around 1 : 2, 1 : 20, 1 : 100, and 1 : 200, four different morphologies, such as near-spherical, snowflake-like, star-shaped, lens-like nanostructures and short nanorods, were obtained, respectively. Meanwhile, similar shapes developed when the molar ratio of H3PO4 to ionic surfactants, such as SDS and CTAB, was varied. In addition, Eu3+ doped and Ce3+/Tb3+ co-doped LaPO4 nanostructures showed morphology evolution similar to undoped LaPO4 nanostructures. The optical properties of these doped LaPO4 were also characterized.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we have reported a facile method for the synthesis of ordered magnetic core-manganese oxide shell nanostructures. The process included two steps. First, manganese ferrite nanoparticles were obtained through a solvothermal method. Then, the manganese ferrite nanoparticles were mixed directly with KMnO4 solution without any additional modified procedures of the magnetic cores. It has been found that Mn element in the core can react with KMnO4 to form manganese oxide which acts as a seed for the in-situ growth of manganese oxide shells. This is significant for the controllable fabrication of symmetrical ordered manganese oxide shell structures. The shell thickness can be easily controlled through the reaction time. Transmission electron microscopy, scanning electron microscopy, X-ray photoelectron spectroscopy, X-ray powder diffraction and energy-dispersive X-ray spectroscopy have been employed to characterize the products at different reaction time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this contribution, we report a facile, gram-scale, low-cost route to prepare monodisperse superparamagnetic single-crystal magnetite NPs with mesoporous structure (MSSMN) via a very simple solvothermal method. The formation mechanism of MSSMN is also discussed and we think that Ostwald ripening probably plays an important role in this synthesis process. It is also interestingly found that the size and morphology of mesoporous Fe3O4 NPs can be easily controlled by changing the amount of NaOH and 1,2-ethylenediamine (ETH). Most importantly, the MSSMN can be used as an effective drug delivery carrier. A typical anticancer drug, doxorubicin (Dox), is used for drug loading, and the release behaviors of Dox in two different pH solutions are studied. The results indicate that the MSSMN has a high drug loading capacity and favorable release property for Dox; thus, it is very promising for the application in drug delivery.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ordered-sphere CePO4 hierarchical architectures have been successfully synthesized by a simple hydrothermal method through the controlled growth of the CePO4 nanorods and self-assemble hierarchical structure under various reaction conditions. The evolution of the morphology of the samples has been investigated in detail. It was found that the coexistence of citric acid and cetaltrimethylammonium bromide in the reaction system plays an important role in the formation of the spherical CePO4 hierarchical architectures. A possible mechanism of the formation and growth of the hierarchical structure was suggested according to the experimental results and analysis. The effects of the reaction time as well as the variation of the morphologies on the luminescent properties of the products were also studied.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simple method to prepare titania nanomaterials of core-shell structure, hollow nanospheres and mesoporous nanoparticles has been developed. The core-shell nanostructures with NH4Cl as core and TiO2 center dot xH(2)O-NH4Cl as shell were prepared in nonaqueous system by the deposition on the surface of the aggregated NH4Cl crystals, which could be transformed into mesoporous anatase nanoparticles or hollow nanospheres by calcination at 500A degrees C or extraction with methanol, respectively. The hierarchical mesoporous nanostructures benefited the photocatalytic activities of the resultant titania nanomaterials, demonstrated by the UV light photodegradation of Methyl Orange.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mesoporous YF3 nanoflowers were successfully prepared via solvent extraction route. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) observations indicated that these nanoflowers with uneven porous architectures had a spherical shape and were consisted of many YF3 nanosheets with a thickness of about 15 not. Energy-dispersive spectroscopy (EDS) analysis was used to check the chemical composition and purity of the products. YF3 nanoflowers had bimodal mesoporous distribution and Brunauer-Emmett-Teller (BET) surface area of 116 m(2)/g.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Well-dispersed palladium nanoparticles in mesoporous SBA- 15 SiO2 were prepared in a facile one-step approach during sol-gel route under reductive atmosphere. X-ray diffraction (XRD) results indicate that as-synthesized nanocomposites basically remain ordered two-dimensional hexagonal mesostructure while transmission electron microscopy (TEM) study exhibits a well dispersion of palladium nanoparticles within the mesoporous SBA-15 channels. The size of Pd nanoparticles is approximately in the range of 5-10nm. However, the resulting nanocomposites exhibit a highly catalytic activity and reused ability at least after five recycles without ligand in air for both the Suzuki and Heck coupling reactions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simple and efficient method has been established for the selective synthesis of mesoporous and nanorod CeVO4 with different precursors by sonochemical method. CeVO4 nanorod can be simply synthesized by ultrasound irradiation of Ce(NO3)(3) and NH4VO3 in aqueous solution without any surfactant or template. While mesoporous CeVO4 with high specific surface area can be prepared with Ce(NO3)(3), V2O5 and NaOH in the same way. Mesoporous CeVO4 has a specific surface area of 122 m(2) g(-1) and an average pore size of 5.2 nm; CeVO4 nanorods have a diameter of about 5 nm, and a length of 100-150 nm. The ultrasound irradiation and ammonia in the reactive solution are two key factors in the formation of such rod-like products. X-ray diffraction (XRD), transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS), thermogravimetric (TG) and differential thermal analyses (DTA), UV/vis absorption spectroscopy and Brunauer-Emmett-Teller (BET) were applied for characterization of the as-prepared products.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Non-isothermal crystallisation kinetics of a polyamide 6/mesoporous silica nanocomposite (PA6-MS) has been investigated by differential scanning calorimetry (DSC) at different cooling rates. Mandelkern, Jeziorny-Ziabicki and Ozawa methods were applied to describe this crystallisation process. The analyses show that the mesoporous silica particles act as nucleating agents in the composite and that the Avrami exponent n varies from 3.0 to 4.6. The addition of mesoporous silica influenced the mechanism of nucleation and the growth of polyamide 6 (PA6) crystallites.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Our previous investigation showed that the ordered hexagonal island pattern in the phase-separating polymeric blend films of polystyrene and poly(2-vinylpyridine) (PS/P2VP) formed due to the convection effect by proper control of PS molecular weight, solvent evaporation rate, and the weight ratio of PS to P2VP. In this paper, we further illustrate that, by adding a proper amount of the surfactant Triton X-100 to the PS/P2VP toluene solution, the ordered hexagonal island pattern can be transformed to the ordered honeycomb pattern. The effects of the amount of Triton X-100 on the surface morphology evolution and the pattern transformation are discussed in terms of the collapse of Triton X-100, phase separation between Triton X-100/P2VP and PS, the interfacial interaction between Triton X-100/P2VP and the mica substrate, and the Benard-Marangoni convection.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, the authors have systematically studied the microphase separation and crystallization during spin coating of an ABC triblock copolymer, polystyrene-b-poly(2-vinylpyridine)-b-poly(ethylene oxide) (PS-b-P2VP-b-PEO). The microphase separation of PS-b-P2VP-b-PEO and the crystallization of PEO blocks can be modulated by the types of the solvent and the substrate, the spinning speed, and the copolymer concentration. Ordered microphase-separated pattern, where PEO and P2VP blocks adsorbed to the substrate and PS blocks protrusions formed hexagonal dots above the P2VP domains, can only be obtained when PS-b-P2VP-b-PEO is dissolved in N,N-dimethylformamide and the films are spin coated onto the polar substrate, silicon wafers or mica. The mechanism of the formation of regular pattern by microphase separation is found to be mainly related to the inducement of the substrate (middle block P2VP wetting the polar substrate), the quick vanishment of the solvent during the early stage of the spin coating, and the slow evaporation of the remaining solvent during the subsequent stage. On the other hand, the probability of the crystallization of PEO blocks during spin coating decreases with the reduced film thickness. When the film thickness reaches a certain value (3.0 nm), the extensive crystallization of PEO is effectively prohibited and ordered microphase-separated pattern over large areas can be routinely prepared.